• 제목/요약/키워드: Steel Rolling

검색결과 563건 처리시간 0.027초

연속식 가열로의 Level 2 제어 시스템 설계 (Design of Level 2 Control System for Continuous Reheat Furnaces)

  • 유보현;이재용;임동렬;차재민;염충섭
    • 시스템엔지니어링학술지
    • /
    • 제12권1호
    • /
    • pp.113-120
    • /
    • 2016
  • Steel in a continuous reheat furnace is heated to higher temperature to be treated in the rolling steel process. Due to this reason the continuous reheat furnace system requires an optimal control system to adjust the temperature inside the furnace. Level 2 control systems for continuous reheat furnaces generate automatic heating set points for the level 1 system of the furnace based on the mathematical thermal model which can give a good estimation of steel heating inside the furnace and is used to adjust heating requirements to optimize furnace combustion. For the current study the analytic methodology based on the design procedure from the systems engineering to develop new level 2 control system of a continuous reheat furnace was proposed. The system analysis and the requirements of the level 2 control system were derived using the unified modeling language (UML) 2.0, and the design of database and the graphic user interface (GUI) for the level 2 control system were conducted.

붕소함유 냉간단조용 비조질강의 경화능 및 기계적 특성평가 (Characterization of Hardenability and Mechanical Properties of B-Bearing Microalloyed Steels for Cold Forging)

  • 박현균;김남규;최회진
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 춘계학술대회 논문집
    • /
    • pp.395-399
    • /
    • 2004
  • Four microalloyed steels containing B were investigated in terms of hardenability, mechanical properties and microstructure depending upon the cooling rates in order to develop the steel grade for the cold forged fasners. The alloy with the largest DI value among 4 alloys, which contains $0.12\%\;C,\;1.54\%\;Mn,\;0.65\%\;Cr,\;0.11\%V,\;0.040\%Ti\;and\;0.0033\%B$, showed the larest shift to the right hand side in the TTT diagram, implying the wide allowable cooling rate range subsequent to hot rolling in long bar processing, Mechanical tests indicated that yield strength are dependent upon the DI value in water quenched specimens but other properties showed almost the same values. In the same grade of steel, the increase in cooling rates causes the decrease in elongation but the increase in strength, reduction of area and Charpy impact values. Microstructural examination in steel grade with the larest DI values revealed martensitic structure In the water quenched state, a mixture of martensite and bainite in the oil quenched, and ferrite + pearlite in the air cooled and the forced air cooled but the latter showed finer microstructure.

  • PDF

Improvement of cold mill precalculation accuracy using a corrective neural network

  • Jang, Min;Cho, Sungzoon;Cho, Yong-Joong;Yoon, Sungcheol;Cho, Hyungsuk
    • 한국경영과학회:학술대회논문집
    • /
    • 대한산업공학회/한국경영과학회 1996년도 춘계공동학술대회논문집; 공군사관학교, 청주; 26-27 Apr. 1996
    • /
    • pp.63-66
    • /
    • 1996
  • Cold rolling mill process in steel works uses stands of rolls to flatten a strip to a desired thichness. At Pohang Iron and Steel Company (POSCO) in Pohang, Korea, precalculation determines the mill settings before a strip actually enters the mill and is done by an outdated mathematical model. A corrective neural network model is proposed to improve the accuracy of the roll force prediction. Additional variables to be fed to the network include the chemical composition of the coil, its coiling temperature and the aggregated amount of processed strips of each roll. The network was trained using a standard backpropagation with 2,277 process data collected form POSCO from March 1995, then was tested on the unseen 200 data from the same period. The combined model reduced the prediction error by 55.4% on average.

