• 제목/요약/키워드: Residual tensile strength

검색결과 268건 처리시간 0.026초

고강도강재의 고온인장특성 및 용접시 잔류응력특징에 관한 연구 (A Study on the High Temperature Tensile Property and the Characteristics of Residual Stress in Welds of High Strength Steels)

  • 장경호;이진형;신영의
    • Journal of Welding and Joining
    • /
    • 제22권4호
    • /
    • pp.50-58
    • /
    • 2004
  • In this study, high temperature tensile properties of high strength steels(POSTEN60, POSTEN80) were investigated. The three-dimensional thermal elastic-plastic analyses were conducted to investigate the characteristics of welding residual stresses in welds of high strength steels on the basis of thermal and mechanical properites at high temperature obtained from the experiment. According to the results, high temperature tensile strength of POSTEN60 steel deteriorated slowly to 10$0^{\circ}C$. As the temperature went up, the tensile strength became better because of blue shortness, and it deteriorated radically after reaching to the maximum value around 30$0^{\circ}C$. For the POSTEN80 steel, high temperature tensile strength deteriorated slowly to 20$0^{\circ}C$. As the temperature went up the tensile strength became better and it deteriorated slowly to $600^{\circ}C$ after reached to the maximum value around 30$0^{\circ}C$. Strain of high strength steels at the elevated temperature increased radically after the mercury rose to $600^{\circ}C$. The strain hardening ratio of POSTEN60 steel was larger then that of POSTEN80 steel at the elevated temperature as in the case at the room temperature and it became smaller radically after the mercury rose to 40$0^{\circ}C$. And, in the welding of high strength steels, increasing tensile strength of the steel (POSTEN60

상수도 금속관의 잔존 인장강도 추정모델 개발 (Development of Residual Tensile Strength Prediction Model for Metallic Water Pipes)

  • 배철호;김정현;우형민;홍성호
    • 한국지반환경공학회 논문집
    • /
    • 제9권3호
    • /
    • pp.17-28
    • /
    • 2008
  • 본 연구에서는 상수도 금속관의 공식특성에 따른 잔존 인장강도 예측모델을 제안하였다. 이들 모델중 회주철관에 대해서는 지수함수형 모델이 실측값에 대한 예측값의 상관성($R^2$)이 높게 나타났으며, 닥타일주철관과 강관 등은 선형함수인 공식특성에 따른 강도손실 모델이 더 예측력이 높은 것으로 나타났다. 국내에서 과거에 제조된 상수도 금속관의 파괴인성은 평균적으로 회주철관이 $40.46kgf/mm^2{\sqrt{mm}}$, 닥타일주철관이 $85.27kgf/mm^2{\sqrt{mm}}$, 그리고 강관이 $97.27kgf/mm^2{\sqrt{mm}}$로 나타났으며, 파괴인성을 이용한 잔존 인장강도 예측모델의 실측값에 대한 예측값의 상관성은 관종에 따라 다르나 0.44에서 0.86로 나타났다. 특히 이들 제안된 모델들을 새로운 지역에 매설된 상수관로에 대하여 적용한 결과, 결정계수가 0.76~0.78로 나타나 향후 노후 상수도 금속관의 잔존 강도를 예측하는데 활용됨으로서 합리적인 개대체 의사결정에도 도움을 줄 수 있을 것으로 판단된다.

  • PDF

Strength properties of lime stabilized and fibre reinforced residual soil

  • Okonta, Felix N.;Nxumalo, Sinenkosi P.
    • Geomechanics and Engineering
    • /
    • 제28권1호
    • /
    • pp.35-48
    • /
    • 2022
  • The effect of discrete polypropylene fibre reinforcement on shear strength parameters, tensile properties and isotropic index of stabilized compacted residual subgrade was investigated. Composites of compacted subgrade were developed from polypropylene fibre dosage of 0%, 1%, 2.5% and 4% and 3% cement binder. Saturated compacted soil benefited from incremental fibre dosage, the mobilized friction coefficient increased to a maximum at 2.5% fibre dosage from 0.41 to 0.58 and the contribution due to further increase in fibre dosage was marginal. Binder stabilization increased the degree of isotropy for unreinforced soil at lower fibre dosage of 1% and then decreased with higher fibre dosage. Saturation of 3% binder stabilized soil decreased the soil friction angle and the degree of isotropy for both unstabilized and binder stabilized soil increased with fibre dosage. The maximum tensile stress of 3% binder stabilized fibre reinforced residual soil was 3-fold that of 3% binder stabilized unreinforced soil. The difference in computed and measured maximum tensile and tangential stress decreased with increase in fibre dosage and degree of stabilization and polypropylene fibre reinforced soil met local and international criteria for road construction subgrade.

