• 제목/요약/키워드: Sintered properties

검색결과 1,953건 처리시간 0.03초

방전플라즈마 소결된 Bi0.5Sb1.5Te3의 열/전기적 특성 (The Electric and Thermal Properties of Spark Plasma Sintered Bi0.5Sb1.5Te3)

  • 이길근;최영훈;하국현
    • 한국분말재료학회지
    • /
    • 제19권4호
    • /
    • pp.285-290
    • /
    • 2012
  • The present study was focused on the analysis of the electric and thermal properties of spark plasma sintered $Bi_{0.5}Sb_{1.5}Te_3$ thermoelectric material. The crystal structure, microstructure, electric and thermal properties of the sintered body were evaluated by measuring XRD, SEM, electric resistivity, Hall effect and thermal conductivity. The $Bi_{0.5}Sb_{1.5}Te_3$ sintered body showed anisotropic crystal structure. The c-axis of the $Bi_{0.5}Sb_{1.5}Te_3$ crystal aligned in a parallel direction with applied pressure during spark plasma sintering. The degree of the crystal alignment increased with increasing sintering temperature and sintering time. The electric resistivity and thermal conductivity of the $Bi_{0.5}Sb_{1.5}Te_3$ sintered body showed anisotropic characteristics result from crystal alignment.

소결첨가재에 의한 텅스텐의 기계적 특성평가 (Evaluation on Mechanical Properties of Tungsten by Sintering Additive Content)

  • 이상필;이진경
    • 한국산업융합학회 논문집
    • /
    • 제25권4_2호
    • /
    • pp.621-626
    • /
    • 2022
  • Tungsten is a high melting point metal unlike other steel materials, and it is difficult to manufacture because of its high melting temperature. In this study, pressure sintering process method was applied to manufacture the tungsten materials at low temperature. Therefore, it is necessary to densify the sintered material by using a sintering additive. Studies have been conducted on how the amount of titanium for sintering tungsten affects the mechanical properties of tungsten in this study. In order to secure the densification mechanism of tungsten powder during the sintering process, the characteristics of the sintered tungsten material according to the change of titanium content were evaluated. It was investigated the relationship between sintering parameters and mechanical properties for densification of microstructures. The sintered tungsten materials according to sintering additive content showed high sintered density (about 16.31g/cm3) and flexural strength (about 584 MPa) when the content of sintering additive was 3 wt%. However, as the content of the sintering additive increases, mechanical property of flexural strength is decreased, and the porosity is increased due to the heterogeneous sintering around titanium.

Properties of Powders and Sintered Bodies of Sialon $Si_3N_4$ and SiC Prepared from Korean Raw Materials

  • 이홍림
    • 한국세라믹학회:학술대회논문집
    • /
    • 한국세라믹학회 1986년도 Priceedings Of The Third Korea-Japan Seminar On New Ceramics
    • /
    • pp.156-161
    • /
    • 1986
  • Sialon $Si_3N_4$ and SiC powders and ceramics were prepared from Korean natural resources. The properties of the powders and sintered ceramics obtained in this work are considered to be comparable to those of foreign articles.

  • PDF

산화물 환원공정에 의해 제조된 Bi2Te2.7Se0.3 분말의 열전특성 (Thermoelectric Properties of Bi2Te2.7Se0.3 Powder Synthesized by an Oxide-Reduction Process)

  • 박배건;이길근;김우열;하국현
    • 한국분말재료학회지
    • /
    • 제18권5호
    • /
    • pp.437-442
    • /
    • 2011
  • The present study focused on the synthesis of Bi-Te-Se-based powder by an oxide-reduction process, and analysis of the thermoelectric properties of the synthesized powder. The phase structure, chemical composition, and morphology of the synthesized powder were analyzed by XRD, EPMA and SEM. The synthesized powder was sintered by spark plasma sintering. The thermoelectric properties of the sintered body were evaluated by measuring its Seebeck coefficient, electrical resistivity, and thermal conductivity. $Bi_2Te_{2.7}Se_{0.3}$ powder was synthesized from a mixture of $Bi_2O_3$, $TeO_2$, and $SeO_2$ powders by mechanical milling, calcination, and reduction. The sintered body of the synthesized powder exhibited n-type thermoelectric characteristics. The thermoelectric properties of the sintered bodies depend on the reduction temperature. The Seebeck coefficient and electrical resistivity of the sintered body were increased with increasing reduction temperature. The sintered body of the $Bi_2Te_{2.7}Se_{0.3}$ powder synthesized at $360^{\circ}C$ showed about 0.5 of the figure of merit (ZT) at room temperature.

