• 제목/요약/키워드: Smooth Specimen

검색결과 166건 처리시간 0.022초

고강도 사이알론의 균열치유와 고온강도 특성 (Characteristics of Crack Healing and High Temperature Strength of High Strength Sialon)

  • 남기우;박상현;박승원;문석재
    • 대한기계학회논문집A
    • /
    • 제33권9호
    • /
    • pp.957-962
    • /
    • 2009
  • Sialon was produced by hot-pressing the mixtures of $Si_3N_4$, AlN and $Y_2O_3$ powders. All fracture tests were performed on a three-point loading system with a 30 mm bending span. Fracture toughness and Vickers hardness of smooth specimen were average 7.05 $MPa{\cdot}m^{0.5}$ and Hv = 1580, respectively. Density of three kinds of specimens, smooth specimen, smooth and healed specimen, smooth with $SiO_2$ colloidal coating and healed specimen, had beyond 99 % of theoretical density. Bending strength of smooth healed specimens had high strength more than 1 GPa. Crack healed specimens recovered as strength as smooth specimen. That is, cracked specimen with $SiO_2$ colloidal coating on cracked part recovered strength by heat treatment, completely. Crack healing of $Si_3N_4$ composite ceramics had contributed glassy $SiO_2$ to strength recovery. Limiting high temperature for bending strength of heat treated smooth specimen for bending strength was about 1273 K.

Cr-Mo강의 수소확산 특성에 관한 유한요소해석 (The Finite Element Analysis on the Characteristics of the Hydrogen Diffusion for the Cr-Mo Steels)

  • 이휘원;하민수
    • 한국기계기술학회지
    • /
    • 제13권2호
    • /
    • pp.115-121
    • /
    • 2011
  • The size of hydrogen molecule is not so small as to invade into the lattice of material, and therefore, hydrogen invades into the material as atom. Hydrogen movement is done by diffusion or dislocation movement in the near crack tip or plastic deformation. Hydrogen appeared to have many effects on the mechanical properties of the Cr-Mo steel alloys. The materials for this study are 1.25Cr-0.5Mo and 2.25Cr-1Mo steels used at high temperature and pressure. The hydrogen amount obtained by theoretical calculation was almost same with the result solved by finite element analysis. The distribution of hydrogen concentration and average concentration was calculated for a flat specimen. Also, finite element analysis was employed to simulate the redistribution of hydrogen due to stress gradient. The calculation of hydrogen concentration diffused into the material by finite element method will provide the basis for the prediction of delayed fracture of notched specimen. The distribution of hydrogen concentration invaded into the smooth and notched specimen was obtained by finite element analysis. The hydrogen amount is much in smooth specimen and tends to concentrate in the vicinity of surface. Hydrogen embrittlement susceptibility of notched specimen after hydrogen charging is more remarkable than that of smooth specimen.

$2_{1/4}$ Cr-1 Mo강의 평활재상의 미소한 표면피로균열의 성장특성 (Propagation Characteristics of Fatigue Microcracks on Smooth Specimen of $2_{1/4}$ Cr-1 Mo Steel)

  • 서창민;우병철;장희락
    • 한국해양공학회지
    • /
    • 제4권2호
    • /
    • pp.100-111
    • /
    • 1990
  • In this paper, fatigue tests were carried out at stress test levels of 461 MPa, 441 MPa, and 431 MPa by using smooth specimen of$2_{1/4}$ Cr-1 Mo steel with the stress ratio(R) of 0.05. The initiation, growth and coalescense process of the major cracks and sub-cracks among the fatigue cracks on the smooth specimen are investigated and measured under each stress level at a constant cycle ratio by the replica technique with optical microscope. Some of the important results are as follows: In spite of the difference of stress levels, the major crack data gather into a small band in the curve of surface crack length and crack depth against cycle ratio N/Nf. The sub-crack data, however, deviate from the band of the major crack. The growth rates, da/dN, of major and sub-crack plotted against the stress intensity factor range, ${\Delta}K$, have the tendency to be compressed on a relatively small band. But it is more effective to predict fatigue life through major cracks. The propagation behavior of surface microcracks on the smooth specimens coincides with that of the specimen having an artificial small surface defect or through crack.

