• Title/Summary/Keyword: Scrap content

Search Result 54, Processing Time 0.029 seconds

Effect of the Binder Content on the Recycling of Scrap Waste Tires (폐타이어 재활용에 있어서 Binder양이 미치는 영향)

  • Kim, Jin-Kuk;Cho, Ha-Na;Lee, Soo-Koo
    • Elastomers and Composites
    • /
    • v.29 no.5
    • /
    • pp.431-435
    • /
    • 1994
  • For recycling of the waste tires, polyurethane binder mixed with the scrapped rubber powders which obtained from tread part of waste tire. This study covered the effect of the binder contents on the mechanical properties of the blend. We also studied the change of the properties after aging on properties compared with those of before aging. The curing reaction of the binder was also investigated in this study. We obtained conclusions the suitable binder content was 15phr in this system.

  • PDF

Effects of Ti on Mechanical Property and Damping Capacity in Hot-rolled Fe-17%Mn Alloy (열간압연한 Fe-17wt%Mn 합금의 기계적 성질과 진동감쇠능에 미치는 티타늄 첨가의 영향)

  • Kim, Tai-Hoon;Kim, Jung-Chul
    • Journal of Korea Foundry Society
    • /
    • v.29 no.2
    • /
    • pp.59-63
    • /
    • 2009
  • Effects of Ti on damping capacity and mechanical properties are investigated in hot rolled Fe-17%Mn alloy. The existing damping alloy with Fe-Mn binary system was limited the use by high production cost, however in case of using scrap iron instead of pure iron although the content of carbon is higher it is possible to be applied wider field especially construction items because the production cost is lower. However, the excellent specific damping capacity is dropped due to the high content of carbon, we developed advanced type of damping alloy included Ti. TiC is formed with added Ti and it holds the specific damping capacity similar to existing damping alloy. The effect of Ti on damping capacity is found to be beneficial in carbon-containing alloy, which is attributed to the depletion of carbon solute due to the formation of TiC.

The Effect of Oxygen Content on the Glass Forming Ability and Mechanical Properties of the Zr-based Amorphous Alloy Return Scrap (Zr기지 비정질 합금 스크랩의 비정질 형성능 및 기계적 성질에 미치는 산소함량의 영향)

  • Kim, Sung-Gyoo;Lee, Byung-Chul;Park, Heung-Il
    • Journal of Korea Foundry Society
    • /
    • v.35 no.4
    • /
    • pp.75-79
    • /
    • 2015
  • Commercial Zr-based amorphous alloy was recycled and oxygen was introduced during the recycling process. The oxygen content can have a great effect on the glass forming ability and the mechanical properties of the alloy. Therefore, it was closely examined. The initial oxygen content in the raw material was 1,244 ppm. It was increased to 3,789 ppm in the alloy after ten recycling processes. As the recycling processes were repeated, the oxygen content increased. Specifically, after four recycling processes, it increased sharply as compared to that after three recycling processes. After ten recycling processes, the glass transition temperature (Tg) increased from 613 K to 634 K and the crystallization temperature (Tx) increased from 696 K to 706 K. On the other hand, the super-cooled liquid region (${\Delta}T=Tx-Tg$) decreased slightly from 83 K to 72 K while the reduced glass transition temperature (Trg = Tg/Tm) was 0.63, remaining constant even when the oxygen content was increased. These results indicated that the increased oxygen content deteriorated the glass forming ability. The bending strength as determined in a three-point bending test showed a sharp decrease from 3,055 to 2,062 MPa as the oxygen content was increased from 1,244 ppm to 3,789 ppm; the extension was also decreased from 3.02 to 1.74 mm. These findings meant that the alloy became brittle.

Development of Ceramic Pigment using Brass Scrap (각종 황동 Scrap를 사용한 Ceramic 안료 개발)

