Ti/Al/STS 클래드재의 접합특성에 미치는 예비 열처리의 영향 (Effect of Pre-Heat Treatment on Bonding Properties in Ti/Al/STS Clad Materials)

  • 배동현;정수정;조영래;정원섭;정호신;강창룡;배동수
    • 대한금속재료학회지
    • /
    • 제47권9호
    • /
    • pp.573-579
    • /
    • 2009
  • Titanium/aluminum/stainless steel(Ti/Al/STS) clad materials have received much attention due to their high specific strength and corrosion-resisting properties. However, it is difficult to fabricate these materials, because titanium oxide is easily formed on the titanium surface during heat treatment. The aim of the present study is to derive optimized cladding conditions and thereupon obtain the stable quality of Ti/Al/STS clad materials. Ti sheets were prepared with and without pre-heat treatment and Ti/Al/STS clad materials were then fabricated by cold rolling and a post-heat treatment process. Microstructure of the Ti/Al and STS/Al interfaces was observed using a Scanning Electron Microscope(SEM) and an Energy Dispersed X-ray Analyser(EDX) in order to investigate the effects of Ti pre-heat treatment on the bond properties of Ti/Al/STS clad materials. Diffusion bonding was observed at both the Ti/Al and STS/Al interfaces. The bonding force of the clad material with non-heat treated Ti was higher than that with pre-heat treated Ti before the cladding process. The bonding force decreased rapidly beyond $400^{\circ}C$, because the formed Ti oxide inhibited the joining process between Ti and Al. Bonding forces of STS/Al were lower than those of Ti/Al, because brittle $Fe_3Al$, $Al_3Fe$ intermetallic compounds were formed at the interface of STS/Al during the cladding process. In addition, delamination of the clad material with pre-heat treated Ti was observed at the Ti/Al interface after a cupping test.

Mg/Al/STS 3층 클래드재의 기계적 특성에 미치는 계면반응층의 영향 (Effect of Interfacial Reaction Layer on Mechanical Properties of 3-plyMg/Al/STS Clad-metal)

  • 김인규;송준영;이영선;홍순익
    • 대한금속재료학회지
    • /
    • 제49권8호
    • /
    • pp.664-670
    • /
    • 2011
  • 3-ply Mg/Al/STS clad-metal was fabricated by the roll bonding process. An interfacial reaction layer was formed at the Mg/Al interface at and above $300^{\circ}C$ whereas no interfacial reaction layer was observed up to $400^{\circ}C$. The effect of the interfacial reaction layer on the mechanical and fracture properties in clad metals after heat treatments were investigated The chemical compositions were analyzed at the Mg/Al interface by an Energy dispersive X-ray analysis (EDX). A tension test was performed to examine the interfacial cracking properties. The Mg layer fractured first, causing a sudden drop of the stress and Al/STS layer continued to deform until the final fracture. Periodic cracks and crack propagation was observed at the reaction layer between Mg and Al.

압연에 의한 STS/AI/STS 클래드판재 제조시 롤과 STS 사이의 마찰의 영향 (The Effect of friction between Roll and STS the Roll Cladding Behavior of STS/Al/STS Sandwich Sheet)

  • 정영훈;지광구;서진유;신명철
    • 소성∙가공
    • /
    • 제11권6호
    • /
    • pp.482-486
    • /
    • 2002
  • Sandwich sheets composed of stainless steel/aluminum/stainless steel were produced by roll cladding. In order to investigate the effect of the friction between roll and cladding sample, the lubrication condition of the roll surface was varied. Clad rolling without lubrication gave rise to a small increment of the normal strain of aluminum in the rolling direction. This experimental result was confirmed by FEM modeling. Through-thickness hardness gradients in the mid aluminum layer was successfully explained by variations of the strain state through thickness layers. FEM modeling implied that cladding without lubrication led to a large shear strain variation at the surface of aluminum layer.

