• 제목/요약/키워드: Seamless Pipe

검색결과 17건 처리시간 0.025초

압축 가공된 비용접 배관의 소성변형 거동에 미치는 내압의 영향 (Effect of Inner Pressure on the Plastic Deformation Behavior of Seamless Pipe Deformed by Compression Process)

  • 서위걸;이문수;손수지;최시훈
    • 소성∙가공
    • /
    • 제28권4호
    • /
    • pp.175-182
    • /
    • 2019
  • In this study, compression process is performed on the seamless E235 pipe using the newly developed compression technology for seamless pipe. Experimental analysis on the heterogeneity of microstructures and mechanical properties of the deformed seamless pipe is conducted. As a result, the correlation between microstructures and mechanical properties are determined. The spatial distribution of effective stress and effective strain developed in the seamless pipe deformed through compression is analyzed using the finite element method (FEM) based on different inner pressure conditions. From the results of the FEM, the impact of the inner pressure on effective stress and effective strain of the seamless pipe deformed through compression can be understood theoretically.

8인치 직경의 304L 스테인리스강관의 부식특성에 미치는 제작공정의 영향 (Effect of Manufacturing Process on the Corrosion Properties of 304L Stainless Steel Pipe with 8-inch Diameter)

  • 김기태;허승영;장현영;김영식
    • Corrosion Science and Technology
    • /
    • 제17권6호
    • /
    • pp.279-286
    • /
    • 2018
  • Austenitic stainless steels used in nuclear power plants mainly use pipes made of seamless pipes, which depend on imports. The manufacturing process and high cost are some of the problems associated with seamless pipes. Therefore, in this study, the corrosion characteristics of the seamless pipe and the SAW pipe were assessed to determine the safety and reliability of the SAW pipe in a bid to replace the seamless pipe. Microstructure was analyzed using an optical microscope and the degree of hardness was measured using a Rockwell B scale. Intergranular corrosion resistance was evaluated by ASTM A262 Practice A, C, and E methods. The degree of sensitization was determined using a DL-EPR test. Anodic polarization test was performed in deaerated 1% NaCl solution at $30^{\circ}C$ and the U-bend method was used to evaluate the SCC resistance in 0.01 M $Na_2S_4O_6$ at $340^{\circ}C$ and 40% NaOH solution at $290^{\circ}C$. Weld metal of the SAW pipe specimen showed relatively high degree of sensitization and intergranular corrosion rate. However, annealing to SAW pipes improved the corrosion properties in comparison to that of the seamless pipe.

재학속도에 따른 용접강관의 모멘트 응답특성에 관한 해석적 연구 (An Analytical Study on Moment Response of Welded Steel Pipe for Loading Rate)

  • 장경호;장갑철
    • 한국공간구조학회논문집
    • /
    • 제11권4호
    • /
    • pp.37-47
    • /
    • 2011
  • 재하속도에 따른 용접강관의 모멘트-곡률 거동특성에 관한 해석적 연구를 수행하였다. 3차원 열역학해석을 통하여 용접이음부의 잔류응력을 산출하였다. 그리고 동적소성모델이 적용된 탄소성 유한요소해석 프로그램을 이용하여 잔류응력을 고려한 용접강관(Welded pipe)의 동적해석을 수행하였다. 그리고 용접이음부가 없는 일반강관(Seamless pipe)에 대한 동적거동과의 비교를 통하여 해석을 수행하여 용접강관의 해석력과 해석결과는 용접강관의 모멘트가 일반강관의 모멘트에 비해 낮은 응답을 보였으나 재하속도가 증가함에 따라 모멘트 응답의 차이는 점차 감소하는 경향을 보였다.

Multi-sensor Visual inspection for Seamless Steel Pipe´s Straightness

  • Tomoo, Aoyama;Zhang, Y.G.
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 제어로봇시스템학회 2001년도 ICCAS
    • /
    • pp.88.3-88
    • /
    • 2001
  • In this paper, an on-line multi-sensor visual inspection technique for seamless steel pipe´s straightness is developed. The basic principle of the visual measuring method is detailed. The modeling of visual sensor, measurement system and data processing are presented. In order to test the accuracy of the multi-sensor visual inspection, an experiment inspecting the straightness of a 1500mm long seamless steel pipe is made. The experiment results show that the visual inspection technique can achieve on-line measurement and offers high precision and stability.

  • PDF

이음매 없는 304L 스테인리스강관의 부식특성에 미치는 열처리의 영향 (Effect of Heat Treatment on the Corrosion Properties of Seamless 304L Stainless Steel Pipe)

  • 김기태;엄상빈;김영식
    • Corrosion Science and Technology
    • /
    • 제16권6호
    • /
    • pp.305-316
    • /
    • 2017
  • Austenitic stainless steels have been widely used for various systems of nuclear power plants. Among these stainless steels, small pipes with diameter less than 14 inch have been produced in the form of seamless pipe. Annealing and cooling process during the manufacturing process can affect corrosion properties of seamless stainless steels. Therefore, 12 inch-diameter of as-received 304L stainless steel pipe was annealed and aged in this study. Intergranular corrosion resistance was evaluated by ASTM A262 Practice A, C, and E methods. The degree of sensitization was determined using a DL-EPR test. U-bend method in an autoclave was used to evaluate the SCC resistance in 0.01 M $Na_2S_4O_6$ or 40% NaOH solution at $340^{\circ}C$. As-received specimen showed relatively high degree of sensitization and intergranular corrosion rate. Carbon segregation was also observed near grain boundaries. Annealing treatment could give the dissolution of segregated carbon into the matrix. Aging treatment could induce segregation of carbon and finally form carbides. Microstructural analysis confirmed that high intergranular corrosion rate of the as-received seamless pipe was due to micro-galvanic corrosion between carbon segregation and grains.

