Fabrication and Physicochemical Properties of Carbon/Titania/Bentonite Monolith for Architecture

  • Oh, Won-Chun;Choi, Jong-Geun;Song, Da-Ye;Kim, Ha-Rry;Chen, Ming-Liang;Zhang, Feng-Jun;Park, Tong-So
    • 한국재료학회지
    • /
    • 제20권3호
    • /
    • pp.167-173
    • /
    • 2010
  • In this study, we used activated carbon (AC) and titanium oxysulfate as a titanium precursor to prepare carbon/titania composites. We then mixed it with bentonite in different ratios to make a carbon/titania/bentonite monolith for use in architecture bricks by using Phenolic rosin (PR) as a bonding agent. The physicochemical properties of the prepared composites were analyzed by BET surface area, scanning electron microscopy (SEM), X-ray diffraction (XRD), energy dispersive X-ray analysis (EDX), self-cleaning effect and bactericidal tests. The BET surface areas increased as the ratio of carbon/titania composites increased. The SEM microscopy showed that the $TiO_2$ and bentonite were coated on the surface of the AC. The XRD patterns showed a mixture structure of anatase and rutile of $TiO_2$ with a clear $SiO_2$ structure. The EDX spectra of the carbon/titania/bentonite monolith confirmed the presence of various elements, namely C, O, Ti and Si, as well as other, impure elements. Moreover, to determine the self-cleaning effect of the carbon/titania/bentonite monolith, we used methylene blue (MB, $C_{16}H_{18}N_3S{\cdot}Cl{\cdot}3H_2O$) in an aqueous solution under the irradiation of visible light. Accordingly, all of the samples had excellent degradation of the MB solution. Furthermore, it was observed that the composites with sunlight irradiation had a greater effect on E. coli than any other experimental conditions.

졸-겔 방법으로 제조한 TiO2박막 광촉매의 물성 분석과 광화학 반응 (Photochemical Reaction and Characterization of TiO2 Thin Film Photocatalyst Fabricated by Sol-Gel Method)

  • 임희섭;이용희;손종윤;유윤식;이동환;성대동
    • 공업화학
    • /
    • 제16권2호
    • /
    • pp.187-193
    • /
    • 2005
  • 광촉매 $TiO_2$박막은 titanium (IV) isopropoxide, 에탄올, HCl을 일정한 비율로 졸-겔방법에 의해 제작하였다. SEM에 의한 표면관찰에서는 $500^{\circ}C$에서 5회 반복해서 코팅하여 제작한 것이 우수했다. EDX에 의한 성분비는 spin코팅이 O : Ti의 atom%가 61 : 39로 dip코팅보다 우수했다. 그리고 박막제작의 온도에 따라서 anatase상에서 rutile상으로 결정구조가 변화되어 가는 것을 XRD측정으로 알았다. 제작한 $TiO_2$박막에 UV빔을 조사해서 얻은 TOC의 광분해효율이 1 h 이내에 20~65%를 나타내었고, 그 이후에는 서서히 감소하는 것을 확인했다.

실란 표면 개질된 나노복합막의 염료 분리 특성 (Surface Modification of Nanofiltration Membrane with Silane Coupling Agents for Separation of Dye)

  • 박희민;임지은;김성애;이용택
    • 멤브레인
    • /
    • 제28권6호
    • /
    • pp.414-423
    • /
    • 2018
  • 본 연구에서는 염색 염료 산업의 폐수 처리 및 재활용 공정에 분리막을 적용하고자 실란 커플링제를 이용하여 상용화된 나노복합막을 표면 개질하였다. 실란 커플링제는 말단 관능기가 다른 octyltrimethoxysilane (OcTMS)와 (3-aminopropyl) trimethoxysilane (APTMS)을 사용하였으며, 표면 개질을 통해 염료 분리 및 내오염성을 향상시키고자 하였다. XPS, FE-SEM, EDX 분석을 통하여 막 표면의 화학 구조 변화 및 실란 적층을 확인하였고, AFM 분석을 통해 개질막의 표면 모폴로지를 확인하였다. Zeta potential을 통해 실란 개질 막이 상용막 대비 표면 전하가 중성으로 변하는 것을 확인하였다. 그 결과, OcTMS와 APTMS로 개질한 막의 내오염성은 NE70에 비해 약 2배 이상 향상되었다. 또한, 실란으로 표면 개질한 나노복합막은 음이온 염료(Orange II) 용액에서 약 90% 이상, 양이온 염료(Safranin-O) 용액에서 약 98% 이상의 염료 제거율을 나타내어 양이온 염료 용액 처리에 적합한 것을 확인하였다.