  • PDF

가스배관재의 탄소성파괴인성에 미치는 측면홈 영향 (Effect of Side Groove on the Elastic Plastic Fracture Toughness of Gas Piping Material)

  • 임만배;차귀준;윤한기;공유식;김정호
    • 한국해양공학회지
    • /
    • 제15권3호
    • /
    • pp.63-68
    • /
    • 2001
  • SG-365 steel is an important material and used for manufacturing a pressure vessel which the gas piping. In this investigation, the elastic plastic fracture toughness of this material is evaluated by the an unloading compliance method according to the ATM E813-97 method on the smooth and side groove 1CT specimens. The effect of smooth and side groove is studied on the elastic plastic fracture toughness. The side grooved specimen is very useful in estimation of the $J_IC. Because it is much easier than the smooth specimen to the onset of the ductile tearing by the R curve method. Besides, it improves the accuracy of toughness values, decreases the scattering of them and tunneling and shear lip by the side groove.

  • PDF

가스배관재의 피로균열진전거동과 파괴저항특성곡선에 관한 연구 (A Study on Fatigue Crack Growth Behavior and R-Curve Characteristics of Gas Piping Material)

  • 손종동;임만배
    • 동력기계공학회지
    • /
    • 제11권1호
    • /
    • pp.127-133
    • /
    • 2007
  • SG-365 steel is an important material and used for manufacturing a pressure vessel which the gas piping. In this investigation, the elastic plastic fracture toughness of this material is evaluated by the unloading compliance method according to the ASTM E813-97 and E1152-97 method on the smooth and side groove 1CT specimens. The effect of smooth and side groove is studied on the elastic plastic fracture toughness. The side grooved specimen is very useful in estimation of the $J_{IC}$. It is much easier than the smooth specimen to the onset of the ductile tearing by the R curve method. Besides, it improves the accuracy of toughness values, decreases a phenomenon of the tunneling and shear lip by the side groove.

  • PDF

SG365강의 파괴저항곡선과 측면홈효과에 관한 연구 (A Study on the Fracture Resistance Curve and Effect of Side Grooves of SG365 Material)

  • 임만배
    • 한국안전학회지
    • /
    • 제16권4호
    • /
    • pp.14-21
    • /
    • 2001
  • SG-365 steel is an important material End used for manufacturing a pressure vessel and gas piping. In this investigation, the elastic plastic fracture toughness of this material is evaluated by the unloading compliance method according to the ASTM E8l3-97 and E1152-97 method on the smooth and side groove In specimens. The effect of smooth and side groove is studied on the elastic plastic fracture toughness. The side grooved specimen is very useful in estimation of the $J_{IC}$. Because it is much easier than the smooth specimen to the onset of the ductile tearing by the R curve method. Besides. it improves the accuracy of toughness values, decreases the scattering of them and crack tunneling effect and shear lip by the side groove.

  • PDF

고인성 열가소성 복합재료 AS4/PEEK의 피로강도에 관한 기초적 검토 (A Preliminary Study on Fatigue Strength of High Toughness Thermoplastic Composite Material AS4/PEEK)

