• 제목/요약/키워드: STS304L stainless steel

검색결과 23건 처리시간 0.027초

열간압연으로 제조된 STS 304L/A516-70N과 STS 316L/A516-70N 클래드재들의 미세조직에 대한 비교 연구 (Comparative Study on Microstructures of Hot-rolled STS 304L/A516-70N and STS 316L/A516-70N Clad Plates)

  • 진주찬;조수철;심호섭;이영국
    • 열처리공학회지
    • /
    • 제34권4호
    • /
    • pp.171-178
    • /
    • 2021
  • In the present study, we comparatively investigated the microstructures of two hot-rolled stainless steel clad plates; STS 304L - low carbon steel A516-70N and STS 316L - A516-70N. The STS 304L/A516-70N clad plate (Clad_304L_Ni) had a Ni-interlayer between stainless steel and carbon steel and a 90 ㎛ thick deformation band of unrecrystallized austenite grains on the stainless steel. The STS 316L/A516-70N clad plate (Clad_316L) had no interlayer and almost fully recrystallized austenite grains. Clad_304L_Ni exhibited the thinner a decarburized layer in carbon steel and a total carburized layer in stainless steel than Clad_316L. However, a severely carburized layer in stainless steel was thicker for Clad_304L_Ni than Clad_316L. Hardness profiles near the interface of clad plates matched well with microstructures at locations where the hardness values were measured.

수퍼 2상 스테인리스강의 부식 저항성에 관한 연구 (Corrosion Resistance of Super Duplex Stainless Steel)

  • 강흥주;남기우;안석환;강창룡;도재윤;박인덕
    • 한국해양공학회지
    • /
    • 제17권2호
    • /
    • pp.40-46
    • /
    • 2003
  • The corrosion resistance of super duplex stainless steel on both its fibrous and dispersed phase was investigated. These structures consist of various volume fraction and distribution of austenite structure, which were obtained by changing the heat treatment temperature and cycle. The fibrous phase had higher austenite volume fraction than that of the dispersed phase at the same temperature. Corrosion resistance of super duplex stainless steel was evaluated through an immersion test and an impingement test, using 35% HCI and sea water, respectively. Super duplex stainless steel was compared with STS316L and STS304. The corrosion resistance of super duplex stainless steel was superior to ST316L and STS304. The dispersed phase of super duplex stainless steel was more stabilized than the fibrous phase in corrosion. The magnitude of corrosion rate was in order STS304, STS316L, fibrous phase of super duplex stainless steel and dispersed phase of super duplex stainless steel.

오스테나이트계 스테인리스강의 고온질화 (High Temperature Gas Nitriding of Austenitic Stainless Steels)

  • 공정현;유대경;박준홍;이해우;성장현
    • 열처리공학회지
    • /
    • 제20권6호
    • /
    • pp.311-317
    • /
    • 2007
  • This study examined the phase changes, nitride precipitation and variation in mechanical properties of STS 304, STS 321 and STS 316L austenitic stainless steels after high temperature gas nitriding (HTGN) at temperature ranges from $1050^{\circ}C\;to\;1150^{\circ}C$. Fine round type of $Cr_2N$ nitrides were observed in the surface layers of 304 and 316L steels, even more in STS 321. Additionally, square type of TiN was found in STS 321 austenitic matrix too. As a result of many precipitates in the surface layer of the STS 321, it was seen $370{\sim}470Hv$ hardness variation depending on the HTGN treatment conditions, and interior region of austenite represented 150Hv. The surface hardness value of STS 304 and STS 316L showed $255{\sim}320Hv$, respectively. The nitrogen content was shown 0.27, 1.7 and 0.4% respectively at the surface layers of the STS 304, STS 321 and STS 316L. After the HTGN it was shown the improvement of corrosion resistance of the STS 321 and STS 316L compared with solution annealed steels in the solution of 1N $H_2SO_4$ whereas the STS 304 was not.

