  • Welded Unreinforced Flange-Welded Web (WUF-W) connection is one of Special Moment Frame (SMF) specified in ANSI/AISC-358. From the experimental test of WUF-W connection specimens conducted by the previous study, fracture occurred in the beam flange before achieving total inter-story drift angle of 0.04radian required for Special Moment Frames (SMF) system even though the specimens satisfied the design and detailing requirement specified in ANSI/AISC-358. These results are estimated as problem of the access hole geometry. In this study, a full-scale WUF-W connection specimen was made with a modified access hole geometry, and tested with the same test setting and loading as the previous test. From test results, the deformation capacity of the tested WUF-W connection specimen exceeded 4%, which is required for connections in SMF system. Comparing with the WUF-W specimens of the previous study, the strain demand of the beam flange in the tested specimen was decreased and energy dissipation capacity of the specimen was improved.

SA508 PCVN 시편의 균열깊이에 따른 구속력 손실 평가 (Constraint Loss Assessment of SA508 PCVN Specimen according to Crack depth)

  • 박상윤;이호진;이봉상
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2008년도 추계학술대회A
    • /
    • pp.161-166
    • /
    • 2008
  • In general structures, cleavage fracture may develop under the low constraint condition of larger scale yielding with a shallow surface crack. However, standard procedures for fracture toughness testing require very severe restrictions of specimen geometry. So the standard fracture toughness data makes the integrity assessment irrationally conservative. In this paper, cleavage fracture toughness tests have been made on side-grooved PCVN (precracked charpy V-notch) type specimens (10 by 10 by 55 mm) with varying crack depth, The constraint effects on the crack depth ratios are quantitatively evaluated by scaling model and Weibull stress method using 3-D finite clement method, After correction of constraint loss due to shallow crack depths, the statistical size effect are also corrected according to the standard ASTM E 1921 procedure, The results snowed a good agreement in the geometry correction regardless of the crack size, while some over-corrections were observed in the corrected values of $T_0$.

  • PDF

GMT 평판의 볼트조인트 강도 평가 (Estimation of Bolted Joint Strength of Flat Plate of Glass-Mat Reinforced Thermoplastics)

  • 강완석;민지현;이재욱;임용택
    • 대한기계학회논문집A
    • /
    • 제27권10호
    • /
    • pp.1636-1643
    • /
    • 2003
  • In this study, bolted joint made of Glass-Mat Reinforced Thermoplastics (GMT) specimen was under tensile loading to investigate the relation between joint strength and glass-fiber weight fraction of the flat plate specimen. The effect of molding conditions such as the initial size of a GMT charge and molding temperatures was investigated under plane strain condition. In consideration of the specimen geometry, minimum end distance and width of the specimen to induce the bearing fracture mode of the bolted joint were determined. And finally, the effect of the outer diameter of washer and clamping pressure on joint strength was also investigated. Since joint strength is dependent on the local glass-fiber weight fraction, experimentally measured strength was modified, considering its irregular values of the specimen molded under various processing conditions in order to obtain a reasonable correlation between the two.

비틀림 시험에 대한 표준시험시편 형상 및 축 정렬 이상 영향 분석 (The analysis on the shape of a Standard Test Specimen for the Torsion Test and The Effects of Misalignments)

  • 김주희;김윤재;;허용학;제진호
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2008년도 추계학술대회A
    • /
    • pp.155-160
    • /
    • 2008
  • Using a three-dimensional (3-D) FE analyses, this paper provides the shape optimization of the standard test specimen for the torsion test, as well as a method for analyzing effects of misalignment under the angular and concentric misalignment. For verification, FE analysis is performed, which is designed for the perfectly full-model. To optimize the design shape of the torsion-controlled fatigue test specimen, we performed sensitivity analysis using shape parameters. Additionally, two kinds of misalignment (angular misalignment and concentric misalignment) are applied to the circular and tubular specimens to show effects of misalignments in the FE analysis. The present results will provide valuable information for designing shafts for every kind of mechanical system under torsional force.

  • PDF

점용접시편의 극한하중과 피로특성에 관한 실험적 고찰 (An Experimental Investigation of Limit Loads and Fatigue Properties of Spot Welded Specimens)

  • 이형일;김남호;이태수
    • 대한기계학회논문집A
    • /
    • 제24권1호
    • /
    • pp.38-51
    • /
    • 2000
  • The study on the mechanical behavior of a spot-welded specimen is largely divided into the quasi-static overload failure analysis and the fatigue failure prediction. The main issue in an overload analysis is to examine the critical loads, thereby providing a generalized overload failure criterion. As the welding spot forms a singular geometry of an external crack type, fatigue failure of spot-welded specimens can be evaluated by means of a fracture parameter. In this study, we first present the limit loads of 4 representative types of single spot-welded specimens in terms of the base metal yield strength and specimen geometries. Recasting the load vs. fatigue life relationships experimentally, obtained here, we then predict the fatigue life of spot-weld specimens with a single parameter denoted the equivalent stress intensity factor. This crack driving parameter is demonstrated to successfully describe the effects of specimen geometry and loading type in a comprehensive manner. The suggested fatigue life formula for a single spot weld can play a key, role in the design and assessment of spot-welded panel structures, in that the fatigue strength of multi-spots is eventually determined by the fatigue strength of each single spot.

