Development of Porous Support with Mine Waste Materials (광산 폐기물을 활용한 다공성 담체 개발)

  • 정문영;정명채;최연왕
    • Economic and Environmental Geology
    • /
    • v.37 no.1
    • /
    • pp.143-151
    • /
    • 2004
  • This study focused on examining the possibility of recycling mine solid waste as environmental materials, especially for porous media. Basic properties including mineralogical compositions, chemical compositions, and particle size distribution of the tailings from the Sangdong W mine were checked. The mineralogical and chemical compositions of the tailings samples were not much different in depth. According to Korean Standard Leaching Test for Wastes(KSLT), concentrations of heavy metals leached from the tailings were below the standard values. As a result of particle size analysis, the median diameter (d$_{50}$) of the tailings was in the range of 10 to 30 ${\mu}{\textrm}{m}$. The stable tailings slurry made up of 3 ${\mu}{\textrm}{m}$ in d$_{50}$ was prepared using Attrition Mill. The milling condition was 40 vol% in slurry concentration, 700 rpm in stirring speed, and 1 hour in milling time. PEI was added as dispersing agent. Concentrated slurry was extended to 3 times by foaming method. In the case of 3 times foamed slurry, the total and open porosity of ceramic supports sintered at 1,075$^{\circ}C$ for 90 minutes was about 80% and 72%, respectively. Pore size was in the range of 30∼350${\mu}{\textrm}{m}$. Therefore, the tailings could be recycled starting material for environmental materials such as macroporous ceramic support.

A Study on the Mix Design and Quality Factors of the Combined High Flowing Concrete Using High Belite Cement

  • Kwon, Yeong-Ho
    • KCI Concrete Journal
    • /
    • v.14 no.3
    • /
    • pp.121-129
    • /
    • 2002
  • This study investigates experimentally into the design factors and quality variations having an effect on the properties of the combined high flowing concrete to be poured in the slurry wall of Inchon LNG in-ground receiving terminal. Especially, high belite cement and lime stone powder as cementitious materials and viscosity agent in order to improve self-compaction and hydration heat are used in this study. Water-cement ratio(W/C), fine aggregate volume ratio(Sr) and coarse aggregate volume ratio(Gv) as design factors of the combined high flowing concrete are applied to determine the optimum mix design proportion. Also quality variations for sensitivity test are selected items as followings. (1)Surface moisture(5cases) and (2)Fineness modulus of fine aggregate(5cases), (3)Concrete temperature(3cases), (4)Specific surface(3cases) and particle size of lime stone powder. As experimental results, water-cement ratio, fine and coarse aggregate volume ratio are shown as the optimum range 51%, 43% and 53% separately considering site condition of slurry wall. Also quality factors by sensitivity test should be controlled in the following ranges. (1) Surface moisture :to.67% and (2)Fineness modulus 2.6$\pm$0.2 of fine aggregate, (3)Concrete temperature l0-20t, (4) Specific surface 6,000$\textrm{cm}^2$/g and particle size 9.7$\pm$1.0${\mu}{\textrm}{m}$ of lime stone powder. Based on the results of this study, the optimum mix design proportion of the combined high flowing concrete are selected and poured successfully in the slurry wall of LNG in-ground tank.

  • PDF

A Study on Slurry Isolation Through Chemical Processing, with Comparative Analysis and Validation (화학적 처리를 적용한 Slurry 분리 및 비교분석 검증 연구)

  • Na, Wonshik
    • Journal of Digital Contents Society
    • /
    • v.14 no.1
    • /
    • pp.35-40
    • /
    • 2013
  • The use of slurry with a mix of abrasives and coolant for making Wire Saw in the photovoltaic industry has sharply increased with the semiconductor wafer. In this paper, the slurry was isolated, purified and dried by microwave drying method with high-purity silicon carbide powder obtained through chemical processing. Dried slurry bulk was first pulverized and chemical treatment was applied to produce powder. The produced slurry powder was then analyzed by going through the following analysis; thermal analysis, particle size analyses: SEM shots, elemental analysis, XRF and XRD. The results of this study found the recovery rate of the power obtained though the chemical processing to be higher than the one obtained from mineral processing. The results anticipate infrastructure building and active responses to increasingly stronger domestic and international environmental regulations through the integration and recycling of large amounts of slurry in the photovoltaic industry.

