액장 소결에 의한 $\beta-SiC-ZrB_2$ 복합체의 제조와 특성 (Properties and Manufacture of the $\beta-SiC-ZrB_2$ Composited Densified by Liquid-Phase Sintering.)

  • 신용덕;주진영
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제48권2호
    • /
    • pp.92-97
    • /
    • 1999
  • The mechanical and electrical properties of the hot-pressed and annealed $\beta-Sic$+39vol.%$ZrB_2$ electroconductive ceramic composites were investigated as a function of the liquid forming additives of $Al_2O_3+Y_2O_3(6:4wt%)$. In this microstructures, no reactions and elongated $\alpha$-SiC grains with equiaxed $ZrB_2$, gains were observed between $\beta-SiC$ and $ZrB_2$, and the relative density was over 97.6% of the theoretical density. Phase analysis of the composites by XRD revealedmostly of $\alpha$-SiC(6H, 4H), $ZrB_2$, and weakly $\beta-SiC$(15R) phase. The fracture toughness decreased with increasing $Al_2O_3+Y_2O_3$ contents and showed the highest of $6.37MPa.m^{\fraction ane-half}$ for composite added with 4wt% $Al_2O_3+Y_2O_3$ additives at room temperature. The electrical resistivity increased with increasing $Al_2O_3+Y_2O_3$contents and showed the lowest of $1.51\times10^{-4}\Omega.cm$ for composite added with $Al_2O_3+Y_2O_3$ additives at $25^{\circ}C$. This reason is the increasing tendency of pore formation according to amount of liquid forming additives $Al_2O_3+Y_2O_3$. The electrical resistivity of the composites was all positive temperature coefficient resistance(PTCR) against temperature up to $700^{\circ}C$.

  • PDF

용탕단조에 의한 $Al_2O_3-SiO_2$ 단섬유 및 SiC whisker강화 알루미늄 합금기 복합재료의 제조 (Fabrication of Aluminum Alloy Composites Reinforced with SiC whisker an $Al_2O_3-SiO_2$ Short Fiber by Squeeze Casting)

  • 홍성길;윤중렬;최정철
    • 한국주조공학회지
    • /
    • 제17권1호
    • /
    • pp.28-35
    • /
    • 1997
  • SiC whisker and $Al_2O_3-SiO_2$ short fiber reinforced AC8A, AC8B and AC8B(J) marix composites were fabricated by squeeze casting method. Preform deformation, change of reinforcement volumefraction and formation of macro-segregation in two composites were investigated by using micro Vickers hardness test, analysis of macro and micro structures with OM, SEM and EDAX. $Al_2O_3-SiO_2$ short fiber preform manufactured with 5% $SiO_2$ binder in this study was considerably deformed and cracked, nevertheless, the short fibers were distributed homogeneously in the composites. In SiC whisker reinforced composites, on the other hand, preform deforming and cracking were not occurred, however, macro segregation zone formed along the infiltration routes by interface reaction during infiltration of molten metal into the preform was observed at center-low area in the composites. The decrease of hardness in the macro segregation zone resulted from the depletion of Si and Mg atoms.

  • PDF

FHD법에 의한 $B_2O_3-P_2O_5-SiO_2$ 실리카막의 효과적인 $P_2O_5$ 도핑 (The Effective $P_2O_5$ Doping into $B_2O_3-P_2O_5-SiO_2$ Silica Layer Fabrication by Flame Hydrolysis Deposition)

  • 심재기;이윤학;성희경;최태구
    • 한국세라믹학회지
    • /
    • 제35권4호
    • /
    • pp.364-370
    • /
    • 1998
  • 광집적회로용 평면도파로를 구현하기 위한 $B_2O_3-P_2O_5-SiO_2$ 실리카 광도파막을 실리콘 기판위에 FDH(Flame Hydrolysis Depositon)법으로 제조하여 미립자의 미세구조, 실리카막의 굴절률과 조성을 고찰하였다. FHD법에서 도펀트(dopant)물질로, $B_1\;P_1\;Ge$ 등의 산화물이 사용되며, $B_1$ Ge 산화물의 경우 $SiO_2$와의 결합특성이 우수하여 비교적 도핑(doping)이 용이하지만 P의 경우 $P_2O_5$의 낮은 융점에 의한 증발 등으로 효과적인 도핑이 어렵다. 수직형 FHD 토치를 사용하고 화염온도, 기판온도, 토치와 기판간의 거리를 최적화하여 P 농도가 3.3 Wt%이상이고 고밀화 온도가 $1180^{\circ}C$ 이하인 양질의 실리카막을 얻었다. 실리카막의 굴절률은 $1.55\;\mu\textrm{m}$ 파장에서 $1.4480{\pm}1{\times}10^{-1}$로 측정되었으며, $22{\pm}1\;\mu\textrm{m}$의 두께를 보였다.