304L 스테인리스강 분말의 내식성 개선을 위한 무전해 구리 도금과 분말 소결체의 내식성 조사 연구 (Electroless Copper Plating on 304L Stainless Steel Powders and Corrosion Resistance of the Sintered Compacts of Composite Powders)

  • 안재우;이재훈
    • 대한금속재료학회지
    • /
    • 제47권2호
    • /
    • pp.79-90
    • /
    • 2009
  • A study has been made about the effects of powder content, reaction temperature, reaction time, and stirring speed on the preparation of the stainless steel(STS) 304L powders plating with copper by an electroless plating method. The behavior of corrosion resistance of the sintered STS-Cu composite powders was also investigated by the salt spraying test The electroless plating technique was an effective method to manufactur the copper-uniform plating composite powders, the corrosion resistance of this sintered specimen was improved bysuppressing Cr precipitates on grain boundaries in the sintered compacts of composite powders.

알루미늄 합금 및 스테인리스강의 해수 농도 변화에 따른 전기화학적 부식 손상 특성 (Electrochemical Corrosion Damage Characteristics of Alumium Alloy and Stainless Steel with Sea Water Concentration)

  • 박일초;김영복;김성종
    • 한국표면공학회지
    • /
    • 제50권4호
    • /
    • pp.259-265
    • /
    • 2017
  • 5000 series aluminium alloys and austenitic stainless steels have excellent corrosion resistance and sufficient strength, which are widely used as materials for marine equipment and their parts in the marine environment. The corrosion characteristics of materials are important factors for selecting the appropriate material due to fluid component changes in the estuarine and coastal areas where seawater and fresh water are mixed. Therefore, for 5083 Al alloy, STS304 and STS316L widely used in the marine environment, anodic polarization experiments were performed to compare the corrosion damage characteristics of each material by three kinds of solutions of 100 % tap water, 50 % tap water+50 % natural seawater and 100 % natural seawater. As a result of the anodic polarization experiments, aluminum alloy (5083) caused locally corrosion on the surface in the tap water, and corrosion damage occurred all over the surface when the seawater was included. Stainless steels (STS304 and STS316L) presented almost no corrosion damage in tap water, but they grew pitting corrosion damage with increasing seawater concentration. STS316L showed better corrosion resistance than STS304.

Investigation on Ultimate Strength of STS304L Stainless Steel Welded Connection with Base Metal Fracture Using Finite Element Analysis

  • Lee, HooChang;Kim, TaeSoo;Hwang, BoKyung;Cho, TaeJun
    • 국제강구조저널
    • /
    • 제18권4호
    • /
    • pp.1139-1152
    • /
    • 2018
  • Many studies on the application of stainless steels as structural materials in buildings and infra-structures have been performed thanks to superior characteristics of corrosion resistance, fire resistance and aesthetic appeal. Experimental investigation to estimate the ultimate strength and fracture mode of the fillet-welded connections of cold-formed austenitic stainless steel (STS304L) with better intergranular corrosion resistance than that of austenitic stainless steel, STS304 commonly used has carried out by authors. Specimens were fabricated to fail by base metal fracture not weld metal fracture with main variables of weld lengths according to loading direction. All specimens showed a block shear fracture mode. In this paper, finite element analysis model was developed to predict the ultimate behaviors of welded connection and its validity was verified through the comparison with test results. Since the block shear behavior of welded connection due to stress triaxiality and shear-lag effects is different from that of bolted connection, stress and strain distributions in the critical path of tensile and shear fracture section were investigated. Test and analysis strengths were compared with those by current design specifications such as AISC, EC3 and existing researcher's proposed equations. In addition, through parametric analysis with extended variables, the conditions of end distance and longitudinal weld length for block shear fracture and tensile fracture were suggested.

오스테나이트 스테인리스강에 대한 가스텅스텐 아크용접 시동종 및 이종 용접부의 용접성 평가 (Evaluation of Weldability on Identical and Dissimilar Welding Parts of Austenite Stainless Steel by GTAW)

  • 한민수;박재철;김성종
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제35권1호
    • /
    • pp.68-74
    • /
    • 2011
  • 본 논문은 LNG 선박의 이중연료엔진의 이중벽 가스파이프의 재료인 STS 304와 STS 316L에 대하여 GTAW에 의해 용접된 동종 및 이종 용접부의 기계적 특성과 용접성을 평가하였다. STS 304 동종 용접부의 경우, STS 316L 동종 용접부에 비해 모재 대비 현저하게 기계적 특성이 감소하는 경향을 나타냈다. 미세조직 관찰 결과, STS 304 동종 용접부가 STS 316L 동종 용접부에 비해 침상 페라이트가 많이 형성되어 상대적으로 높은 경도를 나타냈다.

