Particle Morphology Change and Quantitative Input Energy Variation during Stirred Ball Milling Process by DEM Simulation on Various Experimental Conditions (교반볼밀을 이용한 밀링공정에서 각종실험조건에 따른 구리분말의 입자형상 변화 및 DEM 시뮬레이션에 의한 정량적 에너지 변화)

  • Bor, Amgalan;Batjargal, Uyanga;Jargalsaikhan, Battsetseg;Lee, Jehyun;Choi, Heekyu
    • Korean Journal of Materials Research
    • /
    • v.28 no.3
    • /
    • pp.148-158
    • /
    • 2018
  • This study investigated the effect of the grinding media of a ball mill under various conditions on the raw material of copper powder during the milling process with a simulation of the discrete element method. Using the simulation of the three-dimensional motion of the grinding media in the stirred ball mill, we researched the grinding mechanism to calculate the force, kinetic energy, and medium velocity of the grinding media. The grinding behavior of the copper powder was investigated by scanning electron microscopy. We found that the particle size increased with an increasing rotation speed and milling time, and the particle morphology of the copper powder became more of a plate type. Nevertheless, the particle morphology slightly depended on the different grinding media of the ball mill. Moreover, the simulation results showed that rotation speed and ball size increased with the force and energy.

Preparation and Characterization of Polyurethane Microcapsules Containing Functional Oil (기능성 오일을 함유하는 폴리우레탄 마이크로캡슐의 제조 및 분석)

  • 김인회;서재범;김영준
    • Polymer(Korea)
    • /
    • v.26 no.3
    • /
    • pp.400-409
    • /
    • 2002
  • Polyurethane microcapsules containing functional oil (citronella oil) were successfully prepared by conventional interfacial polymerization of tolulene 2,4-diisocyanate (TDI) and ethylene glycol (EG) and characterized by Fourier transform (FT-IR) spectroscopy, Ultraviolet spectroscopy, particle size analysis, thermogravimetric analysis (TGA), and scanning electron microscopy (SEM). Tile effects of polymerization variables, such as surfactant concentration and agitation speed, on the particle size and particle size distribution were investigated. FT-IR spectroscopic data showed that citronella oil was successfully encapsulated in the microcapsule. Thermogravimetric analysis data showed that the microcapsule was thermally stable up to $220^{\circ}C$. The controlled release of the citronella oil present in the microcapsule core in a methanol medium was demonstrated by ultraviolet spectroscopy showing that the amount of released citronella oil was increased with increasing time. It was observed that the amount of released citronella oil was increased with increasing stirring speed and emulsifier concentration in the rnicrocapsule preparation step. Polyurethane microcapsules containing citronella oil showed excellent anti-moth property.

A STUDY ON THE FRACTURE OF DENTAL AMALGAM (치과용 아말감의 파절에 관한 연구)

  • Huh, Hyeon-Do;Um, Chung-Moon
    • Restorative Dentistry and Endodontics
    • /
    • v.9 no.1
    • /
    • pp.101-106
    • /
    • 1983
  • It was the purpose of this study to investigate the fracture mode of dental amalgam by observing the crack propagation, and to relate this to the microstructure of the amalgam. Caulk 20th Century Regular, Caulk Spherical, Dispersalloy, and Tytin amalgam alloys were used for this study. After each amalgam alloy and Hg measured exactly by the balance was triturated by the mechanical amalgamator (Capmaster, S.S. White), the triturated mass was inserted into the cylindrical metal mold which was 4 mm in diameter and 12 mm in height and was pressed by the Instron Universal Testing Machine at the speed of 1mm/min with 120Kg. The specimen removed from the mold was stored in the room temperature for a week. This specimen was polished with the emery papers from #100 to #200 and finally on the polishing cloth with 0.06${\mu}Al_2O_3$ powder suspended in water. The specimen was placed on the Instron testing machine in the method similar to the diametral tensile test and loaded at the crosshead speed of 0.05mm/min. The load was stopped short of fracture. The cracks on the polished surface of specimen was examined with scanning electron microscope (JSM-35) and analyzed by EPMA (Electron probe microanalyzer). The following results were obtained. 1. In low copper lathe-cut amalgam, the crack went through the voids and ${\gamma}_2$ phase, through the ${\gamma}_1$ phase around the ${\gamma}$ particles. 2. In low copper spherical amalgam, it was observed that the crack passed through the ${\gamma}_2$ and ${\gamma}_1$ phase, and through the boundary between the ${\gamma}_1$ and ${\gamma}$ phase. 3. In high copper dispersant (Dispersalloy) amalgam, the crack was found to propagate at the interface between the ${\gamma}_1$ matrix and reaction ring around the dispersant (Ag-Cu) particles, and to pass through the Ag-Sn particles. 4. In high copper single composition (Tytin) amalgam, the crack went through the ${\gamma}_1$ matrix between ${\eta}$ crystals, and through the unreacted alloy particle (core).