  • Kim, Jun-Ho;Jeon, Ok-Hyun;Suh, Man-Chul;Lee, Byung-Ha
    • Journal of the Korea Safety Management & Science
    • /
    • v.9 no.6
    • /
    • pp.197-204
    • /
    • 2007
  • Ceramic pigments were developed by using 4 kinds of Brass scraps. Each Brass scraps were mixed with same weight-ratio of Husk ash, and fine-ground by Rotate ring mill(RRG-120, Armstech industrial. co. Ltd, Korea) after firing at $900^{\circ}C$, $1000^{\circ}C$ and $1100^{\circ}C$. As a result, analysis of particle size of synthetic pigments by particle size analyser, they are $3{\mu}m$ as average. The resulting pigments were characterized by using XRD, FT-IR, SEM Structure of the crystals are Zn2SiO4,, and ZnO, Cu2O, CuO, and cristobalite are existed and particles' shape are plate or needle. As a result of analysis of chemical composition by XRF, synthetic pigments have high SiO2 and CuO content and have SnO2, ZnO and NiO, too. 1wt%, 3wt% and 5wt% pigments were added in each lime glaze, lime-barium glaze and lime-magnesia glaze, and fired at oxidation and reducing atmosphere to figure hue in glazes out. As a result of analysis of color, chroma and brightness by UV, colors of glazes fired at oxidation atmosphere turned into green from sky blue, and colors of glazes fired at reducing atmosphere turned into pink and red.

Experimental Lnvestigation on Mechanical Characteristics and Environmental Effects on Rubber Concrete

  • Khorrami, Morteza;Vafai, Abolhassan;Khalilitabas, Ahmad A.;Desai, Chandrakant S.;Ardakani, M. H. Majedi
    • International Journal of Concrete Structures and Materials
    • /
    • v.4 no.1
    • /
    • pp.17-23
    • /
    • 2010
  • The feasibility of the use of scrap tire rubber in concrete was investigated. The tests conducted in two groups: replacing of coarse aggregates with crumb rubber and cement particles with rubber powder. To distinguish the properties of new concrete, the following mechanical and durability tests were designed: compressive, tensile and flexural strength, permeability and water absorption. Rubber addition could affect the concrete properties depend on the type and percentage of the rubber added. Although the rubber addition modifies the mechanical characteristics of concrete in a way, but higher rubber content could not be useful. Concrete durability showed more dependency to the type of rubber instead of percentage of rubber. Moreover, to optimize the mechanical and durability of rubberized concrete, the useful percentage of rubber has been recommended.

Mutual Solubility of Mn and Fe in AZ91 Alloy Melts and Its Application to Composition Control of AZ91D Recycled Ingots (AZ91 합금 용탕내 Mn과 Fe의 상호용해도 측정 및 AZ91D 재생지금의 성분조정에의 활용)

  • Kwon, Soon-Il;Byun, Ji-Young;Kim, Seon-Jin;Shim, Jae-Dong
    • Korean Journal of Materials Research
    • /
    • v.13 no.9
    • /
    • pp.619-624
    • /
    • 2003
  • This paper describes a method to control Mn and Fe contents in recycled AZ91D ingots, based on the mutual solubility of Mn and Fe in AZ91 alloy melts. For this purpose, Fe solubility with the change of Mn content and temperature was investigated in the homogenized and re-precipitated liquid AZ91 alloy. The increase of the amount of Mn added to the melt resulted in the decrease of Fe content. The data obtained in this study was adopted to the pilot plant for recycling of the scrap. As a result, Mn and Fe contents measured in the recycled ingot were in good agreement with ASTM B93 standard.

Preparation and Characteristics of Anionic Surfactant Using Waste Fleshing Scrap (피혁 제조 공정 중 발생하는 폐돈지를 이용한 음이온성 계면활성제 제조 및 특성)

  • Shin, Soo-Beom;Min, Byung-Wook;Yang, Seung-Hun;Park, Min-Seok;Won, Gi-Chun;Paek, Doo-Hyeon
    • Textile Coloration and Finishing
    • /
    • v.18 no.6 s.91
    • /
    • pp.31-36
    • /
    • 2006
  • Study has been made for producing anionic surfactant using waste fleshing scraps from the leather making process through refining, esterification, sulfonation and blending processes. As a most optimum lard oil refining method, refining was carried out for 4 hours under temperature of $120^{\circ}C$ and approximately 200 mbar vacuum, which gave a recovery of more than 80% lard oil. Refined lard oil obtained thus was undergone methlyl-esterification, then sulfonated to make a degreasing agent. By methyl-esterification using lard oil, more than 85% of fatty acid and $12{\sim}13%$ of glycerine were extracted from the oil. Sulfonation of the extracted fatty acid ester lard oil has shown most optimum at $15{\sim}20%$ chlorosulfonic acid content, and the content of bonding sulfate at this time was higher than 3.5%. Finally the followed anionic surfactant having degreasing force of 80% and higher could be made by blending process.

