• 제목/요약/키워드: SCM420

검색결과 28건 처리시간 0.026초

SCM 420강의 프레팅 피로 특성에 관한 연구 (A Study on Fretting Fatigue Characteristic of SCM 420 Steel)

  • 김태규;김현수;윤수종;김혜성
    • 열처리공학회지
    • /
    • 제19권1호
    • /
    • pp.30-36
    • /
    • 2006
  • Fretting fatigue behavior of SCM420 steel commonly used in the automotive industry for structural applications was investigated in this study. In addition, the effect of bridge pad on the fretting fatigue test was evaluated from different pad materials and following conclusions were drawn. Simple fatigue limit of SCM 420 steel was determined to be 350 MPa while this value was 225 MPa and 285.5 MPa with SCM420H and with SM45C pad, respectively. Reduction in fatigue limit was, thus found to be 35.7% and 17.9% with SCM 420H pad and SM45C pad, respectively. Results of fracture surface observation revealed that typical striation pattern of fatigue failure existed as well as dimpled and cleavage frature appearance was found in final fractured region. From the EDS compositional analysis, test sample and pad part all had high signals for oxygen and iron, suggesting that worn particles might be iron oxide, although exact chemical composition has to be confirmed. Considerable reduction in fatigue life was apparent in SCM 420 steel under fretting fatigue against simple fatigue. Such reduced fatigue life by fretting damage should be considered as an important factor not only in the viewpoint of repairing but also inevitably in the design stage of structural components.

SCM420H 유성기어의 호닝효과에 관한 연구 (A Study on the Effect of the Honing in SCM420H Planetary Gear)

  • 안인효;안민주;허철수;류성기
    • 한국기계가공학회지
    • /
    • 제10권3호
    • /
    • pp.13-18
    • /
    • 2011
  • This study deals with the effect of the honing in SCM420H planetary gears. The hardness, tooth profile, lead and roughness of the gear surface can be improved by honing. Therein, the honing techniques are welcomed especially as one of the physical surface improvement methods. As a result, gear honing reduces vibration and noise, and will increase the life of gear. And gear honing also changes the surface of gear tooth in a short time and price, so it is a very important method in manufacturing industry. But nowadays, it is hard to find the detail information of gear honing. The test gear is a planetary gear which is used in the automotive industry. It is manufactured by the hobbing, shaving, carburizing and honing. This study investigates the effect of honing in surface shape of SCM420H planetary gears, including fatigue strength test and characteristics of honing of SCM420H planetary gears.

크롬-몰리브덴강(SCM420)에 대한 프레팅 피로수명 예측에 관한 연구 (A Study on Fretting Fatigue Life Prediction for Cr-Mo Steel(SCM420))

  • 곽동현;노홍래;김진광;조상봉
    • 한국정밀공학회지
    • /
    • 제24권4호
    • /
    • pp.123-130
    • /
    • 2007
  • Recently, a lot of work and interest have been devoted to the development of multiaxial fatigue parameters for fretting fatigue life prediction. In this study, the fretting fatigue lift and critical location ware estimated and evaluated through the multiaxial fatigue theories in a cylinder-on-flat contact configuration far Cr-Mo steel, SCM420, the material commonly is used in gears of the automobile and rollers of the conveyor. The strain-life curve was obtained from fatigue test for SCM420. The Fretting fatigue life and critical location were estimated through stress distributions, SWT-parameters and FS-parameters obtained from FEA. This paper showed possibility of applying multiaxial fatigue theories to fretting fatigue lift prediction comparing predicted life with experimental results.