도재용착용 Ni-Cr계 합금의 이트륨 첨가물이 도재전단결합강도에 미치는 영향 (Effect of yttrium additives on the shear bond strength of porcelain fused to Ni-Cr alloy for porcelain fused metal crown)

  • 우제승;노세라;노형록;임청하;이정환
    • 대한치과기공학회지
    • /
    • 제41권2호
    • /
    • pp.71-80
    • /
    • 2019
  • Purpose: In this study, to evaluate the effect of oxide changes on the shear bond strength according to the composition of Ni-Cr alloys for porcelain fused matal crown, T-4 alloys, Zeroy alloys and Zeroy-X alloys were selected. Methods: 20 specimens were fabricated using selected Ni-Cr alloys and porcelain powders. A Ni-Cr alloy having a diameter of 5 mm and a height of 25 mm was produced and the metal surface was polished. Porcelain powder was fired on the polished metal surface to a diameter of 5 mm and a height of 3 mm. The experiment group consisted of three groups, T-4(TNA), Zeroy(ZNA) and Zeroy-X(ZXA). The fabricated specimens were mounted on a jig of a universal testing machine(UTM) and fracture strength was measured by applying a shear force at a UTM crosshead speed of 0.5 mm/min. The fracture strength was calculated as the bond strength between the porcelain and the alloy. The surface of the fractured alloy was analyzed by X-ray diffraction(XRD) and scanning electron microscopy(SEM), and the components of the oxide were measured by energy dispersive X-ray spectroscopy(EDX) line profile method. Results: In SEM, XRD and EDX analysis, yttrium tended to increase the mechanical and chemical bonding forces. The shear bond strength of ZXA group containing yttrium showed the highest value at 27.53 MPa. Conclusion: Based on the results of this study, it is considered that the yttrium-added Ni-Cr alloy is clinically acceptable in porcelain shear bond strength.

폐석면광산 주변 지역의 주택 침적먼지의 석면 검출과 석면폐증의 관련성 (Exposure Assessment and Asbestosis Pulmonum among Inhabitants near Abandoned Asbestos Mines Using Deposited Dust)

  • 안호기;양원호;황보영;이용진
    • 한국환경보건학회지
    • /
    • 제41권6호
    • /
    • pp.369-379
    • /
    • 2015
  • Objectives: The lack of reliable information on environmental pollution and health impacts related to asbestos contamination from abandoned mines has drawn attention to the need for a community health study. This study was performed to evaluate asbestos-related health symptoms among residents near abandoned asbestos mines located in the Chungcheong Provinces. In addition, exposure assessment for asbestos is needed although the exposure to asbestos was in the past. Methods: Past exposure to asbestos among inhabitants near abandoned asbestos mines was estimated by using surface sampling of deposited dust in indoor and outdoor residences. A total of 54 participants were divided into two groups with (34 cases) and without (20 controls) diseases related to asbestos. Surface sampling of deposited dust was carried out in indoor and outdoor residences by collecting 105 samples. Deposited dust for sampling was analyzed by polarization microscope (PLM) and scanning electron microscope?energy dispersive x-ray spectrometer (SEM-EDX) to detect asbestos. Subsequently, the elements of the deposited dust with asbestos were analyzed by SEM-EDX to assess the contribution of sources such as abandoned mines, slate and soil. Results: Among the 105 samples, asbestos was detected by PLM in 29 (27.6%) sampling points, and detected by SEM in 56 (48.6%) sampling points. Asbestos in indoor residences was detected by PLM in four sampling points, and by SEM in 12 sampling points. Asbestos detection in indoor residences may be due to ventilation between indoors and outdoors, and indicates long-term exposure. The asbestos detection rate for outdoor residences in the case group was higher than that in the control group. This can be explained as the case group having had higher exposure to asbestos, and there has been continuous exposure to asbestos in the control group as well as the case group. Conclusion: Past residential asbestos exposure may be associated with asbestosis among local residents near abandoned asbestos mines. Odds ratios were calculated for asbestos detection in outdoor residence by logistic regression analysis. Odds ratio between asbestos detection and asbestosis pulmonum was 3.36 (95% CI 0.90-12.53) (p=0.072), adjusting for age, sex, smoking status and work history with multi-variable logistic regression by PLM analysis method.