디젤엔진용 소결(W/C35%Ni) 태핏의 마멸거동에 관한 연구 (A Study on Friction and Wear Characteristics of Sintered W/C-35%Ni Tappets for Diesel Engine Application)

  • 류병진;오세일;박맹로;양승호
    • Tribology and Lubricants
    • /
    • 제16권1호
    • /
    • pp.33-38
    • /
    • 2000
  • Abstract- In this paper tribological characteristics of solid and liquid phase sintered W/C-35%Ni tappets were investigated. Three test methods were performed to investigate the wear and surface damage mechanism of sintered tappets. First, block-on-ring wear test was performed to investigate the wear characteristics under pure sliding condition. Second, simplified cam and tappet tests (called component wear test hereafter) were carried out to simulate the real contact history of cam and tappet. Also, after the test, contact surfaces were analyzed with scanning electron microscope to study the wear mechanism. As a final screening, engine dynamo tests were performed. Results showed that in the block on ring sliding wear test, solid phase sintered specimens showed superior wear resistance to liquid phase sintered specimens. The component wear tests and engine dynamo tests also showed the same results. Therefore, in these tests, solid phase sintered tappet material revealed superior wear resistant properties to liquid phase sintered one.

Effects of Sintering Conditions on the Properties of Sintered Molybdenum

  • Kadokura, Takanori;Hiraoka, Yutaka;Nakabayashi, Seiji;Yamamoto, Yoshiharu
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1153-1154
    • /
    • 2006
  • Effects of sintering conditions such as sintering temperature and heating rate on oxygen content, density, microstructure and toughness of sintered Mo were investigated. The oxygen content of the sintered Mo significantly depended on the sintering conditions. The oxygen content of the primary sintered(below 1673 K) Mo influenced the densifications. The number of pores at grain boundaries of the secondary sintered(at 2073 K)Mo depended on the oxygen content of the primary sintered Mo. Grain growth of the secondary sintered Mo was inhibited by the existence of pores at the grain boundaries. The secondary sintered Mo having larger number of pore and smaller grain size demonstrated higher strength.

  • PDF

주철분말(鑄鐵粉末)의 소결성에(燒結性) 미치는 산화철(酸化鐵) 첨가(添加)의 효과(效果) (The Effect of Fe-Oxide Addition on the Sintering Properties of Cast Iron Powder)

  • 김형수;김철범;나형용
    • 한국주조공학회지
    • /
    • 제10권1호
    • /
    • pp.64-70
    • /
    • 1990
  • In order to lower the cabon content of sintered products below the solubility of austenite, Fe-oxide was added to cast iron powder of which matrix was pearlite. And the effects of it on some sintering properties and mechanical properties were investigated. Roughly speaking, the linear shrinkage, density, and tensile strendth of sintered properties increased as the sintering temperature became higher, the size distribution of powder became finer, and the amount of Fe-oxide added became less. The maximum tensile strength of sintered products was $78㎏f/mm^2$ more or less, of which carbon content was 1.4% and sintering temperature was $1180^{\circ}C$.

