• Title/Summary/Keyword: Sc$_2O_3-CeO_2$ Doped ZrO$_2$

Search Result 5, Processing Time 0.017 seconds

Electrical Conductivity of ZrO2 Doped with Sc2O3 and CeO2 (Sc2O3와 CeO2가 첨가된 ZrO2의 전기전도도)

  • Lee, Dong-Suek;Heo, Jang-Weon;Kim, Jae-Dong;Kim, Joo-Sun;Lee, Hae-Weon;Kim, Gyeung-Ho;Kim, Dae-Jun;Lee, Jong-Ho
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.4
    • /
    • pp.346-351
    • /
    • 2002
  • The electrical conductivity and phase stability of $ZrO_2$ doped with $Sc_2O_3$ and $CeO_2$ were investigated in order to search for better solid electrolyte material for solid oxide fuel cell. Present study showed that $ZrO_2$ doped with $Sc_2O_3$ and $CeO_2$ exhibited no phase transition during the heat treatment up to $1350^{Circ}C∼1550^{Circ}C$ and was stable as a cubic phase in whole temperature ranges. The $ZrO_2$ doped with $Sc_2O_3$ and $CeO_2$ showed much higher electrical conductivity than YSZ in the temperature range of $300∼^{Circ}C$ and better long term stability than other sc-$ZrO_2$ based electrolyte that showed the possibility as a strong candidate electrolyte material for intermediate-or low-temperature SOFC.

Effects of Partial Substitution of CeO2 with M2O3 (M = Yb, Gd, Sm) on Electrical Degradation of Sc2O3 and CeO2 Co-doped ZrO2

  • Shin, Hyeong Cheol;Yu, Ji Haeng;Lim, Kyoung Tae;Lee, Hee Lak;Baik, Kyeong Ho
    • Journal of the Korean Ceramic Society
    • /
    • v.53 no.5
    • /
    • pp.500-505
    • /
    • 2016
  • Scandia-stabilized zirconia co-doped with $CeO_2$ is a promising electrolyte for intermediate temperature SOFC, but still shows rapid degradation during a long-term operation. In this study, $CeO_2$ (1 mol%) as a stabilizer is partially substituted with lanthanum oxides ($M_2O_3$, M=Yb, Gd, Sm) to stabilize a cubic phase and thus durability in reducing atmosphere. 0.5M0.5Ce10ScSZ electrolytes were prepared by solid state reaction and sintered at $1450^{\circ}C$ for 10 h to produce dense ceramic specimens. With addition of the lanthanum oxide, 0.5M0.5Ce10ScSZ showed lower degradation rates than 1Ce10ScSZ. Since $Gd_2O_3$ showed the highest ionic conductivity among the co-dopants, an electrolyte-supported cell with 0.5Gd0.5Ce10ScSZ was prepared to compare its long-term performance with that of 1Ce10ScSZ-based cell. Maximum power density of 0.5Gd0.5Ce10ScSZ-based cell was degraded by about 2.3% after 250 h, which was much lower than 1Ce10ScSZ-based cell (4.2%).

Electrochemical Performance of LSCF Cathode with GDC lnterlayer on ScSZ Electrolyte

  • Hwang, Hae-Jin;Moon, Ji-Woong;Lim, Yongho;Lee, Seunghun;Lee, Eun-A
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.12 s.283
    • /
    • pp.787-792
    • /
    • 2005
  • A symmetrical LSCF $(La_{0.6}Sr_{0.4}Co_{0.2}Fe_{0.8}O_{3-\delta})\;ScSZ(89ZrO_2-10Sc_2O_3-1CeO_2)/LSCF$ electrochemical cell with a GDC (Gadolinium-Doped Ceria, $90CeO_2-10Gd_2O_3$) interlayer that was inserted between the LSCF cathode and ScSZ electrolyte was fabricated, and the electrochemical performance of these cells was evaluated. The GDC interlayer was deposited on a ScSZ electrolyte using a screen-printing technique. The GDC interlayer prevented the unfavorable solid-state reactions at the LSCF/ScSZ interfaces. The LSCF cathode on the GDC interlayer had excellent electrocatalytic performance even at $650^{\circ}C$. The Area Specific Resistance (ASR) was strongly dependent on the thickness and heat-treatment temperature of the GDC interlayer. The impedance spectra showed that the cell with a $15\~27{\mu}m$ thick GDC interlayer heat-treated at $1200^{\circ}C$ had the lowest ASR.

