• 제목/요약/키워드: Sand iron

검색결과 155건 처리시간 0.021초

TCE제거를 위한 반응층과 고정화층의 결합 실험

  • 조현희;박재우
    • 한국지하수토양환경학회:학술대회논문집
    • /
    • 한국지하수토양환경학회 2002년도 추계학술발표회
    • /
    • pp.67-70
    • /
    • 2002
  • Remediation of groundwater contaminated with chlorinated organics, nitro aromatics, and heavy metals using zero valent iron (ZVI) filings has paid considerable attention in recent years. When the contaminants of high concentration leaked abundantly in subsurface environment, permeable reactive barrier technology using iron filing is taken a long time for the remediation of contaminated groundwater, The problem of contaminant shock is able to be solved using surfactant (hexadecyltrimethylammonium, HDTMA) modified bentonite (SMB) as immobilizing material. Therefore, the purpose of this research was to develop the combined remediation technology using conventional permeable reactive and immobilizing barrier for the enhanced decontamination of chlorinated compounds. Four column experiments were conducted to assess the performance of the mixed reactive materials with Ottawa sand, iron filing, and HDTMA-bentonite for trichloroethylene (TCE) removal under controlled groundwater flow conditions. TCE reduction rates with sand/iron filing/HDTMA-bentonite were highest among four column due to dechlorination of TCE by iron filing and sorption of TCE by SMB.

  • PDF

Humic Acid Removal from Water by Iron-coated Sand: A Column Experiment

  • Kim, Hyon-Chong;Park, Seong-Jik;Lee, Chang-Gu;Han, Yong-Un;Park, Jeong-Ann;Kim, Song-Bae
    • Environmental Engineering Research
    • /
    • 제14권1호
    • /
    • pp.41-47
    • /
    • 2009
  • Column experiments were performed in this study to investigate humic acid adhesion to iron oxide-coated sand (ICS) under different experimental conditions including influent humic acid concentration, flow rate, solution pH, and ionic strength/composition. Breakthrough curves of humic acid were obtained by monitoring effluents, and then column capacity for humic acid adsorption ($C_cap$), total adsorption percent (R), and mass of humic acid adsorbed per unit mass of filter media ($q_a$) were quantified from these curves. Results showed that humic acid adhesion was about seven times higher in ICS than in quartz sand at given experimental conditions. This indicates that humic acid removal can be enhanced through the surface charge modification of quartz sand with iron oxide coating. The adhesion of humic acid in ICS was influenced by influent humic acid concentration. $C_cap$ and $q_a$ increased while R decreased with increasing influent humic acid concentration in ICS column. However, the influence of flow rate was not eminent in our experimental conditions. The humic acid adhesion was enhanced with increasing salt concentration of solution. $C_cap$, $q_a$ and R increased in ICS column with increasing salt concentration. On the adhesion of humic acid, the impact of CaCl2 was greater than that of NaCl. Also, the humic acid adhesion to ICS decreased with increasing solution pH. $C_cap$, $q_a$ and R decreased with increasing solution pH. This study demonstrates that humic acid concentration, salt concentration/composition, and solution pH should be controlled carefully in order to improve the ICS column performance for humic acid removal from water.

인산염의 존재 하에서 Escherichia coli의 석영 및 철피복 모래에의 부착 (Adhesion of Escherichia coli to Quartz and Iron-coated Sands in the Presence of Phosphate)

  • 박성직;이창구;김현정;한용운;김성배
    • 대한환경공학회지
    • /
    • 제30권6호
    • /
    • pp.616-620
    • /
    • 2008
  • 본 연구의 목적은 다공성 여재에서 인산염이 Escherichia coli의 부착에 미치는 영향을 분석하는 것이다. 석영모래와 철피복 모래에서 박테리아 부착에 대한 인산염의 영향을 분석하기 위하여 칼럼실험을 수행하였다. 실험결과, 석영모래에서 인산염의 농도가 0에서 16 mg/L로 증가함에 따라 박테리아의 질량 회수율은 74.5에서 35.4%로 감소하였다. 이는 석영모래에서 인산염의 농도가 증가함에 따라 박테리아의 부착이 향상됨을 나타내는데, 이러한 현상은 이온강도의 증가 때문이다. 반면, 철피복 모래에서는 인산염의 농도가 증가함에 따라 질량 회수율이 2.9에서 26.0%로 증가하였다. 이는 인산염에 의한 호의적 흡착지역 선점과 박테리아와의 경쟁적인 흡착으로 인하여, 인산염의 농도가 증가함에 따라 철피복 모래에서 박테리아의 부착이 감소함을 나타낸다.