  • PDF

다결정 $Y_3Fe_5O_{12}$의 미세구조와 자기적 특성 연구 (The Study on the Microstructure and Magnetic Properties of Polycrystalline $Y_3Fe_5O_{12}$)

  • 이재동;김성재;이승호;김태옥
    • 한국세라믹학회지
    • /
    • 제30권12호
    • /
    • pp.1015-1022
    • /
    • 1993
  • The formation process of polycrystalline YIG(Y3Fe5O12) prepared by conventional method in Fe2O3-Y2O3 system was investigated. Effect of the microstructure of sintered body on electromagnetic properties was also investigated. Orthoferrite (YFeO3) was formed between 900 and 110$0^{\circ}C$. Formation of YIG phase begin at 110$0^{\circ}C$ with sharp increased saturation magnetization simultaneously. YIG phase is identified as single phase above 120$0^{\circ}C$. The microstructures and electromagnetic properties of sintered bodies are varied due to calcination condition of starting materials. The sintered YIG of calcined sample at 110$0^{\circ}C$ has such magnetic properties as Bs=1580G, BHC=1.89Oe, Tc=570K, ΔH(9.3GHz)=78Oe.

  • PDF

20mol% Gd-doped 소결체 CeO$_2$ 전해질의 전기적 특성분석 (Characterization for Electrical Properties of Sintered 20mol% Gd-doped CeO$_2$ Electrolyte)

  • 김선재;국일현
    • 한국세라믹학회지
    • /
    • 제35권1호
    • /
    • pp.97-105
    • /
    • 1998
  • 20mol% Gd-doped CeO2 ultrafine powders as a promising electrolyte for the low temperature solid ox-ide fuel cells were synthesized with particle sizes of 15-20 nm using glycine nitrate process(GNP) fol-lowed by sintering their pellets at 150$0^{\circ}C$ for various times in air and then the electrical properties of the sintered pellets were investigated. The sintering behaviors and electrical properties for the sintered 20 sintered mol% Gd-doped CeO2 pellets were analyzed using dilatometer and SEM and AC two-terminal impedance technique respectively. As the heating temperature increased the synthesized powder had the sintering behaviors to show the start of the significant shrink at temperature of about $700^{\circ}C$ and to show the end of the shrink at the temperature of about 147$0^{\circ}C$. When the pellets were sintered with the vaious times at 150$0^{\circ}C$ the temperatuer which the shrink had been already completed the grain sizes in the sintered 20 mol% Gd-doped GeO2 pellets increased with the increase of the sintering time but their electrical resis-tivities showed the minimum value at the sintering time of 10h. It is due that the pellet sintered for 10h had the minimum activation energy fior the electtrical conduction. Thus it is thought that the decrease of the activation energy with the increase of the sintering time to 10h is induced by the enhanced mi-crostructure like the decrease of pore amount and the grain growth and its increase with the sintering times more than 10h is induced by the increase of the amounts of the impurities such as Mg. Al and Si from the sintering atmosphere.

  • PDF

치과보철용 Ni-Cr-Ti 소결체합금의 포셀린결합력 및 기계적 특성 (Porcelain Bonding Strength and Mechanical Properties of Sintered Ni-Cr-Ti Alloy for Dental Prosthodontics)

  • 최한철;박선영;심명섭
    • 한국표면공학회지
    • /
    • 제49권6호
    • /
    • pp.560-566
    • /
    • 2016
  • In this study, porcelain bonding strength and mechanical properties of sintered Ni-Cr-Ti alloy for dental prosthodontics have been researched experimentally. Mechanical and morphological characteristics of the alloys were examined by Vickers hardness test, tensile and bonding strength test, surface roughness test, field-emission scanning electron microscopy, energy dispersive X-ray spectroscopy, and X-ray diffraction. In the sintered Ni-13Cr-xTi alloys, morphology of sintered alloy showed porous matrix diffused with alloying elements of Cr and Ti, and showed dendritic structure after melting process. From the XRD results, the second phases of NiCr, $Ni_3Cr$, and $Ni_3Ti$ were formed in the case of sintered and melted Ni-13Cr-xTi alloys. The tensile strength and hardness of Ni-13Cr-xTi alloys increased, as Ti content increased. Surface roughness increased, as Ti content increased. The bonding strength between metal and porcelain of Ni-13Cr-5Ti alloy was higher than those of Ni-13Cr and Ni-13Cr-10Ti alloys