실배관 파괴특성 평가에 관한 연구 (I) (A Study on the Evaluation of the Pipe Fracture Characteristic (I))

  • 박재실;석창성
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집A
    • /
    • pp.345-350
    • /
    • 2001
  • In order to perform elastic-plastic fracture mechanical analyses, fracture resistance curves for concerned materials are required. 1T-CT specimen was used to obtain fracture resistance curves. But the fracture resistance curve by the 1T-CT specimen was very conservative to evaluate the integrity of the structure. And fracture resistance curve was affected by the specimen geometry and crack plane orientation. The objective of this paper is to be certain the conservativeness of the fracture resistance curve by the 1T-CT specimen and to provide the additional safety margin. For these, the fracture tests using the real pipe specimen and standard 1T-CT specimen test were performed. 4-point bending jig was manufactured for pipe test and direct current potential drop method was used to measure the crack extension and length for pipe test. From the pipe and the 1T-CT specimen test results, it was observed that the J-integral of the 1T-CT specimen test at the crack initiation point was very small compare to that of the pipe specimen test.

  • PDF

실배관 파괴특성 평가에 관한 연구 (A Study on the Evaluation of the Pipe Fracture Characteristic)

  • 박재실;김영진;석창성
    • 대한기계학회논문집A
    • /
    • 제29권1호
    • /
    • pp.107-114
    • /
    • 2005
  • In order to analyze the elastic-plastic fracture behavior of a structure, the fracture resistance curve of the material should be known first. The standard CT specimen was used to obtain the fracture resistance curves of a piping system. However, it is known that the fracture resistance curve by the standard CT specimen is very conservative to evaluate the integrity of a structure. Also the fracture resistance curve is effected by the specimen geometry and the dimensions because of the constraint effect. The objective of this paper is to be certain the conservativeness of the fracture resistance curve by the standard CT specimen and to provide an additional safety margin. For these, the fracture tests using a real pipe specimen and the standard CT specimen test were performed. A 4-point bending jig was manufactured for the pipe test and the direct current potential drop method was used to measure the crack extension and the length for the pipe test. Also finite element analyses were performed with a CT specimen and a pipe in order to prove the additional safety margin. From the result of tests and analyses of the pipe and the standard CT specimen, it was observed that the fracture analysis with the standard CT specimen is conservative and the additional safety margin was proved.

초음파 피로시험편 결정법의 연구동향 (Technical Review of Specimens under Ultrasonic Fatigue Test)

  • 명노준;한승욱;박정훈;최낙삼
    • 대한기계학회논문집A
    • /
    • 제37권8호
    • /
    • pp.967-973
    • /
    • 2013
  • 본 논문에서는 초고주기피로영역(VHCF)에 대한 가속시험 방법인 초음파 피로시험을 소개하고 이와 관련된 이론을 검토하였다. 초음파피로시험은 20 kHz 영역에서 시험편의 공진을 이용하므로 동탄성계수와 파장을 고려하여 시험편의 길이와 형상을 설계하여야 한다. 공진시험을 통하여 20 kHz 에 맞는 파장을 구하고 시험편의 길이와 동탄성계수를 계산한다. 이렇게 계산된 시험편의 형상과 시험시 형성되는 변위값을 측정하여 응력을 구한다. 초음파 피로시험결과는 기존의 피로시험법에 따른 결과와 비교되어 주파수 및 시험편 형상의 효과가 검증되어야 한다.

이축하중을 받는 십자형 시편의 파괴인성 및 구속효과 평가 (Evaluation of Fracture Toughness and Constraint Effect of Cruciform Specimen under Biaxial Loading)

  • 김종민;김민철;이봉상
    • 한국압력기기공학회 논문집
    • /
    • 제12권1호
    • /
    • pp.62-69
    • /
    • 2016
  • Current guidance considers that uniaxially loaded specimen with a deep crack is used for the determination of the ductile-to-brittle transition temperature. However, reactor pressure vessel is under biaxial loading in real and the existence of deep crack is not probable through periodic in-service-inspection. The elastic stress intensity factor and the elastic-plastic J-integral which were used for crack-tip stress field and fracture mechanics assessment parameters. The difference of the loading condition and crack geometry can significantly influence on these parameters. Thus, a constraint effect caused by differences between standard specimens and a real structure can over/underestimate the fracture toughness, and it affects the results of the structural integrity assessment, consequentially. The present paper investigates the constraint effects by evaluating the master curve $T_0$ reference temperature of PCVN (Pre-cracked Charpy V-Notch) and small scale cruciform specimens which was designed to simulate biaxial loading condition with shallow crack through the fracture toughness tests and 3-dimensional elastic-plastic finite element analyses. Based on the finite element analysis results, the fracture toughness values of a small scale cruciform specimen were estimated, and the geometry-dependent factors of the cruciform specimen considered in the present study were determined. Finally, the transferability of the test results of these specimens was discussed.

이종 접합재의 굽힘 및 인장강도에 미치는 시험편 형상의 효과 (Effect of Specimen Geometry on Bending and Tensile Strength of Material Used in Dissimilar Joints)

  • 허장욱
    • 대한기계학회논문집A
    • /
    • 제34권3호
    • /
    • pp.341-346
    • /
    • 2010
  • 이종 접합재($\beta-Si_3N_4/S45C$)의 굽힘강도와 인장강도에 미치는 시험편 형상의 영향을 정량적으로 평가하였다. 평균 굽힘강도와 평균 인장강도는 원형단면 시험편이 4각형 단면 시험편보다 약간 높았다. 또한, 초음파(AE)를 이용하여 균열발생응력을 성공적으로 측정할 수 있었으며, 균열발생응력은 굽힘강도의 60~80% 이었다. 아울러, 세라믹측 접합계면 근처의 잔류응력 측정을 굽힘강도 시험전에 X선 회절법에 의해 실시하였으며, 굽힘강도와 균열발생응력은 잔류응력 증가와 더불어 감소하였다. 마지막으로 인장시험에서 굽힘변형률 성분의 영향을 평가하였으며, 인장강도는 굽힘변형률 성분의 증가와 더불어 감소하고 굽힘강도의 약 80%에 해당되었다.