  • PDF

Fabrication Characteristics of Slag Fiber by 4 Wheel System (4휠 시스템을 이용한 슬래그 섬유의 제조)

  • Song, Yeong-Hwan;Seong, Hwan-Goo;Park, Soo-Han;Wang, Xiaosong;Hur, Bo-Young
    • Journal of Korea Foundry Society
    • /
    • v.26 no.5
    • /
    • pp.222-226
    • /
    • 2006
  • Steel making slag has gained a considerable attraction as one candidate of eco-materials in research fields for recycling resources. Thus, many researches have been performed but were limited to development of substitute for cement being used in the construction field. A little research work also has been done on development of higher value-added materials, including heat resistant and sound absorbing materials. For this reason, the present study were focused on macrostructure characterization of fabricated slag fibers which are applicable to heat resistant materials. The slag fibers were fabricated through a modified melt extraction method. The processing variables employed were the wheel speed and molten slag temperature. The synthesized fibers were characterized by optical microscope and scanning electron microscopy. It was found that the wheel speed of 1400 rpm generated better quality of mineral fibers in terms of the relative amount of shot, diameter and length. This was attributed to the relative extent of contact width between the flowing melt and the rotating wheel. The thickness of the slag fibers also were decreased with increasing the slag melt temperature due mainly to significant decrease in the viscosity of the slag melt. In addition, the lower melt temperature caused an increase in number of shots plus the mineral fibers.

Characteristics of Surface Hardening of Dies Steel for Plastic Molding using Continuous Wave Md:YAG Laser (연속파형 Nd:YAG 레이저를 이용한 플라스틱성형용 금형강의 표면경화 특성)

  • Shin, Ho-Jun;Yoo, Young-Tae;Oh, Yong-Seak
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.26 no.1
    • /
    • pp.71-81
    • /
    • 2009
  • Die steel for plastic molding were used as mold material of automobile parts and electronic component industry. The material of this paper has superior to mechanical properties, such as repair weldability, corrosion resistance and high temperature strength, required mold parts for semitransparent. Laser-induced surface hardening technology is widely adopted to improver fatigue life and wear resistance via localized hardening at the surface of mold parts. The objective of this research work is to investigate on the characteristics of surface hardening of the laser process parameters, such as beam travel speed, laser power and defocsued spot position, for the case of die steel for plastic molding. Lens for surface hardening of large area is plano-convex type with elliptical profile to maintain uniform laser irradiation. According to the experimental results, large size of hardened layer at the surface of die steel for plastic molding was achieved, and microstructure of this layer was lath martensite. Optimal surface status and mechanical property of hardened layer could be obtained at 1095Watt, $0.25{\sim}0.3m/min$, 0mm (focal length: 232mm) for laser power, beam travel speed, and focal position. Where, heat input was $0.793{\times}10^{3}J/cm^2$, and width of hardened layer was 27.58mm.

