Magnetic Properties of Sr-ferrite Powders via Modified Low Temperature Co-spray Roasting Process (저온 분무 열분해법으로 제조된 Sr-ferrite의 자기특성)

  • 김효준;조태식;남효덕;양충진
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.11 no.10
    • /
    • pp.931-939
    • /
    • 1998
  • Preparation of the hexagonal Sr-ferrite powsers with high performance by co-spraying precusor of the FeCl$_2$+SrCO$_3$ at a low temperature was proved as a cost =-effective method. The co-spray roasting was carried out in the temperature range of 300~$700^{\circ}C$ after SrCO$_3$ powders were mixed into 12FeCi$_2$.4$H_2O$ liquor. By this low temperature roasting method fine particles of multi-phased FeO$_2$+SrCO$_3$ were formulated. Powders calcined at 105$0^{\circ}C$ for 1 hour show the best magnetic property of M\ulcorner=69.96 emu/g, M\ulcorner=36.98 emu/g, and \ulcornerH\ulcorner=4.31 Oe. This calcining temperature is lower than that of the conventional dry method by 10$0^{\circ}C$.

  • PDF

Formulation and Magnetic properties of Sr-ferrite powders by Modified spray co-roasting (단순화된 분무열분해법을 이용한 Sr-ferrite 제조와 자기특성)

  • 김효준;조태식;남효덕;양충진
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1998.06a
    • /
    • pp.49-52
    • /
    • 1998
  • Preparation of hexagonal strontium-ferrite by modified spray co-roasting(MSC:H) which is expected to shorkn the length of the process and to elevate the magnetic properties of hard ferrite was studied. We prapared $Fe_2O_3/SrCO_3$ mixture powders by MSCR after stirring ionized $FeCI_2$ in distilled water with solid state $SrCO_3$. And then calcined the mixture powders up to $1150^{\circ}C$ for Sr-ferrite powders It is possible to prepare hexaferrite powders with high saturation magnetization (Ms > 69 emu/g) , coercivity (Hc > 4000 Oe) The nlagnetic values of saturation magnetization iire higher than those achieved by the conventional technique.

  • PDF

Effect of Reaction Factors on the Properties of Complex Oxide Powder Produced by Spray Roasting Process (분무배소법에 의해 생성되는 복합산화물 분말들의 특성에 미치는 반응인자들의 영향)

  • 유재근;이성수;박희범;안주삼;남용현;손진군
    • Resources Recycling
    • /
    • v.9 no.4
    • /
    • pp.16-27
    • /
    • 2000
  • In order to produce raw material powder of advanced magnetic material by spray roasting process, newly modified spray roasting system was developed in this work. In this spray roasting system, raw material solution was effectively atomized and sprayed into the reaction furnace. Also, uniform temperature distribution inside reaction furnace made thermal decomposition process fully completed, and produced powder was effectively collected in cyclone and bag filter. This system equipped with apparatus which can purify hazard produced gas. In this study complex acid solution was prepared by dissolution of mill scale and ferro-Mn into the acid solution, and the pH of this complex acid solution was controlled about to 4. It was conformed that mill scale and ferro-Mn containing a lot of impurities such as $SiO_2$, P and Al could be used as raw material by reducing the impurities content of complex acid solution below 20 ppm. Complex oxide powder of Fe-Mn system was produced by spraying purified complex acid solution into the spray roaster through nozzle, and the variations of produced powder characters were studied by changing he reaction conditions such as reaction temperature, the injection velocity of solution and air, nozzle tip size and concentration of solution. The morphology of produced powder had spherical shape under the most experimental conditions, and concentration of solution. The morphology of produced powder has spherical shape under the most experimental conditions, and the composition and the particle size distribution were almost uniform, which tells the excellence of this spray roasting system. The grain size of most produced powder was below 100 nm. From the above results, it will be possible to produce ultra fine oxide powder from the chloride of Fe, Mn, Ni, Cu and rare earth by using this spray roasting system, and also to produce ultra fine pure metal powder by changing reaction atmosphere.

