Kwon, Seung-Jun;Choi, Jeong-Il;Nguyen, Huy Hoang;Lee, Bang Yeon
Computers and Concrete
/
v.21
no.3
/
pp.231-237
/
2018
A strain-hardening highly ductile composite based on an alkali-activated slag binder and synthetic fibers is a promising construction material due to its excellent tensile behavior and owing to the ecofriendly characteristics of its binder. This study investigated the effect of different types of synthetic fibers and water-to-binder ratios on the compressive strength and tensile behavior of slag-based cementless composites. Alkali-activated slag was used as a binder and water-to-binder ratios of 0.35, 0.45, and 0.55 were considered. Three types of fibers, polypropylene fiber, polyethylene (PE) fiber, and polyparaphenylene-benzobisethiazole (PBO) fiber, were used as reinforcing fibers, and compression and uniaxial tension tests were performed. The test results showed that the PE fiber series composites exhibited superior tensile behavior in terms of the tensile strain capacity and crack patterns while PBO fiber series composites had high tensile strength levels and tight crack widths and spacing distances.
Kim, Daesuk;Lee, Sangwook;Park, Dongho;Yu, TaeU;Moon, ByungMoon;Min, DongJoon
한국신재생에너지학회:학술대회논문집
/
2010.11a
/
pp.43.2-43.2
/
2010
In this study, metallurgical grade (MG) silicon with 99% purity produced by arc furnace process was systematically investigated for slag refining. The most problematic impurities to remove from MG silicon are boron (B) and phosphorus (P). To remove B and P from MG-silicon, we used synthetic slag in the molten state. MG-silicon with synthetic slag of CaO, $SiO_2$, and $CaF_2$ was melted using by high-frequency induction furnace with electrical output of 50kW. Specimens prepared by various refining process conditions(holding time, mixture ratio) were inspected by combined analysis of ICP-MS and XRF. With this approach, B has been reduced to <5ppm, P to <1ppm and other impurities to 0.1~0.2% except for Calcium. Calcium has been increased from 17ppm to 1500ppm. Problem of calcium contamination will be resolved by additional refining processes.
The effects of mineral admixtures on the bonding properties of cement mortar to polyolefin based synthetic fiber were evaluated. The mineral admixtures consisted of 0%, 5%, 10%, and 15% fly ash, blast furnace slag, and metakaolin in cement. Bond interactions between the cement mortar and the polyolefin based synthetic fiber were determined by Dog-bone bond tests. Bond tests of the polyolefin based synthetic fiber showed an increase in pullout load with the strength of the cement mortar. Also, the interface toughness of polyolefin based synthetic fiber in cement mortar increased as the fly ash, blast furnace slag, and metakaolin contents increased. The microstructure of polyolefin based synthetic fiber surface was examined after the pullout test to analyze the frictional resistant force according to the replacement ratio of fly ash, blast furnace slag, and metakaolin during the pullout process of polyolefin based synthetic fiber in cement mortar. The scratched of polyolefin based synthetic fibers increased with the replacement ratio of fly ash, blast furnace slag, and metakaolin. Also, the interface toughness was enhanced by adhesion forces induced by the fly ash, blast furnace slag, and metakaolin.
Journal of The Korean Society of Agricultural Engineers
/
v.54
no.5
/
pp.25-34
/
2012
It has been well known that concrete structures exposed to acid and sulfate environments such as sewer etc. show significant decrease in their durability due to chemical attack. Such deleterious acid and sulfate attacks lead to expansion and cracking in concrete, and thus, eventually result in damage to cement mortar by forming expansive hydration products due to the reaction between cement hydration products and acid and sulfate ions. In this study, the effect of fly ash and blast furnace slag on the bond performances of structural synthetic fiber in latex modified cement mortar under sulfate environments. Fly ash and blast furnace slag contents ranging from 0 % to 20 % are used in the mix proportions. The latex modified cement mortar specimens were immersed in fresh water, 8 % sodium sulfate ($Na_2SO_4$) solutions for 28 and 50 days, respectively. Pullout tests are conducted to measure the bond performance of structural synthetic fiber from latex modified cement mortar after sulfate environments exposure. Test results are found that the incorporation of fly ash and blast furnace slag can effectively enhance the PVA fiber-latex modified cement mortar interfacial bond properties (bond behavior, bond strength and interface toughness) after sulfate environments exposure. The microstructural observation confirms the findings on the interface bond mechanism drawn from the fiber pullout test results under sulfate environments.
The study objective was to evaluate the enhanced removal of high concentrations of phosphorus from synthetic wastewater (solely phosphorus-containing) and real wastewater (pig manure) by using carbon nanotube (CNT)-coated steel slag. Generally, phosphorus removal by steel slag is attributed to Ca2+ eluted from the slag. However, in this study, CNT was used to control the excess release of Ca2+ from steel slag and increase the phosphorus removal. The phosphorus removal rate by the uncoated steel slag was lower than that of the CNT-coated steel slag, even though the Ca2+ concentrations were higher in the solution containing the uncoated steel slag. Therefore, the phosphorus removal could be attributed to both precipitation with Ca2+ eluted from steel slag in aqueous solution and adsorption onto the surface of the CNT-coated steel slag. Furthermore, the protons released from the CNT surface by exchanging with divalent cations acted to reduce the pH increase of the solution, which is attributed to the OH- eluted from the steel slag. The adsorption isotherm and kinetics of the CNT-coated steel slags followed the Freundlich isotherm and pseudo-second-order model, respectively. The maximum adsorption capacity of the uncoated and CNT-coated steel slags was 6.127 and 9.268 mg P g-1 slag, respectively. In addition, phosphorus from pig manure was more effectively removed by the CNT-coated steel slag than by the uncoated slag. Over 24 hours, the PO4-P removal in pig manure was 12.3% higher by the CNT-coated slag. This CNT-coated steel slag can be used to remove both phosphorus and metals and has potential applications in high phosphorus-containing wastewater like pig manure.