Machining Characteristics of Cemented Carbides in Micro Cutting within SEM

  • Heo, Sung-Jung
    • International Journal of Precision Engineering and Manufacturing
    • /
    • v.5 no.3
    • /
    • pp.35-42
    • /
    • 2004
  • This research describes that the cutting characteristics and tool wear behavior in the micro cutting of three kinds of wear resistant cemented carbides (WC-Co; V40, V50 and V60) using PCD (Poly Crystalline Diamond) and PCBN (Poly crystalline Cubic Boron Nitride) cutting tools by use of the SEM (Scanning Electron Microscope) direct observation method. The purpose of this research is to present reasonable cutting conditions from the viewpoint of high efficient cutting refer to a precise finished surface and tool wear. Summary of the results is as follows: (1) The cutting forces tend to increase as the increase of the weight percentage of WC particles, and the thrust forces was larger than the principal forces in the cutting of WC-Co. These phenomena were different from the ordinary cutting such as cutting of steel or cast iron. (2) The cutting speed hardly influenced the thrust force, because of the frictional force between the cutting tool edge and small WC particles at low cutting speed region such as 2$\mu\textrm{m}$/s. It seemed that the thrust cutting force occurred by the contact between the flank face and work material near the cutting edge. (3) The wear mechanism for PCD tools is abrasion by hard WC particles of the work materials, which leads diamond grain to be detached from the bond. (4) From the SEM direct observation in cutting the WC-Co, it seems that WC particles are broken and come into contact with the tool edge directly. This causes tool wear, resulting in severe tool damage. (5) In the orthogonal micro cutting of WC-Co, the tool wear in the flank face was formed bigger than that in the rake face on orthogonal micro cutting. And the machining surface integrity on the side of the cutting tool with a negative rake angle was better than that with a positive one, as well as burr in the case of using the cutting tool with a negative rake angle was formed very little compared to the that with a positive one.

Development of an Objective Softness Evaluation Method and Its Standardization for Hygiene Paper (위생용지 부드러움의 객관적 평가 방법 개발 및 표준화)

  • Ko, Young Chan;Park, Jong-Moon;Moon, Byoung-Geun
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.47 no.5
    • /
    • pp.80-84
    • /
    • 2015
  • Softness is considered one of the most important attributes of hygiene paper such as tissue and towel. Being subjective in nature, however, softness attribute has been generally believed to be impossible to evaluate using objective methods. Hallmark in his pioneering work proposed that tissue subjective softness should be mainly consisted of the bulk softness component and surface softness component. The bulk softness component can be determined by tensile stiffness; the surface softness component by surface tester. The surface friction turns out far more important than the surface roughness in determining the surface softness component. It cannot be too much emphasized that both results of the tensile stiffness and the surface friction should depend on measuring conditions such as an instrument used, sample sizes (e.g., basis weight, length, and width) and operating conditions of the instrument (e.g., gauge length, cross-head speed, size of stylus, and its scanning speed). This indicates that a direct comparison of the test results would be impossible or misleading unless they have been tested under the identical conditions. This may explain why the standard objective test method for tissue softness has not been available at present.

Hybrid (CNC+Laser) process for polymer welding (하이브리드 방식 (CNC+Laser)을 이용한 폴리머용접공정)

  • Yoo, Jong-Gi;Lee, Choon-Woo;Kim, Soon-Dong;Choi, Hae-Woon;Shin, Hyun-Myung
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.4-4
    • /
    • 2009
  • Polycarbonate (PC) and Acrylonitrile Butadiene Styrene (ABS) was welded through a combination of a diode laser and CNC. Laser beam passed the transparent PC and was absorbed in an opaque ABS. Polymers were melted and welded by absorbed and conducted heat. Experiments were carried out by varying working distance from 44mm to 50mm for the focus spot diameter control, laser input power from 10W to 25W, and scanning speed from 100 to 400mm/min. The weld bead size and the specimen cross-section were analyzed, and tensile results were presented through the joint force measurement. With focus distance at 48mm, laser power with 20W, and welding speed at 300mm/min, experimental results showed the best welding quality which bead size was 3.75mm and the shear strength was $22.8N/mm^2$. Considering tensile strength of ABS is $43N/mm^2$, shear strength was sufficient to hold two materials. A single process was possible in CNC machining processes, surface processing, hole machining and welding. As a result, the process cycle time was reduced to 25%. Compared to a typical process, specimens were fabricated in a single process, with high precision. By combining two operations processes developed process gained 50% more efficiency.

