  • Transition metal chalcogenides are promising cathode materials for next-generation battery systems, particularly sodium-ion batteries. Ni3Co6S8-pitch-derived carbon composite microspheres with a yolk-shell structure (Ni3Co6S8@C-YS) were synthesized through a three-step process: spray pyrolysis, pitch coating, and post-heat treatment process. Ni3Co6S8@C-YS exhibited an impressive reversible capacity of 525.2 mA h g-1 at a current density of 0.5 A g-1 over 50 cycles when employed as an anode material for sodium-ion batteries. However, Ni3Co6S8 yolk shell nanopowder (Ni3Co6S8-YS) without pitch-derived carbon demonstrated a continuous decrease in capacity during charging and discharging. The superior sodium-ion storage properties of Ni3Co6S8@C-YS were attributed to the pitch-derived carbon, which effectively adjusted the size and distribution of nanocrystals. The carbon-coated yolk-shell microspheres proposed here hold potential for various metal chalcogenide compounds and can be applied to various fields, including the energy storage field.

화학물질의 재현을 통한 악취발생원인 규명 (Investigation on the Cause of Malodor through the Reproduction of Chemicals)

  • 박상준;오영환;조보연;이재신;김의용
    • KSBB Journal
    • /
    • 제29권5호
    • /
    • pp.392-398
    • /
    • 2014
  • It was confirmed that malodor connected with an air-conditioner in an automobile is caused by microbial volatile organic compounds (MVOCs) produced by microorganisms and through microorganisms coexisting with each other to form a biofilm on the evaporator surface. A bacterium, Methylobacterium aquaticum, can form a biofilm on the evaporator surface. The biofilm was composed of 45.79% C (Carbon), 42.36% O (Oxygen), 1.85% Na (Sodium), 5.42% Al (Aluminum), 1.39% P (Phosphorus), 0.74% Cl (Chlorine) and 2.45% K (Potassium). This result matches the composition of the biofilm formed on the surface of the used evaporator. It was determined that sulfur compounds (Hydrogen sulfide, Dimethyl sulfide) and organic acids (n-Butyric acid, n-Valeric acid, iso-Valeric acid) in the air which was blown into the automobile were generated by Methylobacterium aquaticum and Aspergillus versicolor, respectively. On the other hand, volatile organic compounds (Toluene, Xylene, 2-Ethylhexanol, 2-Phenyl- 2-propanol, Ethylbenzene) were not found. It is estimated that the reason is due to the low concentration of generated MVOCs or is caused by the change of some MVOCs depending on the nutrients (medium).

폐탄광수에서 분리한 황화수소 분해 세균 Thiobacillus sp. IW.의 성장조건 (Effects of Cultivation Condition on Growth of the Hydrogen Sulfide-Degradating Thiobacillus sp. IW. Isolated from Waste Coal Mine Water)

  • 차진명;박열이인화
    • KSBB Journal
    • /
    • 제9권3호
    • /
    • pp.287-293
    • /
    • 1994
  • 황화수소 산화반응에 이용할 수 있는 균주를 전남 화순 근교의 폐탄광수에서 분리하였다. 분리균주는 형태적, 생리학적 빛 화학합성 특정에 기준으로 보 면 Thiobacillus sp. IW.로 동정되어진다. 분리된 균주의 최적 배양온도는 $30^{\circ}C$였고, 최적 pH는 7이며, pH 3~pH 9 사이의 넓은 성장범위를 가지고 있었다. 액상배지에 축적된 sulfate 농도가 배지의 pH를 감소시켜 결국 균의 성장을 억제하는 작용을 하였다. 최대 비증식속도인$\mu_{max}=0.78^{-1}$이었고, 세대시 간은 0.9시간으로 나타났다. 분리균주는 질소원으로 potassium nitrate나 glutamic acid를 이용하였으나, urea나 ammonium chloride는 이용하지 못하였다. 기본배지에 첨가된 malate는 전혀 이용하지 못 하였고, Sodium thiosulfate를 에너지원으로 이용하 면 균체량은 $6.25mg/\ell.h$였으며, 대수성장기는 18 시간으로 나타났다. 이의 결과로 미루어 보아 분리 균주는 황화수소 등의 악취 제거에 유용한 균주로 사료되어 진다.