  • PDF

Mini-Mill 연속주고기의 동적 Bulging해석 Model(I) -주편의 변형거동을 중심으로- (A Deformation Behavior Analysis of Dynamic Bulging in the Mini-Mill Continuous Casting System)

  • 한성욱;정영진;강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1998년도 춘계학술대회논문집
    • /
    • pp.138-143
    • /
    • 1998
  • The continuous casting process has been adopted increasingly in recent years to save both energy and labor. It has experienced a rapid development in the production of semi-finished steel products, replacing the conventional route of ingot casting plus rolling. To achieve this good merit, however, more studies about a heat transfer mechanism between roll and slab are needed. So this paper shows the results of the deformation behavior of steel cast slabs, which are about the solidification and heat transfer. This study is used to prevent internal cracks of a slab in a bending and unbending zone. The value of moving strand shell bulging between two supporting rollers under ferrostatic pressure and slab-self weight has been computed in terms of creep and elastic-plasticity. The high strand distributions in solidified shell undergoes a series of bulging are calculated with boundary condition a very closed to continuous steel cast slabs productions.

  • PDF

고 Mn 오스테나이트계 스테인리스강의 감쇠능에 미치는 역변태의 영향 (Effect of Reverse Transformation on the Damping Capacity of High Manganease Austenitic Stainless Steel)

  • 강창룡
    • 동력기계공학회지
    • /
    • 제16권4호
    • /
    • pp.60-65
    • /
    • 2012
  • This study was carried out to investigate the effect of reverse transformation on the damping capacity in high manganese austenitic stainless steel. ${\alpha}^{\prime}$-martensite was formed with the specific direction and surface relief by deformation. Over 95% of the austenite phase was transformed to deformation-induced ${\alpha}^{\prime}$-martensite by 70% cold rolling. Reverse transformation became rapid above an annealing temperature of $550^{\circ}C$, but there was no significant transformation above $700^{\circ}C$. In addition, with increasing annealing time at $700^{\circ}C$, reverse transformation was induced rapidly, but the transformation was almost completed at 10 min. Damping capacity was increased up to $700^{\circ}C$, and than unchanged with the increasing annealing temperature. Damping capacity increased steeply with an increasing reverse treatment time up to 10min, whereas there were no significant change with a treatment time of more than 10 min. Damping capacity increased with an increasing the reversed austenite and was strongly affected by reversed austenite.

저항복비·고강도 구조용 내화강의 피로특성 및 비파괴평가 (Fatigue Characteristics and its Nondestructive Evaluation of Fire-resistance Steel for Construction with Low Yield Ratio and High Strength)

  • 김현수;남기우;강창룡
    • 열처리공학회지
    • /
    • 제14권4호
    • /
    • pp.212-219
    • /
    • 2001
  • The fatigue test was carried out to evaluate the fatigue characteristics of fire resistance steel for frame structure and heat affected zone (HAZ) by the one side Gas Metal Arc Welding (GMAW). In this paper, the fatigue crack growth behavior was investigated with the compact tension specimen of base metal and the HAZ according to chemical composition and rolling end temperature, respectively. And the acoustic emission signals obtained from the fatigue test were analyzed by the time-frequency analysis method as a nondestructive evaluation. Main results obtained are summarized as follows; The hardness was appeared softening phenomenon that weld metal and HAZ are lower than that of base metal. Fatigue life of welded specimen was longer than that of base metal. m was 3~4.5 in base metal and 3.8~5.8 in HAZ. The main frequency range of acoustic emission signal analyzed from time-frequency method is different with the range by noise and crack. Also, it could be classified that it was also generated by fracture mechanics of dimple, inclusion etc.

  • PDF

304 스테인리스강이 고온 유동응력곡선과 미세 조직의 예측 (Prediction on Flow Stress Curves and Microstructure of 304 Stainless Steel)

  • 한형기;유연철;김성일
    • 소성∙가공
    • /
    • 제9권1호
    • /
    • pp.72-79
    • /
    • 2000
  • Dynamic recrystallization (DRX), which may occur during hot deformation, is important for the microsturctural evolution of 304 stainless steel. Especially, the current interest in modelling hot rolling demands quantitative relationships among the thermomechanical process variables, such as strain, temperature, strain rate, and etc. Thus, this paper individually presents the relationships for flow stress and volume fraction of DRX as a function of processing variables using torsion tests. The hot torsion tests of 304 stainless steel were performed at the temperature range of 900~110$0^{\circ}C$ and the strain rate range of 5x10-2~5s-1 to study the high temperature softening behavior. For the exact prediction of flow stress, the equation was divided into two regions, the work hardening (WH) and dynamic recovery (DRV) region and the DRX region. Especially, The flow stress of DRX region could be expressed by using the volume fraction of DRX (XDRX). Since XDRX was consisted of the critical strain($\varepsilon$c) for initiation of dynamic recrystallization (DRX) and the strain for maximum softening rate ($\varepsilon$*), that were related with the evolution of microstructure. The calculated results predicted the flow stress and the microstructure of the alloy at any deformation conditions well.

