  • The roll forming produces mass products using the continuous production process. Also we need the process that continuous long material or goods cutting into a desired length. Our study uses 3-D driving cutter and roll forming material as SPCC to investigate this. When we cut the material using the process of roll forming, the shear resistance is raised at the cutting punch's edge. The result is remained the trouble about burr and progressive deformation on the material. This study shows the method minimizing the above trouble. The material of punch was considering heat generated on the continuous production process. So we used the type of STD 61 for the material of punch and had the vacuum heat treatment for the surface hardness of HRC 53. The structure of the mold is designed with forming a double cam die at the upper punch and the both sides of central core. We conducted the experiment three times. In the result when had to make V-groove within the angle between 105 and 110 on the punch front end, we could get the minimum shear resistance on the punch front end. Also with the same condition we minimizes the material jams in the continuous production process.

TiCrN 박막의 고온 산화시 생성되는 산화막 분석 (Analyses of Oxide Scales Formed on TiCrN Coatings)

  • 이동복;이영찬;김성훈;권식철
    • 한국표면공학회지
    • /
    • 제34권4호
    • /
    • pp.321-326
    • /
    • 2001
  • The TiCrN Coatings haying three kinds of Compositions of $Ti_{36}$ $Cr_{26}$ $N_{38}$ , $Ti_{31}$ $Cr_{35}$ $N_{34}$ / and $Ti_{14}$ $Cr_{52}$ $N_{34}$ were deposited on STD 61 steel substrate by arc ion plating and were oxidized between 700 and 100$0^{\circ}C$ to identify the oxide scales formed on the coatings. The oxide scales were then analyzed using EPMA, XRD and GAXRD. During oxidation, the coatings consisting of TiN and CrN phases were reduced to TiO2 and $Cr_2$$O_3$, respectively. Titania tended to form at the outer oxide layer, whereas chromia tended to form at the inner oxide layer, owing to the different oxygen affinity. The substrate elements as well as coating elements diffused outwardly toward the oxide layer due to the concentration gradient. The growth of oxide from the TiCrN coatings was schematically expressed on the basis of thickness measurement of the reacted and unreacted coatings. The Cr element showed its stronger role to keep the TiCrN coatings from oxidation, when compared with Ni.

  • PDF

AISI M2 파우더를 이용한 레이저 메탈 디포지션의 트랙 특성 분석 (The Characteristics Analysis of Track of Laser Metal Deposition Using AISI M2 Powder)

  • 김원혁;송명환;박인덕;강대민
    • 한국자동차공학회논문집
    • /
    • 제24권4호
    • /
    • pp.463-470
    • /
    • 2016
  • In this paper, the characteristics analysis of LMD track, such as including track structure, track wear resistance and track thickness, were analyzed to enhance the deposition efficiency using a diode-pumped disk laser. SKD61 hot work steel plate and Fe based AISI M2 alloy were used as a the substrate and powder for the LMD process, respectively. The laser power, track pitch and powder feed rate among LMD parameters were adopted to estimate the deposition efficiency. As the laser power is increased, heat input and melting pool on the substrate is grown also increases, so resulting in the increased LMD track thickness was increased. Through EPMA mapping analysis of the cross-section in the LMD track, it was observed that all the elements are evenly distributed inside. Therefore, the entire hardness in the LMD track is expected to be almost uniform regardless of location. The characteristics of the LMD specimen were excellent compared to the STD11 specimen in terms of the wear track width and the wear rate as well as the coefficient of friction. Especially the wear rate of LMD specimen has been significantly reduced by 60 % or more. From Based on the experimental results, the prediction formula of LMD thickness was calculated by using laser power, track pitch and powder feed rate.