• Title/Summary/Keyword: Sheath-core monofilament

Search Result 2, Processing Time 0.018 seconds

Biodegradable sheath-core biphasic monofilament braided stent for bio-functional treatment of esophageal strictures

  • Han, Cheol-Min;Lih, Eugene;Choi, Seul-Ki;Bedair, Tarek M.;Lee, Young-Jae;Park, Wooram;Han, Dong Keun;Son, Jun Sik;Joung, Yoon Ki
    • Journal of Industrial and Engineering Chemistry
    • /
    • v.67
    • /
    • pp.396-406
    • /
    • 2018
  • In this study, a polydioxanone (PDO) and poly(L-lactic acid) (PLLA) sheath-core biphasic monofilament was designed to develop an esophageal stent with improved mechanical properties and controlled biodegradability. The radial force of PDO/PLLA sheath-core stent was 10.24 N, while that of PDO stent was 5.64 N. Deteriorations of tensile strength, elastic modulus and elongation during degradation test were also delayed on PDO/PLLA group. Hyaluronic acid-dopamine conjugate and $BaSO_4/PDO$ conjugate coating layers provided improved tissue adhesion strength and reasonable X-ray contrast, respectively. Taken all together, the sheath-core filaments with tissue adhesive and radiopaque properties will be useful in designing esophageal stents.

Fabrication of Superconducting Joints between 61 Filaments of BSCCO 2223 Tapes (61심 BSCCO 2223 고온초전도 선재의 접합부 제조)

  • 김철진;박성창;유재무
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.2
    • /
    • pp.137-144
    • /
    • 1998
  • High-temperature superconducting joints between 61 filaments of Bi-2223 tapes were fabricated by chem-ical corrosion and repeated thermomechanical process. The silver sheath of the superconducting tape was chemically removed using chemical etchant(NH4OH:H2O2=1:1) from one side of each tape without altering the form of lap joint. The joined region was formed by uniaxial pressing and a series of thermomechanical process and then subjected to properties measurement and microstructural analysis. The critical current(Ic) variation and I-V characteristics along the joint were mesured with several configuration of proble points. Ic value of the transition region of the joint inthe multifilament tape which limit the total current carring capacity of the superconducting tape was higher than that of monofilament tape. But the transition ex-ponent n-value of the multi-filament tape was lower than that of monofilament wire due to the interaction of the individual superconducting core of the multi-filament. The critical current through the joint area was improved by respeated press and reaction annealing treatment.