주철관의 잔존강도 평가에 관한 연구 (Assessment of Residual Tensile Strength on Cast Iron Water Pipes)

  • 배철호;김주환;김정현;홍성호
    • 상하수도학회지
    • /
    • 제20권6호
    • /
    • pp.867-874
    • /
    • 2006
  • The goal of this study is to assess cast iron pipes (CIPs) and present a residual tensile strength prediction model using pit characteristics and fracture toughness. The results is the followings. First, average pit depths of collected CIPs were in the range from 0.63 to 6.49 mm, loss of tensile strength compared with net metallic tensile strength were from -7.06 to 67.91 percent. Second, fracture toughness for NS-CR-1, NS-CR-2, and NS(2)-CR-1 were in the range from 62.85 to $89.39kgf/mm^2{\sqrt{mm}}$, and average of those samples was $73.69kgf/mm^2{\sqrt{mm}}$ on CIPs. Third, the models developed in this study by using pit characteristics and fracture toughness showed a little good correlation for measured residual tensile strength, and the results will be expected to help for water utilities to manage CIPs in the aspect of rehabilitation and assessment of structural safety on CIPs.

구속된 건조수축이 철근콘트리트 인장거동에 미치는 영향 (Tensile Behavior of Reinforced Concrete Member due to Restrained Shrinkage)

  • 안태송;김진철
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 봄 학술발표회 논문집(I)
    • /
    • pp.315-320
    • /
    • 1998
  • The experimental set-up and one-dimensional analytical model have been developed to investigate the tensile behavior of reinforced concrete member due to restrained drying shrinkage. The experimental results have been compared with the analytical prediction of the maximum residual stress of steel and concrete due to restrained shrinkage. The tensile residual stress concrete by one-dimensional bilinear model shows 0.19 and 0.63 of tensile strength for 0.83% and 3.29 of steel ratio. The residual tensile stress of concrete increases as the steel ratio increases. The effect of steel fiber has not influenced the residual stress due to restrained shrinkage of concrete.

  • PDF

Al-7020의 Pulse-GMA용접에 관한 연구 2

  • 김재웅;허장욱;나석주;백운형
    • Journal of Welding and Joining
    • /
    • 제6권4호
    • /
    • pp.54-62
    • /
    • 1988
  • Major problems in welding Al-7020 include shrinkage, rpopositgy in welds and loss of strength in the heat affected zone. Thus it is important to examine the mechanical properties and reliability of welds. In this study, a series of experiments was carried out to determine the mechanical properties such as micro-hardness distribution, tensile strength, porosity and residual stress distribution of the Al-7020 weldment made by pulse-GMA welding. The resuts of the experiemnts are as folows. 1) The micro-hardness of weld metal and heat affected zone was lower than that of the base metal. 2) The tensile strength of the deposited metal was much lower than that of the base metal. 3) The porrosity in weld metal zone was negligible under the adopted conditsion of experiemnts. 4) The residual stress in the weld metal was lower than that of the heat affected zone, because the weld metal was softened. And the mciro-hardness distribution, the tensile strength and the residual stess distribution of the weldment in the as-welded condition were compared with those of the weldment after heat treatment.

  • PDF

고감성 니트디자인을 위한 무봉제 니트 조직패턴의 성능과 이미지간의 연구 (1) - 암홀 접속부(마치)의 역학적 특성을 중심으로 - (Study of the Relation between Quality and Image of the WholeGarment Knit Structured Patterns for High Sensible knit Design (1) - On mechanical property to armhole connecting part (Machi) -)

  • 이유진;최원정
    • 패션비즈니스
    • /
    • 제16권1호
    • /
    • pp.52-68
    • /
    • 2012
  • To achieve the aim of this study, 9 different types of samples were made to examine mechanical property according to structured pattern and type of Machi of pullover armhole of WholeGarment(seamless knitwear). With respect to samples, from which comparisons are made and anaylzed among basic characteristics of material, tensile strength & elongation and residual elongation due to repeated extension of armhole connecting part, the following conclusions could be obtained. It's revealed that the tensile strength of Machi part as being armhole connecting part of samples is more affected by Machi type than pattern structure. Of Machi types, it showed stronger tensile strength in the order of Normal(Normal Machi)< Machi_B(unilateral Machi)

