• 제목/요약/키워드: Spheroidal graphite cast iron

검색결과 62건 처리시간 0.022초

저사이클 피로수명에 영향을 미치는 구상흑연주철의 흑연입자수의 영향 (Effect of the Number of Nodular Grains on Low Cycle Fatigue Life in Spheroidal Graphite Cast Iron)

  • 김민건;이병현;유병호
    • 산업기술연구
    • /
    • 제20권B호
    • /
    • pp.3-8
    • /
    • 2000
  • Low cycle fatigue life of spheroidal graphite cast iron is determined by the morphological parameters of internal graphite. The aim of this study is to clarify the effect of the number of nodular grain of spheroidal graphite cast iron on low cycle fatigue life. Two specimens that have identical average nodular grain size by changing nodular grain volume fraction and different number of nodular grain count was tested. In this paper, the parameter governing fatigue life through fatigue test, the number of nodular grain seriously affect fatigue life and nodular grain size is no longer governing parameter of it.

  • PDF

구상흑연주철재의 화상해석에 의한 흑연의 극치통계 평가 (Evaluation of Statistical distribution of extreme values of Graphite in Ductile Cast Iron by Image Analyzer)

  • 윤명진
    • 한국기계가공학회지
    • /
    • 제9권6호
    • /
    • pp.71-77
    • /
    • 2010
  • Although the problems of defects and nonmetallic inclusion in metal fatigue are very complicated, it is particularly important to view these problems from the perspective that defects and inclusions are virtually equivalent to small cracks. This concept will help one to understand various fatigue phenomena caused by Ductile Cast Iron. For different ferrite-pearlite matrix structure, containing more than 90% spheroidal ratio of graphite, GCD 45-3, GCD 50, GCD 60 series and 70%, 80%, 90% spheroidal ratio of graphite, GCD 40, GCD 45-1, GCD 45-2 series, this paper has carried out image analyzer, estimated maximum and mean size of graphite, investigated correlation. It was concluded as follows. (1) A good quality of Ductile cast iron using in this experiment, the graphite was separated well. The effect of the interaction by graphite was verified by microscopic observation and by fracture mechanics investigation in surface, interior of the specimen. (2)${\sqrt{area}}_{max}$ of graphite can be used to predict fatigue limit of Ductile Cast Iron. The Statistical distribution of extreme values of ${\sqrt{area}}$ may be used as a guide line for the control of inclusion size in the steel making processes.

삽입금속을 사용한 구상흑연주철과 2024 알루미늄합금의 마찰압접에 관한 연구 (Friction Welding of Spheroidal Graphite Cast Iron and 2024 Aluminium Alloys using Insert Metal)

  • 김창규;김치옥;김광일
    • 한국해양공학회지
    • /
    • 제17권5호
    • /
    • pp.76-81
    • /
    • 2003
  • Friction welding of GCD45 spheroidal graphite cast iron and 2024 aluminum alloy has been studied, especially in terms of the joint faces and strength of friction welding. For appropriate results of the friction welding of GCD45 graphite cast iron and 2024 aluminum alloy, an insert of A1050 pure aluminum metal was used. The joint strength of the A1050 pure aluminum insert approached the maximum strength of 165.7Mpa, compared to 128MPa for the joint between GCD45 graphite cast iron and A1050 pure aluminum without the insert metal. Maximum strength, 165.7Mpa, was possible for the following optimum conditions: 20MPa for the friction pressure, P1, 60MPa for the upsetting pressure, P2, 1 second for the friction time, t1, 3000rpm for the rotation, N, and 0.3 seconds for the brake time, tB.