  • 송지호;강재윤
    • 대한기계학회논문집A
    • /
    • 제24권4호
    • /
    • pp.1055-1064
    • /
    • 2000
  • First, various specimen geometries, namely, coupon type, waisted type and dog-bone type, were examined to determine appropriate fatigue specimen of thermoplastic composite material AS4/PEEK and the n, fatigue strength of smooth and notched specimens of AS4/PEEK [-45/0/+45/90]2s was investigated. Fatigue tests were performed under load controlled condition at a stress ratio of 0. 1 at a frequency of 5Hz. Stiffness degradation of specimens with fatigue cycling was monitored using an automated unloading compliance technique. The waisted type specimen is found appropriate for smooth fatigue specimen geometry of AS4/PEEK. As for the effect of stress concentration, it is found that fatigue strength is higher for a 2mm-diameter hole notched specimen than a 5mm-diameter one. Fatigue notch factor decreases with the increase of fatigue life. These results are far different from the trend of fatigue strength of metallic materials. The stiffness variation of smooth specimen was only 4% at maximum until final fracture. On the other hand, the stiffness of hole notched specimen was reduced by 45% at maximum. Notched fatigue strength was compared between thermoplastic composite AS4/PEEK and thermosetting composite Graphite/Epoxy. In long-life fatigue (>104), the AS4/PEEK composite shows superior fatigue strength, but in short-life fatigue, the fatigue strength of the Graphite/Epoxy composite is nearly equal or somewhat higher than that of the AS4/PEEK composite.

미소피로균열의 검출과 정류균열 (Detection and non-propagating cracks of small fatigue crack)

  • 이종형
    • 대한기계학회논문집
    • /
    • 제14권3호
    • /
    • pp.603-609
    • /
    • 1990
  • 본 연구에서는 미소균열의 정의로서 균열의 크기가 재료의 조직의 크기와 order적으로 같은 균열의 특성이라는 것과 균열의 크기가 소성역 크기와 order적으로 같은 균열의 특성에 착안해서 탄소강 평활재와 예균열재(pre-cracked specimen)에 대 해서 응력비 R=-1 및 R=0의 피로한도 특성과 평활재의 미소균열의 검출 및 정류균열의 생성기구를 균열 열림 닫힘에 주목해서 검토하였다.

$2_{1/4}$ Cr-1 Mo강의 평활재상의 미소한 표면피로균열의 성장특성 (Propagation Characteristics of Fatigue Microcracks on Smooth Specimen of $2_{1/4}$ Cr-1 Mo Steel)

  • 서창민;우병철;장희락
    • 한국해양공학회지
    • /
    • 제4권2호
    • /
    • pp.250-250
    • /
    • 1990
  • In this paper, fatigue tests were carried out at stress test levels of 461 MPa, 441 MPa, and 431 MPa by using smooth specimen of$2_{1/4}$ Cr-1 Mo steel with the stress ratio(R) of 0.05. The initiation, growth and coalescense process of the major cracks and sub-cracks among the fatigue cracks on the smooth specimen are investigated and measured under each stress level at a constant cycle ratio by the replica technique with optical microscope. Some of the important results are as follows: In spite of the difference of stress levels, the major crack data gather into a small band in the curve of surface crack length and crack depth against cycle ratio N/Nf. The sub-crack data, however, deviate from the band of the major crack. The growth rates, da/dN, of major and sub-crack plotted against the stress intensity factor range, ${\Delta}K$, have the tendency to be compressed on a relatively small band. But it is more effective to predict fatigue life through major cracks. The propagation behavior of surface microcracks on the smooth specimens coincides with that of the specimen having an artificial small surface defect or through crack.

가스배관재의 탄소성파괴인성에 미치는 측면홈영향 (Effect of Side Grooved on the Elastic Plastic Fracture Toughness of Gas Piping Meterial)

  • 임만배;차귀준;윤한기;김정호
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.350-356
    • /
    • 2001
  • SG-50 steel is an important material and used for manufacturing a pressure vessel which the gas piping. In this investigation, the elastic plastic fracture toughness of this material is evaluated by the an unloading compliance method according to the ASTM E813-97 and E1152-97 method on the smooth and side groove 1CT specimens. The effect of smooth and side groove is studied on the elastic plastic fracture toughness. The side grooved specimen is very useful in estimation of the J$_{IC}$. Because it is much easier than the smooth specimen to the onset of the ductile tearing by the R curve method. Besides, it improves the accuracy of toughness values, decreases the scattering of them and tunneling and shear lip by the side groove.e.

  • PDF