탄소강배관 다중 UT 측정두께를 활용한 감육여부 판별법 개발 (Development of Wall Thinning Distinction Method using the Multi-inspecting UT Data of Carbon Steel Piping)

  • 황경모;윤훈;이찬규
    • Corrosion Science and Technology
    • /
    • 제11권5호
    • /
    • pp.173-178
    • /
    • 2012
  • To manage the wall thinning of carbon steel piping in nuclear power plants, the utility of Korea has performed thickness inspection for some quantity of pipe components during refueling outages and determined whether repair or replacement after evaluating UT (Ultrasonic Test) data. When the existing UT data evaluation methods, such as Band, Blanket, PTP (Point to Point) Methods, are applied to a certain pipe component, unnecessary re-inspecting situations may be generated even though the component does not thinned. In those cases, economical loss caused by repeated inspection and problems of maintaining the pipe integrity followed by decreasing of newly inspected components may be generated. EPRI (Electric Power Research Institute) in USA has suggested several statistical methods, TPM (Total Point Method), LSS (Least Square Slope) Method, etc. to distinguish whether multiple inspecting components have thinned or not. This paper presents the analysis results for multiple inspecting components over three times based on both NAM (Near Area of Minimum) Method developed by KEPCO-E&C and the other methods suggested by EPRI.

고온 나트륨 히트파이프에서 열이송 조건에 따른 열전달 특성에 대한 실험 연구 (An Experimental Study on the Heat Transfer Characteristics of a High-temperature Sodium Heat Pipe Depending on the Thermal Transport Conditions)

  • 박철민;부준홍;김진수
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2008년도 추계학술대회B
    • /
    • pp.2340-2345
    • /
    • 2008
  • Cylindrical stainless-steel/sodium heat pipe for a high-temperature application was manufactured and tested for transient and steady-state operations. Two layers of Stainless-steel screen mesh wick was inserted as a capillary structure. The outer diameter of the heat pipe was 12.7 mm and the total length was 250 mm. As thermal transport conditions, the effective transport length, the heat flux, the tilt angle and the operating temperature were varied. The heat was supplied by an electric furnace up to 1 kW and the cooling was performed by forced convection of air. The effective thermal conductivity and the thermal resistance were investigated as a function of heat flux, heat transport length, and vapor temperature. Typical range of the total thermal resistance was as low as $0.036^{\circ}C/W$ at $175.8\;kW/m^2$ of heat flux and $700^{\circ}C$ of operating temperature.

  • PDF

Laser based impedance measurement for pipe corrosion and bolt-loosening detection

  • Yang, Jinyeol;Liu, Peipei;Yang, Suyoung;Lee, Hyeonseok;Sohn, Hoon
    • Smart Structures and Systems
    • /
    • 제15권1호
    • /
    • pp.41-55
    • /
    • 2015
  • This study proposes a laser based impedance measurement system and impedance based pipe corrosion and bolt-loosening monitoring techniques under temperature variations. For impedance measurement, the laser based impedance measurement system is optimized and adopted in this paper. First, a modulated laser beam is radiated to a photodiode, converting the laser beam into an electric signal. Then, the electric signal is applied to a MFC transducer attached on a target structure for ultrasonic excitation. The corresponding impedance signals are measured, re-converted into a laser beam, and radiated back to the other photodiode located in a data interrogator. The transmitted impedance signals are treated with an outlier analysis using generalized extreme value (GEV) statistics to reliably signal off structural damage. Validation of the proposed technique is carried out to detect corrosion and bolt-loosening in lab-scale carbon steel elbow pipes under varying temperatures. It has been demonstrated that the proposed technique has a potential to be used for structural health monitoring (SHM) of pipe structures.

탄소성 유한요소 해석을 통한 곡관 두께에 따른 파손 위치 및 균열 진전 방향 분석 (Analysis of the Elbow Thickness Effect on Crack Location and Propagation Direction via Elastic-Plastic Finite Element Analysis)

  • 김재윤;이종민;김윤재;김진원
    • 한국압력기기공학회 논문집
    • /
    • 제18권1호
    • /
    • pp.26-35
    • /
    • 2022
  • When piping system in a nuclear power plant is subjected to a beyond design seismic condition, it is important to accurately determine possibility of crack initiation and, if initiation occurs, its location and time. From recent experimental works on elbow pipes, it was found that the crack initiation location and crack propagation direction of the SA403 WP316 stainless steel elbow pipe were affected by the pipe thickness. In this paper, the crack initiation location and crack propagation direction for SA403 WP316 stainless steel elbow pipes with different thickness were analyzed via elastic-plastic finite element analysis. Based on FE results, the effect of the pipe thickness on different crack initiation location and crack propagation direction was analyzed using ovality, stress and strain components. It was also confirmed that the presence of internal pressure had no effect on the crack initiation location and crack propagation direction.