고 Si-P 첨가가 박육구상흑연주철의 미세 조직과 기계적 성질에 미치는 영향 (Effects of high Si-P Addition on Microstructure and Mechanical Properties of Thin Ductile Cast Iron)

  • 박용진;최양진;박인선;김영환;이효상
    • 한국주조공학회지
    • /
    • 제15권6호
    • /
    • pp.558-565
    • /
    • 1995
  • Effects of high Si-P addition on microstructure and mechanical properties of thin ductile cast iron have been investigated. The amount of silicon addition have fixed on 4.0wt% and the amounts of phosphorus addition and thickness of specimen have been varied from 0.05 to 0.8wt% and ${\phi}13mm$, ${\phi}10mm$ and ${\phi}6mm$, respectively. As the casting thickness decreased, the average diameter of spheroidal graphite was decreased and the hardness of the cast iron increased. By adding P, the average diameter of spheroidal graphite was increased and the count of the spheroidal graphite was decreased continuously. And the tensile strength and the elongation was decreased, and the hardness was increased. With the P added more than 0.2wt%, the abraded amount was decreased significantly. The addition of P improved the wear resistance and the hardness of thin ductile cast iron.

  • PDF

극치통계에 의한 구상흑연주철재의 피로강도의 정량적 평가 (Quantitative Evaluation of Fatigue Strength in Ductile Cast Iron by Extreme Value Distribution)

  • 윤명진
    • 한국공작기계학회논문집
    • /
    • 제10권6호
    • /
    • pp.42-47
    • /
    • 2001
  • In this study, fatigue limit of ductile cast iron is evaluated based on phenomena of the microscopic observation, such as matrix structure, spheroidal ratio, size of graphite and distribution. Three different ferrite-pearlite matrix structure, GCD 45-), GCD 50, GCD 60 series, all of which contain more than 70% spheroidal ratio of graphite, were used to obtain the correlation between maximum size of graphite and fatigue strength. It was concluded as fellows. (1) In Ductile cast iron of ferrite-pearlite matrix, the fatigue limit of GCD 60 series with 73% pearlite structure was the highest. (2) From observation of the starting point of crack of all specimens, it is noted that the crack initiates, in graphite, goes through ferrite and propagates into pearlite. (3) A good quality of Ductile cast iron used in this experiment can be checked from uniformly distributed graphite. The negligible interaction effect between graphites was verified by microscopic observation and fracture mechanics investigation in surface and interior of the specimen.

  • PDF

AE방법에 의한 구상화흑연(球狀化黑鉛) 주철재의 파괴기구 구명(究明) (An Investigation of Fracture Mechanism of Spheroidal Graphite Cast Iron by Acoustic Emission Method)

  • 김상철;함경춘;오범석
    • 비파괴검사학회지
    • /
    • 제6권2호
    • /
    • pp.17-36
    • /
    • 1987
  • In this experimental research, fracture mechanisms of spheroidal graphite cast iron (As Cast, annealed and normalized) were investigated by using Acoustic Emission (AE) technique. In this study, the data (AE signal) are digitized and processed with the 8 bits micro-computer (APPLE II) connected to the AE measuring device without data processing unit. The source of AE signal was estimated by fractography analysis. The results obtained in this experimental study are summarized as follows : For the heterogeneous materials (spheroidal graphite cast iron) with inclusions which may considered as cracks, it is found that low and high AE amplitude appear simultaneously and the load is found to be fluctuated in the final stage of deformation. But the lad is not fluctuated in tension test with low AE amplitude only. AE is measured within elastic region and it is confirmed that 0.2% offset yield load agrees approximately with the load point where AE counts decrease steeply after the point of maximum AE counts.

  • PDF

구상흑연주철의 피로수명분포에 대한 통계적 해석 (A Statistical Analysis on Fatigue Life Distribution in Spheroidal Graphite Cast Iron)

  • 장성수;김상태
    • 대한기계학회논문집A
    • /
    • 제24권9호
    • /
    • pp.2353-2360
    • /
    • 2000
  • Statistical fatigue properties of metallic materials are increasingly required for reliability design purpose. In this study, static and fatigue tests were conducted and the normal, log-normal, two -parameter Weibull distributions at the 5% significance level are compared using the Kolmogorov-Smirnov goodness-of-fit test. Parameter estimation were compared with experimental results using the maximum likelihood method and least square method. It is found that two-parameter Weibull distribution and maximum likelihood method provide a good fit for static and fatigue life data. Therefore, it is applicable to the static and fatigue life analysis of the spheroidal graphite cast iron. The P-S-N curves were evaluated using log-normal distribution, which showed fatigue life behavior very well.