Effect of Heat-Treated Temperature on Surface Crystal Structure and Catalytic Activity of ACF/ZnO Composite under Ultraviolet Irradiation and Ultrasonication

  • Zhang, Kan;Oh, Won-Chun
    • 한국세라믹학회지
    • /
    • 제47권2호
    • /
    • pp.136-141
    • /
    • 2010
  • ACF/ZnO photocatalyst was synthesized by a sol-gel method using activated carbon fiber (ACF) and Zn $(NO_3)_2$ as precursors. Samples were characterized by Brunauer-Emmett-Teller measurements (BET), scanning electron microscope (SEM), X-ray diffraction (XRD), and energy dispersive X-ray (EDX). The XRD results showed that ACF/ZnO composites only included a hexagonal phase by heat-treated temperature at $400^{\circ}C$, $500^{\circ}C$, $600^{\circ}C$, and $700^{\circ}C$. The SEM analysis revealed that the ACF/ZnO composites did not exhibit any morphological changes of the catalyst surface according to the different heat-treated temperatures. The photocatalytic activity of the samples was tested for degradation of methylene blue (MB) solutions under ultraviolet (UV) light and ultrasonication respectively. The results showed that the photocatalytic activity of ACF/ZnO composites heat-treated at $500^{\circ}C$ was higher than other samples, which is ascribed to the fine distribution of ZnO particles on the surface of the ACF. In addition, an ultrasound of low power (50 W) was used as an irradiation source to successfully induce ACF/ZnO composites to perform sonocatalytic degradation of MB. Results indicated that the sonocatalytic method in the presence of ACF/ZnO composites is an advisable choice for the treatments of organic dyes.

Novel Synthesis and Characterization of Pt-graphene/TiO2 Composite Designed for High Photonic Effect and Photocatalytic Activity under Visible Light

  • Ye, Shu;Oh, Won-Chun
    • 한국세라믹학회지
    • /
    • 제54권1호
    • /
    • pp.28-32
    • /
    • 2017
  • The degradation of methyl blue (MB) catalyzed by platinum (Pt)-graphene/$TiO_2$ in dark ambiance was studied. Pt-graphene/$TiO_2$ composites were prepared by simple hydrothermal method. Characterizations of composites were studied by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), specific surface area (BET) analysis, and energy dispersive X-ray (EDX) analysis. UV-spectroscopic analysis of the dyes was performed by measuring the change in absorbance. The degradation of the organic dyes was calculated based on the decrease in concentration of the dyes with respect to regular time intervals. Rate coefficients for the catalytic process were successfully established and reusability tests were performed to test the stability of the used catalysts.

초정밀 반도체 금형 제작을 위한 슈퍼드릴 방전가공기 전극가이드 개발과 미세홀 방전가공 (Development of Electrode Guide of Super-drill EDM and Electrical Discharge Machining of Small Hole for High Precision Semiconductor Die)

  • 박찬해;김종업;왕덕현;김원일
    • 한국기계가공학회지
    • /
    • 제4권3호
    • /
    • pp.32-38
    • /
    • 2005
  • Electrical discharge machining is the method of using thermal energy by electrical discharge. Generally, if the material of workpiece has conductivity even though very hard materials and complicated shape which are difficult to cut such as quenching steel, cemented carbide, diamond and conductive ceramics, the EDM process is favorable one of possible machining processes. But, the process is necessarily required of finish cut and heat treatment because of slow cutting speed, no mirror surface, brittleness and crack due to the residual stress for manufactured goods. In this experimental thesis, the super EDM drilling was developed for high precision semiconductor die steel and for minimization of leadframe width. It was possible to development of EDM drilling machine for high precision semiconductor die with the electrode guide and its modelling and stress analysis. The development of electrode with the copper pipe type was conducted to drill the hole from the diameter of 0.1mm to 3.0mm with the error of from 0.02mm to 0.12mm. From the SEM and EDX analysis, the entrance of the EDM drill was found the resolidification of not only the component of tungsten but also the component of copper.

