• Title/Summary/Keyword: Roll Wear

Search Result 93, Processing Time 0.026 seconds

Study on Structural Integrity and Dynamic Characteristics of Knuckle Parts of KTX Anti-Roll Bar (KTX 고속열차 안티롤바 너클부의 동특성 및 구조 안전성 평가)

  • Jeon, Kwang Woo;Shin, Kwang Bok;Kim, Jin Woo;Jeong, Yeon Il
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.37 no.8
    • /
    • pp.1035-1041
    • /
    • 2013
  • To evaluate the structural integrity and dynamic characteristic of the knuckle part of a KTX anti-roll bar, an experimental and a numerical approach were used in this study. In the experimental approach, the acceleration and strain data for the knuckle parts of the KTX and KTX-SANCHUN anti-roll bar were respectively measured to evaluate and compare its structural dynamic characteristics under the operating environments of the Honam line. In the numerical approach, the evaluation of its structural integrity was conducted using LS-DYNA 3D, and then, the reliability of the finite element model used was ensured by a comparative evaluation with the experiment. The numerical results showed that the stress and velocity field of the knuckle part composed of a layered structure of a thin steel plate and rubber were more moderate than those of the knuckle part made of only a thick steel block owing to the reduction of relative contact between the knuckle and the connecting rod. It was found that the knuckle part made of a thin steel plate and rubber was recommended as the best solution to improve its structural integrity resulting from the elastic behavior of the KTX anti-roll bar being enabled under a repeating external force.

An Investigation of Mechanical Properties and Sliding Wear Behavior of Ultra-Fine Grained 5052 Aluminum Alloy Fabricated by a Accumulative Roll-Bonding Process (누적압연접합공정에 의해 제조된 초미세립 5052 알루미늄 합금의 상온 기계적 특성 및 미끄럼 마멸거동에 대한 연구)

  • 하종수;강석하;김용석;신동혁
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2003.03a
    • /
    • pp.26-26
    • /
    • 2003
  • 본 연구에서는 누적압연접합공정(ARB)을 통하여 5052 알루미늄 합금의 결정립을 약 0.2$\mu\textrm{m}$ 크기로 미세화 하였다. 누적압연에 의한 변형량 증가에 따른 미세 조직 변화와 결정립 간의 상대적인 방위각 차이를 TEM을 이용하여 관찰하였다. 누적 변형량을 함수로 상온 인장특성을 분석하였고, 초미세립 소재를 후속 열처리한 후 미세 조직 변화를 관찰하여 제조된 초미세립 소재의 열적 안정성을 평가하였다. 상온 대기 중에서 pin-on-disk 형태의 마멸시험기를 사용하여 초미세립 소재의 미끄럼 마멸시험을 변형량과 하중을 변수로 행하였다. 강소성 변형에 의해 제조된 5052 알루미늄 합금 소재의 마멸저항성은 강소성 변형 전과 비교하여 소재의 경도가 크게 증가하였음에도 불구하고 오히려 감소하였다. 마멸시험 후 마멸면의 SEM, 마멸단면의 OM 관찰과 마멸면 직하의 깊이에 따른 경도측정을 통하여 초미세립 소재의 마멸기구를 분석하였고 마멸표면의 변형 층을 관찰하였다. 또한 마멸면 직하 조직의 TEM 관찰을 통해서 마멸시험 중의 미세 조직 변화를 연구하였다.

  • PDF

Application of Ultrasonic Vibration Energy on Eco-superfinishing and Surface Hardening Treatment of Cold Work Roller (초음파 진동에너지를 이용한 냉간 압연롤러 표면의 환경 친화적 초정밀 사상 및 표면 경화 처리 및 시험)

  • Y.S. Pyoun;Park, J.H.;C.H. Han;Park, Y.;I.S. Cho;N. Azuma;Lee, J.H.;Kim, C.S.;Park, C.H.
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2002.05a
    • /
    • pp.39-39
    • /
    • 2002
  • In order to improve wear and fatigue resistance of the structural materials, especially cold work roller for 304 stainless steel, an eco-super-finishing and surface hardening treatment using ultrasonic vibration energy was developed and applied to the SKD-ll roller. The eco-super-finishing machine was designed and fabricated by DesignMecha Co, by its own technology. It was observed that the surface roughness, hardness and residual stress were changed from $Ra{\;}={\;}O.25\mu\textrm{m}$, Hv=710 and ${\sigma}$={\;}+400{\;}MPa{\;}to{\;}Ra{\;}={\;}0.165\mu\textrm{m}$, Hv = 1200 and ${\sigma}=-610$ MPa after 20 KHz micro-cold forging, which means almost equal to the 300 % improvement of life-time.