굽힘시험시의 Mg/Al/STS 3층 클래드재의 변형 및 파단특성 분석 (Failure and Deformation Analyses of 3-ply Mg/Al/STS Clad-Metalin Bending)

  • 김인규;송준영;오기환;홍순익
    • 대한금속재료학회지
    • /
    • 제50권5호
    • /
    • pp.345-351
    • /
    • 2012
  • A three-point bending test was performed on roll-bonded Mg/Al/STS clad-metal plates under two different testing conditions (Mg layer in tension, or STS in tension) and their mechanical response and fracture behavior were investigated. Bending strength was found to be greater under the condition of Mg layer in tension. Heat treatment at $200^{\circ}C$ increased the bending formability, suggesting the interfacial strength increased at $200^{\circ}C$. Under the condition of Mg in tension, the clad heat-treated at $300^{\circ}C$ and $400^{\circ}C$ fractured in two steps, with the first step associated with the interfacial fracture between Mg and Al, and the second the fracture of the Mg layer. STS/Al layers were found to be bent without complete fracture. Under the condition of STS in tension, the clad heat-treated at $300^{\circ}C$ and $400^{\circ}C$ exhibited a very small load drop at the displacement, which is similar to that of the first load drop associated with the interfacial fracture under the condition of Mg in tension. In this case, no interfacial cracks were found and the complete cut-through fracture of clad was observed at low temperature heat treatment conditions, suggesting excellent interfacial strength. When the heat treatment temperature was higher than $300^{\circ}C$, interfacial cracks were observed. The local stress condition and the position of the interface with respect to the surface were found to have a great influence on the fracture behaviors of clad metals.

316계 스테인리스강과 소듐 냉각재와의 양립성 연구 (Compatibility Study between 316-series Stainless Steel and Sodium Coolant)

  • 김준환;김종만;차재은;김성호;이찬복
    • 대한금속재료학회지
    • /
    • 제48권5호
    • /
    • pp.410-416
    • /
    • 2010
  • Studies were carried out to establish the technology for sodium-clad compatibility and to analyze the compatibility behavior of the Sodium-cooled Fast Reactor (SFR) cladding material under a flowing sodium environment. The natural circulation facility caused by the thermal convection of the liquid sodium was constructed and the 316-series stainless steels were exposed at $650{^{\circ}C}$ liquid sodium for 1458 hours. The weight change and related microstructural change were analyzed. The results showed that the quasi-dynamic facility represented by the natural convection exhibited similar results compared to the conventional dynamic facility. Selective leaching and local depletion of the chromium, re-distribution of the carbide, and the decarburization process took place in the 316-series stainless steel under a flowing sodium environment. This process decreased as the sodium flowed along the channel, which was caused by the change in the dissolved oxygen and carbon activity in the liquid sodium.

STS/Al/Cu 클래드재의 파괴거동 및 기계적 물성에 미치는 인장시험 온도의 영향 (Effect of Tension-Test Temperature on Fracture Behavior and Mechanical Properties in STS/Al/Cu Clad Materials)

  • 배동현;최영준;정원섭;배동수;조영래
    • 대한금속재료학회지
    • /
    • 제47권12호
    • /
    • pp.811-818
    • /
    • 2009
  • In order to meet increasingly complex and rigorous technical specifications, extensive effort has been devoted to fabricate clad materials with multi-layered metal plates. In this study, novel stainless steel/aluminum/copper (STS/Al/Cu) three-ply clad materials were fabricated by a hot rolling process for cookware applications. The effect of the testing temperature on the mechanical properties of the clad materials and on each component metal was investigated during the tensile tests. The interface properties of the clad materials were also examined by optical microscopy (OM) and an electron probe micro-analyzer (EPMA). The best mechanical and interfacial properties for a warm working process were found in a sample annealed at a temperature of $300^{\circ}C$. For the sample annealed at $400^{\circ}C$, the results of the tensile test indicated that interface delamination occurred only in the region of the Al/Cu interfaces. This was due to the formation of the thick and brittle intermetallic compound of $Al_2Cu$ in the Al/Cu interface. In contrast, no interface delamination was observed in the STS/Al interface, most likely due to its strong bond strength.

Evaluation and Development of Corrosion Resistant Materials for Smokestacks

  • Ebara, Ryuichiro
    • Corrosion Science and Technology
    • /
    • 제6권4호
    • /
    • pp.211-218
    • /
    • 2007
  • In this paper, evaluation and development of corrosion resistant materials for smokestacks is summarized mainly on the basis of the author's experimental results. Operating environments of smokestacks and the problems of conventional lining materials for smokestacks are described briefly. The emphasis is focused upon the evaluation and development of recently developed corrosion resistant steels such as YUS260 for heavy oil fired smokestacks, WELACC5 for LNG fired smokestacks and NSL310MoCu Clad steel for coal fired smokestacks. Corrosion resistance of these steels under laboratory corrosion testing environments and actual environments are evaluated. Finally future problems of corrosion resistant materials for smokestacks are touched on briefly.