SCM420H 유성기어의 연삭효과에 관한 연구 (A Study on Effect of the Grinding in SCM420H Planetary Gear)

  • 안인효;허남수;이인범;류성기
    • 한국기계가공학회지
    • /
    • 제11권5호
    • /
    • pp.54-59
    • /
    • 2012
  • This study dealt with effect of the grinding in SCM420H planetary gears. The hardness, tooth profile, lead and roughness of the gear surface can be improved by grinding process. Therein, the grinding techniques are widely used especially as one of the physical surface improvement methods. As the results, the gear grinding process reduced vibration and noise, and increased the life of the gear. And the gear grinding improved the surface of gear tooth in a short time and low cost, thus, it is a very important process in manufacturing industry. But nowadays, it is hard to find the detail information of gear grinding process. The test piece is a planetary gear which is used in the industrial machine. The manufacture process of the test piece contains hobbing, shaving, carburizing and grinding. This study investigated the effect of the grinding process to the physiognomy and the fatigue strength of test piece which was made by SCM420H.

SCM420기어의 피로강도에 미치는 열처리효과에 관한 연구 (A Study on the Effect of Heat-treatment on the Fatigue Strength of SCM420 Spur Gears)

  • 류성기;신용호
    • 한국안전학회지
    • /
    • 제14권4호
    • /
    • pp.13-19
    • /
    • 1999
  • This study deals with effects of heat-treatment on the bending fatigue of SCM420 spur gears. The test gears are heat-treated by two different treatments. After carburization, one group of the test gears is quenched directly, while another group is furnace cooled, reheated then quenched. The fatigue test at a constant stress amplitude is performed by using an electrohydraulic serve-controlled pulsating tester. The S-N curves are obtained and illustrated. By comparing the estimated strength with the experimental results, the validity of the previous experimental formula, presented by the authors for estimating the fatigue strength of carburized gears, was discussed for these tested gears.

  • PDF

표면개질에 따른 자동차 트랜스미션 기어의 내마멸성 평가 (Wear Resistance Evaluation of Automobile Transmission Gear on Surface Modification)

  • 박재상;류을현;김동호;김영희;박흥식
    • Tribology and Lubricants
    • /
    • 제19권2호
    • /
    • pp.78-84
    • /
    • 2003
  • The SCM420 used mainly to automobile transmission gear has problems that it costs transmission gear maker much money in carburising treatment. For this, it needs to alternate the existing material and heat treatment to new gear material and surface modification. For this, friction and wear experiment according to sliding speed and applied load was carried out to evaluate the wear resistance of two transmission gear materials with carburising SCM420 and nitrocarburising NT100, The presumed wear volume was calculated with the image processing for evaluation of wear resistance of two transmission gear materials. The results show that nitrocarburising NT100 has a distinguished wear resistance than carburising SCM420.

SCM420H 유성기어의 쇼트피닝 효과에 관한 연구 (A Study on the Effect of the Shot Peening in SCM420H Planetary Gear)

  • 안인효;안민주;류성기
    • 한국안전학회지
    • /
    • 제26권1호
    • /
    • pp.15-20
    • /
    • 2011
  • This study deals with the effect of the shot peening in SCM420H planetary gears. The hardness and roughness of the gear surface can be improved by shot blast and shot peening. there in, the shot peening techniques are welcomed especially as one of the physical surface improvement methods. The two treatments are used widely, because of the qualitative analysis of shot blast and shot peening has become possible and the surface treatment can be done with little costs compared with other surface improvement methods. Therefore, this study investigates the effects of shot blast and shot peening in surface shape. The fatigue strength test at a constant stress amplitude is performed by using an electrohydraulic serve-controlled pulsating tester. And fatigue test also explained characteristics of shot blast and shot peening of planetary gears.

열처리한 HSLA 강의 유동특성 (Flow Stress of HSLA Steel by Heat Treatment)

  • 김정민;최노진;강성수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 춘계학술대회 논문집
    • /
    • pp.178-181
    • /
    • 2004
  • Heat treatment is one of important manufacturing process that determine the quality of the products. Because of a difference of mechanical property by heat treatment, It is necessary to This papers presents flow stress and yield point through tensile test. The goal of this study is to obtain the data of flow stress and yield point at martensite, bainite, ferrite/pearlite phase structure using SCM420, SCr420. The result of tensile test is satisfied and is expected to develop an available FEM analysis.

  • PDF