주철의 열적 성질에 미치는 흑연현상 및 첨가원소(Mn, Ni)의 영향 (The Influences of Graphite Shape and Alloying Elements(Mn, Ni) on the Thermal Properties of Cast Iron.)

  • 노무근;권혁무
    • 한국주조공학회지
    • /
    • 제9권1호
    • /
    • pp.80-88
    • /
    • 1989
  • SGCI(Spheroidal Graphite Cast Iron), CVGCI(CV Graphite Cast Iron) and FGCI(Flake Graphite Cast Iron) having different contents of Mn($0.25%{\sim}0.85%$) and Ni($0.3%{\sim}1.2%$) were produced, respectively. The thermal expansion and thermal conductivity of the cast iron were investigated in the temperature range of $50^{\circ}C{\sim}300^{\circ}C$. As the graphite nodularity of the cast iron increases, thermal expansion coefficient increases, thermal conductivity and electrical conductivity to thermal conductivity ratio decrease. The thermal expansion coefficient of the cast iron increases with increasing Mn content and decreases with increasing Ni content. The thermal conductivity of the cast iron decreases with increasing Mn and Ni contents.

  • PDF

구상흑연주철 FCD60과 Cr-Mo강 SCM440 확산접합부의 인장성질에 미치는 접합조건의 영향 (The Effect of Bonding Condition on Tensile Properties of Diffusion Bonds of Graphite Cast Iron FCD60 to Cr-Mo Steel SCM440)

  • 송우현;김정길;강정윤
    • Journal of Welding and Joining
    • /
    • 제22권1호
    • /
    • pp.77-82
    • /
    • 2004
  • The effect of bonding condition on tensile properties of joints diffusion bonded spheroidal graphite cast iron, FCD60 to Cr-Mo steel, SCM 440 was investigated. Diffusion bonding was performed with various temperatures, holding times, pressures and atmospheres. All tensile specimens were fractured at the bonding interface. The tensile strength and elongation was increased with increasing bonding temperature. Especially, tensile strength of joints bonded at 1123K was higher than that of a raw material, FCD60, and tensile strength of joints bonded at 1173K was equal to that of a raw material, SCM440, but elongation of all joints was lower than those of raw materials. There was little the effect of holding time on the tensile properties. In comparison with bonding atmosphere, the difference of tensile strength was not observed, but elongation of joint bonded at vacuum(6.7mPa and 67mPa) was higher than that of Ar gas. Higher the degee of vacuum, elongation increased. Tensile properties of diffusion bonds depended on microstructures of cast iron at the interface and void ratio. Microstructures of cast iron at interface changed with temperature, because decarburizing and interdiffusion at the interface occurs and transformation of austenite-1 ferrite + graphite occurs on the cooling process. The void ratio decreased with increasing temperature, especially, effected on the elongation.

흑연의 구상화기구를 이용한 주철본드 다이어몬드 숫돌의 개발 (Development of Cast Iron Bonded Grinding Wheel by Using Spheroidization Mechanism of Graphite)

  • 유기태;정해도;전형일
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1995년도 추계학술대회 논문집
    • /
    • pp.61-64
    • /
    • 1995
  • Grinding has been adapted as a finishing process,which can carry out form and surface integrity at the same time. Recently, high efficient and precise grinding technique is required bacause the needs for functional parts such as silicon wafer,ceramic,and electric materials are increasing. Accordingly, the development of grinding wheel appropriate to that purpose is very important. So, in this paper we newly developed a diamond grinding wheel by applying the superior characteristics of spheroidal graphite of the cast iron sintered product. Especially, a electric resistance sintering method was applied in which rapid heat treatment is possible. Finally, we have achieved successful results that the grinding wheel has high hardness,durability and grinding ability,and satisfies above conditions.

  • PDF