Selective Laser Sintering of Cu/Polyamide Mixed Powder (Cu/Polyamide 혼합분말의 선택적 레이저 소결)

  • 박흥일;이길근
    • Journal of Powder Materials
    • /
    • v.8 no.4
    • /
    • pp.239-244
    • /
    • 2001
  • To investigate the effect of process parameters on selective laser sintering of Cu/polyamide mixed powder, Cu/polyamide mixed powder was sintered by selective laser with changing laser power and scanning speed. The properties of sintered body were evaluated by measuring the density and tensile strength, and analysis of XRD, FT-Raman and microstructure. With an increase in the laser power, the density and ultimate tensile strength of sintered Cu/polyamide body increase and then decrease. The maximum values of the density and ultimate tensile strength were decreased with increasing laser scanning speed. These changes were concerned with the difference of irradiation energy of laser into the powder layer. It was considered that the change of the mechanical property of the sintered body with irradiation energy of laser is due to the changes of amount of copper particle and property of polyamide.

  • PDF

The Evaluation of Fracture Toughness on Mode I for Twill CFRP/GFRP Laminated Hybrid Composites (능직 CFRP/GFRP 적층하이브리드 복합재의 Mode I 파괴인성 평가)

  • Roh, Young Woo;Kang, Ji Woong
    • Journal of the Korean Society of Safety
    • /
    • v.35 no.5
    • /
    • pp.9-14
    • /
    • 2020
  • In order to realize high strength and light weight for various industrial facilities and structural materials, various new materials are applied to product design. Among them, CFRP has excellent specific strength and non-rigidity, and the scope of use is expanding throughout the industry, such as mobility products and building materials. GFRP is cheaper than CFRP, and has excellent specific strength and non-rigidity, and has excellent heat resistance and sound insulation, so it has been adopted as a core material for flooring and interior flooring. CFRP of twill weave structure has better resistance to deformation of fiber than plain weave structure, so the outermost layer is applied as twill weave structure in product design. After fabrication with DCB specimens, Mode I fracture toughness was evaluated according to the crack length. As the crack length increases, the energy release rate and stress intensity factor values tended to decrease overall.

Effect of Shot Blasting Treatment on the Formability of Thin High Strength Steels (고강도 강판의 성형성에 미치는 Shot Blasting 가공 조건의 영향)

  • Park, K.C.;Kim, J.I.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.05a
    • /
    • pp.341-344
    • /
    • 2008
  • In order to study the effect of shot blasting condition on the formability of thin high strength steels, specimens were made by changing line speed of a commercial shot blasting plant with maintaining constant impeller condition. Surface roughness of prepared specimens was multiplied by lowering line speed or increasing density of shot impact. Formability was reduced as increasing shot impact. The elongation and stretching formability of shot blasted sheet were decreased by about 10% compared to original sheet. More significant decrease in bending formability was observed after shot blasting. This might be due to the concentrated impact near the surface where major strain occurs during bending process.

  • PDF

An Experimental Study on the Neutralization of High-Flowable Concrete (고유동콘크리트의 중성화에 관한 실험적 연구)

  • Jeon, Hyun-Kyu;Lim, Jin-Kyu;Seo, Chee-Ho
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.3 no.3
    • /
    • pp.177-185
    • /
    • 1999
  • In this study, study about fly ash and blast-furnace slag used as substitutive materials for cement, and the influence on the neutralization of high flow concrete durability with these substitutive materials was performed and analyzed. The results are as follows 1) Aggregate segregation was partially improved with the progress of the admixture input at the mix proportion above slump flow 65 cm 2) Compressive strength with the progress of the increasement of fly ash input was decreased in early age, but decrease range was improved in long term age. Also, in case of blast-furnace, similar or improved compressive strength was appeared. 3) The neutralization depth with fly ash input was noticeably increased. But blast-furnace slag was effective to prevent. 4) In this experiment, high powder content was advantageously affected on preventive effect of the neutralization, and the relationship between the compressive strength and the neutralization depth was inversely proportional.

