• 제목/요약/키워드: Si/Al 복합

검색결과 350건 처리시간 0.027초

자전연소법으로 제조한 Al2O3.SiC 입자로 보강된2024/(Al2O3.SiC)p 복합재료의 기계적특성 (Mechanical Properties of 2024/(Al2O3.SiC)p Composite Reinforced with Al2O3.SiC Particle Prepared by SHS Process)

  • 맹덕영
    • 한국분말재료학회지
    • /
    • 제7권1호
    • /
    • pp.35-41
    • /
    • 2000
  • Al2O3$.$SiC particle was prepared was prepared by the self-propagting high temperature sYthesis(SHS) process from a mixture of SiO2, Al and C powders, The fabricated Al2O3$.$SiC particle was applied to 2024Al/(Al2O3$.$SiC)pcomposite as a reinforcement. Aluminum matix composites were fabricares by the powder extrusion method using the synthesized Al2O3$.$SiC particle and commercial 2024Al powder. Theoptimum preparation conditions for Al2O3$.$SiC partticle by SHS process were described. The influence of the Al2O3$.$SiC voiume fraction on the mechanical was composite was also discussed. Despite adiabatic temperature was about 2367K, SHs reaction was completed not by itself, but by using pre-heating. Mean particle size of final particle synthesized was 0.73 ${\mu}$m and most of the particle was smaller than 2${\mu}$m. Elastic modulus and tensile strength of the composite increased with increase the volume fraction of reinforcement but, tensile strength depreciated at 30 vol% of reinforcement.

  • PDF

알루미나 탄화규소 복합세라믹스 균열치유재의 강도와 탄성파 특성 (Strength of Crack Healed-Specimen and Elastic Wave Characteristics of Al2O3/SiC Composite Ceramics)

  • 김해숙;김미경;김진욱;안석환;남기우
    • 대한기계학회논문집A
    • /
    • 제31권4호
    • /
    • pp.425-431
    • /
    • 2007
  • [ $Al_2O_3/SiC$ ]composite ceramics were sintered to evaluate the bending strength and elastic wave characteristics. The three-point bending test was carried out under room temperature. The elastic wave was detected by fracture wave detector. The crack healing behavior was investigated from 1373 K to 1723 K. The bending strength of $Al_2O_3/SiC$ composite by nanocomposite is higher than that of $Al_2O_3$ monolithic. Crack-healing behavior depended on an amount of additive powder $Y_2O_3$. In $Al_2O_3/SiC$ composite ceramics with 3 wt. % $Y_2O_3$ for additive powder, the bending strength at 1573 K is about 100% increase than that of the smooth specimens. From the result of wavelet analysis of elastic wave signal, the smooth specimen and heat treated specimen of $Al_2O_3$ monolithic and $Al_2O_3/SiC$ composite ceramics showed characteristics of frequency about 58 kHz. The strength of $Al_2O_3/SiC$ composite ceramics was a little higher than those of $Al_2O_3$ monolithic. The dominant frequencies were high with increasing of $Y_2O_3$ for additive powder. The dominant frequencies had direct connection with the bending strength.

용사법에 의한 Al/Al-SiC 복합재료의 제조 (Fabrication of Al/Al-SiC Composites by Thermal Spray Process)

  • 김균택;김영식
    • 동력기계공학회지
    • /
    • 제10권2호
    • /
    • pp.93-98
    • /
    • 2006
  • Metal matrix composites(MMCs) reinforced with ceramic particulates are receiving increasing attention because their high specific strength, low coefficient of thermal expansion and excellent wear resistance. Especially, Al-based composites(AMCs) have been widely applied for the aerospace and automotive industries. Such composites are mainly fabricated by the cast, powder metallurgy and infiltration process. In this study, SiC particulate reinforced Al-based composites were fabricated by thermal spray process and their wear behavior were investigated. Composites with different spray parameter were fabricated by using flame spray apparatus. Microstructure and wear behavior of the composites were observed by scanning electron microscope(SEM) and electron probe micro-analysis(EPMA).

  • PDF

($\textrm{Al}_2\textrm{O}_3$+SiCp)/AZ91 하이브리드 Mg 복합재료의 기계적 특성에 미치는 SiCp크기의 영향 (The Effect of SiCp Size on the Mechanical Preperties of ($\textrm{Al}_2\textrm{O}_3$+SiCp)/AZ91 Hybrid Mg Composites)