철코팅 모래흡착제 제조 및 비소흡착 (Preparation of Iron-Coated Sand and Arsenic Adsorption)

  • 장윤영;김광섭;정재현;이승목;양재규;박준규
    • 대한환경공학회지
    • /
    • 제27권7호
    • /
    • pp.697-703
    • /
    • 2005
  • 본 연구에서는 주문진사 입경, 일차 및 이차 코팅온도, 코팅시간, 및 초기 3가철 주입농도를 변화시키면서 철을 코팅시킨 모래흡착제(Iron-Coated Sand, ICS)를 제조하였다. ICS 제조의 최적조건은 코팅효율, 코팅된 철의 안정성, 및 비소제거능 으로부터 선정하였다. 철코팅 효율은 입경이 작은 모래를 지지체로 사용하고 일차코팅온도를 높여주었을 때 뚜렷이 향상되었다. 철의 코팅효율은 이차코팅온도 및 코팅시간에는 크게 영향을 받지 않았지만 As(V) 흡착능은 이차코팅온도가 증가됨에 따라 크게 감소하는 것으로 나타났다. 이러한 결과들을 고려하여 ICS의 최적 이차코팅 조건을 $150^{\circ}C$ 온도조건과 1시간의 가열시간으로 선정하였다. Fe(III) 주입농도 변화에 따른 철 코팅효율은 0.8 Fe(III) mol/kg sand 될 때 까지는 뚜렷이 증가하였지만 그 이상에서는 큰 차이가 없었다. 기리고 Fe(III) 주입농도를 증가시킬수록 As(V) 흡착능도 증가하였으며 0.8 Fe(III) mol/kg sand 조건에서 최대값을 보여주었다. 이차 코팅온도 및 시간은 ICS 안정성의 주요변수로서 코팅온도를 높이고 코팅시간을 길게 할수록 ICS로 부터 용출되는 철의 양은 감소하였다. ICS에 대한 As(V)의 흡착은 낮은 pH에서 흡착량이 증가하는 전형적인 음이온형 흡착경향을 보여서 ICS는 강한 산성을 띄는 오염수내에 함유된 As(V)를 제거하는데 적용이 가능함을 알 수 있었다.

주형재료로서 덩어리 활석의 이용 (Application of Bulk Talc to Molding Material)

  • 하만진;이진형;이상수;은희준
    • 한국주조공학회지
    • /
    • 제14권1호
    • /
    • pp.45-51
    • /
    • 1994
  • The possibility of using bulk talc as molding material was reviewed and tested with the measurement of thermal properties and computer simulations. The measured thermal conductivity and heat diffusivity($k{\rho}c$) of talc were $2.4W/m^{\circ}C$ and $6.6{\times}10^6J^2/m^4^{\circ}C^2s$, respectively. Thermal properties of talc could be ranked between those of sand mold and iron mold. Talc transforms into cristobalite and enstatite at $910^{\circ}C$, During the transformation volume and structure change, cracks appear on the surface and distortion occurs. Therefore talc can be used for molding material below $910^{\circ}C$ if carefully treated. Computer simulation was carried out to test whether talc insert could promote directional solidification in sand mold and iron mold. In sand mold, it was possible to achieve directional solidification of thin plate casting with the length to thickness ratio of 15, if both iron insert and talc insert were used. In iron mold, it was possible to achieve directional solidification only with talc insert.

  • PDF

전통 제철법을 적용하여 제작한 철제 칼의 금속학적 특성에 관한 비교 연구 (A Comparative Study on the Metallurgical Characteristics of the Iron Knife Using Traditional Iron-Making Method)