Rheological Properties and Particle Size Distribution of Northeast Mixed Hardwood for Enzymatic Saccharification Processing with High Substrates Loading

  • Um, Byung-Hwan
    • Journal of the Korean Wood Science and Technology
    • /
    • v.36 no.5
    • /
    • pp.56-65
    • /
    • 2008
  • In this paper experimental results are presented for the rheological behavior of high-solids saccharification of mixed northeast hardwood as a model feedstock. The experimental determination of the viscosity, shear stress, and shear rate relationships of the 10 to 20 percent slurry concentrations with constant enzyme concentrations were performed under variable rotational speed of a viscometer (2.0 to 200 RPM) at combined temperatures (50 to $30^{\circ}C$) for the initial four hours. The viscosities of saccharification slurries observed were in the ranges of 0.024 to 0.028, 0.401 to 0.058, and 0.840 to 0.087 Pa s for shear rates up to 100 reciprocal seconds at 10, 15, and 20 percent initial solids (w/v) respectively. The fluid behavior of the suspensions was modeled using the power-law, the Herschel-Bulkley, the Casson, and the Bingham model. The results showed that broth slurries were pseudoplastic with a yield stress. The model slope increased and the model intercept decreased with increasing fermentation time at shear rates normal for the fermentor. The broth slurries exhibited Newtonian behavior at high and low shear rates during initial saccharification process. The solid particle size ranged from 57.8 to $70.0{\mu}m$ for $40^{\circ}C$ and from 44.0 to 57.5 11m for combined temperatures at 10, 15, and 20 percent initial solids (w/v) respectively.

Effect of Operating Parameters on Microbial Desulfurization of Coal by Acidithiobacillus ferrooxidans. (Acidithiobacillus ferrooxidans에 의한 생물학적 석탄탈황에 미치는 조업인자의 영향)

    • Microbiology and Biotechnology Letters
    • /
    • v.31 no.4
    • /
    • pp.400-407
    • /
    • 2003
  • In microbial coal desulfurization process (MCDP) by using Acidithiobacillus ferrooxidans, the effect of process variables on pyritic sulfur removal efficiency has been investigated. The inhibitory effect of toxic materials contained in coal matrix on the activity of desulfurizing bacteria have been evaluated in coal extracts, and the results showed that the method was useful to evaluate the applicability of a coal which is to be desulfurization to MCDP. The removal efficiency increased with decreasing particle size and decreases with increasing pulp density, but has no significant influence of particle size and pup densities at high pulp densities over 20 wt%. The mass transfers of gaseous nutrients such as oxygen and carbon dioxide into coal slurry with various pulp densities and coal particle size has been studied in an airlift bioreactor. Mass transfer coefficient was independent of pulp density in coal slurry with fine particle below 175 $\mu\textrm{m}$, but significantly decreased with increasing pulp density over 225 $\mu\textrm{m}$. The coal particles over 575 $\mu\textrm{m}$ were significantly settled to the bottom of bioreactor resulting in poor mixing. Considering mass transfer, pulp density and coal mixing, an optimal size of coal particle for the microbial coal desulfurization process seems to be about 500 $\mu\textrm{m}$.

Microstructure and Formability of Semi-solid A390 Alloys made by uniform heating (균일가열법으로 제조한 반용융 A390합금의 미세조직 및 성형성)

  • 엄정필;장동훈;김득규;윤병은;임수근
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1997.06a
    • /
    • pp.160-173
    • /
    • 1997
  • Microstructure of hypereutectic Al-17wt.% Si alloy, fabricated by mechanical stirring and by reheating at semi-solid state, was investigated by optical microscope. Flow behavior semi-solid metal also was investigated at diffentent mould temperatures 280$^{\circ}C$, 290$^{\circ}C$ and 300$^{\circ}C$. Size of silicon particles were increased over 100$\mu\textrm{m}$ during solidification as a result of stirring. It is considered as microstructural coarsening by bonding between neighbouring primary silion particles during stirring of slurry. In case of reheating at semi-solid state, however, primary silicon particle was not increased at size of 40$\mu\textrm{m}$ and nearly spherical aluminum solde particle also could be obtained uniformly in distribution. The fludity of Al-17wt.% Si alloys at semi-solid state was improved when solid fraction was 0.7 at mould temperature of 300$^{\circ}C$ than other conditions.

  • PDF

Material Removal Rate Modeling of SiO2/TiO2 Mixed-Abrasive Slurry CMP for SiC (SiO2/TiO2 혼합입자 슬러리 SiC CMP의 재료제거율 모델링)

  • Hyunseop Lee
    • Tribology and Lubricants
    • /
    • v.39 no.2
    • /
    • pp.72-75
    • /
    • 2023
  • Silicon carbide (SiC) is used as a substrate material for power semiconductors; however, SiC chemical mechanical polishing (CMP) requires considerable time owing to its chemical stability and high hardness. Therefore, researchers are attempting to increase the material removal rate (MRR) of SiC CMP using various methods. Mixed-abrasive CMP (MAS CMP) is one method of increasing the material removal efficiency of CMP by mixing two or more particles. The aim of this research is to study the mathematical modeling of the MRR of MAS CMP of SiC with SiO2 and TiO2 particles. With a total particle concentration of 32 wt, using 80-nm SiO2 particles and 25-nm TiO2 particles maximizes the MRR at 8 wt of the TiO2 particle concentration. In the case of 5 nm TiO2 particles, the MRR tends to increase with an increase in TiO2 concentration. In the case of particle size 10-25 nm TiO2, as the particle concentration increases, the MRR increases to a certain level and then decreases again. TiO2 particles of 25 nm or more continuously decreased MRR as the particle concentration increased. In the model proposed in this study, the MRR of MAS CMP of SiC increases linearly with changes in pressure and relative speed, which shows the same result as the Preston's equation. These results can contribute to the future design of MAS; however, the model needs to be verified and improved in future experiments.

