Numerical analysis of center cracked orthotropic fgm plate: Crack and material axes differ by θ°

  • Kaman, Mete Onur;Cetisli, Fatih
    • Steel and Composite Structures
    • /
    • 제13권2호
    • /
    • pp.187-206
    • /
    • 2012
  • In this study, fracture analysis of orthotropic FGM (Functionally Graded Material) plate having center crack is performed, numerically. Material axis arbitrarily oriented and there is an angle ${\theta}^{\circ}$ between material and crack axes. Stress intensity factors at the crack tips for Mode I are calculated using Displacement Correlation Method (DCM). In numerical analysis, effects of material properties and variation of angle ${\theta}^{\circ}$ between material and crack axes on the fracture behavior are investigated for four different boundary conditions. Consequently, it is found that the effect of ${\theta}^{\circ}$ on stress intensity factor depends on variation of material properties.

복부절단법에 의한 레일의 잔류응력에 관한 연구 (A study ell the residual stress in rail by the web saw-cut method)

  • 서정원;구병춘;정우현
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 1999년도 추계학술대회 논문집
    • /
    • pp.234-241
    • /
    • 1999
  • Rails have residual stresses produced during manufacturing processes. The residual stresses play all important role on brittle fracture, fatigue strength and derailment by producing cracks in the web of rail. The web saw-cut test is a technique developed to measure the bulk longitudinal residual stress level. It is a simple mettled to estimate a stress intensity factor, $_{4}$ for a web crack by using the radii of curvature of the upper and lower portions of a cut rail. But according to this method, $_{4}$ varies along the rail length because the curvatures along tile rail length vary In this paper, tile residual stress was estimated by Finite Element Method and tile web saw-cut method. In addition tile variation of the residual stress with time was investigated.

  • PDF

MFC 센서를 이용한 응력 확대 계수 측정에 관한 연구 (A Study of Stress Intensity Factors using Micro Fiber Composite Sensors)

  • 오동진;김명현
    • Journal of Welding and Joining
    • /
    • 제29권3호
    • /
    • pp.76-81
    • /
    • 2011
  • Recently, the structural failures due to fatigue occur frequently with the increase of size of ships and offshore structures. In this respect, the assessment of fatigue life and the residual strength are very important. Currently, the smart materials technology has demonstrated a variety of possibilities for a diagnosis of structural strength and structural health condition for large structures. The benefits and feature of the MFC sensor are more flexible, durable and reliable than conventional smart material. In this study, Micro Fiber Composite (MFC) sensor for the measurement of stress intensity factor (SIF) of two dimensional cracks induced in a structure is developed. Two MFC sensors are placed in the vicinity of the crack tip close to each other with the crack tip in between them. The SIFs of Mode I($K_I$) as well as of Mode II($K_{II}$) based on the piezoelectric constitutive law and fracture mechanics are calculated. In this study, the SIF values measured by MFC sensors are compared with the theoretical results and measured value.

구름마찰접촉하중 시 Polyethylene tibia 요소의 표면균열 복합전파 거동에 관한 연구 (Study for Possible Crack Propagation Mechanisms for a Surface Cracked in a Polyethylene Tibia Component Subject to Rolling and Sliding Contact)

  • 김병수;문병영
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 추계학술대회
    • /
    • pp.1222-1227
    • /
    • 2003
  • Pitting wear is a dominant form of polyethylene surface damage in total knee replacements, and may originate from surface cracks that propagate under repeated tribological contact. In this study, stress intensity factors, $K_{I}$ and $K_{II}$, were calculated for a surface crack in a polyethylene - CoCr - bone system under the rolling and/or sliding contact pressures. Crack length and load location were considered in determination of probable crack propagation mechanisms and fracture modes. Positive $K_{I}$ values were obtained for shorter cracks in rolling contact and for all crack lengths when the sliding load was apart from the crack. $K_{II}$, was the greatest when the load was directly adjacent to the crack $(g/a={\pm}1)$. Sliding friction caused a substantial increase of both $K_{I}^{max}$ and $K_{II}^{max}$. The effective Mode I stress intensity factors, $K_{eff}$, were the greatest at $g/a={\pm}1$, showing the significance of high shear stresses generated by loads adjacent to surface cracks. Such behavior of $K_{eff}$ suggests mechanisms for surface pitting by which surface cracks may propagate along their original plane under repeated rolling or sliding contact.

  • PDF

CAUSTICS방법에 의한 응력확대계수 결정 (Determination of the Stress Intensity Factor by the Method of Caustics)

  • 김상철;이억섭;한민구
    • 비파괴검사학회지
    • /
    • 제8권1호
    • /
    • pp.22-29
    • /
    • 1988
  • The optical method of reflected and transmitted caustics has been utilized in mechanics investigations. This relatively new experimental technique has been successfully applied on various fracture analysis such as static and dynamic c rack propagation studies, some elasticity problems and contact stress, etc, In this study, the stress intensity factors in thin polycarbonate specimens, a kind of optically anisotropic material, under Mode I loading condition are estimated by the method of caustics. The values of stress intensity factors obtained from theoretical caustics shape are compared by the experiment. It is confirmed that the two stress intensity factors agree well with Srawley's solution.

