THE COMPARISON OF SHEAR STRENGTH AND BRACKET PLACEMENT BETWEEN BONDING TECHNIQUES (접착술식에 따른 전단강도 및 Bracket위치의 비교)

  • Pak, Yun-Kyong;Kook, Yoon-A;Kim, Sang-Cheol
    • The korean journal of orthodontics
    • /
    • v.21 no.3
    • /
    • pp.513-520
    • /
    • 1991
  • The purpose of this study was to compare the bracket placement and the shear bond strength of indirect-bonded brackets with those of direct-bonded ones. Forty eight extracted human teeth were collected and attached with brackets and tested on shear bond strength, using Instron. Fourteen patients from Wonkwang University Dental Hospital were selected for direct bonding of brackets and their teeth were measured on bracket angulation and bracket height. The obtained results were as follows: 1. The shear bond strengths of incisors were higher in direct-bonding,group, rather than in-direct-bonding group. But, the shear bond strength of premolars showed no significant differences between groups. 2. The bracket angulations of indirect-bonding group were preciser than those of direct-bonding group, especially in upper first premolars, lower lateral incisors, canines, premolars. 3. In bracket height, there were no significant differences between groups.

  • PDF

Investigation of the effects of connectors to enhance bond strength of externally bonded steel plates and CFRP laminates with concrete

  • Jabbar, Ali Sami Abdul;Alam, Md Ashraful;Mustapha, Kamal Nasharuddin
    • Steel and Composite Structures
    • /
    • v.20 no.6
    • /
    • pp.1275-1303
    • /
    • 2016
  • Steel plates and carbon-fiber-reinforced polymer (CFRP) laminates or plates bonded to concrete substrates have been widely used for concrete strengthening. However, this technique cause plate debonding, which makes the strengthening system inefficient. The main objective of this study is to enhance the bond strength of externally bonded steel plates and CFRP laminates to the concrete surface by proposing new embedded adhesive and steel connectors. The effects of these new embedded connectors were investigated through the tests on 36 prism specimens. Parameters such as interfacial shear stress, fracture energy and the maximum strains in plates were also determined in this study and compared with the maximum value of debonding stresses using a relevant failure criterion by means of pullout test. The study indicates that the interfacial bond strength between the externally bonded plates and concrete can be increased remarkably by using these connectors. The investigation verifies that steel connectors increase the shear bond strength by 48% compared to 38% for the adhesive connectors. Thus, steel connectors are more effective than adhesive connectors in increasing shear bond strength. Results also show that the use of double connectors significantly increases interfacial shear stress and decrease debonding failure. Finally, a new proposed formula is modified to predict the maximum bond strength of steel plates and CFRP laminates adhesively glued to concrete in the presence of the embedded connectors.

The Effect of Resin Base Surface Treatment on Shear Bond Strength in Indirect Bracket Bonding Technique (브라켓 간접부착술식시 레진베이스의 표면처리가 전단결합강도에 미치는 영향)

  • Yim, Byeong-Cheol;Hwang, Hyeon-Shik
    • The korean journal of orthodontics
    • /
    • v.28 no.5 s.70
    • /
    • pp.681-688
    • /
    • 1998
  • The purpose of this study was to evaluate the effects of the surface treatments of resin bases in indirect bracket bonding technique by study of shear bond strengths and failure patterns. Ninety metal brackets were bonded to the stone models of specimens involving bovine lower incisor with light-cured adhesive(Light-Bond). After removal of brackets with the resin base from the stone models, the surfaces of resin bases in thirty brackets were treated with Plastic Conditioner and the surfaces of resin bases in another thirty brackets were treated with sandblaster and the remaining thirty brackets were served as controls. All brackets were transferred to the specimens and bonded using sealant. The shear bond strength was tested on universal testing machine, and failure pattern was assessed with the adhesive remnant index(ARI). The results were as follows: 1. Surface treatments of resin bases with Plastic Conditioner or sandblasting showed statistically higher shear bond strengths than no treatment group. 2. No significant difference in shear bond strength was found between Plastic Conditioner treatment and sandblasting treatment groups. 3. No significant difference in ARI scores was found among the three groups. 4. As the result of correlation analysis between shear bond strengths and hnl scores, failure at adhesive/bracket base interface tends to increase when the shear bond strength was high, but it was not significant statistically. The above results suggest that improvement of bond strength can be obtained by surface treatment of resin base in the indirect bonding technique.