  • PDF

YAG와 기공에 의한 $SiC-TiB_2$ 전도성세라믹 복합체의 특성 평가 (Estimation of the Properties for the $SiC-TiB_2$ Electroconductive Ceramic Composites by YAG and Porosity)

  • 신용덕;이동윤
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제50권11호
    • /
    • pp.544-549
    • /
    • 2001
  • The mechanical and electrical properties of the hot-pressed and pressureless annealed SiC-39vo1.%TiB$_2$electroconductive ceramic composites were investigated as functions of the liquid additives of $Al_2O_3+Y_2O_3$ and the sintering temperature. The result of phase analysis for the SiC-39vo1.%TiB$_2$ composites by XRD revealed $\alpha -SiC(6H),\; TiB_2,\; and YAG(Al_5Y_3O_{12})$ crystal phase. The relative density of SiC-39vo1.% $TiB_2$ composites was increased with increased $Al_2O_3+Y_2O_3$ contents. The fracture toughness showed the highest value of $7.8 MPa.m_{1/2}$ for composites added with 12 wt% $Al_2O_3+Y_2O_3$additives at $1750^{\circk}C$. The electrical resistivity of the SiC-39vo1.%$TiB_2$composites was all positive temperature coefficient resistance(PTCR) in the temperature range of $25S^{\circ}C \;to\; 700^{\circ}C$.

  • PDF

고체산화물 연료전지용 밀봉유리의 제조 및 물성평가 (Preparation and Characterization of Sealing Glass for Solid Oxide Fuel Cell)

  • 손성범;오승한;최세영;김긍호;송휴섭
    • 한국세라믹학회지
    • /
    • 제38권2호
    • /
    • pp.158-165
    • /
    • 2001
  • 고체산화물 연료전지용 밀봉재로서 전지 구성원과 열팽창계수가 유사하고 비젖음성 특성을 가지며 전지 작동온도에서 화학적 안정성을 갖는 밀봉유리를 개발하고자, BaO-Al$_2$O$_3$-La$_2$O$_3$-Ba$_2$O$_3$-SiO$_2$계 유리를 제조하여 조성 변화에 따른 열적 특성 변화와 접합후의 젖음성 및 반응성 등을 조사하였다. 유리망목 형성산화물인 B$_2$O$_3$와 SiO$_2$의 함량비 및 BaO의 망목 형성산화물(B$_2$O$_3$+SiO$_2$)에 대한 함량비 변화에 따른 유리의 열적 특성을 조사한 결과, 0.33~0.71의 B$_2$O$_3$/SiO$_2$함량비하에서 BaO/(B$_2$O$_3$+SiO$_2$)가 0.70일 때 유리의 열팽창계수는 106~111$\times$$10^{-7}$/K 이었으며 이때 연료전지 구성원인 YSZ(yttria stabilized zirconia)와의 열팽창 불일치(thermal expansion mismatch)가 가장 작았다. 또한 이러한 조성의 유리로부터 분말성형체를 제조하여 YSZ에 접합을 시도한 결과, 우수한 접합성 및 비젖음성을 확인할 수 있었으며, 800~8$50^{\circ}C$의 전지 작동온도에서 100시간까지 유지시에도 YSZ와의 계면반응이 일어나지 않음을 관찰할 수 있었다.

  • PDF

Refractive-index Prediction for High-refractive-index Optical Glasses Based on the B2O3-La2O3-Ta2O5-SiO2 System Using Machine Learning

  • Seok Jin Hong;Jung Hee Lee;Devarajulu Gelija;Woon Jin Chung
    • Current Optics and Photonics
    • /
    • 제8권3호
    • /
    • pp.230-238
    • /
    • 2024
  • The refractive index is a key material-design parameter, especially for high-refractive-index glasses, which are used for precision optics and devices. Increased demand for high-precision optical lenses produced by the glass-mold-press (GMP) process has spurred extensive studies of proper glass materials. B2O3, SiO2, and multiple heavy-metal oxides such as Ta2O5, Nb2O5, La2O3, and Gd2O3 mostly compose the high-refractive-index glasses for GMP. However, due to many oxides including up to 10 components, it is hard to predict the refractivity solely from the composition of the glass. In this study, the refractive index of optical glasses based on the B2O3-La2O3-Ta2O5-SiO2 system is predicted using machine learning (ML) and compared to experimental data. A dataset comprising up to 271 glasses with 10 components is collected and used for training. Various ML algorithms (linear-regression, Bayesian-ridge-regression, nearest-neighbor, and random-forest models) are employed to train the data. Along with composition, the polarizability and density of the glasses are also considered independent parameters to predict the refractive index. After obtaining the best-fitting model by R2 value, the trained model is examined alongside the experimentally obtained refractive indices of B2O3-La2O3-Ta2O5-SiO2 quaternary glasses.

투명 유전체 (PbO-B2O3-SiO2-Al2O3 계)와 Ag 전극과의 반응에 의한 Ag+과 Sn2+의 거동 (Behavior of Ag+ and Sn2+ After Reaction Between the Transparent Dielectric PbO-B2O3-SiO2-Al2O3 and Ag Electrodes)

  • 홍경준;박준현;허증수;김형준
    • 한국재료학회지
    • /
    • 제12권5호
    • /
    • pp.347-352
    • /
    • 2002
  • A transparent dielectric of the $PbO-B_2O_3-SiO_2-A1_2O_3$ system which was a low melting glass has been used for PDP (Plasma Display Panel), but it has a problem which is a reaction to be occurred between a transparent dielectric layer and electrodes (Ag, ITO) after firing. This research was conducted for ion migration of $Ag^+\$ and $Sn^ {2+}$ during firing three different frits of low melting glass. The result showed that yellowing phenomena occurred through a chemical reaction between $Ag^+\$and $Sn^ {2+}$ at 550~58$0^{\circ}C$ for 20~60 min. In addition, it was confirmed that the migration of $Sn^{2+}$ from ITO electrode made a strong effect on the yellowing phenomena.