• 제목/요약/키워드: Ratio of Mineral Admixture

검색결과 117건 처리시간 0.027초

고내구성콘크리트의 염해저항성에 관한 실험적 연구 (An Experimental Study on the Salt Damage Resistance of High Durable Concrete)

  • 윤재환;정재동
    • 한국건축시공학회지
    • /
    • 제3권3호
    • /
    • pp.73-81
    • /
    • 2003
  • In this paper, salt damage resistance of high durable concrete was tested. High durable concrete was made by using low water cement ratio, chemical admixture called super-durable admixture and mineral admixtures such as fly-ash, ground granulated blast-furnace slag, silica fume. Two kinds of salt damage resistance test were carried out. One method is chloride ion penetration test(ASTM C1202), and the other one is depth of chloride penetration test in saline solution. Test results were as followers: 1) The depth of chloride ion penetration increased exponentially as water cement ratio was increased and time passed. 2) Super-durable admixture had little effect on the improvement of salt damage resistance of concrete. 3) Silica fume and ground granulated blast-furnace slag were effective on salt damage resistance because of pozzolanic reaction, but fly-ash had a little effect.

염소 고함유시멘트의 페이스트 유동성과 모르타르 강도발현성에 미치는 무기질 혼화재의 영향 (Effects of Mineral Admixture on the Paste Fluidity and Mortar Strength Development of High Chloride Cement)

  • 정찬일;박수경;이의학;이경희
    • 한국세라믹학회지
    • /
    • 제44권1호
    • /
    • pp.43-51
    • /
    • 2007
  • Fluidity, setting time, hydration heat, bond water ratio, compressive strength, SEM and BET of OPC were measured by adding 1.0 wt% KCl and replacing 20 wt% mineral admixture in order to examine effects of blast furnace slag (BFS), limestone powder (LSP), and fly ash (FA) on fluidity and strength development of the cement contained much chloride. In general, the cement contained much chloride was high in heat of hydration, short in its setting time, low in its fluidity and low in its strength at 28 days due to the rapid hydration in its initial stage. As a result of the experiment, it has been demonstrated that fluidity became improved but the compressive strength at 28 days was decreased as replaced LSP to the cement contained much chloride. the fluidity and compressive strength at 28 days was improved as replaced BFS, the initial compressive strength development was improved due to the activation of initial reaction by KCl. Fluidity, initial compressive strength and late compressive strength at 28 days of cement contained much chloride replaced 5 wt% LSP and 15 wt% BFS concurrently was better than OPC, but the hydration heat was lower.

동제련 슬래그를 혼입한 고강도 콘크리트의 유동특성에 관한 연구 (The Fluidity Properties of High Strength Concrete adding Copper Slag as Mineral Admixture)

  • 이동운;윤종진;김대영
    • 한국산학기술학회논문지
    • /
    • 제17권10호
    • /
    • pp.271-279
    • /
    • 2016
  • 본 연구의 목적은 고강도 콘크리트에 광물성 혼화재로서 동제련 슬래그를 혼입하였을 때 유동특성을 파악하기 위한 것이다. 이를 위해 동제련 슬래그를 고강도 콘크리트의 결합재로 사용하여 10 %, 20 %, 30 %, 40 %, 50 %를 시멘트로 대체하여 사용하였다. 그리고 굳지않은 콘크리트에서 슬럼프플로, 500mm도달시간, V-Funnel과 U-Boxt시험을 실시하여 유동성 및 충전성을 알아보았고, 굳은 콘크리트에서는 재령 3, 7, 14, 28일의 콘크리트 압축강도를 측정하였다. 상기의 실험결과, 동제련 슬래그를 광물설 혼화재료로 혼입한 콘크리트의 굳지 않은 콘크리트 특성을 살펴보면 동제련 슬래그의 치환율이 30%까지는 유동성이 증가하였으며, 충전성이 우수한 것을 알 수 있었다. 그리고 굳은 콘크리트의 특성을 살펴보면 동제련 슬래그의 치환율이 30 %일때까지 모든 재령에서 압축강도가 증가하는 것을 확인할 수 있었다. 그러나 동제련 슬래그의 치환율이 30%를 초과하였을 때는 유동성, 충전성 및 압축강도가 감소하는 것을 확인할 수 있어 동제련 슬래그의 최적 치환율은 30 %이내가 적정할 것으로 판단된다.