  • PDF

Research on chloride ion diffusivity of concrete subjected to CO2 environment

  • Zhang, Shiping;Zhao, Binghua
    • Computers and Concrete
    • /
    • v.10 no.3
    • /
    • pp.219-229
    • /
    • 2012
  • Carbonation is a widespread degradation of concrete and may be coupled with more severe degradations. An experimental investigation was carried out to study the effect of carbonation on chloride ion diffusion of concrete. The characteristic of concrete after carbonation was measured, such as carbonation depth, strength and pore structure. Results indicated that carbonation depth has a good linear relation with square root of carbonate time, and carbonation can improve compressive strength, but lower flexural strength. Results about pore structure of concrete before and after carbonation have shown that carbonation could cause a redistribution of the pore sizes and increase the proportion of small pores. It also can decrease porosities, most probable pore size and average pore diameters. Chloride ion diffusion of concrete after carbonation was studied through natural diffusion method and steady state migration testing method respectively. It is supposed that the chloride ion concentration of carbonation region is higher than that of the sound region because of the separation of fixed salts, and chloride ion diffusion coefficient was increased due to carbonation action evidently.

Sulfuric Acid Resistance Evaluation of Repair Mortar Substituted Blast Furnace (고로슬래그를 치환한 보수 모르타르의 내 황산성 평가)

  • Kim, Wan-Su;Jang, Jong-Min;Lee, Han-Seung
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2019.11a
    • /
    • pp.25-26
    • /
    • 2019
  • The Reinforced concrete structure is deteriorated in durability due to various deterioration factors such as acid, salt, etc., and thus requires repair and reinforcement. In this study, compressive strength and weight change were measured by substituting blast furnace slag with excellent chemical resistance. As a result, the decrease in compressive strength decreased in proportion to the blast furnace slag substitution rate, and in the case of BFS40, the strength increased after sulfuric acid immersion. The weight change also decreased in proportion to the replacement amount.

  • PDF

Effect of Oral Hygiene Management Process using Natural Gargle Fluid (Cinnamon) on Occlusal Force and Changes in Oral Environment

  • Bo Ram Kim;Kyung Min Kim;Yu mi Kim;Min-Kyoung Park;Min Kyung Lee
    • Biomedical Science Letters
    • /
    • v.30 no.1
    • /
    • pp.17-23
    • /
    • 2024
  • In this study, the changes in occlusal strength and oral environment before and after the use of natural gargles containing cinnamon were confirmed. This study involved 42 adults aged 19 or older living in Busan from November 25 to December 2, 2023. Twenty-one people were randomly selected for each of the regular and natural gargles. In this study, the group using natural gargles confirmed an increase in saliva buffering power, a decrease in O'Leary index, and an increase in occlusal strength. Through this, it was confirmed that natural gargles containing cinnamon are helpful in improving the oral environment and occlusal strength.

Strength and failure characteristics of the rock-coal combined body with single joint in coal