  • PDF

Inductively Coupled Plasma Reactive Ion Etching of MgO Thin Films Using a $CH_4$/Ar Plasma

  • Lee, Hwa-Won;Kim, Eun-Ho;Lee, Tae-Young;Chung, Chee-Won
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.02a
    • /
    • pp.77-77
    • /
    • 2011
  • These days, a growing demand for memory device is filled up with the flash memory and the dynamic random access memory (DRAM). Although DRAM is a reasonable solution for current demand, the universal novel memory with high density, high speed and nonvolatility, needs to be developed. Among various new memories, the magnetic random access memory (MRAM) device is considered as one of good candidate memories because of excellent features including high density, high speed, low operating power and nonvolatility. The etching of MTJ stack which is composed of magnetic materials and insulator such as MgO is one of the vital process for MRAM. Recently, MgO has attracted great interest in the MTJ stack as tunneling barrier layer for its high tunneling magnetoresistance values. For the successful realization of high density MRAM, the etching process of MgO thin films should be investigated. Until now, there were some works devoted to the investigations on etch characteristics of MgO thin films. Initially, ion milling was applied to the etching of MgO thin films. However, ion milling has many disadvantages such as sidewall redeposition and etching damage. High density plasma etching containing the magnetically enhanced reactive ion etching and high density reactive ion etching have been employed for the improvement of etching process. In this work, inductively coupled plasma reactive ion etching (ICPRIE) system was adopted for the improvement of etching process using MgO thin films and etching gas mixes of $CH_4$/Ar and $CH_4$/$O_2$/Ar have been employed. The etch rates are measured by a surface profilometer and etch profiles are observed using field emission scanning emission microscopy (FESEM). The effects of gas concentration and etch parameters such as coil rf power, dc-bias voltage to substrate, and gas pressure on etch characteristics will be systematically explored.

  • PDF

Preparation of Poly(vinyl alcohol)/polypropylene Nano-filter by High Speed Centrifugal Solution Spinning (초고속 용액 원심방사를 이용한 폴리비닐알코올/폴리프로필렌 나노필터 제조)

  • Yang, Seong Baek;Lee, Jungeon;Park, Jae Min;Jung, Jae Hoon;Kim, Tae Young;Kim, Ki Young;Lee, Sang Jun;Yeum, Jeong Hyun
    • Textile Coloration and Finishing
    • /
    • v.34 no.1
    • /
    • pp.20-26
    • /
    • 2022
  • Centrifugal spinning is an emerging technique for fabricating micro-to-nano-fibers in recent years. To obtain fibers with the desired size and morphology, it is necessary to configure and optimize the parameters used in centrifugal spinning. In this study, it was controlled by changing the solution's concentration (7.5, 10, and 12.5 wt.%) and disk's rotational velocity (6,000, 8,000, and 10,000 rpm) to prepare centrifugal spun nano-filter. The morphological property, air permeability, and dust collection efficiency of the PVA/PP bi-layer nanoweb prepared by centrifugal spun PVA on the PP micron nonwoven substrate are studied using a field emission scanning electron microscope, an air permeability tester, and a filter tester equipment, and the analysis results indicate that it is suitable as a nano-filter when the concentration of PVA solution is 10 wt.% and the rotational velocity of the disk is 8,000 rpm. The resultant reduced diameter and uniform fibers also proved that an excellent dust collection efficiency filter could be made.