  • PDF

해양구조물용 TMCP강의 피로균열진전거동에 미치는 용접이방성 및 과대하중의 영향 (The effect of the excessive loading and welding anisotropy on the fatigue crack propagation behavior of TMCP steel for offshore structure)

  • 최성대;이종형
    • 한국생산제조학회지
    • /
    • 제9권6호
    • /
    • pp.82-88
    • /
    • 2000
  • The effect of the welding for the offshore structure in the TMCP steel on the fatigue crack propagation rate and crack opening-and-closure behavior was examined. The welding anisotropy of the TMCP steel and crack propagation characteristics of the excessive loading were reviewed. (1) It seemed that a heat which was generated by the welding made a compressive residual stress over the base metal, so fatigue crack propagation rate was placed lower than in case of the base metal. (20 In the base metal, an effect of the anisotropy which has an effect of fatigue crack propagation rate of the excessive load and the constant amplitude laos was not found but in the welding material case, fatigue crack propagation rate of the excessive load in the specimen of the width direction was located in the retard side as compared with a specimen rolling direction. (3) A crack opening ratio of the used TMCP stel in this study was not changed after excessive loading but a retard phenomenon of crack propagation was observed. Consequently, it was thought that all of the retard phenomenon of crack propagation did not only a cause of the crack opening-and-closure phenomenon.

  • PDF

HR Coil재 Box형 용접구조물의 피로강도평가에 관한 연구 (Fatigue Strength Evaluation of Welded Box Type with HR Coil)

  • 강성원;김명현;장용원;이진우
    • Journal of Welding and Joining
    • /
    • 제23권5호
    • /
    • pp.20-24
    • /
    • 2005
  • Due to the difficulties associated with the supply of steel plates, hot rolled coil (Steel grade: SM490A) is considered fur structural materials in replace of the existing SWS50A-M1. However, it is found that SM490A exhibits a significant anisotropy in terms of impact energy with respect to transverse and longitudinal directions. In this study, an experimental investigation is carried out to examine the relationship between the anisotropy in impact values and the fatigue strengths of SM490A with respect to the rolling direction of test specimens. All test specimens failed around 1,500,000 cycles regardless of the test specimen direction. Therefore, it is found that the anisotropy in impact energy is not related to the fatigue strength of the materials considered in this study. However, the transverse direction specimen showed more rapid brittle fracture mode compared to that of longitudinal direction specimen, and this appears to be related to the lower impact values in transverse direction.

Nb 첨가된 페라이트계 스테인리스강의 인장 및 부식 특성 (Tension and Corrosion Properties of Nb-added Ferritic Stainless Steel for Industrial Applications)

  • 한다인;카프란 기젬;최상규;조상헌;고영건
    • 소성∙가공
    • /
    • 제30권6호
    • /
    • pp.301-305
    • /
    • 2021
  • The role of Nb addition in the tension and corrosion responses of ferrite-based stainless-steel sheets processed by cold-rolling and annealing treatment at 1173 °K was studied to evaluate the possibility for commercialization. For this purpose, the grain sizes in the samples with and without Nb content were controlled to be reasonably identical by utilizing different heat treatments within the specific range for 60 seconds. The corrosion properties of both samples were evaluated based on the analysis of polarization curves. Room-temperature tension testing showed that the strength of the sample with Nb was much higher than that without Nb whereas the elongation of the sample with Nb was slightly lower than that without Nb. The polarization curves revealed that the addition of Nb contributed to the significant improvement in protective capabilities. We thought that such combinational behavior was mainly due to the formation of niobium carbides found in the ferritic matrix.