PRD 강환 말뚝의 연직지지력 특성에 관한 사례 연구 (Case Study on the Characteristics of Vertical Bearing Capacity for Steel Pipe Pile Installed by PRD)

  • 최용규;정창규;정성기;김동철;정태만
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 1999년도 봄 학술발표회 논문집
    • /
    • pp.225-232
    • /
    • 1999
  • Construction case of PRD (Percussion Rotary Drill) pipe pile and matters to be attended in construction of PRD pile were reviewed. The compressive and uplifting static pile load tests for PRD piles were performed and, also, analysis by Pile Driving Analyzer was done. Based on these results, bearing components in each resisting part (that is: steel toe, external skin, and internal skin) were measured separately. The measured resisting force was compared to the value calculated by the estimated formula. The pile capacity was mobilized in steel toe area and the external skin friction and the internal friction were not produced. Thus, it could be considered that toe of PRD pile should be supported in hard bearing stratum (for example, the fresh soft rock).

  • PDF

후판 파이프 제작시 잔류응력 (Residual stress analysis of thick plate pipe)

  • 최광;임성우
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 추계학술발표대회 개요집
    • /
    • pp.150-152
    • /
    • 2004
  • This study was aimed at evaluation of residual stress of steel pipe structures. The production process of pipes was complex (at first bending was done by roll forming or press forming and welding was final process of making of steel pipes). So there could be effected high residual stresses in steel pipes. In order to evaluate the changes of residual stress the locations of measurement were selected carefully. Measurements of residual stress were done for various kinds of pipes (shapes in circular and square). For the evaluation of residual stress, hole-drilling method (ASTM E837 was applied. The results showed that along the weld Eine high tensile stress were measured as effected, and high tensile stresses were measured where large plastic deformation developed. Through these efforts, experimental results could be more effectively assisted by numerical method.

  • PDF

항타강관말뚝의 주면마찰저항 특성에 관한 현장실험 연구 (A Field Test Study on Skin Friction Behavior of Driven Steel Piles)

  • 이민희;이충숙;정창규;최용규
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2005년도 춘계 학술발표회 논문집
    • /
    • pp.575-582
    • /
    • 2005
  • Static pile load tests for three instrumented driven steel pipe pies were performed. Based on the distributions of pile axial loads along the pile depth, Characteristics of unit skin friction were analyzed.

  • PDF

지하매설 유체함입 강파이프의 감쇠특성 규명 (Attenuation Characteristics of the Buried Steel Water Pipes)

  • 박경조;강우석;김이곤
    • 동력기계공학회지
    • /
    • 제13권1호
    • /
    • pp.39-45
    • /
    • 2009
  • The attenuation of the fundamental non-torsional modes that propagate down buried steel water pipes has been studied. The mode shapes, mode attenuation due to leakage into the surrounding medium and the scattering of the modes as they interact with pipe joints and fittings have been investigated. In the low frequency region the mode predicted to dominate over significant propagation distances approximates a plane wave in the water within pipe. The established acoustic technique used to locate leaks in buried steel water pipes assumes that leak noise propagates as a single non-dispersive mode at a velocity related to the low frequency asymptote of this water borne mode.

  • PDF

용융아연 도금강판으로 제조된 파형강관의 내구수명예측 (Estimation of Durability of corrugated Steel Pipes Made of Hot-Dip Galvanized Sheet Steels)

  • 김종상
    • 한국표면공학회지
    • /
    • 제27권6호
    • /
    • pp.347-358
    • /
    • 1994
  • Estimation of durability for corrugated steel pipe(CSP) has been evaluated by using several analytical methods. This study, using a plain hot-dip galvanized CSP as the base line, addresses additional coatings such as polymers sand bituminous coatings that may be used to achieve a desired design life of at least 50years. The behavior of both the soil side and the effluent side of the pipe have been studied. It is estimated that CSP generally provides outstanding dura-bility with regard to soil side effects, and that virtually any required service life can be attained by selecting appropri-ate coatingss and/or thickness of steel substrate. This study is limited to storm drainage systemss carrying naturally oc-curring surface water only. The recommendation in this report do not apply to sanitary or industrial waste sewers or other conduits used to carry corrosive effluents.

  • PDF

울진 원자력 발전소 3, 4호기 1차계통 배관소재의 파괴저항특성 평가 (Evaluation of Fracture Resistance Characteristic for Primary Piping System of Ulchin 3,4 Nuclear Power Plants)

  • 석창성;강병구;김수용;박재실;윤병곤
    • 한국안전학회지
    • /
    • 제14권1호
    • /
    • pp.25-32
    • /
    • 1999
  • The objective of this paper is to evaluate the fracture resistance characteristics of SA508 CL.1a carbon steel, TP347 stainless steel and their associated welds manufactured for primary coolant system of Ulchin 3,4 nuclear power plants. The effect of various parameters such as pipe size, welding method, chemical composition, crack plane orientation, metallography and fractography on the material properties were discussed. Test results showed that the effect of pipe size on fracture toughness is negligible while the effect of welding method on fracture toughness is significant. In addition, the drop of fracture toughness in the field fabrication weld of TP347 stainless steel is probably due to the large amount of $\sigma$-phase precipitated on the $\delta$-ferrite boundary and the large size dimples.

  • PDF