수산염법으로 합성한 $SrTiO_3$ 소결체의 유전특성에 관한 연구 (A Study on the Dielectric Properties of $SrTiO_3$ Sintered Body Synthesized by Oxalate Method)

  • 김병호;이만규;김석우
    • 한국세라믹학회지
    • /
    • 제28권3호
    • /
    • pp.215-224
    • /
    • 1991
  • The synthesis of SrTiO3 powders having high purity and homogeneous submicron particle size was attempted by the oxalate method. The microstructure and dielectric properties of SrTiO3 based boundary layer capacitor (BLC) were investigated. Strontium titanyl oxalate[SrTiO(C2O4)2.4H2O] was prepared from the mixing solution of (Sr, Ti) using oxalic acid(H2C2O4) as a precipitating agent at 8$0^{\circ}C$. The crystalline SrTiO3 powder was obtained by thermal decomposition of the precipitate above $600^{\circ}C$. The crystalline SrTiO3 powder containing Nb2O5 as a dopant, TiO2 and SiO2 as additives was sintered at 1360~144$0^{\circ}C$ in the reducing atmosphere to get semiconductive SrTiO3. Insulating material containing PbO-Bi2O3-B2O3 frit was printed on the sintered semiconductive SrTiO3 and fired at 120$0^{\circ}C$ for 2h to get the grain boundary diffusion.

  • PDF

$0.96MgTiO_3-0.04SrTiO_3+xLa(0{\sim}1.0wt%)$ 세라믹스의 마이크로파 유전 특성 (The Microwave Dielectric Properties of $0.96MgTiO_3-0.04SrTiO_3+xLa(0{\sim}1.0wt%)$ Ceramics)

  • 박보근;임성수;김강;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.118-120
    • /
    • 2001
  • The $0.96MgTiO_3-0.04SrTiO_3+xLa(0{\sim}1.0wt%)$ ceramics were prepared by conventional mixed oxide method. The structural properties of $0.96MgTiO_3-0.04SrTiO_3+xLa(0{\sim}1.0wt%)$ ceramics with sintering temperature were investigated by the XRD and SEM. From the X-ray diffraction patterns, it was found that the perovskite $SrTiO_3$ and ilmenite $MgTiO_3$ structures were coexisted in the $0.96MgTiO_3-0.04SrTiO_3$ ceramics. The second phase of $Sr_{0.5}LaTi_2O_6$ was shown with addition of the $La_2O_3$. The dielectric constant(${\varepsilon}_r$), $Q{\times}f$ value and the temperature coefficient of the $0.96MgTiO_3-0.04SrTiO_3+0.2La$ ceramics were 21. 41, 39991, $-3.3ppm/^{\circ}C$, respectively.

  • PDF

$BaTiO_3/SrTiO_3$ 이종층 박막/후막의 유전특성 ($BaTiO_3/SrTiO_3$ Heterolayered Thin/Thick films Dielectric Properties)

  • 한상욱;김지헌;박인길;이성갑;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2005년도 제36회 하계학술대회 논문집 C
    • /
    • pp.1850-1852
    • /
    • 2005
  • $SrTiO_3$ and $BaTiO_3$ sol-liquids and powders were prepared by the sol-gel method. $SrTiO_3/BaTiO_3$ heterolayered thin/thick films have been prepared on the $Al_2O_3$ substrates by screen printing and spin-coating method. The thin films were sintered at $750^{\circ}C$ in the air for 1 hour and the thick films sintered at $1325^{\circ}C$ in the air for 2 hours, respectively. The $SrTiO_3/BaTiO_3$ thin/thick films's structural and dielectric properties were investigated. Increasing the spin-coating times, (110), (200), (211) peaks of the $SrTiO_3$ were increased. The X-ray diffraction(XRD) patterns and SEM photographs indicated that the $SrTiO_3$ phase were formed in the surface of $BaTiO_3$ thick films. The average thickness of a $BaTiO_3$ thick films and $SrTiO_3$ thin films were $50{\mu}m$ and 400nm, respectively The dielectric constant and dielectric loss of the $SrTiO_3/BaTiO_3$ thin/thick films with $SrTiO_3$ coated 5 times were 1598 and 0.0436 at 10KHz.