  • PDF

Sonochemical Synthesis, Thermal Studies and X-ray Structure of Precursor [Zr(acac)3(H2O)2]Cl for Deposition of Thin Film of ZrO2 by Ultrasonic Aerosol Assisted Chemical Vapour Deposition

  • Hussain, Muzammil;Mazhar, Muhammad;Rauf, Muhammad Khawar;Ebihara, Masahiro;Hussain, Tajammal
    • Bulletin of the Korean Chemical Society
    • /
    • 제30권1호
    • /
    • pp.92-96
    • /
    • 2009
  • A new precursor [$Zr(acac)_{3}(H_{2}O)_{2}$] was synthesized by Sonochemical technique and used to deposit thin $ZrO_{2}$ film on quartz and ceramic substrate via ultrasonic aerosol assisted chemical vapour deposition (UAACVD) at 300 ${^{\circ}C}$ in oxygen environment followed by annealing of the sample for 2-3 minutes at 500 ${^{\circ}C}$ in nitrogen ambient. The molecular structure of the precursor determined by single crystal X-ray analysis revealed that the molecules are linked through intermolecular hydrogen bonds forming pseudo six and eight membered rings. DSC and TGA/FTIR techniques were used to determine thermal behavior and decomposition temperature of the precursor and nature of evolved gas products. The optical measurement of annealed $ZrO_{2}$ film with tetragonal phase shows optical energy band gap of 5.01 eV. The particle size, morphology, surface structure and composition of deposited films were investigated by XRD, SEM and EDX.

충북대학교 박물관소장 16-19세기 지류문화재의 특성 (Scientific Evaluation of 16-l9th Century Historic Paper Artefacts from Chungbuk National University Museum)

  • ;;최태호;조남석
    • 보존과학회지
    • /
    • 제16권
    • /
    • pp.27-38
    • /
    • 2004
  • 지류문화재는 원료, 종이의 기원, 제조년대 및 제조기술과 관련된 많은 흥미로운 정보를 제공해 주고 있다. 지류문화재연구의 제 1단계로서 구성되는 섬유의 식별이며, 지류문화재에 포함된 조성분의 파악이 이의 보존처리 및 수복처리방법을 결정하는데 매우 중요한 정보를 제공하게 된다. 본 연구에서는 대한민국 충북대학교 박물관(CNUM)에 소장중인 16-19세기 지류문화재의 특성을 분석하였다. 측정수단으로서 광학현미경, 주사전자현미경, Energy 분산 X-ray 분광분석법 (EDX)등을 사용하였다. 16-19 C에 제조된 것으로 생각되는 지류문화재를 분석한 결과, 원료는 섬유장 2.79-16.03 mm, lumen 폭 $4.5-26{\mu}m$, 광학 및 주사전자현미경으로 관찰한 섬유들의 형태적 특성으로부터 닥나무 인피섬유로 만들어진 것으로 확인되었으며, 대부분의 종이들이 잘 보존된 상태였다. EDX분석결과, 지류시료들은 많은 종류의 무기성분들(적게는 6종, 많은 경우에는 13종)을 함유하고 있었으며, 그 가운데 S, Si. Ca, P, Al 등이 많았던 결과로부터 충전제로서 주로 석고, 백토, 활석 등이 사용된 것으로 생각된다. 약 반정도의 시료에서 종이의 장기간 보존을 저해할 것으로 생각되는 S, Cl, Fe등이 검출되었는데, 보존처리시 고려해야 할 것으로 생각된다.

  • PDF