  • PDF

Change in shear bond strength of orthodontic brackets using self-etching primer according to adhesive types and saliva contamination (Self-etching primer를 사용하여 교정용 브라켓 접착 시 접착제와 타액오염에 따른 전단결합강도 변화)

  • Nam, Eun-Hye;Yoon, Young-Ah;Kim, Il-Kyu
    • The korean journal of orthodontics
    • /
    • v.35 no.6 s.113
    • /
    • pp.433-442
    • /
    • 2005
  • The purpose of this study was to evaluate and compare the shear bond strength of orthodontic brackets depending on the variety of adhesives and whether saliva exists, by using self-etching primer (SEP). Groups were divided according to the type of adhesive into resin adhesive (Trans bond XT) and resin-modified glass ionomer cement (Fuji Ortho LC). One group of resin adhesive used XT primer after etching with 37% phosphoric acid, and the other group used self-etching primer. One group of resin-modified glass ionomer cement only used etching for bonding, and the other group used SEP. Each of the groups were also classified by whether saliva was contaminated or not. and then the shear bond strength was measured. The results showed that when using resin adhesive, the shear bond strength of SEP was lower than the XT primer. In the resin-modified glass ionomer cement groups, the shear bond strength which depends on the priming method, did not have a meaningful difference statistically When saliva was contaminated, the group which used SEP, regardless of the adhesive variety, had a greater shear bond strength than the normal priming group. From these results, SEP showed a shear bond strength that is possible to be used clinically, regardless of the adhesive variety. It can especially be clinically useful to use SEP to bond brackets even on tooth surfaces contaminated with saliva, because it offers the appropriate bonding strength as well as shorter treatment time and easy application.

Effect of Shear Key and Edge Length of Near Surface-Mounted FRP Plate in Concrete (콘크리트에 표면매입 보강된 FRP판의 전단키 및 연단거리 효과)

  • Seo, Soo-Yeon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.20 no.1
    • /
    • pp.41-47
    • /
    • 2016
  • This paper presents a bond test to find the effect of shear key and edge length from the bonded FRP in near surface-mounted(NSM) retrofit using FRP plate. Main parameters in the test are the location and size of shear key and the edge length. For the test, 10 specimens were made by embedding FRP plate of $3.6mm{\times}16mm$ into $400mm{\times}200(300)mm{\times}400mm$ concrete block and fixing it by using epoxy. Tensile load was applied to the FRP of the specimens until failure and was recorded at each load increase. In addition, the bond slip and elongation of FRP were measured during the test. From the test, it was found that the further the shear key located from the loading, the higher strength we could get. The bond strength inversely depended on the size of shear key. Especially, when the size of shear key was to be lagger than certain size, the bond strength decreased to very low value; even less than that of the case without shear key. The bond strength somewhat increased corresponding to the increase of edge length from the bonded end of FRP to loading in spite of same bond length. The bond-slip between FRP and concrete governed overall deformation in the bond test of NSM FRP so that the effect of excessive slip is necessary to be considered in the design.