  • 하창식;김봉룡;조경목;박익민;최일동
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2001년도 춘계학술발표대회 논문집
    • /
    • pp.29-33
    • /
    • 2001
  • In the present study, AZ91Mg/$\textrm{Al}_2\textrm{O}_3$ short fiber+SiC particulates hybrid metal matrix composites(MMCs) were fabricated by squeeze casting method. Different particulate sizes of 45, 29 and $9\mu\textrm{m}$ were hybridized with 5% volume fraction to investigate the effect of SiC particulates size on microstructure, mechanical and thermal properties such as hardness, flexural strength, wear resistance and thermal expansion. Results show that the microstructure of the hybrid composites were quite satisfactory, namely revealing relatively uniform distribution of reinforcements. Some aggregation of SiC particulates caused by particle pushing was observed especially in the hybrid composites containing in fine particulates($9\mu\textrm{m}$). The hardness and flexural strength were improved by decreasing particulates size, whereas wear resistance improved by increasing particulates size because of large particulates restricting matrix wear from contacted stress. Regardless of particulates size, thermal expansion of composites was the same. This may be because the content of particulates was in all cases 5 volume fraction.1

  • PDF

Al-Si-SiC 복합분말과 Al-Zn-Mg계 합금분말이 혼합된 분말의 소결 거동 및 기계적 특성연구 (Investigation on the Sintering Behavior and Mechanical Properties of Al-Zn-Mg Alloy Powders Mixed with Al-Si-SiC Composite Powders)

  • 장광주;김경태;양상선;김용진;박용호
    • 한국분말재료학회지
    • /
    • 제21권6호
    • /
    • pp.460-466
    • /
    • 2014
  • Al-Si-SiC composite powders with intra-granular SiC particles were prepared by a gas atomization process. The composite powders were mixed with Al-Zn-Mg alloy powders as a function of weight percent. Those mixture powders were compacted with the pressure of 700 MPa and then sintered at the temperature of $565-585^{\circ}C$. T6 heat treatment was conducted to increase their mechanical properties by solid-solution precipitates. Each relative density according to the optimized sintering temperature of those powders were determined as 96% at $580^{\circ}C$ for Al-Zn-Mg powders (composition A), 97.9% at $575^{\circ}C$ for Al-Zn-Mg powders with 5 wt.% of Al-Si-SiC powders (composition B), and 98.2% at $570^{\circ}C$ for Al-Zn-Mg powders with 10 wt.% of Al-Si-SiC powders (composition C), respectively. Each hardness, tensile strength, and wear resistance test of those sintered samples was conducted. As the content of Al-Si-SiC powders increased, both hardness and tensile strength were decreased. However, wear resistance was increased by the increase of Al-Si-SiC powders. From these results, it was confirmed that Al-Si-SiC/Al-Zn-Mg composite could be highly densified by the sintering process, and thus the composite could have high wear resistance and tensile strength when the content of Al-Si-SiC composite powders were optimized.

Si/Al 복합 무기염을 적용한 모르타르의 염소이온침투깊이에 대한 실험적 연구 (An Experimental Study on Chloride Ions Penetration of Mortar containing Si/Al Hybrid-Inorganic Salt)

  • 길배수;김도수;강용식;김우재;최세진;김성수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2009년도 춘계 학술대회 제21권1호
    • /
    • pp.417-418
    • /
    • 2009
  • 해안 및 매립지 구조물은 염화물의 침투로 인해 매입된 철근의 피막파괴로 철근부식이 일어나 콘크리트 구조체에 열화가 급속하게 진행되기 때문에 앞으로의 해안 구조물의 수밀성, 내염해성을 필요로 한다. 따라서 본 연구에서는 내염해성 개선에 효과적인 액상형태의 Si/Al 복합 무기염을 모르타르에 적용하여 시간경과(7, 14, 28, 56일)에 따른 내염해특성을 파악하고자 하였다.

  • PDF

1.55 $\mu\textrm{m}$ 광증폭기용 Er/Al 첨가 광도파막의 제조 (The Fabrication of Er/Al Co-doped Silica Films for 1.55 $\mu\textrm{m}$ Optical Amplifier)

  • 노성인;김재선;정용순;신동욱;송국현
    • 한국세라믹학회지
    • /
    • 제38권12호
    • /
    • pp.1144-1149
    • /
    • 2001
  • 본 연구에서는 화염가수분해증착법(Flame Hydrolysis Deposition : FHD)을 이용하여 실리콘(Si)/실리카(SiO$_2$) 광도파막을 제조하고, 이 박막에 Solution Doping 법을 이용해 Er/Al을 복합 첨가하여 광증폭 매질을 제작하는 연구를 수행하였다. 형광 측정을 통해 Al의 복합첨가에 의한 형광효율의 감소 방지 및 형광 스펙트럼의 반치폭 증가를 확인할 수 있었다. 즉, Al가 0.48wt%가 첨가된 경우, Er가 0.14wt% 첨가되는 경우에도 형광세기가 감소하지 않음을 확인하였으며, $1.5mu extrm{m}$ 대역의 형광스펙트럼의 대역폭이 약 5nm 정도 증가됨을 관찰하였다.

  • PDF