Mechanism on Extraction of Heavy Metals from Soil by Ultrasonication (초음파 조사에 의한 토양내 중금속 추출 기작 연구)

  • Shin, Yeon-Jun;Lee, Cha-Dol;Yoo, Jong-Chan;Yan, Jung-Seok;Kim, Ho-Sub;Baek, Kitae
    • Journal of Soil and Groundwater Environment
    • /
    • v.20 no.1
    • /
    • pp.28-35
    • /
    • 2015
  • In this study, the mechanisms on ultrasonication enhanced metals extraction were investigated compared with the conventional washing technique. We hypothesized the mechanisms on enhanced extraction of ultrasonication: ultrasonication increased the temperature of soil slurry and decreased average particle size of soil due to breakdown of soil aggregate. Actually, the ultrasonication increased the temperature of soil slurry to $60^{\circ}C$ in this study, and the increase in the temperature enhanced the metal extraction to 15-20% even in the conventional simple mixing. The conventional washing technique decreased average size of soil particles because of breakdown of soil aggregate, and the ultrasonication decreased the size more than that of washing. The breakdown of soil aggregate improved the contact between metals and washing agent, which enhanced the extraction of metals in the ultrasonication. Therefore, we concluded that the main mechanisms of ultrasonication are increase in the temperature and breakdown of the soil aggregate. Finally, the ultrasonicaiton increased the extractability of metals upto 40% compared to conventional washing technique.

Effect of Concentration and Surface Property of Silica Sol on the Determination of Particle Size and Electrophoretic Mobility by Light Scattering Method (광산란법에서 실리카 졸의 농도 및 표면특성이 입자 크기 및 전기영동 이동도 측정결과에 미치는 영향)

  • Cho, Gyeong Sook;Lee, Dong-Hyun;Kim, Dae Sung;Lim, Hyung Mi;Kim, Chong Youp;Lee, Seung-Ho
    • Korean Chemical Engineering Research
    • /
    • v.51 no.5
    • /
    • pp.622-627
    • /
    • 2013
  • Colloidal silica is used in various industrial products such as chemical mechanical polishing slurry for planarization of silicon and sapphire wafer, organic-inorganic hybrid coatings, binder of investment casting, etc. An accurate determination of particle size and dispersion stability of silica sol is demanded because it has a strong influence on surface of wafer, film of coatings or bulks having mechanical, chemical and optical properties. The study herein is discussed on the effect of measurement results of average particle size, sol viscosity and electrophoretic mobility of particle according to the volume fraction of eight types of silica sol with different size and surface properties of silica particles which are presented by the manufacturer. The measured particle size and the mobility of these sol were changed by volume fraction or particle size due to highly active surface of silica particle and change of concentration of counter ion by dilution of silica sol. While in case the measured sizes of small particles less than 60 nm are increased with increasing volume fraction, the measured sizes of larger particles than 60 nm are slightly decreased. The mobility of small particle such as 12 nm are decreased with increase of viscosity. However, the mobility of 100 nm particles under 0.048 volume fraction are increased with increasing volume fraction and then decreased over higher volume fraction.

Recover of gypsum from waste plaster board and the refining process

  • Song, Young-Jun;Hiroki Yotsumoto
    • Proceedings of the IEEK Conference
    • /
    • 2001.10a
    • /
    • pp.342-348
    • /
    • 2001
  • This study was conducted to obtain granular crystalline gypsum that can be used as raw material for plaster boards or cements from waste Plaster board. We could disintegrate preferentially gypsum to gypsum needle in 10${\mu}{\textrm}{m}$ or less size among the contents of waste plaster board (gypsum, paper, fiber, and inorganic material .etc.) by hydration afterwards the dehydration of crushed waste plaster board. In this case, the optimum conditions for minimizing the size of gypsum were dehydration rate of 75%~ 85%, hydration concentration of 10~20%, agitation speed of 250~400rpm, crushing size of 2cm or less. Gypsum of 98.21% grade was recovered with 99.0% yield from under screenings of 325mesh wet screening which followed by the dehydration-hydration process performed in the conditions of dehydration rate of 80%, hydration concentration of 15%, agitation speed of 300rpm, crushing size of 2cm or less. Subsequently, Plate-like Crystalline gypsum of is 151${\mu}{\textrm}{m}$ size and the grade of 99.49% with the Yield of 98.0% from the upper screenings of 270mesh wet screening carried out after the re-crystallization of the recovered gypsum needle slurry.