An SOFC Cathode Composed of LaNi0.6Fe0.4O3 and Ce(Ln)O2 (Ln=Sm, Gd, Pr)

  • Chiba, Reiichi;Komatsu, Takeshi;Orui, Himeko;Taguchi, Hiroaki;Nazawa, Kazuhiko;Arai, Hajime
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.12
    • /
    • pp.766-771
    • /
    • 2008
  • We fabricated single cells with a cathode consisting of a $LaNi_{0.6}Fe_{0.4}O_3-Ce_{0.8}Sm_{0.2}O_{1.9}$ composite (LNF-S20DC composite) active layer and an LNF current collecting layer on a ${0.89ZrO_2}-{0.10Sc_2}{O_3}-0.01{Al_2}{O_3}$ electrolyte sheet. The cathode layers were prepared by the screen-printing method. The cathode properties of these cells were measured by the AC impedance method at $800^{\circ}C$. The cathodes with the ceria-LNF composite active layer exhibited high power performance prior to current loading. We investigated the influence of the mixture ratio of LNF and S20DC on the cathodes properties. The Sm in the ceria particles of the composite cathode was substituted with other rare-earth elements. Cathodes with Pr and Gd co-doped ceria in the active layer provided the better performance than those with Sm- or Gd-doped ceria.

Influence of Gd0.1Ce0.9O2-δ Interlayer between La0.6Sr0.4Co0.2Fe0.8O3-δ Cathode and Sc-doped Zirconia Electrolyte on the Electrochemical Performance of Solid Oxide Fuel Cells (La0.6Sr0.4Co0.2Fe0.8O3-δ 공기극과 Sc이 도핑된 지르코니아 전해질 사이에 삽입한 Gd0.1Ce0.9O2-δ 중간층이 고체산화물 연료전지의 전기화학적 성능에 미치는 영향)

  • Lim, Jinhyuk;Jung, Hwa Young;Jung, Hun-Gi;Ji, Ho-Il;Lee, Jong-Ho
    • Ceramist
    • /
    • v.21 no.4
    • /
    • pp.378-387
    • /
    • 2018
  • The optimal fabrication conditions for $Gd_{0.1}Ce_{0.9}O_{2-{\delta}}$(GDC) buffer layer and $La_{0.6}Sr_{0.4}Co_{0.2}Fe_{0.8}O_{3-{\delta}}$ (LSCF) cathode on 1mol% $CeO_2-10mol%\;Sc_2O_3$ stabilized $ZrO_2$ (CeScSZ) electrolyte were investigated for application of IT-SOFCs. GDC buffer layer was used in order to prevent undesired chemical reactions between LSCF and CeScSZ. These experiments were carried out with $5{\times}5cm^2$ anode supported unit cells to investigate the tendencies of electrochemical performance, Microstructure development and interface reaction between LSCF/GDC/CeScSZ along with the variations of GDC buffer layer thickness, sintering temperatures of GDC and LSCF were checked, respectively. Electrochemical performance was analyzed by DC current-voltage measurement and AC impedance spectroscopy. Microstructure and interface reaction were investigated by scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS). Although the interfacial reaction between these materials could not be perfectly inhibited, We found that the cell, in which $6{\mu}m$ GDC interlayer sintered at $1200^{\circ}C$ and LSCF sintered at $1000^{\circ}C$ were applied, showed good interfacial adhesions and effective suppression of Sr, thereby resulting in fairly good performance with power density of $0.71W/cm^2$ at $800^{\circ}C$ and 0.7V.