• 제목/요약/키워드: Ta powder

검색결과 126건 처리시간 0.03초

Chemical Design of Highly Water-Soluble Ti, Nb and Ta Precursors for Multi-Component Oxides

  • Masato Kakihana;Judith Szanics;Masaru Tada
    • Bulletin of the Korean Chemical Society
    • /
    • 제20권8호
    • /
    • pp.893-896
    • /
    • 1999
  • Novel citric acid based Ti, Nb and Ta precursors that are highly stable in the presence of water were developed. No alkoxides of Ti, Nb and Ta were utilized in the preparation, instead much less moisture-sensitive metallic Ti, NbCl5 and TaCl5 were chosen as starting chemicals for Ti, Nb and Ta, respectively. The feasibility of these chemicals as precursors is demonstrated in the powder synthesis of BaTi4O9, Y3NbO7 and LiTaO3. The water-resistant Ti precursor was employed as a new source of water-soluble Ti in the amorphous citrate method, and phase pure BaTi4O9 in powdered form was successfully synthesized at 800 ?. The Pechini-type polymerizable complex method using the water-resistant Nb and Ta precursors was applied to the synthesis of Y3NbO7 and LiTaO3, and both the powder materials in their pure form were successfully synthesized at reduced tempera-tures, viz. 500-700 ?. The remarkable retardation of hydrolysis of these water-resistant precursors is explained in terms of the partial charge model theory.

Preparati on and Characterization of $LnTaO_4$ (Ln = La, Nd, Sm, Dy, Er and Tm)

  • Fujita, Atsushi;Matsushita, Hiroaki;Katsui, Akinori
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1116-1117
    • /
    • 2006
  • Lanthanide tantalite $LnTaO_4$ (Ln= La, Nd, Sm, Dy, Er and Tm) was synthesized by a solid state reaction between mixed powders of $Ln_2O_3$ and $Ta_2O_5$. The single-phase $LnTaO_4$ was prepared by sintering at temperatures of 1423-1673 K in air. The SEM observation showed that the particles were provided with the growth steps and the depeloped facets. The photocatalytic activity for water splitting of $LnTaO_4$ prepared was measured under UV light irradiation. The activity obtained was higher than that previously reported. These results suggested the crystallinity of $LnTaO_4$ photocatalysts correlates closely with the efficiency of water splitting.

  • PDF

초미립 WC-l0wt%Co 초경 분말의 소결시 입자 성장 억제제 첨가 효과 연구 (Effect of Grain Growth Inhibitor on Sintering of Nanophase WC-10wt%Co)

  • 김병기
    • 한국분말재료학회지
    • /
    • 제1권2호
    • /
    • pp.208-216
    • /
    • 1994
  • A radically new approach to the in situ synthesis of the consituent phases of a composite structure has enabled the production of a new WC/Co materials with an ultrafine microstructure. The process for synthesizing nanophase WC/Co powders consists of spray drying from solution to form a homogeneous precursor powder, and thermochemical conversion of the precursor powder to the nanophase WC/Co powder. Near theoretical density of pure nanophase WC-10 wt%Co has been obtained in only 30 sec at 140$0^{\circ}C$. But WC particles were grown up very rapidly with longer sintering time to get full density. To overcome coarsening of WC particle during sintering, VC, TaC and VC/TaC were used as the grain growth inhibitor with different amount respectively. VC/TaC doped WC-10 wt%Co was shown superior hardness and TRS and microstructure was maintained ultrafine scale (average WC size is less than 0.1 ${\mu}{\textrm}{m}$).

  • PDF

산소결핍 탄탈륨 산화물을 활용한 탄탈륨 산질화물 및 질화물 합성 (Synthesis of Tantalum Oxy-nitride and Nitride using Oxygen Dificiency Tantalum Oxides)

  • 박종철;피재환;김유진;최의석
    • 한국분말재료학회지
    • /
    • 제15권6호
    • /
    • pp.489-495
    • /
    • 2008
  • Colored tantalum oxy-nitride (TaON) and tantalum nitride ($Ta_{3}N_{5}$) were synthesized by ammonolysis. Oxygen deficient tantalum oxides ($TaO_{1.7}$) were produced by a titration process, using a tantalum chloride ($TaCl_5$) precursor. The stirring speed and the amount of $NH_{4}OH$ were important factors for controling the crystallinity of tantalum oxides. The high crystallinity of tantalum oxides improved the degree of nitridation which was related to the color value. Synthesized powders were characterized by XRD, SEM, TEM and Colorimeter.

Na환원법에 의한 희석제량에 따른 탄탈 분말 제조와 특성 (Characteristics and Production of Tantalum Powder on the amount of Diluent By Na Reduction Method)

  • 윤재식;박형호;배인성;김병일;정성만
    • 한국재료학회지
    • /
    • 제12권9호
    • /
    • pp.706-711
    • /
    • 2002
  • High-pure tantalum powder was fabricated through Na reduction process and has been produced by using $K_2$TaF$_{7}$, and KCI, KF for raw material and diluent, respectively. A raw material and diluent were charged at the hestalloy bomb by the weight rate of 1:2, 1:1, 1:0.5 and 1:0.25 each other, investigated properties of morphology, chemical composition and yield and particle size after reduced. Ta metal has been achieved by reduction of $K_2$$TaF_{7}$ 500g with 1% sodium in excess of stoichiometric amount in the charge at a reduction temperature of $850^{\circ}C$ for 3hours. According to amount of the diluent, a formation of the powder doesn't have an effect. The diluent prevented the temperature rising caused from the heat of reaction and it maintained the speed of reducing reaction. But in the mixture ratio of raw material and diluent in the 1 : 2 and 1 : 0.25, an oxide and partially not reacted K were detected. As the amount of diluent increased, the size of tantalum powder decreased. According as raw material and the mixture ratio of diluent change from 1:0.25 to 1:2, the size is decreased from 5$\mu\textrm{m}$ to 1$\mu\textrm{m}$, and a particle size distribution which is below 325 mesh in fined powder increases from 71% to 83%. In the case of average size of Tantalum powder which is the mixture ratio (1:0.5), we would get the Ta powder with grain size about 3$\mu\textrm{m}$, which come close to the average size (2~4$\mu\textrm{m}$) of tantalum powder which is used commonly in the present is Ta powder about 3$\mu\textrm{m}$.