용접방향에 따른 오스트나이트계 스테인리스강(STS304L) 용착금속파단 용접접합부의 내력에 관한 실험적 연구 (Experimental Study on Strength of Austentic Stainless Steel (STS 304L) Fillet-Welded Connection with Weld Metal Fracture According to Welding Direction)

  • 김태수;이후창;황보경;조태준
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제22권1호
    • /
    • pp.81-89
    • /
    • 2018
  • 오스테나이트계 스테인리스강은 우수한 내식성, 내구성 및 내화성을 지닌다. 특히, 오스테나이트계 스테인리스강중의 대표인 STS304에 비해 저탄소를 함유하고 있는 STS304L은 현장용접 후 별도의 열처리 없이 높은 내입계부식성능을 지니고 있어 용접후 내입계 부식이 우려되는 부재 접합에 적용할 수 있다. 본 연구에서는 티그(TIG)용접으로 필릿 용접된 STS304L 용접접합부의 용접재(용착금속부) 내력과 파단 메카니즘을 조사하고자 한다. 주요변수인 하중방향에 대한 용접선의 배치에 따라 TFW(하중직각방향 용접), LFW(하중방향용접), FW(하중방향용접과 하중직각방향 용접조합)시리즈의 실험체를 제작하여 인장실험을 실시하였고, 각각 인장파단,전단파단, 블록전단파단(인장파단과 전단파단의 조합)이 발생하였다. 동일 용접길이에 대해 TFW 시리즈의 접합부가 가장 높은 내력을 나타났으며, 현행기준식(KBC2016/AISC2010)과 기존 연구자의 식에 의한 예측내력과 비교한 결과, TFW와 LFW접합부는 과소평가되었고 FW실험체는 과대평가되었다. 실제 파단 위험단면과 블록전단파단 메카니즘을 고려한 내력식을 제안하였다.

STS304L 캡슐의 펄스형 GTA 용접에서 용접변수들이 용접부 형상에 미치는 영향 (The Effect of Welding Parameters on the Weld Shape in Pulsed GTA Welding of a STS304L Stainless Steel Capsule)

  • 이형근;한현수;손광재
    • Journal of Welding and Joining
    • /
    • 제25권5호
    • /
    • pp.64-71
    • /
    • 2007
  • The aim of this paper is to investigate the effects of welding parameters on the weld shape in seal-welding of STS304L capsule for manufacturing a radioisotope source which is widely used in nondestructive testing of metal structures using gamma ray. Pulsed gas tungsten arc (Pulsed GTA) welding is performed for thin cross sectional area of the capsule. Seven welding parameters including current waveform parameters and arc length etc. are selected as main process parameters using design of experiment. The weld shape such as bead width, penetration depth, weld area, aspect ratio and area rate is investigated to assess the effects of welding parameters. As results, the combination of pulse duty/welding speed largely affects on bead width, penetration depth, area and aspect ratio. Finally, it is concluded that the key parameters are the combination of pulse duty/welding speed, base current and arc length, and their optimal conditions are 50%/1.77mm/s, 6.4A and 1 mm.

무윤활 수직-수평 복합하중 조건에서 재료조합에 따른 마모특성 변화에 관한 실험적 연구 (Experimental Study on Wear Behavior of Material Pairs under Normal and Sliding Mixed Loading Conditions)

  • 최성우;민준기;정일욱;박상후
    • 한국정밀공학회지
    • /
    • 제26권11호
    • /
    • pp.131-137
    • /
    • 2009
  • A pair of connectors for transferring torque is widely used in various types of a mechanical system. By the repetition of mechanical contact between a pair of connector, wear occurs easily. This kind of defect sometimes can cause a serious problem of health in case of the connector is used in a refrigerator. In this work, the material combination of connectors was experimentally studied to reduce the amount of wear; for the combination of connectors, various types of engineering materials including polyacetal, polycabonate, stainless steel (STS-304), NiP coated STS-304, and STS-310 were evaluated to check each wear behavior. Also an effective method of wear test was suggested for precise controlling of wear conditions such as contact area, contact force, and relative motion speed. From the test results, it was found out that a pair of polyacetal to STS-304 and STS-310 showed the lowest specific wear rates among other pairs.