  • PDF

$Nb_2O_5$를 첨가한 $SrTiO_3$의 비정상 입성장에 미치는 Ti/Sr 비의 영향 (The Effect of Ti/Sr Ratio on Abnormal Grain Growth of Nb-doped $SrTiO_3$)

  • 배철휘;전형탁;박재관;김윤호
    • 한국세라믹학회지
    • /
    • 제34권8호
    • /
    • pp.791-796
    • /
    • 1997
  • The influence of Ti/Sr ratio on abnormal grain growth of Nb-doped SrTiO3 was investigated. For specimens which were isothermally sintered at temperatures above 144$0^{\circ}C$, the nucleation and growth rates of abnormal grain growth were decreased with increasing Ti/Sr ratio. But the onset time of abnormal grain growth was increased with increasing Ti/Sr ratio. The cross-section of abnormally grown grains was mostly hexagonal. When the specimens were quenched in air after they reached their setting temperatures at a heating rate of 3$^{\circ}C$/min, the onset temperature of abnormal grain growth was increased with increasing Ti/Sr ratio and the final grain size was independent of Ti/Sr ratio. The cross-section of abnormally grown grains was mostly rectangular.

  • PDF

Crystalline Phases and Dielectric Properties of Crystallized Glasses in the System (Ca, Sr, Ba) O-Al2O3-B2O3-SiO2-TiO2

  • Tuzuku, Koichiro;Kishi, Hiroshi;Taruta, Seiichi;Takusagawa, Nobuo
    • The Korean Journal of Ceramics
    • /
    • 제5권2호
    • /
    • pp.189-194
    • /
    • 1999
  • Crystallization of glasses in the system (Ca, Sr, Ba)$O-Al_2O_3-B_2O_3-SiO_2-TiO_2$ and dielectric properties of crystallized glasses were investigated. As increasing B2O3 content and decreasing SiO2 content in the glass, the major crystalline phase changed from $(Sr, Ba)_2TiSi_2O_8$ to (Ca, Sr, Ba)TiO3, the dielectric constant of crystallized glasses increased and the Temperature Coefficient of Capacitance (TCC) changed to negative. The dielectric constant and TCC was estimated for (Sr, Ba)2TiSi2O8 phase as 18 and -440 $ppm/^{\circ}C$, respectively and for (Ca, Sr, Ba)TiO3 phase as 307 and -1900 $ppm/^{\circ}C$, respectively. The dielectric properties of (Ca, Sr, Ba)TiO3 phase (in this study) were similar to those of (Ca, Ba) TiO_3 solid-solution^12)$, but $(Sr, Ba)_2TiSi_2O_8$ phase (in this study) and $Sr_2TiSi_2O_\;8^4$ showed the different properties.

  • PDF

A Tailored Investigation for $(Ba,Sr)TiO_3$ FGMs

  • Jeon, Jae-Ho
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.289-290
    • /
    • 2006
  • [ $SrTiO_3$ ] is usually added as shifters in order to move the $T_C$ of $BaTiO_3$ to lower temperatures because it is well established that the $T_C$ of $BaTiO_3$ decreases linearly with a solid solution of $Sr^{+2}$ in place of $Ba^{+2}$. It is not fully understood yet, however, how $SrTiO_3$ influences on the peak value of the dielectric constant $(\varepsilon_{max})$ at the $T_C$ of $BaTiO_3$. This research reports the effect of $SrTiO_3$ addition on εmax at the $T_C$ of $BaTiO_3$ ceramics. Based on the chemical composition and the grain size dependence of the dielectric property of $BaTiO_3$ ceramics, functionally graded $(Ba,Sr)TiO_3$ composites were designed and fabricated. Multi-layered $(Ba,Sr)TiO_3$ composites with a compositional gradient of $SrTiO_3$ exhibited a low temperature coefficient and high dielectric constant in a wide temperature range.