극저온 열처리가 7075 알루미늄 합금의 잔류응력과 기계적 특성에 미치는 영향 (Effects of Cryogenic Treatment Cycles on Residual Stress and Mechanical Properties for 7075 Aluminum Alloy)

  • 김회봉;정은욱;고대훈;김병민;조영래
    • 한국재료학회지
    • /
    • 제23권1호
    • /
    • pp.18-23
    • /
    • 2013
  • In this study, the effects of cryogenic treatment cycles on the residual stress and mechanical properties of 7075 aluminum alloy (Al7075) samples, in the form of a tube-shaped product with a diameter of 500 nm, were investigated. Samples were first subjected to solution treatment at $470^{\circ}C$, followed by cryogenic treatment and aging treatment. The residual stress and mechanical properties of the samples were systematically characterized. Residual stress was measured with a cutting method using strain gauges attached on the surface of the samples; in addition, tensile strength and Vickers hardness tests were performed. The detailed microstructure of the samples was investigated by transmission electron microscopy. Results showed that samples with 85 % relief in residual stress and 8% increase in tensile strength were achieved after undergoing three cycles of cryogenic treatments; this is in contrast to the samples processed by conventional solution treatment and natural aging (T4). The major reasons for the smaller residual stress and relatively high tensile strength for the samples fabricated by cryogenic treatment are the formation of very small-sized precipitates and the relaxation of residual stress during the low temperature process in uphill quenching. In addition, samples subjected to three cycles of cryogenic treatment demonstrated much lower residual stress than, and similar tensile strength compared to, those samples subjected to one cycle of cryogenic treatment or artificial aging treatment.

용접 토우부의 국부적 변형률 측정을 통한 용접부의 정적 과하중에 따른 피로강도의 변화 평가 (The Static Overload Effect Estimations on Fatigue Strength by The Measurement of Local Strain Variation at The Weldment Toe)

  • 이현우;김주환;김현재
    • 한국정밀공학회지
    • /
    • 제18권6호
    • /
    • pp.59-66
    • /
    • 2001
  • Fatigue strength of the welding structure is governed by the residual stress at the weldment toe and static tensile overloads were known as relieving the residual stresses. In this study, static tensile overloads were applied to the welding structures which caused the relief of residual stresses. The amount of residual stress relief was found as proportional to the change of fatigue limit at the given conditions. Based on the fact of the proportionality between the change of fatigue limit and that of residual stress, simple measurement technique is proposed. Modified stress-life curves base on proposed technique gave good agreement with test results.

  • PDF

플라즈마 스프레이방법을 이용하여 Ti 언더코트를 제작한 SUS316L강의 부식피로 특성 (Corrosion Fatigue Characteristics of SUS316L Steel with Ti Undercoat using Plasma Spray Method)

  • 한창석;김우석
    • 한국재료학회지
    • /
    • 제31권3호
    • /
    • pp.172-180
    • /
    • 2021
  • In this study, using the plasma spray method, tensile and compression fatigue tests are performed in saline solution to examine the effect of Ti undercoat on corrosion fatigue behavior of alumina-coated specimens. The alumina-coated material using Ti in the undercoat shows better corrosion fatigue strength than the base material in the entire stress amplitude range. Fatigue cracking of UT specimens occurs in the recess formed by grit-blasting treatment and progresses toward the base metal. Subsequently, the undercoat is destroyed at a stage where the deformation of the undercoat cannot follow the crack opening displacement. The residual stress of the UT specimen has a tensile residual stress up to about 100 ㎛ below the surface of the base material; however, when the depth exceeds 100 ㎛, the residual stress becomes a compressive residual stress. In addition, the inside of the spray coating film is compressive residual stress, which contributes to improving the fatigue strength characteristics. A hardened layer due to grit-blasting treatment is formed near the surface of the UT specimen, contributing to the improvement of the fatigue strength characteristics. Since the natural potential of Ti spray coating film is slightly higher than that of the base material, it exhibits excellent corrosion resistance; however, when physiological saline intrudes, a galvanic battery is formed and the base material corrodes preferentially.