A STUDY ON THE SHEAR BOND STRENGTH OF LIGHT-CURED GLASS IONOMER CEMENT (광중합형 글래스아이오노머 시멘트의 전단결합강도에 대한 연구)

  • Kim, Hyun-Yang;Tae, Ki-Chul;Kook, Yoon-Ah;Kim, Sang-Cheol
    • The korean journal of orthodontics
    • /
    • v.28 no.5 s.70
    • /
    • pp.689-698
    • /
    • 1998
  • The purpose of this study was to evaluate the shear bond strength of light cured glass ionomer cement to enamel surface which treated with $37\%$ phosphoric acid, $10\%$ polyacrylic acid, $1.23\%$ acidulated phosphate fluoride gel and no etching agent. To compare the shear bond strength of glass ionomer cement, light-cured composite resin and chemically-cured composite resin were empoloyed as controls. Eight experiments groups were composed. 10 specimens of each group were bonded by metal bracket by tested in universal testing machine for shear bond strength, in stereoscope for adhesive remnants index. The data were evaluated statistically by SPSS/PC+. The results were as follows. 1. Among the groups of $37\%$ phosphoric acid treated and dry and bonded with light cured glass ionomer, light cured composite resin, and chemically cured composite resin, the shear bond strength of glass ionomer group showed no significant difference to the others, but the shear bond strength of chemically cured resin showed statistically lower than that of light cured resin (p<0.05). 2. The shear bond strengths of glass ionomer cement to enamel treated group with $1.23\%$ acidulated phosphate fluoride gel and $10\%$ polyacrylic acid and $37\%$ phosphoric acid showed statistically higher than that of no etched enamel group(p<0.U). 3. In the groups of glass ionomer cement, the presence of moisture was not significantly effect to the shear bond strength (p<0.05). 4. After debonding, no etched enamel group showed less residual materials on the enamel surface than the group of enamel etched with $37\%$ Phosphoric acid.

  • PDF

The study on Comparison Evaluation of Shear Bond Strength of Co-Cr Based Alloy using for Porcelain Fused Metal (도재용착주조관용 Co-Cr계 비귀금속 합금의 전단결합강도 비교평가에 관한 연구)

  • Kim, Hee-Jin;Kim, Bu-Sob
    • Journal of Technologic Dentistry
    • /
    • v.32 no.3
    • /
    • pp.195-207
    • /
    • 2010
  • Purpose: The purpose of this study was to observe the microstructural changes of surface in the specimens, performing the shear bond strength testing. The currently most used non-precious alloys are nickel-chromium based alloys with or without beryllium. However, their biocompatibility has been questioned concerning possible damages to the health of the patient and professionals involved in the fabrication of prosthesis caused by long exposure to Ni and Be. An option to nickel-chromium alloys is the cobalt-chromium alloy, an alternative that does not sacrifice the physical properties of the metal porcelain systems. Studies in the animals substantially show that the cobalt-chromium alloys are relatively well tolerated, being therefore more biocompatible than the nickel-chromium alloys. Methods: Non-addition Be to nickel-chromium based alloy(Bellabond plus) and cobalt-chromium alloy which has been widely used(Wirobond C) fused with ZEO light porcelain classified control group and cobalt-chromium alloy which is developing alloy of Alphadent company in Korea(Alphadent alloy) fused with ZEO light porcelain classified experimental group. The specimens of $4mm{\times}4mm{\times}0.5mm$ were prepared as-cast and as-opaque to cast body to analyze the mechanical characteristic change, the microstructure of alloy surface. The phase change was used to observe through XRD analysis and OM/SEM was used to observe the surface of specimens as-cast and as-opaque to cast body. Chemical formation of their elements was measured with EDS. Then hardness was measured with Micro Vicker's hardness tester. Shear bond strength test thirty specimens of $10mm{\times}10mm{\times}2mm$ was prepared, veneered, 3mm high and 3mm in diameter, over the alloy specimens. The shear bond strength test was performed in a universal testing machine(UTM) with a cross head speed of 0.5mm/min. Ultimate shear bond strength data were analyzed with one-way ANOVA and the Scheffe's test (P<0.05). Within the limits of this study, the following conclusions were drawn: The X-ray diffraction analysis results for the as-cast and as-opaque specimens showed that the major relative intensity of Bellabond plus alloy were changed smaller than Wirobond C and Alphadent Co-Cr based alloys. Results: Microstructural analysis results for the opaque specimens showed all the alloys increased carbides and precipitation(PPT). Alphadent Co-Cr based alloy showed the carbides of lamellar type. The Vickers hardness results for the opaque specimens showed Wirobond C and Alphadent Co-Cr based alloys were increaser than before ascast, but Bellabond plus alloy relatively decreased. The mean shear bond strengths (MPa) were: 33.11 for Wirobond C/ZEO light; 25.00 for Alphadent Co-Cr alloy/ZEO light; 18.02 for Bellabond plus/ZEO light. Conclusion: The mean shear bond strengths for Co-Cr and Ni-Cr based alloy were significantly different. But the all groups showed metal-metal oxide modes in shear bond strengths test at the interface.