  • PDF

소결온도에 따른 $0.9MgTiO_3-0.1SrTiO_3$ 세라믹스의 구조 및 마이크로파 유전특성 (Structural and Microwave Dielectric Properties of the $0.9MgTiO_3-0.1SrTiO_3$ Ceramics with Sintering Temperature)

  • 최의선;이문기;류기원;배선기;이영희
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제49권5호
    • /
    • pp.294-298
    • /
    • 2000
  • The $MgTiO_3\; and \;$0.9MgTiO_3-0.1SrTiO_3$ ceramics were fabricated by the conventional mixed-oxide method. The sintering temperature and time were $1300^{\circ}C~1600^{\circ}C$, 2hr., respectively. The structural and microwave dielectric properties were investigated with sintering temperature and the application for the satellite communication microwave dielectric resonator was investigated. The coexistence of cubic $SrTiO_3$ and hexagonal TEX>$MgTiO_3$ structures in $0.9MgTiO_3-0.1SrTiO_3$ ceramics were found from X-ray diffraction patterns. In the case of $MgTiO_3$ ceramics, sphere phase and needle-like phase were coexisted. The $0.9MgTiO_3-0.1SrTiO_3$ ceramics observed sphere phase. The dielectric constants and temperature coefficient of resonant $frequency(\tauf)$ were increased with addition of $SrTiO_3$ but the quality factor was decreased. The dielectric constant, quality factor and $\tau$f of the;$0.9MgTiO_3-0.1SrTiO_3$ ceramics were 22.61, 10.928(at 1GHz) and $+50.26ppm/^{\circ}C$, respectively.

  • PDF

제일원리적 계산에 의한 격자 변형된 Sr$TiO_3$$BaTiO_3$ 격자의 optical phonon mod와 Born effective charge의 특성 (First-principle study: Optical phonon mode and Born effective charge of strained Sr$TiO_3$ and $BaTiO_3$ lattices)

  • 김이준;정동근;김주호;이재찬
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2003년도 추계학술발표강연 및 논문개요집
    • /
    • pp.55-55
    • /
    • 2003
  • Ferroelectric 물질은 고유전성, 자발분극과 전기장에 따른 유전상수의 변화 등의 특성을 가지고 있으므로 많은 연구가 진행중이다. 이러한 ferroelectric 물질의 유전 특성에 미치는 요소로는 물질의 조성비, 박막의 스트레스, 결정성 등이 있다. 특히 스트레스에 대한 연구가 활발히 진행중이다. 본 연구에서 산화물 인공격자를 이용하여 단일박막에서 얻을 수 없는 격자변형도를 얻어 격자 변형이 박막의 유전특성에 미치는 영향을 연구하였다. BaTiO$_3$ (BTO)/SrTiO$_3$ (STO) 산화물 인공격자를 Pulsed laser deposition (PLD)법으로 (La,Sr)CoO$_3$ 전극이 코팅된 MGO (100) 단결정 기판위에 증착시켰다. 적층 주기에 변화를 주어 BTO와 STO 각각 1.01~1.095와 0.925 ~ 1.003의 단일 막에서는 얻을 수 없는 격자 변형도를 얻었다. 이 실험적 데이터를 기초로 하여 density functional theory (DFT)라고 불리는 범함수밀도론를 기초한 제일원리적 계산 방법을 통하여 격자 변형된 SrTiO$_3$의 구조적, 전기적 특성을 계산하였다. SrTiO$_3$와 BaTiO$_3$ 격자의 안정성을 분석하기 위하여 Vienna Ab-intio Simulation Package (VASP) code가 사용되었다. SrTiO$_3$와 BaTiO$_3$ 산화물 격자의 안정성 분석 후, frozen-phonon 계산 방법을 사용하여 zone-centered optical phonon mode가 계산되었으며, mode effective charge는 Berry-phase polarization 으로부터 얻어졌다. SrTiO$_3$ 격자가 격자변형이 일어나지 않은 상태로부터 c/a= 0.985로 격자 변형 이 일어남에 따라 optical phonon mode는 점차 hardening되었다. BaTiO$_3$ 격자의 경우 SrTiO$_3$ 격자와는 달리 격자 변형이 1.01~1.023으로 진행됨에 따라 optical phonon mode의 증가를 가져왔으나 Born effective charge의 증가하였으며, 더 이상 격자 변형이 진행됨에 따라 optical phonon mode의 감소를 가져왔으나 Born effective charge의 증가 유전상수는 증가했다. 격자 변형이 SrTiO$_3$ 와 BaTiO$_3$ 산화물 격자의 optical phonon mode와 Born effective charge에 크게 영향을 미쳤다.