국내.외산 메타카올린을 사용한 고강도 콘크리트의 내구특성에 관한 실험적 연구 (An Experimental Study on the Properties of Durability of High Strength Concrete Using Domestic.Foreign Meta-kaolin)

  • 이강필;이승민;이상수;송하영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2009년도 춘계 학술논문 발표대회 학계
    • /
    • pp.239-242
    • /
    • 2009
  • As the high-rise building increase due to the gravitation of population to big cities recently, it requires high quality and high performance of Concrete. As a result, people are keenly interested in Meta-kaolin as new admixture favorable from an economic perspective, which has strength and endurance with admixture at the same level like Silica-fume. Accordingly, as to Meta-kaolin, this study was to set by three levels like domestic one, foreign one, and Silica-fume, the water-binding material ratio 25%, and four level substitute like 0, 10, 20, and 30(%) in order to compare and analyze the quality durability of high-concrete according to the substitute of Meta-kaolin applicable with replacement of Silica-fume. As a result of performing experiment it was found that when water-binding material ratio increases, resistance of neutralization, carbonation, salt damage and sulfate decrease, and when replacement ratio of mineral admixture increases, depth of accelerating carbonation gets greater. Also, the combination of SF and MK-B favored resistance to chloride ion penetration better than MK-A, and it was found that when replacement ratio of binding material increases, the resistance to sulphuric acid increases. Therefore, based on this study, it was understood that meta-kaolin is useable in replacement of silicafume.

  • PDF

강섬유 보강 시멘트 복합체의 시공성 향상에 관한 연구 (A Study on the Improvement of Construction Performance of Steel Fiber Reinforced Cementitious Composites)

  • 고경택;박정준;김방욱;이종석;김성욱;이장화
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.749-754
    • /
    • 2002
  • In this study, it is investigate to influence on tile dispersion of fiber and the flowability of matrix of type and amount of superplasticizer, velocity agent, mineral admixture and steel fiber to improve for construction performance of steel fiber reinforced cementitious composites. As for the test results, it was found that the dispersion of fiber and the flowability of matrix in steel fiber reinforced cementitious composites can improve by using of properly amount and combination of superplasticizer, velocity agent, mineral admixture. Furthermore, It show that the aspect ratio of steel fiber affect the construction performance of fiber reinforced cementitious composites, and the improvement for construction performance is the more effective the smaller aspect ration of steel fiber.

  • PDF

메타카올린 및 실리카퓸의 혼입이 고강도 콘크리트의 압축강도와 염소이온 투과에 미치는 영향에 관한 통계적 가설검증 (The Statistical Hypothesis Verification to Influence of Addition of Metakaolin and Silica Fume on Compressive Strength and Chloride Ion Penetration of High Strength Concrete)

  • 민정욱
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제15권1호
    • /
    • pp.215-225
    • /
    • 2011
  • 메타카올린은 고령토나 카올린으로 알려진 카올린 광물의 풍화물로, 도자기 산업에 주로 사용되는 원료로, 일반적으로 메타카올린의 입자 크기는 시멘트보다는 작지만, 마이크로 실리카퓸보다는 크다. 본 연구에서는 콘크리트용 혼화재로 메타카올린을 사용한 콘크리트의 압축강도와 염소이온 투과저항 특성에 관한 영향에 관해 조사하였다. 메타카올린과 실리카퓸의 혼입률이 압축강도와 염소이온 투과저항에 주는 영향을 비교하기 위해 물-결합재비를 30%로 고정하고 각각 0, 5, 10, 15, 20%인 배합수준을 설정하여 비교하였다. 연구결과 메타카올린을 혼입한 콘크리트는 실리카퓸을 혼입한 콘크리트와 유사한 강도특성을 보였지만, 염소이온 투과저항성은 다소 불리한 것으로 나타났다. 따라서, 강도와 염소이온 투과저항 성능을 동시에 만족하기 위한 메타카올린의 혼입률은 10% 정도인 것으로 나타났다.