  • Yin, Da W.;Chen, Shao J.;Chen, Bing;Liu, Xing Q.;Ma, Hong F.
    • Geomechanics and Engineering
    • /
    • v.15 no.5
    • /
    • pp.1113-1124
    • /
    • 2018
  • Geological dynamic hazards during deep coal mining are caused by the failure of a composite system consisting of the rock and coal layers, whereas the joint in coal affects the stability of the composite system. In this paper, the compression test simulations for the rock-coal combined body with single joint in coal were conducted using $PFC^{2D}$ software and especially the effects of joint length and joint angle on strength and failure characteristics in a rock-coal combined body were analyzed. The joint length and joint angle exhibit a deterioration effect on the strength and affect the failure modes. The deterioration effect of joint length of L on the strength can be neglected with a tiny variation at ${\alpha}$ of $0^{\circ}$ or $90^{\circ}$ between the loading direction and joint direction. While, the deterioration effect of L on strength are relatively large at ${\alpha}$ between $30^{\circ}$ and $60^{\circ}$. And the peak stress and peak strain decrease with the increase of L. Additionally, the deterioration effect of ${\alpha}$ on the strength becomes larger with the increase of L. With the increase of ${\alpha}$, the peak stress and peak strain first decrease and then increase, presenting "V-shaped" curves. And the peak stress and peak strain at ${\alpha}$ of $45^{\circ}$ are the smallest. Moreover, the failure mainly occurs within the coal and no apparent failure is observed for rock. At ${\alpha}$ between $30^{\circ}$ and $60^{\circ}$, the secondary shear cracks generated in or close to the joint tips, cause the structural instability failure of the combined body. Therefore, their failure models present as a shear failure along partial joint plane direction and partially cutting across the coal body or a shear failure along the joint plane direction. However, at ${\alpha}$ of $60^{\circ}$ and L of 10 mm, the "V-shaped" shear cracks cutting across the coal body cause its final failure. While crack nucleations at ${\alpha}$ of $0^{\circ}$ or $90^{\circ}$ are randomly distributed in the coal, the failure mode shows a V-shaped shear failure cutting across the coal body.

Strength Development of Fly ash Substituted Concrete due to Blast Furnace Slag Powder and Gypsum Addition (고로슬래그 미분말 및 석고혼입에 따른 플라이애시 치환 콘크리트의 강도발현 특성)

  • Han, Cheon-Goo;Han, Min-Cheol;Jeon, Kyu-Nam
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.2
    • /
    • pp.97-104
    • /
    • 2010
  • In this study, the effect of blast furnace slag and gypsum addition on strength development of fly ash substituted concrete is investigated experimentally. As a result, the fluidity represented a similar or larger level than that of OPC but showed a tendency to decrease the fluidity according to the increase in the replacement level of BS and GS for the FA replacement concrete. In the case of the air content, although it showed a larger decrease compared to that of OPC, it also represented that BS and GS did not affect the air content significantly. Regarding the compressive strength in the case of the replacement of BS and GS for the FA 10% replacement concrete, it showed a higher early strength than OPC. Whereas, in the case of the BS 5% replacement and GS 1% incorporation for the FA 10% replacement concrete showed the most excellent performance due to its high strength. In the correlation of the compressive strength according to the kinds of admixtures, it was evident that the GS incorporation played an important role in high strength gain.

  • PDF

SHEAR BOND STRENGTH AND FAILURE PATTERNS ACCORDING TO THE THICKNESS OF RESIN BASE IN BRACKET BONDING (브라켓 부착시 레진 베이스의 두께에 따른 전단결합강도와 파절양상에 관한 연구)

  • Kim, Jae-Hyuk;Hwang, Hyeon-Shik
    • The korean journal of orthodontics
    • /
    • v.28 no.4 s.69
    • /
    • pp.659-668
    • /
    • 1998
  • The purpose of this study was to evaluate the possibility of the decrease of bond strength due to increased thickness of resin base in indirect bracket bonding technique. Metal brackets were bonded to the resin blocks involving bovine lower incisors and the thickness of resin bases was increased by increments of 0.5 mm from 0.0 mm to 2.0 mm. They were divided into two groups, one group is that the thickness of resin base was increased but the loading point from the tooth surface was maintained constantly, the other group is that the loading point from the tooth surface and the resin base thickness were increased concomitantly. The shear bond strength was tested on universal testing machine and the failure patterns were assessed with the adhesive remnant index(ARI). The results were as follows: 1. When the distance from the tooth surface to the loading point was maintained constantly, shear bond strength was increased significantly according to the decrease of distance from the bracket base to the loading point and the increase of resin base thickness. 2. When the distance from the tooth surface to the loading point and the resin base thickness were increased concomitantly, shear bond strength was decreased according to the increase of resin base thickness but significant differences were ignorable. 3. There were no significant differences in ARI scores according to the change in the thickness of resin base. The results of the present study indicated that shear bond strength was not much affected by the thickness of resin base, whereas was decreased according to the increase of distance from bracket base to the loading point.

  • PDF