심리스 파이프 제조를 위한 일롱게이션 공정의 유한요소해석 (Finite Element Analysis of an Elongation Rolling Process for Manufacturing Seamless Pipes)

  • 정승현;신유인;송철기
    • 한국정밀공학회지
    • /
    • 제31권10호
    • /
    • pp.923-928
    • /
    • 2014
  • Elongation rolling process is an intermediate process to make the uniform thickness and uniform surface roughness during producing seamless pipes. The thickness and surface roughness of seamless pipes are generally affected by the distance of rolls and guide shoes, the roll shape, and its cross angle. In this study, finite element analysis for shape forming process is based on the analysis model of elongation rolling mill with guide shoes. This paper shows how the cross angle of the roll, the rolling rpm, and the distance of the guide shoe influence on the outer diameter and the thickness of seamless pipes. The rolling rpm did not give much influence on outer diameter.

Infrared Thermography Characterization of Defects in Seamless Pipes Using an Infrared Reflector

  • Park, Hee-Sang;Choi, Man-Yong;Park, Jeong-Hak;Lee, Jea-Jung;Kim, Won-Tae;Lee, Bo-Young
    • 비파괴검사학회지
    • /
    • 제32권3호
    • /
    • pp.284-290
    • /
    • 2012
  • Infrared thermography uses infrared energy radiated from any objects above absolute zero temperature, and the range of its application has been constantly broadened. As one of the active test techniques detecting radiant energy generated when energy is applied to an object, ultrasound infrared thermography is a method of detecting defects through hot spots occurring at a defect area when 15~100 kHz of ultrasound is excited to an object. This technique is effective in detecting a wide range affected by ultrasound and vibration in real time. Especially, it is really effective when a defect area is minute. Therefore, this study conducted thermography through lock-in signal processing when an actual defect exists inside the austenite STS304 seamless pipe, which simulates thermal fatigue cracks in a nuclear power plant pipe. With ultrasound excited, this study could detect defects on the rear of a pipe by using an aluminium reflector. Besides, by regulating the angle of the aluminium reflector, this study could detect both front and rear defects as a single infrared thermography image.

유한요소법을 이용한 분기배관의 성형해석에 관한 연구 (A study on the Analyses of T-branch Pipe Forming using a Finite Element Method)

  • 남준석;백창선;임광규;사공성호;소수현;민경탁
    • 한국화재소방학회논문지
    • /
    • 제21권1호
    • /
    • pp.98-105
    • /
    • 2007
  • 본 연구에서는 소방 건축분야에 가장 많이 사용되는 배관인 배관용 탄소강관 및 이에 상응하는 스테인리스 강관을 분기배관으로 제작이 가능한지 여부를 상용유한요소프로그램(ABAQUS)을 이용하여 확인하였다. 이러한 배관을 분기배관으로 성형할 경우 심이 없는 배관 사용을 원칙으로 하고 배관에 심이 있는 경우 심과 정반대방향을 성형면으로 하여야 한다. 배관의 성형시 플러그의 경사면과 길이가 성형에 가장 큰 영향을 미치는 요소임을 알 수 있었다. 분기배관의 성형해석결과를 토대로 분기부분의 최소 높이와 두께를 제안했다.

파이프 인발 각도에 따른 기계적 효과 및 재료에 따른 감소율에 관한 연구 (Mechanical Effects of Pipe Drawing Angle and Reduction Rate on Material)

  • 서영진
    • 한국기계가공학회지
    • /
    • 제19권12호
    • /
    • pp.8-13
    • /
    • 2020
  • Seamless pipes are fabricated by drilling a hole in a cylindrical material and drawing the material to the desired diameter. These pipes are used in environments where high reliability is required. In this study, the pipe drawing process was simulated using DEFORM, a commercial finite element method (FEM) analysis program. The outer diameter of the steel cylinder used herein before drawing was 70 mm, and the target outer diameter was 58 mm. The drawing process consisted of two stages. In this study, the effect of cross-sectional reduction rate on the pipe was investigated by varying the cross-sectional reduction rate in each step to achieve the target outer diameter. The results of this study showed that the first section reduction rate of 26% and the second section reduction rate of 13.9% caused the lowest damage to the material. Moreover, the FEM simulation results confirmed the influence of the drawing die angle on the pipe drawing process. The drawing die angles of 15° in the first step and 9° in the second step caused the least damage to the material.