Evaluation of the Asph81t Mixture Performance with Waste Materials

  • Lee, Kwan-Ho;Lovell, C
    • Geotechnical Engineering
    • /
    • v.12 no.3
    • /
    • pp.17-34
    • /
    • 1996
  • The objective of this paper is to evaluate the asphalt mixture performance with pyrolyzed carbon black(CBP) and air -cooled iron blast furnace slag. Marshall mix design was performed to determine the optimum binder content, The optimum binder content ranged from 6.3 percent to 7.75 percent. Dynamic creep testing was carried out using mixtures at the optimum binder content. Based on the test results, the use of pyrolyzed carbon black and slag in the asphalt pavement showed a positive result, such as the increase of Marshall stability, the decrease of the strain rate and the decrease in the mix stiffness rate at high temperature(5$0^{\circ}C$) and 137.9 kPa confinement. Within the limits of this research. it was concluded that pyrolyzed carbon black as an additive and slag as a coarse aggregate could be used to produce an asphalt paving mixture that has good stability, stiffness, and rutting resistance.

  • PDF

Recycling and Applications of Titanium Alloy Scraps (티타늄 합금 스크랩의 재활용 및 응용 기술 현황)

  • Oh, Jung-Min;Kwon, Hanjung;Lim, Jae-Won
    • Clean Technology
    • /
    • v.19 no.2
    • /
    • pp.75-83
    • /
    • 2013
  • In the present paper, we review recycling and applications of titanium binary alloy scraps. The recycling techniques are to successfully prepare low oxygen content ingots using hydrogen plasma arc melting (HPAM) and to produce low oxygen content titanium alloy powders by Hydrogenation-dehydrogenation (HDH) and Deoxidation in solid state (DOSS) process. In addition, as applications of the titanium binary alloy scraps, Ti based solid-solution carbide powders, which would be used for producing Ti based solid-solution cermets with high toughness, were prepared using the titanium binary alloy scraps. These results confirmed that the titanium alloy scraps could be recycled and refined using the HPAM. The resulting oxygen content of the titanium alloy powders were below 1,000 ppm after powderizing. Finally, we had confirmed that the refined titanium alloy powders were able to be utilized as raw materials for preparing the toughened cermets.

Evaluating Cultured Sea Mussels Mytilus edulis Extractions Methods and Extract Quality Characteristics (진주담치(Mytilus edulis) 추출물의 제조 및 품질특성)

  • Kim, Seon-Geun;Cho, Jun-Hyun;Hwang, Young-Sook;Lee, In-Seok;Oh, Kwang-Soo
    • Korean Journal of Fisheries and Aquatic Sciences
    • /
    • v.50 no.6
    • /
    • pp.650-655
    • /
    • 2017
  • Extraction methods for cultured sea mussels Mytilus edulis and the quality characteristics of resulting extracts were investigated. The crude protein, carbohydrate and volatile basic nitrogen content of raw sea mussels was 15.2%, 1.9%, and 11.2 mg/100 g, respectively. Extracts were prepared using three different methods: hot-water extract (WE), scrap enzymatic hydrolysate extraction (SE), and complex extraction (CE). The respective extracts contained 5.5%, 8.6%, and 6.6% crude protein; 281.7, 366.0, and 343.0 mg/100 g amino nitrogen,: and 2.0%, 1.1% and 1.8% salinity. Their extraction yields were 689, 323, and 1,012 mL/kg. The CE method was superior to the traditional WE method in terms of extraction yield, amino-nitrogen content, and organoleptic qualities, but not odor. Active taste components were evaluated and the total free amino acid content of the WE and CE methods was 5,667.0 and 7,006.3 mg/100 g, respectively. The concentrations of major components (for WE and CE methods, respectively) were as follows: glutamic acid (1,244.0 and 955.4 mg/100 g), taurine (987.9 and 746.8 mg/100 g), glycine (721.2 and 847.0 mg/100 g), alanine (341.9 and 423.8 mg/100 g), arginine (265.5 and 376.5 mg/100 g), lysine (199.8 and 270.4 mg/100 g), and proline (253.9 and 220.3 mg/100 g). In conclusion, these results demonstrate that there is potential for using the CE method to expand the commercial utilization of sea mussels as a flavoring substance resource.