  • PDF

소결온도에 따른 $0.94MgTiO_3-0.06SrTiO_3$ 세라믹스의 구조 몇 마이크로파 유전특성 (Structural and Microwave Dielectric Properties of the $0.94MgTiO_3-0.06SrTiO_3$ Ceramics with Sintering Temperature)

  • 최의선;이문기;박인길;류기원;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 춘계학술대회 논문집 전자세라믹스 센서 및 박막재료 반도체재료 일렉트렛트 및 응용기술
    • /
    • pp.60-63
    • /
    • 2000
  • The $0.94MgTiO_3-0.06SrTiO_3$ ceramics were prepared by the conventional mixed oxide method. The structural properties were investigated with sintering temperature and composition ratio by XRD, SEM and DT-TGA. According to the X-ray diffraction patterns of the $0.94MgTiO_3-0.06SrTiO_3$ ceramics, the cubic $SrTiO_3$ and hexagonal $MgTiO_3$ structures were coexisted. Increasing the sintering temperature from $1325^{\circ}C$ to $1400^{\circ}C$, average grain size was increased from $5.026{\mu}m$ to $8.377{\mu}m$. In the case of the $0.94MgTiO_3-0.06SrTiO_3$ ceramics sintered at $1325^{\circ}C$, dielectric constant, quality factor and temperature coefficient of resonant frequency were 21.66, 2,522(at 7.34GHz), $+71ppm/^{\circ}C$, respectively.

  • PDF

$SrTiO_3$ 고용에 따른 $(x)BaTiO_3-(1-x)SrTiO_3$ 세라믹의 전기적 특성 (Electrical Properties of $(x)BaTiO_3-(1-x)SrTiO_3$ Ceramic with Variation of $SrTiO_3$ Substitution)

  • 장동환;기현철;홍경진;정우성;김태성
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1998년도 추계학술대회 논문집 학회본부 C
    • /
    • pp.795-797
    • /
    • 1998
  • A $BaTiO_3$, ferroelectric material, was mixed $SrTiO_3$, $(x)BaTiO_3-(1-x)SrTiO_3$($0.7{\leq}x{\leq}1$) ceramic capacitor with stable electrical properties in high voltage was fabricated. And microstructure, electrical property were investigated with $SrTiO_3$ mol ratio. The shrinkage, open porosity, sintering density were predominated at $9BaTiO_3-0.1SrTiO_3$. Increasing $SrTiO_3$ mol ratio, curie temperature was shifted at low temperature and maximum permittivity was increased. Also, $0.9BaTiO_3-0.1SrTiO_3$ was showed stable dielectric properties at $25{\sim}80[^{\circ}C]$. V-I properties of specimen were observed in the temperature range of $21{\sim}143[^{\circ}C]$, were divided into three regions. The region I below 10[kV/cm] was shown Ohmic conduction, the region II from 10 to 30[kV/cm] was explained by the Poole-Frenkel emission theory and the region III above 30[kV/cm] was analysed by the tunneling effect.

  • PDF