International Journal of Advanced Culture Technology
/
v.10
no.1
/
pp.284-293
/
2022
After extracting the calcium component from the KR slag and the converter slag using ammonium chloride solution, the extract was reacted with carbon dioxide to synthesize precipitated calcium carbonate (PCC). In order to understand the effect of ultrasonic waves on calcium extraction from slags and calcium carbonate synthesis, the efficiency of calcium carbonate synthesis according to the with or without of ultrasonic waves was analyzed. The synthetic efficiency of PCC was investigated according to various experimental conditions, and the synthesized calcium carbonate was analyzed using XRD and SEM. In both slags, the amount of PCC decreased as the reaction temperature increased. The pH at the end of the experiment capable of synthesizing the maximum PCC in the carbonation reaction was 7 (irradiated with ultrasound) and 8 (irradiated without ultrasound), respectively. Because the pH of the extraction filtrate is different when irradiated with or without ultrasound, the pH was adjusted to 9 by injecting an additive (10 M NaOH) before the carbonation experiment, and then the experiment was performed. When calcium was extracted from KR slag, the crystal phase appeared as calcite regardless of the pH at the end of the experiment. However, when calcium was extracted from the converter slag and the pH was set to 7 at the end of the experiment, the crystal phase of PCC appeared as a mixture of calcite and vaterite.
Journal of the Korean Society of Groundwater Environment
/
v.6
no.4
/
pp.206-212
/
1999
In order to evaluate the applicability of steel mill slag as a AMD (Acid Mine Drainage) neutralizer and to compare capacity of slag with that of limestone lab scale experiments were conducted. The fixed treatment experiments of AMD with slag and limestone separately for 24 hours under the stagnant condition showed that slag has higher capacity of pH increase and removal of Fe. Al and other trace elements. During the 10 days continuous step experiment the pH has been maintained and any decrease in the removal capacity of Fe and Al has not bun observed. In the trace element removal experiment slag showed higher capacity for removal of Ni, Co. Cu and Zn than limestone. The removal of trace element was more effective in AMD than in distilled water that the pH was adjusted to the same level of AMD (synthetic acid solution). It means that Fe and Al in AMD adsorbed trace elements during or after precipitation as oxide forms. In the size effect experiment, the slag of the smaller size with larger specific surface area exhibited higher capacity of pH increase and removal efficiencies of Fe. Al and other trace elements.
For crystalline slags, of which the viscosity rapidly increases at $T_{cv}$ due to the formation of crystalline phases, the Tcv is affected by measurement conditions. In this study, we investigated the effect of cooling rate, and alumina dissolution on the determination of $T_{cv}$. Using synthetic slag samples based on the composition of Alaska Usibelli slag, $T_{cv}$ were determined under a constant cooling rate of $2^{\circ}C$/min, and under rapid cooling with holding time to allow the slag to reach thermal and rheological equilibrium. The effect of alumina dissolution was investigated using platinum lined crucibles. The constant cooling resulted in lower $T_{cv}$ by $33^{\circ}C$ as compared to the equilibrium measurements. Under $2^{\circ}C$/min cooling, the blocking alumina dissolution resulted in lower $T_{cv}$ by $23^{\circ}C$. When the $T_{cv}$ was measured under $2^{\circ}C$/min cooling using an alumina crucible, therefore, the effects of a constant cooling is somewhat offset by the alumina dissolution effect, and bring the measured value closer to the true value.
Park, Jung-Hwan;Kim, Jin-Han;Jung, Jong-Tai;Jun, Se-Jin;Park, Han-Bong
Journal of Wetlands Research
/
v.12
no.2
/
pp.67-73
/
2010
This study was performed to figure out what would be effective to maintain good water quality in the retention pond which was badly polluted before. In order to keep the good water quality of the retention pond it is necessary to prevent outer non-point source pollutants from flowing into the pond. In this study, we proposed to use porous slag as a blockage of the inflow into the pond from external non-point sources. We experimented with porous slag nets to see how the water is effected. With the results of the experiments, we found out there is a close correlation($r^2=0.9765$) between contact time and the removal rate of phosphorus, therefore we can conclude that contact time affects removal rate greatly. Synthetic wastewater, activated sludge effluent, and sewage were passed through a porous slag packed bed, both phosphorus and the suspended solid in water were removed highly. With the results of these tests, we proposed to set up a porous slag packed bed inside of the retention pond and revetment to prevent external non-point source pollutants flowing into the retention pond.
Proceedings of the Korean Society of Soil and Groundwater Environment Conference
/
2004.04a
/
pp.260-265
/
2004
Acid mine drainage(AMD) is one of the most serious environmental concerns associated with the mining industry around the world. The objective of this study is to assess the potential of sewage sludge as a carbon source for sulfate reducing bacteria and waste lime and steel slag as a neutralize agent for acid mine drainage bioremediation for use in permeable reactive materials. The study was performed using synthetic AMD in six column experiments. The effluent solution was systematically analysed throughout the experiments. The results of the study indicated that sewage sludge, waste lime and steel slag were the most effective for the AMD treatment as a permeable reactive materials.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.