  • PDF

Microstructure and Mechanical Properties of β-SiAlON Ceramics Fabricated Using Self-Propagating High-Temperature Synthesized β-SiAlON Powder

  • Kim, Min-Sung;Go, Shin-Il;Kim, Jin-Myung;Park, Young-Jo;Kim, Ha-Neul;Ko, Jae-Woong;Yun, Jon-Do
    • Journal of the Korean Ceramic Society
    • /
    • v.54 no.4
    • /
    • pp.292-297
    • /
    • 2017
  • ${\beta}-SiAlON$, based on its high fracture toughness, good strength and low abrasion resistance, has been adopted in several industrial fields such as bearings, turbine blades and non-ferrous metal refractories. In general, ${\beta}-SiAlON$ is fabricated by reactive sintering using expensive $Si_3N_4$ and AlN as starting materials. On the other hand, in this study, a cheaper ${\beta}-SiAlON$ starting powder synthesized by SHS was employed to improve price competitiveness compared to that of the reactive sintering process. ${\beta}-SiAlON$ ceramics with various content of the sintering additive $Y_2O_3$ up to 7 wt% were fabricated by conventional pressureless sintering at $1800^{\circ}C$ for 2 to 8 h under $N_2$ pressure of 0.1 MPa. The specimen with 3 wt% $Y_2O_3$ exhibited the best mechanical properties: hardness of 14 GPa, biaxial strength of 830 MPa, fracture toughness of $5MPa{\cdot}m^{1/2}$ and wear rate of about $3{\times}10^{-6}mm^3/N{\cdot}m$.

A Scanning Electron Microscope Study of the Bristles (시판 잇솔의 특성 및 잇솔모의 주사전자현미경적 연구)

  • Yang, Jung-Seung
    • Journal of Korean society of Dental Hygiene
    • /
    • v.2 no.2
    • /
    • pp.159-173
    • /
    • 2002
  • The 180 toothbrushes out of 18 models( ten brushes for each model) were used for this examination among the toothbrushes for adults which were sold in the domestic markets. After three-month brushings through a roll ing method and Bass method were practiced with Toothbrush Stroke Tester which reproduced brushing methods outside the mouth, I investigated the morphology bristle tips of using scanning electron microscope(SEM). The conclusions are as follows. 1. Soft bristle toothbrushes(of 8 models out of 9 models) were badly damaged at the bristles end after 3 month toothbrushing. 2. Medium bristle toothbrushes(of four models out of five models) were irregularly worn at the bristles end after 3 month toothbrushing. 3. Hard bristle toothbrushes(of three models out of four models) were chisel-shapedly worn at the bristles end after 3 month toothbrushing. 4. Taper-shaped toothbrushes were very irregularly bent at the bristles end after 3 month toothbrushing. 5. It was examined in the bristle stiffness that soft bristle toothbrushes were found in 9 models(50.00%), medium bristle toothbrushes in 5 models(27.78%), and hard-bristle toothbrushes in 4 models(22.22%).

  • PDF

Analysis of Dynamic Characteristics for a Tapered Roller Bearing Cage (테이퍼 롤러 베어링 케이지의 동특성 해석)

  • Park, Jang-Woo;Heo, Jun-Young
    • Journal of the Korea Convergence Society
    • /
    • v.8 no.5
    • /
    • pp.179-184
    • /
    • 2017
  • The cage of a tapered roller bearing keeps the gap between the rollers, which prevents friction, wear and suppresses heating. The material of the cage is changing from metal to plastic for lightening the weight. If the cage is severely deformed due to resonance, the roller may not be able to roll and even get off the cage. In this paper, the dynamic characteristics of the cage is analyzed according to the cage material. Under the assumption that a train runs at the highest speed, frequency harmonics of that speed is calculated, and the comparative analysis is carried out in order to select the optimum thickness of the cage, which is easy to change among the cage design variables for avoiding the resonance.

Effects of Alloying Elements and Heat Treatments on the Microstructures and Mechanical Properties of Ductile Cast Iron by Strip Casting (스트립캐스팅한 구상흑연주철박판의 합금원소 및 열처리에 따른 미세조직과 기계적 성질의 변화)

  • Lee, Gi-Rak;Ra, Hyung-Yong
    • Journal of Korea Foundry Society
    • /
    • v.20 no.2
    • /
    • pp.122-128
    • /
    • 2000
  • Strip casting process is a new technology that makes a near net shape thin strip directly from molten metal. With this process, a large amount of energy and casting cost could be decreased from the abbreviation of reheating and/or hot rolling process. Ductile cast iron which has spheroidal graphite in the matrix is the most commercial and industrial material, because of its supreme strength, toughness, and wear resistance etc. But it cannot be produced to the thin strip owing to difficulty in rolling of ductile cast iron. In this study, ductile cast iron strips are produced by the twin roll strip caster, with different chemical compositions of C, Si, and Mn contents. And then heat-treated, microstructures and mechanical properties are examined. The microstructures of as-cast strip are that of white cast iron which consists of the mixture of cementite and pearlite, but the equiaxed crystal zone of the pearlite or segregation zone of cementite exists in the center region of the strip thickness, which cannot be observed in the rapidly solidified metallic mold cast specimens. This structure is supposed to be formed from the thermal distribution of strip and the rolling force. Comparing with the structures of each strips after heat treatment, increasing Si content makes smaller spheroidal graphite and more compact in the matrix, furthermore the less of Mn content makes the ferrite matrix be obtained clearer and easier. As a result of the tensile test of graphitization heat-treated strips, the yield strengths are about 250 MPa, the tensile strengths are about $430{\sim}500$ MPa, and the elongations are about $10{\sim}13%$. In the case of the strip which has the smaller and more compact spheroidal graphite in the ferrite matrix, the higher tensile strength and better drawability could be obtained.