  • PDF

Miniaturized Chromatography에 의한 $^{99m}Tc$-표지 방사성의약품의 정도 관리 (Miniaturized Chromatographic Quality Control of $^{99m}Tc$ Radiopharmaceuticals)

  • 염미경;정재민;진광호;조규진;정준기;이명철;고창순
    • 대한핵의학회지
    • /
    • 제24권1호
    • /
    • pp.133-137
    • /
    • 1990
  • The general use of a number of $^{99m}Tc-labelled$ compounds makes the need for good routine quality control procedures, especially the labelling efficiency measurements. The purpose of these study were to measure the labelling efficiency of $^{99m}Tc-labelled$ MDP, DTPA, Tin colloid, and Antimony sulfide colloid using miniaturized paper and instant thin layer chromatography. The chromatographic systems include whatman 3 MM paper and acetone, Gelman ITLC-SG and 0.9% sodium chloride. The chromatographic strips are miniaturized $(1\times10\;cm)$, marked and numbered. Labelling efficiencies of $^{99m}Tc-labelled$ DTPA and Tin colloid were above 98.0%. $^{99m}Tc-labelled$ Antimony sulfide colloid was 90.0%. And labelling efficiency of $^{99m}Tc-labelled$ MDP was 89.0% Coefficient variance of $^{99m}Tc-labelled$ MDP, DTPA, Tin colloid, and Antimony sulfide colloid were 5.14%, 2.06%, 1.82% and 4.90%, respectively. We found that this miniaturized chromatographic quality control was simple and reliable.

  • PDF

Hydrogen sulfide protects from acute kidney injury via attenuating inflammation activated by necroptosis in dogs

  • Wang, Shuang;Liu, XingYao;Liu, Yun
    • Journal of Veterinary Science
    • /
    • 제23권5호
    • /
    • pp.72.1-72.14
    • /
    • 2022
  • Background: The treatment of acute kidney injury (AKI), a common disease in dogs, is limited. Therefore, an effective method to prevent AKI in veterinary clinics is particularly crucial. Objectives: Hydrogen sulfide (H2S) is the third gaseous signal molecule involved in various physiological functions of the body. The present study investigated the effect of H2S on cisplatin-induced AKI and the involved mechanisms in dogs. Methods: Cisplatin-injected dogs developed AKI symptoms as indicated by renal dysfunction and pathological changes. In the H2S-treated group, 50 mM sodium hydrosulfide (NaHS) solution was injected at 1 mg/kg/h for 30 min before cisplatin injection. After 72 h, tissue and blood samples were collected immediately. We performed biochemical tests, optical microscopy studies, analysis with test kits, quantitative reverse-transcription polymerase chain reaction, and western blot analysis. Results: The study results demonstrated that cisplatin injection increased necroptosis and regulated the corresponding protein expression of receptor interacting protein kinase (RIPK) 1, RIPK3, and poly ADP-ribose polymerase 1; furthermore, it activated the expressions of inflammatory factors, including tumor necrosis factor-alpha, nuclear factor kappa B, and interleukin-1β, in canine kidney tissues. Moreover, cisplatin triggered oxidative stress and affected energy metabolism. Conversely, an injection of NaHS solution considerably reduced the aforementioned changes. Conclusions: In conclusion, H2S protects the kidney from cisplatin-induced AKI through the mitigation of necroptosis and inflammation. These findings provide new and valuable clues for the treatment of canine AKI and are of great significance for AKI prevention in veterinary clinics.