  • 조성모;조남철;한정욱
    • 보존과학회지
    • /
    • 제34권5호
    • /
    • pp.433-442
    • /
    • 2018
  • 본 연구에서는 전통 제철법을 이용해 사철강괴와 사철강괴에 현대강을 접합한 응용강괴 2개를 생산한 후 철제 칼 3자루를 제작하여 금속학적 특성을 비교하였다. 금속현미경과 SEM-EDS 분석결과, Fe-C 합금의 아공석강이었으며, 미세한 Ferrite와 Pearlite가 전체적으로 관찰되며, 칼날에 Martensite가 관찰되었다. 비커스 경도 분석 결과, 사철강 칼(K1)이 533.38 HV, 사철-니켈탄소강 칼(K3)은 514.8 HV, 사철-탄소강 칼(K2)가 477.02 HV로 측정되었다. 마모에 의한 질량감소율은 K1이 0.058%, K3는 0.060%, K2가 0.144%로 측정되었다. 시료의 표면무늬에 대한 EPMA 분석 결과, 표면무늬는 C의 함량의 차이 혹은 화학조성에 의해 무늬가 드러난다는 것을 확인하였다. 향후 칼날의 경도 값을 올려 내마모성을 증가시키기 위해서는 열처리 공정에 대한 추가적인 연구가 필요하며, 전통 제철법으로 제작한 강괴는 니켈 탄소강과 접합하여 사용한다면 우수한 품질의 철제품을 제작할 수 있을 것이다.

부패조와 모래트렌치를 이용한 소규모 오수 처리 (Small Sewage Treatment Using Septic Tank and Sand Trench)

  • 박영식
    • 한국환경보건학회지
    • /
    • 제29권1호
    • /
    • pp.28-33
    • /
    • 2003
  • This study was carried out to treat sewage using sand trench combined with septic tank process in rural areas. In order to find optimum parameters, design and operation mode was changed from Run 1 to Run 4. In order to facilitate nitrification and T-P removal, diffuser and iron plate was installed in the 3rd trench of Run 2 period. The septic tank played a role as pre-application process of sand trench system. The removal efficiencies of COD, NH$_4$-N, T-P at steady state were 94.6%, 87.9% and 54.5%, respectively. Addition of diffuser and iron plate in the 3rd trench has increased the removal efficiencies of the NIL-N and T-P. In this system, denitrification were not occurred because of the high DO.

여수 봉산동 출토의 사철 쇠똥에 대하여 (Metallography of Iron Slag Excavated from Bongsan-dong, Yeosu City in the Period of the 16th to 19th Century)

  • 최주;김수철;도정만
    • 보존과학회지
    • /
    • 제3권1호
    • /
    • pp.13-18
    • /
    • 1994
  • Chemical analysis and metallographic observations of the iron slag were carried out in an attempt to estimate the old iron-making process. The slag containing $9.3\%\;TiO_2$ without Cu indicates that the ore used for smelting was sand iron, not rock ore. The phases identified in the slag were $ulv\ddot{o}spinel$, magnetite, $w\ddot{u}stite$, fayalite etc. This also supports the fact that the smelted ore was iron sand. The total amount of Fe and slag-making components$(=SiO_2+Al_2O_3+MgO+CaO)$ were $40.7\%\;and\;36.1\%$, respectively. These values were average ones found in the old slags formed in the ancient iron-making process. Assuming that $TiO_2$ in the ore combines with FeO, resulting in the formation of $ulv\ddot{o}spinel$, the estimated temperature of smelting was found to be about $1200^{\circ}C$.

  • PDF

반응벽체에 쓰인 주물사의 용출특성에 관한 연구 (Leaching Characteristics of Foundry Sands When Used as Reactive Media in Permeable Reactive Barriers)

  • 이태윤;;박재우
    • 한국지반공학회논문집
    • /
    • 제18권5호
    • /
    • pp.179-193
    • /
    • 2002
  • 폐주물사가 반응벽체의 매체로 쓰였을 때의 중금속, 음이온과 PAMs의 용출 특성을 12개의 폐주물사와 3개의 기준 물질(Peerless iron, local fill soil, and torpedo sand)을 선택하여 batch와 column 실험을 통하여 밝혔다. 3개의 기준 물질은 이들로부터 얻어진 용출특성을 폐주물사와 비교하기 위해 사용되었다. Water leach test와 total elemental analyses로부터 얻어진 결과에 따라 모든 폐주물사는 그룹 2에 속하였다. 하지만, 일반적으로 지하수면 아래에 건설재료로 이용되는 3개의 기준물질도 역시 그룹 2로 분류되었다. 따라서, 폐주물사의 반응벽체에의 사용은 일반적인 건설재료를 지하수면 아래에 사용하였을 시와 비교했을 때에 비해 비슷한 농도의 중금속과 음이온이 용출됨을 알 수 있다.