EFFECTS OF RESIN CEMENTS, CERAMIC SURFACE TREATMENTS AND THERMOCYCLING ON SHEAR BOND STRENGTH OF IPS EMPRESS CERAMIC (레진시멘트, 표면처리 및 열순환에 따른 IPS Empress의 전단결합강도)

  • Han, Jeong-Min;You, Young-Dae;Lee, Yong-Keun;Im, Mi-Kyung;Lee, Su-Jong
    • Restorative Dentistry and Endodontics
    • /
    • v.24 no.3
    • /
    • pp.473-481
    • /
    • 1999
  • This study evaluated the shear bond properties of IPS Empress glass ceramic to enamel and dentin surfaces with three ceramic surface treatments, and three resin cements. The influence of thermocycling was also investigated. The purpose of this study was to investigate the influences of resin cements, ceramic surface treatments, and thermocycling on shear bond properties. Ninety freshly extracted, noncarious human molars were selected for this study. The surface treatments of ceramic were etching <5.0% hydrofluoric acid, application of silane coupling agents(Tokuso Ceramic Primer, Clearfil porcelain bond, Monobond-S), and the combination of the two methods. Empress cylinders were bonded to enamel and dentin surfaces with three kinds of resin cements(Bistite resin cement, Panavia 21, Variolink). The specimens were aged in $37^{\circ}C$ distilled water for 24 hours. Half of the specimens were then thermocycled 500times between $5^{\circ}C$ and $55^{\circ}C$ with a dwell time of 15 seconds. Each specimen was debonded in shear mode and measured shear bond properties by using the universal testing machine(Zwick 020, Germany). The data were analyzed by SPSS/PC+(one-way ANOVA, Scheffe' s test and t-test). The results were as follows : 1. Without thermocyling, there was significant difference of shear bond strength to enamel surface between Bistite Resin Cement and Panavia 21 in case of etched and silane-treatment(p<0.05). 2. Without thermocyling, the shear bond strength of a group treated with silane and etching was significantly higher than that of a group treated with silane or etching with the application of Panavia 21 and Variolink(p<0.05). 3. A group treated with etching with the application of Variolink only showed a decrease of shear bond strength after thermocycling(p<0.05).

  • PDF

THE EFFECT OF SMEAR LAYER REMOVAL AND POSITION OF DENTIN ON SHEAR BOND PROPERTIES OF DENTIN BONDING SYSTEMS TO INTERNAL CERVICAL DENTIN (도말층 제거와 상아질의 부위가 치수강 내부 상아질에 대한 수종 상아질 결합제의 전단결합성질에 미치는 영향)