PPS/PPSS 공중합체의 합성 및 열적 성질 (Synthesis and Thermal Properties of PPS/PPSS Copolymer)

  • 박이순;이태형;곽규대;허정림
    • 공업화학
    • /
    • 제9권3호
    • /
    • pp.440-444
    • /
    • 1998
  • p-Dichlobenzene(DCB), p-dibromobenzene(DBB), p-diiodobenzene(DIB) 및 4-chlorophenyl sulfone(CPS)을 공단량체로, 그리고 N-methyl-2-pyrrolidinone(NMP)를 용매로 사용하여 고온, 고압하에서 poly(phenylene sulfide-co-phenylene sulfide sulfone), PPS/PPSS 공중합체를 합성하고 공중합 반응 특성과 합성된 공중합체들의 구조 및 열적성질에 대해 조사하였다. PPS/PPSS 공중합체의 수율은 [DBB]/[CPS] 및 [DIB]/[CPS] 공단량체 조합의 경우 [DCB]/[CPS] 공단량체 조합보다 낮은 온도인 $190^{\circ}C$에서 최고 수율을 나타내었으며 [DCB]/[CPS] 공단량체 조합의 경우는 이보다 높은 온도인 $230^{\circ}C$에서 최고 수율을 나타내어 leaving group이 I>Br>Cl의 순서로 공중합 반응이 잘 진행되었으며 이것으로부터 공중합 반응은 nucleophilic aromatic substitution(SNAr) 기구에 적합함을 알 수 있었다. [DBB]/[CPS] 공단량체 조합중에서 CPS의 공급비가 10 mol%일 때 생성된 PPS/PPSS 공중합체의 분자량은 8,330g/mol로 가장 높게 나타났다. CPS 단량체의 공급비가 30 mol% 이상일 경우 생성되는 PPS/PPSS 공중합체는 $T_m$을 나타내지 않았으나, CPS의 공급비가 10 mol%인 PPS/PPSS 공중합체 시료의 경우 $T_g$는 약 $15^{\circ}C$ 증가하였고 $T_m$은 약 $15^{\circ}C$ 감소하여 열적 성질이 향상되는 것을 볼 수 있었다. 또 중합 온도를 $240^{\circ}C$로 고정하고 [DBB]/[CPS]의 공급비를 95/5 mol%로 하여 얻어진 PPS/PPSS 공중합체는 PPS 단독 중합체보다 분자량이 높게 나타나 PPS 단독 중합체의 고결정성 및 내열성을 유지한채 PPS 단독 중합체의 결점의 하나인 중합도를 향상시킬 수 있는 방법으로 이용될 수 있다고 생각되었다.

  • PDF

염화알루미늄 존재하에서의 수소화붕소나트륨과 대표적 유기화합물과의 반응 (Reaction of Representative Organic Compounds with Sodium Borohydride in the Presence of Aluminum Chloride)

  • 윤능민;이호준;정진순
    • 대한화학회지
    • /
    • 제17권4호
    • /
    • pp.275-285
    • /
    • 1973
  • 유기화합물의 선택환원에 필요한 자료를 얻기 위하여 수소화붕소나트륨과 염화알루미늄의 3:1 혼합물의 테트라히드로푸란 용액에서의 환원성을 규명하였다. 49개의 대표적 유기화합물을 골라 이시약과 실온에서 작용하여 대략의 반응속도와 정량관계를 알아보았다. 테트라히드로푸란 용액에서 염화알루미늄 1몰에 수소화붕소나트륨 3몰을 가하면 현탁용액이 생기는데 수소화붕소나트륨 보다는 훨씬 환원성이 강하다. 알데히드와 케톤은 한시간 이내에 빨리 환원되고 아실유도체는 서서히 그러나 카르복시산은 매우 느리게 환원되었다. 에스테르, 락톤, 에폭시드는 수소화붕소나트륨이나 보란보다 훨씬 빨리 환원되었다. 삼차 아미드는 서서히 환원되었으나 일차 아미드는 수소는 발생하지만 환원은 거의 일어나지 않았다. 벤조니트릴은 30분에 환원이 완결되었으나 카프로니트릴은 느리게 환원되었다. 니트로화합물, 이황화물, 술폰등은 이 시약과 반응하지 않으나 아조, 아족시, 옥심기는 서서히 반응하고 이소시안산페닐은 도중단계까지만 환원되었다 올레핀은 쉽게 수소화붕소화 반응을 하였다.