  • PDF

Study on the Manufacturing Process of Complex Oxide by Co-Roasting Process and Magnetic Properties Mn-Zn Ferrite (분무 배소법에 의한 복합산화물의 제조공정 및 Mn-Zn ferrite의 자기 특성에 관한연구)

  • 유재근;이경익;이성수
    • Resources Recycling
    • /
    • v.8 no.4
    • /
    • pp.45-56
    • /
    • 1999
  • The purpose of tlus sludy was to preparc raw material powder for Mn-Zn iclrile, h m mined mill scale and fero-Mn, usins a co-spray roasting process The mill scale and ferra-Mn uscd in this raalins process was rcf~nedb y mesn-ns of a slxc~apl rxcss ~nvolvinm~a te~ialsc ontalning imp~u-ltleso r less than 100 pprn In this study an effeclive spray roaster system. wllich produces fme complex oxide powder, collects produccd ~owder.,m d prcvel~tse ~~llssiooifi HCI gas. was also manufactured. By means of spray~ngp urifcd raw malerial solu~lionl nln a manufacued high tcmpervture rumace. &-ferrite powder and a comnpleu o ~ d e powder of Fe,O; and M,x203 were manufactured. The chmcterlstics of the composllion. surface urca, and p'miicle size dismbulion or the produced powder were exmined. ptoduced powdcr was then ~ m e dwi tli ZnO powder. aid olher addilives of defined cornposnion, and Mn-Zn femite cares werc praiuccil by meuns of Sorlning and closely controlled sintering processes. The magpelic p~oprlieso f c olo~ss, initlal permeability. mauin~u~mnn agnehc flux. coz~civcr orcc and residual magnccic flux for the above cores we,= measured, and fmm Il~ase I-csulls the eflicacy of lhe co-spray roasling pncess to pl.ellare raw material powder lor Mn-Zn ferntc was established

  • PDF

Purification of Waste Acid and Manufacture of Complex Oxide and Mn-Ferrite Powder by Co-Roasting Process (폐산의 정제 기술 및 분무 배소법에 의한 복합 산화물과 Mn-Ferrite 분말의 제조)

  • 유재근;김정석;민병구;성낙일
    • Resources Recycling
    • /
    • v.7 no.4
    • /
    • pp.64-75
    • /
    • 1998
  • The purpose of this study is to produce high putity composite powder composed of Fe-oxide, Mn-oxide and Mn-ferrite having superior homogencity in composition and particle size distribution by co-roasting process. Binary component metal (Fe, Mn) chloride solutions were produced by dissolving mill scale and ferro-mangancse alloy in hydrochloric acid. These chloride solutions contained the impurities such as SiO$_{2}$, P, Al, Ca and Na, which were originated from the Fe/Mn source materials. The neutralization and polymeric coagulant method were adoped to refine the hydrochloric liquor. When pH is far below the isoelectric point (pH 2-3), the SiO$_{2}$ was the most effectively reduced element, while other impurities remained unchanged. By increasing pH above 3, most of the impurities could be reduced effectively due to the coprecipitation reaction. The polymeric coagulants such as poly vinyl alcohol, resin amine and ammonium molybdate were found to have no effect on the spray roaster designed by the authors. The produced oxide powders were confirmed to be mixtures of Fe-oxide, Mn-oxide and mn-ferrite. the powders were homogeneously mixed and the particle size increased sleeply with increasing co-roasting temperature.

  • PDF

Making Process for Magnetite Powder (Magnetite 분말의 제조)

  • Ho-Sang Lee;Kyu-Jin Kim
    • Resources Recycling
    • /
    • v.9 no.5
    • /
    • pp.28-32
    • /
    • 2000
  • In this study, the new processing method to produce magnetite for mono-component black toner was studied using spray roaster. The produced magnetite is compared with TMB 125 made by Magnox, USA. When the weight ratio of the ferrous chloride and the ferric chloride is varied from 3:7~7:3 under $N_2$ atmosphere, the 100% major phase of magnetite is obtained. However, when the content of he ferrous chloride is higher than 70wt%, the content of FeO is increased. The phase of $\Gamma-Fe_2O_3$ is shown in th range of over 70wt% of the ferric chloride. The magnetite produced by spray roasting has a saturation magnetization of 80~85 emu/g and a coercivity of 110~130 Oe. The shape of the particle is irregular sphere and hte size of the magnetite is the range of $0.3~0.5\mu\textrm{m}$. It is shown that the magnetite made by spary roasting is enough to apply to the magnetic material of toner.

  • PDF