  • Lim, Yoen-Ah;You, Young-Dae;Lee, Yong-Keun;Lee, Su-Jong;Im, Mi-Kyung
    • Restorative Dentistry and Endodontics
    • /
    • v.24 no.3
    • /
    • pp.465-472
    • /
    • 1999
  • The aim of this study was to determine the shear bond properties of four dentin bonding systems to internal cervical dentin, and to investigate the effect of the pretreatment for removing smear layer and position of dentin on shear bond strength of dentin bonding agents. The materials tested in this study were consisted of four commercially available dentin bonding systems[Allbond 2(AB), Clearfil Linerbond 2(CL), Optibond FL(OP), Scotchbond Multi-purpose(SB)], a restorative light-cured composite resin[Z100]J and a chelating agent[RC-prep(RC)]. Fifty-six freshly extracted human molars were used in this study. Dentin specimens were prepared by first cutting the root of the tooth 1mm below the cementoenamel junction with a diamond bur in a high speed handpiece under air-water coolant, and then removing occlusal part at pulp horn level by means of a second parallel section, The root canal areas were exposed by means of cutting the dent in specimens perpendicular to the root axis. Dentin specimens were randomly assigned to two groups(pretreated group, not-pretreated group) based on the pretreatment method of dentin surface. In pretreated group, RC was applied to dentin surface for 1minute and then rinsed with NaOCl. In not-pretreated group, dentin surface was rinsed with saline Each groups were subdevided into four groups according to dentin bonding systems. Four dentin bonding systems and a restorative resin were applied according to the directions of manufacturer. The dentin-resin specimens were embedded in a cold cure acrylic resin, and were cut with a low speed diamond saw to the dimension of $1{\times}1mm$. The cut specimens were divided into three groups according to the position of internal cervical dentin. The shear bond properties of dentin-resin specimens were measured with Universal testing machine (Zwick, 020, Germany) with the cross head speed of 0.5mm/min. From this experiment. the following results were obtained : 1. In case of shear bond strength, there was no significant difference among dentin bonding systems in not-pretreated groups, whereas in pretreated groups, the shear bond strengths of AB and of SB were statistically significantly higher than those of CL and of OP. 2. The shear bond strengths of AB and of SB in pretreated groups were significantly higher than those in not-pretreated groups. 3. The shear bond strengths of radicular layer of OP were higher than those of occlusal layer of OP in not-pretreated groups, and of AB in pretreated groups. The shear bond strengths of radicular layer of AB and of CL in not-pretreated groups were higher than those in pretreated group.

  • PDF

Effects of light direction and exposure times of plasma arc light on shear bond strength of metal brackets (Plasma arc light를 이용한 금속 브라켓의 부착시 광조사 방향과 중합시간이 전단결합강도에 미치는 영향)

  • Roh, Sang-Jeong;Lee, Hyun-Jung;Jeon, Young-Mi;Kim, Jong-Ghee
    • The korean journal of orthodontics
    • /
    • v.34 no.5 s.106
    • /
    • pp.429-438
    • /
    • 2004
  • The purpose of this study was to compare the effects of different light direction exposure times and setting times when using plasma arc light on shear bond strength of metal brackets. 240 extracted human premolars were randomly assigned to one of 16 groups Standardized brackets were bonded to enamel using different light curing units (Plasma arc light and Halogen light), exposure times (Plasma arc light 2. 4, 6 seconds and Halogen light 20 seconds). and light directions [Vertical direction [V] and Oblique direction [O]). 8 groups were tested after 5 minutes and the remaining 8 groups after 24 hours. The metal brackets were bonded with Transbond XT. Shear bond strength was measured by a universal testing machine. The results were as fellows: There were as differences between the shear bond strengths of the Vertical groups (V) and Oblique groups (O). regardless of exposure times and types of light curing units (p>0.05). The shear bond strength of the group with 2 seconds of plasma light were significantly lower than other exposure time groups (P<0.05). The shear bond strength tested after 5 minutes was lower than after 24 hours (p<0.05) The Adhesive Remment Index (ARI) score showed no statistically significant difference among the different groups. The results of this study suggested that the light direction of plasma arc light had no influence on the shear bond strength of metal brackets to enamel. and exposure times more than 4 seconds produced shear bond strengths similar to those Produced with a conventional halogen curing light.