• Title/Summary/Keyword: Rubber Materials

Search Result 1,020, Processing Time 0.033 seconds

Effect of NR/BR Blends ratio and Oil Content on the Mechanical Properties of Rubber Isolator at Low Temperature (저온환경에서 NR/BR 블렌드 조성비 및 오일함량이 방진고무재료의 기계적 특성에 미치는 영향)

  • Kim, Wan-Doo;Kim, Wan-Soo;Woo, Chang-Soo;Choi, Sung-Seen
    • Elastomers and Composites
    • /
    • v.39 no.2
    • /
    • pp.95-104
    • /
    • 2004
  • New compounds were made using various NR/BR blend ratio and oil content to improve mechanical properties of rubber isolator at low temperature. Mechanical properties were investigated as a function of NR/BR blend ratio and oil content. Hardness and tensile modulus generally increased, but tensile strength and elongation at break decreased with increasing BR content. Hardness, tensile modulus and tensile strength decreased, but elongation at break were nearly the same with increasing oil content. The glass transition temperature of NR and BR were found to be $-50^{\circ}C$ and $-90^{\circ}C$ respectively based on the abrupt drops in storage elastic modulus and peak of loss factor. Two distinct transition temperature were observed in NR/BR blend compounds and each transition point was not affected by blend level indicating incompatible nature of NR/BR blend.

Rubber Composites with Piezoresistive Effects (고무 복합재료의 압저항 효과)

  • Jung, Joonhoo;Yun, Ju Ho;Kim, Il;Shim, Sang Eun
    • Elastomers and Composites
    • /
    • v.48 no.1
    • /
    • pp.76-84
    • /
    • 2013
  • The term 'Piezoresistive effect' describes a change in the electrical resistance of the material from deformed to its original shape by the external pressure, e.g., elongation, compression, etc. This phenomenon has various applications of sensors for monitoring pressure, vibration, and acceleration. Although there are many materials which have the piezoresistive effect, rubber (nano)composites with conductive fillers have attracted a great deal of attention because the piezoresistive effect appears at the various range of pressure by controlling the type of filler, particle size, particle shape, aspect ratio of particles, and filler content. Especially one can obtain the composites with elasticity and flexibility by using the rubber as a matrix. This paper aims to review the piezoresistive effect itself, their basic principles, and the various conductive rubber-composites with piezoresistive effect.

Comparison on Mechanical Properties of SSBR Composites Reinforced by Modified Carbon black, Silica, and Starch

  • Lee, Dam-Hee;Li, Xiang Xu;Cho, Ur-Ryong
    • Elastomers and Composites
    • /
    • v.53 no.3
    • /
    • pp.175-180
    • /
    • 2018
  • Solution-styrene-butadiene rubber (SSBR) composites were manufactured using four kinds of fillers: silica-silane coated carbon black (SC-CB) hybrid, starch-SC-CB hybrid, pure silica, and pure starch. The influence of filler type on the mechanical properties of the rubber matrix was studied in this work. SC-CB was prepared by silane-graft-coating using vinyl triethoxy silane and carbon black, which enhanced the dispersion effect between the rubber matrix and the filler, and improved the mechanical properties of the compounds. The morphology of the composites was observed by field-emission scanning electron microscopy (FE-SEM). The thermal decomposition behavior of the composites was determined by thermogravimetric analysis (TGA), and the crosslinking behavior of the composites was tested using a rubber process analyzer (RPA). The hardness, tensile strength, swelling ratio, and gas transmittance rate of the composites were evaluated according to ASTM. The test results revealed that with the addition of SC-CB, the hybrid fillers, especially those blended with silica, showed a better reinforcement effect, the highest hardness and tensile strength, and stable thermal decomposition behavior. This implies that the silica-SC-CB hybrid filler has a notable mechanical reinforcement effect on the SSBR matrix. Because of self-crosslinking during its synthesis, the starch-SC-CB hybrid filler produced the most dense matrix, which improved the anti-gas transmittance property. The composites with the hybrid fillers had better anti-swelling properties as compared to the neat SSBR composite, which was due to the hydrophilicity of silica and starch.

Comparison on the Performance Medical Radiation Shielding Made of Rubber Sheet (의료방사선 차폐 고무시트의 제작과 성능 비교)

  • Kim, Seon-Chil
    • Korean Journal of Digital Imaging in Medicine
    • /
    • v.12 no.1
    • /
    • pp.15-18
    • /
    • 2010
  • Main component of radiography barrier aprons is lead. To manufacture a lead-free barrier sheath, barium sulfate and organic iodine-based chemicals should be mixed with rubber. Barrier capacity was tested in the medical field. To improve adaptation of rubber with the mixture, raw materials went through milling, agitation, and extruding processes. Three sheaths were manufactured with 30%, 80%, and 120% sulfate barium, respectively. This study found 10% lower barrier capacity of lead-free barrier than the traditional lead-containing rubber sheath. Problems, however, were confronted during the agitation and extruding processes. Mixing with rubber was a technically demanding job. Inconsistent depth, problems with thermal processing and dissipation were encountered as well.