  • PDF

오존발생장치와 흡수환원법을 이용한 배기가스 동시 탈황 탈질 공정 (Simultaneous Removal of $SO_2$ and NOx Using Ozone Generator and Absorption- Reduction Technique)

  • 목영선;이주혁;신동남;고동준;김경태
    • 대한환경공학회지
    • /
    • 제28권2호
    • /
    • pp.191-196
    • /
    • 2006
  • 유전체장벽방전에 의해 발생된 오존을 배기가스에 주입하면 질소산화물의 주성분인 NO가 빠르게 $NO_2$로 산화된다. 일단 NO가 $NO_2$로 산화되면 다음 단계에서 황화나트륨이나 아황산나트륨과 같은 환원제에 의해 쉽게 $N_2$로 환원될 수 있다. 본 연구에 사용된 환원제들은 $SO_2$도 효과적으로 제거시킬 수 있으므로 $NO_x$$SO_2$를 동시에 처리하는 것이 가능하다. 오존처리실과 흡수환원반응기로 구성된 본 연구의 2단계 공정은 모사 배기가스에 포함된 $NO_x$를 95%, $SO_2$를 100% 제거시킬 수 있었다. 환원제인 황화나트륨으로부터 발생되는 황화수소는 강염기인 수산화나트륨을 환원제와 함께 사용함으로써 방지할 수 있었다. $NO_x$$SO_2$를 동시에 처리하기 위한 환원제로 $Na_2SO_3$보다 $Na_2S$가 더 우수한 성능을 보여주었다.

AA1100의 부식에 미치는 Na2S, NaCl, H2O2 농도의 영향 (Effects of Na2S, NaCl, and H2O2 Concentrations on Corrosion of Aluminum)

  • 이주희;장희진
    • Corrosion Science and Technology
    • /
    • 제18권6호
    • /
    • pp.312-317
    • /
    • 2019
  • The objective of this study was to investigate the corrosion behavior of aluminum (AA1100) in a mixed solution of 0 ~ 0.1 g/L Na2S + 0.3 ~ 3 g/L NaCl + 0 ~ 10 mL/L H2O2. Potentiodynamic polarization tests were performed. Effects of solution compositions on corrosion potential, corrosion rate, and pitting potential of aluminum were statistically analyzed with a regression model. Results suggested that localized corrosion susceptibility of aluminum was increased in the solution with increasing concentration of NaCl because the pitting potential was lowered linearly with increasing NaCl concentration. On the contrary, H2O2 mitigated the galvanic corrosion of aluminum by increasing the corrosion potential. It also mitigated localized corrosion by increasing the pitting potential of aluminum. Na2S did not exert a noticeable effect on the corrosion of aluminum. These effects of different chemical species at various concentrations were independent of each other. Synergy or offset effect was not observed.

Paper Chromatogaphy 법(法)에 의한 SH화합물간(化合物間)의 수은(水銀)에 대(對)한 친화력(親和力) 비교(比較) (Affinity of Mercury to SH Compounds Compared by Using the Paper Chromatography)

  • 김영희;이만정
    • 한국식품영양과학회지
    • /
    • 제10권1호
    • /
    • pp.67-76
    • /
    • 1981
  • Paper Chromatography 법(法)으로 아미노산류(酸類)와 이노신산(酸) 및 수은중독(水銀中毒) 치료제(治療劑)인 BAL의 수은(水銀)에 대(對)한 친화력(親和力)의 크기를 비교(比較)하였다. 그 결과(結果) Cysteine Cystine 및 Methionine의 3종(種)의 합류황(合硫黃) 아미노산(酸)은 수은(水銀)과 쉽게 결합(結合)하였으나 다른 아미노산(酸)들과의 결합(結合)은 확인(確認)하지 못하였다. 수은(水銀)은 SH기(基)를 가지는 Sodium thiosulfate 및 BAL과는 쉽게 결합(結合)하였으며 이노신산(酸)과도 쉽게 결합(結合)하였다. 이들 함류황(含硫黃) 아미노산(酸) 류(類)보다 큰 것으로 판단(判斷)되었다.

  • PDF