  • PDF

쇼트피이닝 가공된 스프링강의 고온 피로균열진전 평가 (A Study on the Shot Peening on the High Temperature Fatigue Crack Propagation)

  • 박경동;정찬기;하경준
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2001년도 추계학술대회 논문집
    • /
    • pp.264-268
    • /
    • 2001
  • In this study, CT specimens were prepared from spring steel(SUP9) processed shot peening which was room temperature, low temperature and high temperature experiment. And we got the following characteristics from fatigue crack growth test carried out in the environment of room, and high temperature at $25^{\circ}C,\; 50^{\circ}C, \;100^{\circ}C,\; 150^{\circ}C,\; and\; 180^{\circ}C$ in the range of stress ratio of 0.05 by means of opening mode displacement. The threshold stress intensity factor range $\DeltaK_{th}$ in the early stage of fatigue crack growth (Region I ) and stress intensity factor range $\Delta$K in the stable of fatigue crack growth (Region II) was decreased in proportion to descend temperature. It assumed that the fatigue resistance characteristics and fracture strength at low temperature and high temperature is considerable higher than that of room temperature in the early stage and stable of fatigue crack growth region.

  • PDF

A fracture criterion for high-strength steel cracked bars

  • Toribio, J.
    • Structural Engineering and Mechanics
    • /
    • 제14권2호
    • /
    • pp.209-221
    • /
    • 2002
  • In this paper a fracture criterion is proposed for cracked cylindrical samples of high-strength prestressing steels of different yield strength. The surface crack is assumed to be semi-elliptical, a geometry very adequate to model sharp defects produced by any subcritical mechanism of cracking: mechanical fatigue, stress-corrosion cracking, hydrogen embrittlement or corrosion fatigue. Two fracture criteria with different meanings are considered: a global (energetic) criterion based on the energy release rate G, and a local (stress) criterion based on the stress intensity factor $K_I$. The advantages and disadvantages of both criteria for engineering design are discussed in this paper on the basis of many experimental results of fracture tests on cracked wires of high-strength prestressing steels of different yield strength and with different degrees of strength anisotropy.

박용 구조물용 일반압연강 용접부의 피로균열 전파거동에 미치는 $K_{II}$의 영향 (Effects of $K_{II}$ on fatigue crack propagation behavior of wedzone in generally rolled steel for marine structure)

  • 한문식;김상철
    • Journal of Welding and Joining
    • /
    • 제6권3호
    • /
    • pp.43-55
    • /
    • 1988
  • An experimental study was carried out to identify the fatigue fractue behavior of weld zone in generally rolled steel for marine structure. The bending an shear loads were applied simultaneously on the specimens to simulate real load condition for marine structure. The effect of the stress intensity factor under mode I with II loading condition on the initiation and the propagation of a crack were investigated, with particular emphaiss on mode II. When the $K_{II}$ stress intensiy factor in mode II was applied under mode I load condition, the growth behavior of a crack seems to be affected mainly by the anisotropic characteristic of materials. Especially, when the crack was located in and near the weld zone and parallel to th weld line, the propagation behaviour was turned out to be quite different from that of the base metal along the direction transverse to the weld line. In general, the propagation veiocity of the cracks in and near the weld zone was found to be slower that the velocity in base metal.

  • PDF

응력확대계수 측정용 고정 슬랩상사 장치의 개발 (Development of the Fixed Slab Analogy Device for the Measurement of Stress Intensity Factor)

  • 정진석;최선호;황재석
    • 대한기계학회논문집
    • /
    • 제16권11호
    • /
    • pp.1999-2010
    • /
    • 1992
  • 본 연구에서는 (1)의 방법의 문제점.즉, 두꺼운 판에 강체 균열을 열매립하는 과정에서 균열 첨단에 열변형이 일어나, 변위측정시 측정 오차가 발생하는 점을 해결 하기 위해, 매유 얇은 P.V.C.판(t=0.15mm)에 강체 균열을 열매립 하는 대신 접착제로 부착하는 방법을 채택하여 강체균열 경계상의 곡률 영향을 검토하였으며, (2)의 방법 의 해결책으로서, 강체균열에서 충분히 먼곳의 곡률은 얇은 합금공구강판(alloy tool steel plate`t=1mm)으로 제작한 프레임(Frame)으로 원방곡률을 미리 슬랩 경계조건과 일치하도록 하였고, 또한 변위도 고정(동결)할수있는 새로운 고정 하중장치를 개발하 여 실험 측정치의 정도를 높였다.

쐐기 분열 시험을 이용한 암석의 모드 I 파괴인성 측정 (Determination of Mode I Fracture Toughness of Rocks Using Wedge Splitting Test)

  • 고태영;김택곤;이대혁
    • 터널과지하공간
    • /
    • 제29권6호
    • /
    • pp.523-531
    • /
    • 2019
  • 암석역학이나 암반공학의 여러 활용 분야 중 발파, 천공 및 기계굴착의 경우에는 파괴인성이 중요한 요소이며, 암석의 파괴인성을 측정하기 위한 여러 가지 방법들이 제안되었다. 본 연구에서는 간단히 시험편을 제작할 수 있고, 압축 하중으로 암석의 모드 I 파괴인성을 구할 수 있도록 쐐기 분열 시험편(Wedge Splitting Test Specimen)을 이용하였다. 쐐기의 작용하는 연직하중에 의한 수직 및 수평하중 모두를 고려한 균열선단의 응력상태로부터 수치해석을 통한 응력확대계수의 식을 제안하였다. 쐐기 분열 시험편에 의해 구해진 모드 I 파괴인성값을 GD와 SENB 시험편의 시험 결과와 비교하여 시험법의 타당성을 확인하였다.