  • PDF

Study on the Adhesive Properties of Polyesters Reinforcing Materials

  • Krump, H.;Hudec, I.;Cernak, M.;Janypka, P.
    • Elastomers and Composites
    • /
    • v.37 no.3
    • /
    • pp.192-194
    • /
    • 2002
  • Polyester cord yarns have been treated in an atmospheric-pressure nitrogen plasma reactor in order to enhance their adhesion to rubber. A thin layer or the plasma was generated in the close vicinity of the yam surface using various types or surface discharge. To assess the effect of the plasma treatment on fiber surface properties, the cord thread/rubber matrix adhesion values measured using the untreated and threads cord threads were compared. The static and dynamic adhesion of the cord thread to rubber was characterized by using the standard Henley test. The dynamic adhesion values for the reference and plasma treated fiber were $7,3{\pm}1,2\;N$ and $83,5{\pm}3,5\;N$. The surface properties were investigated by scanning electron microscopy, infrared spectroscopy and electron spin resonance spectroscopy. It is concluded that both polar group interactions and increased surface area of the fibers are responsible for the improved adhesive strength.

Development of micromolding technology using silicone rubber mold (실리콘 고무형을 이용한 미세복제기술 개발)

  • 정성일;임용관;박선준;최재영;정해도
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.46-49
    • /
    • 2003
  • Microsystem technology (MST) which originated from semiconductor processes has been widely spreaded into tile other industry such as sensors, micro fluidics and displays. The MST, however. has been troubled in spreading with its high cost and material limitations. So, in this paper, new process for micromolding technology using silicone rubber mold was introduced. Silicone rubber mold, which was fabricated by vacuum casting. can be transferred a master pattern to a final product with the same shape but different materials. In order to verify the possibility of application of silicone rubber mold to the MST, its transferability was evaluated. and then it applied to the fabrications of polishing pad and PDP barrier ribs.

  • PDF

Effects of silicone fluid in silicone rubber composite (실리콘 고무 복합재료의 물성에 대한 실리콘 오일의 영향)

  • Han, D.H.;Kang, D.P.
    • Proceedings of the KIEE Conference
    • /
    • 1996.07c
    • /
    • pp.1670-1672
    • /
    • 1996
  • Silicone rubber composite is very suitable for insulation materials because of it's hydrophobicity, mass productivity, and design flexibility. A study of the diffusion of silicone fluid from the bulk to the surface of the silicone rubber composite using dynamic contact angle meter and scanning electron microscopy(SEM) is reported. A study of the mechanical strength of the silicone rubber composite having various silicone fluids and fluid contents is also reported. It has been found that the kind of silicone fluid affects the diffusion rate of the silicone fluid from the bulk to the surface of the silicone rubber composite after artificial pollution.

  • PDF

Development of Micromolding Technology using Silicone Rubber Mold (실리콘 고무형을 이용한 미세복제기술 개발)

  • Chung, Sung-Il;Im, Yong-Gwan;Kim, Ho-Youn;Choi, Jae-Young;Jeong, Hae-Do
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.27 no.8
    • /
    • pp.1380-1387
    • /
    • 2003
  • Microsystem technology (MST) which originated from semiconductor processes has been widely spreaded into the other industry such as sensors, micro fluidics and displays. The MST, however, has been troubled in spreading with its high cost and material limitations. So, in this paper, new process for micromolding technology using silicone rubber mold was introduced. Silicone rubber mold, which was fabricated by vacuum casting, can be transferred a master pattern to a final product with the same shape but different materials. In order to verify the possibility of application of silicone rubber mold to the MST, its transferability was evaluated, and then it applied to the fabrications of polishing pad and PDP barrier ribs.

Applications of the Silicone Rubber in EHV Electric Appliances (초고압 전력기기에서의 실리콘 고무 응용)

  • 김영호;지응서;박현득;허근도
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.05a
    • /
    • pp.560-564
    • /
    • 1999
  • In general, the main dielectric materials for EHV electric appliances were epoxy, EPDM and Silicone rubber. The Silicone rubber has been rosed so many among them in EHV appliances in the worldwide, especially in Europe and North America. The reason why it is very stable in the thermal, mechanical and electrical environment. Therefore it is still becoming increasingly widespread in the application of the EHV appliances as a main dielectric material. On this study, investigated about real appliances and tested on basic properties of the Silicone rubber compared to organic dielectric material that is EPDM. At the result, the Silicone rubber is more dominant as main dielectric material for EHV appliances than any other organic polymers.

  • PDF

THE ABSORPTION PROPERTIES OF Cu-Zn FERRITE/RUBBER COMPOSITE MICROWAVE ABSORBER WITH PZT ADDITIVE

  • Shin, Kwang-Ho;Geon, Sa-Gong
    • Journal of the Korean Magnetics Society
    • /
    • v.5 no.5
    • /
    • pp.556-560
    • /
    • 1995
  • The absorption properties of Cu-Zn ferrite/rubber composite microwave absorbers with PZT(Lead Zirconate Titanate) additive were evaluated. The composite specimens have prepared by molding and curing the mixture of matrix rubber and Cu-Zn ferrite powders which are synthesized by the coprecipitation method using Fe Cl/sub 3/ .center dot. 6H/sub 2/O, CuCl/sub 2/ .center dot. 2H/sub 2/O and Zn Cl/sub 2/ as a starting raw materials. PZT is used as another filler particles to adjust the material constants of Cu-Zn ferrite/rubber composite specimens. We have found that the material constants of specimens could be controlled by various PZT mixing ratio. On the Cu-Zn ferrite/rubber composite specimens with PZT 10[wt%] additive, the reflection losses were larger than 30[dB] in the frequency range from 2.72 to 4.4[GHz]' by adjusing the thickness.