집합조직 분석에 의한 5겹 STS/Al 복합재 클래드 압연 시 변형상태 해석 (Interpretation of Strain States during Clad-Rolling of STS/Al 5 Ply Composites by Means of Texture Analysis)

  • 강형구;박준수;박수호;허무영
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.303-306
    • /
    • 2005
  • Two composites of five plies of STS/Al/Al/Al/STS and STS/Al/STS/Al/STS were produced by roll-cladding at $350^{\circ}C$ from ferritic stainless steel (STS) and aluminum (Al) sheets. In order to analyze the strain states during roll-cladding, the evolution of textures at different through-thickness positions in the roll-clad composites was investigated. Simulations with the finite element method (FEM) disclosed that a strain state which was similar to that of normal rolling with a high friction between roll surface and Al sample led to the formation of texture gradients in the Al sheets in the STS/Al/Al/Al/STS composite. Differences in the material velocity of STS and Al in the rolling direction gave rise to the formation of the shear texture in the Al sheets in the STS/Al/STS/Al/STS composite.

  • PDF

히트 싱크용 클래드메탈에서 두께 방향의 열전도 특성에 미치는 계면의 영향 (Effect of Interface on Thermal Conductivity of Clad Metal through Thickness Direction for Heat Sink)

  • 김종구;김동용;김현;한병동;조영래
    • 마이크로전자및패키징학회지
    • /
    • 제22권3호
    • /
    • pp.67-72
    • /
    • 2015
  • 히트 싱크용 소재에 응용할 목적으로 단층금속과 2층금속 클래드메탈에 대해 열전도 특성에 대한 연구를 하였다. 단층시편으로는 스테인리스강과 알루미늄을 선택하였으며, 2층 금속으로는 스테인리스강과 알루미늄을 압연해서 제조한 클래드메탈을 사용하였다. 열전도도는 섬광법으로 측정한 열확산계수와 비열 및 밀도를 사용해 얻었다. 실험을 통해 얻은 측정값을 참고문헌에 보고된 자료를 사용해 얻은 계산값과 비교하였다. 단층시편의 경우, 실험을 통해 얻는 열확산계수와 열전도도는 계산값보다 작았다. 스테인리스강의 경우, 측정한 열전도도는 계산값에 비해 6% 정도 작았으며, 알루미늄의 경우 18% 정도 작았다. 반면, 2층 금속인 스테인리스강과 알루미늄의 클래드메탈은 측정한 열전도도가 계산값에 비해 55% 정도 낮게 나타났다. 섬광법으로 측정한 열전도도가 계산값보다 55% 정도 낮게 나타난 이유는 스테인리스강과 알루미늄의 사이에 존재하는 계면의 영향 때문이다. 스테인리스강과 알루미늄의 사이에 존재하는 계면은 열전도 특성을 지배하는 전자와 탄성파의 이동을 어렵게 하기 때문이다. 우수한 방열특성을 갖는 다층구조 방열모듈을 개발하기 위해서는 열전도 특성에 결정적으로 영향을 주는 계면 특성의 조절이 중요하다.

압력용기용 SA508 class3강에 대한 underclad 균열의 감수성 평가 - 입열량의 최적화 (Evaluation of Underclad Crack Susceptibility of the SA508 Class 3 Steel for Pressure Vessels -Optimization of Heat Input-)

  • 김석원;양성호;김준구;이영호
    • Journal of Welding and Joining
    • /
    • 제13권2호
    • /
    • pp.139-149
    • /
    • 1995
  • Many pressure vessels for the power plants are fabricated from low alloy ferritic steels. The inner sides of the pressure vessels are commonly weld_cladded with austenitic stainless steels to minimize problems of corrosive attack. The submerged-arc welding(SAW) process is now used in preference to other processes because of the possibilities open to automation to reduce the overaII welding times. The most reliable way to avoid underclad cracks(UCC) which are often detected at the overlap of the clad beads is to use nonsusceptible steels such as SA508 class 3. At present domestically developed forging steel of SA508 cl.S is now being cladded with single layer by using 90mm wide strip, which transfers higher heat input into the base metal compared to the conventional two layers strip cladding which has been in wide use with 30-60 mm wide strip. But the current indices for the influence of heat input on crack susceptibility are not accurate enough to express the subtle difference in crack susceptibility of the steel. Therefore, the purpose of this present study is: l) To determine UCC susceptibility on domestic forging steel, SA508 cl.S cladded with single layer by using submerged arc 90mm strip and, 2) To optimize heat input range by which the crack susceptibility could be eliminated.

  • PDF