  • PDF

Formation and Progression of Intermetallic phase on Iron Base Alloy PTA weld overlay in Molten Zn Alloys (용융 Zn 합금에서 Fe합금의 PTA 오버레이 용접 금속간 상의 형성과 진행)

  • Zulkarnain, Zulkarnain;Baek, E.R.
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.95-95
    • /
    • 2009
  • Zinc coatings provide the most effective and economical way of protecting steel against corrosion. There are three types of galvanizing lines typically used in production line in galvanizing industries,Galvanize (GI) coating (Zn-0.1-0.3%Al), Galfan coating (Zn-5%Al), Galvalume(GL) coating (45%Zn-Al). In continuous Galvanizing lines, the immersed bath hardware (e.g. bearings, sink, stabilizer, and corrector rolls, and also support roll arms and snout tip) are subjected to corrosion and wear failure. Understanding the reaction of these materials with the molten Zn alloy is becomes scientific and commercial interest. To investigate the reaction with molten Zn alloys, static immersion test performed for 4, 8, 16, and 24 Hr. Two different baths used for the static immersion, which are molten Zn and molten Zn-55%Al. Microstructures characterization of each of the materials and intermetallic layer formed in the reaction zone was performed using optical microscope, SEM and EDS. The thickness of the reaction layer is examined using image analysis to determine the kinetics of the reaction. The phase dominated by two distinct phase which are eutectic carbide and matrix. The morphology of the intermetallic phase formed by molten Zn is discrete phase showing high dissolution of the material, and the intermetallic phase formed by Zn-55wt%Al is continuous. Aluminum reacts readily with the materials compare to Zinc, forming iron aluminide intermetallic layer ($Fe_2Al_5$) at the interface and leaving zinc behind.

  • PDF

The Effects of Geometrical Imperfections on the Dynamic Characteristics of a Tapered Roller Bearing Cage (테이퍼 롤러 베어링 케이지의 불완전성이 통특성에 미치는 영향)

  • Ahn, Tae-Kil;Park, Jang-Woo
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.20 no.4
    • /
    • pp.464-469
    • /
    • 2019
  • Tapered roller bearings are used widely in vans, trucks, and trains because they can support the vehicle in a stable manner even under a heavy load. The cage of a tapered roller bearing maintains the gap between the rollers, which prevents friction wear and suppresses heating. If the cage is severely deformed due to resonance, the roller may not be able to roll smoothly and even leave the cage. Consequently, it is very important to analyze the dynamic characteristics of the cage for reliable performance of a bearing. The cage essentially has geometrical tolerance in the manufacturing process. In this paper, the effects of those geometrical imperfections on the dynamic characteristics of the cage were investigated. As a result, natural frequency separation occurred near the natural frequency of the ideal cage due to geometrical imperfections. In addition, the interval was proportional to the magnitude of the geometric error, and the interval increased with increasing mode number.

Effects of Alloying Elements on Sticking Occurring During Hot Rolling of Ferritic Stainless Steels (페라이트계 스테인리스강의 열간압연 시 발생하는 Sticking에 미치는 합금원소의 효과)

  • Ha, Dae Jin;Kim, Yong Jin;Lee, Jong Seog;Lee, Yong Deuk;Lee, Sunghak
    • Korean Journal of Metals and Materials
    • /
    • v.46 no.9
    • /
    • pp.593-603
    • /
    • 2008
  • In this study, effects of alloying elements on the sticking occurring during hot rolling of five kinds of ferritic STS430J1L stainless steels were investigated by analyzing high-temperature hardness and oxidation behavior of the rolled steels. Hot-rolling simulation tests were conducted by a high-temperature wear tester which could simulate actual hot rolling. The simulation test results revealed that the sticking process proceeded with three stages, i.e., nucleation, growth, and saturation. Since the hardness continuously decreased as the test temperature increased, whereas the formation of Fe-Cr oxides in the rolled steel surface region increased, the sticking of five stainless steels was evaluated by considering both the high-temperature hardness and oxidation effects. The addition of Zr, Cu, or Si had a beneficial effect on the sticking resistance, while the Ni addition did not show any difference in the sticking. Particularly in the case of the Si addition, Si oxides formed first in the initial stage of high-temperature oxidation, worked as initiation sites for Fe-Cr oxides, accelerated the formation of Fe-Cr oxides, and thus raised the sticking resistance by about 10 times in comparison with the steel without Si content.