3성분계 혼화재료로 사용한 콘크리트 특성 (Properties of Concrete Containing third binary mineral Admixture)

  • 조일호;양재성;김진희
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 봄 학술발표회 논문집(I)
    • /
    • pp.95-101
    • /
    • 1999
  • This study was performed to evaluate the characteristics of workability and strength of the concrete containing mineral admixtures such as flyash, blast furnace slag, zeolite powder. As a result, considering their workability and strength, the optimum replacement ratio of them to plain concrete were obtained for each ternary admixture. This increased compressive strength was ascribed to both the closer parkinof fine particles and pozzolan reactivity of powders. This work showed that could be effectively utilized as a blending material without any decrease in the strength of early hydration stage. On the other hand, we found that the compressive strength at early ages ternary ordinary and high strength concrete untill 7 days was small, but that ternary concrete at 28days was highly increased about 31% and 15% extent.

  • PDF

해상교량 주탑용 고성능 콘크리트의 기준재령 염소이온 확산계수 (Chloride Diffusion Coefficient at Reference Time for High Performance Concrete for Bridge Pylons in Marine Environment)

  • 윤철수;김기현;양우용;차수원
    • 콘크리트학회논문집
    • /
    • 제24권4호
    • /
    • pp.435-444
    • /
    • 2012
  • 기준재령 염소이온 확산계수를 측정하기 위하여 고성능 콘크리트 배합을 선정하고 공시체를 제작하였다. 배합은 해양환경에 건설되는 교량에 적합하도록 선정되었으며 배합설계 변수는 결합재 종류, 물-결합재비, 광물질 혼화재 치환율, 잔골재 종류, 고강도 및 고유동성을 얻기 위한 화학 혼화제 종류, 목표 슬럼프 또는 슬럼프 플로우이다. 시험 결과로부터 기준재령 염소이온 확산계수는 결합재 종류와 그 치환율에 따라 크게 다름을 확인하고, 결합재 종류와 치환율을 고려한 기준재령 확산계수 모델을 개발하였다. 개발된 모델의 확산계수를 기존 모델의 확산계수 및 추가 확산 계수 측정시험 결과 비교하여 개발된 모델의 타당성을 확인하였다.

고성능 콘크리트의 자기수축 예측모델에 관한 연구 (Prediction Model on Autogenous Shrinkage of High Performance Concrete)

  • 유성원;소양섭;조민정;고경택;정상화
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제10권3호
    • /
    • pp.97-105
    • /
    • 2006
  • 고성능 콘크리트의 자기수축은 초기균열을 유도할 수 있기 때문에 내구성 측면에서 매우 중요하다. 이에 따라, 본 연구에서는 실험을 통해 혼화재료를 혼입한 고성능 콘크리트의 자기수축 특성을 분석한 후 예측모델을 제안하였다. 이를 위해 다양한 실험변수를 가진 시편에 대해 광범위한 실험을 수행하였다. 주요 실험변수는 혼화재료의 종류 및 혼입률로 설정하였으며 물-시멘트비는 30%로 고정하였다. 실험결과 플라이애시를 치환한 경우에는 자기수축량이 다소 감소하였으며, 고로슬래그를 사용한 경우에는 자기수축이 증가하였다. 또한, 수축저감제 및 팽창재의 혼입량이 클수록 고성능 콘크리트의 자기수축은 감소하는 경향을 보였다. 한편, 본 논문에서는 회귀분석을 통해 혼화재료를 사용한 고성능 콘크리트의 자기수축 예측식을 제안하였으며, 제안된 자기수축 예측식은 실험결과와 비교적 일치하였다

Experimental studies on rheological properties of smart dynamic concrete

  • Bauchkara, Sunil D.;Chore, H.S.
    • Advances in concrete construction
    • /
    • 제5권3호
    • /
    • pp.183-199
    • /
    • 2017
  • This paper reports an experimental study into the rheological behaviour of Smart Dynamic Concrete (SDC). The investigation is aimed at quantifying the effect of the varying amount of mineral admixtures on the rheology, setting time and compressive strength of SDC containing natural sand and crushed sand. Ordinary Portland cement (OPC) in conjunction with the mineral admixtures was used in different replacement ratio keeping the mix paste volume (35%) and water binder ratio (0.4) constant at controlled laboratory atmospheric temperature ($33^{\circ}C$ to $35^{\circ}C$). The results show that the properties and amount of fine aggregate have a strong influence on the admixture demand for similar initial workability, i.e., flow. The large amounts of fines and lower value of fineness modulus (FM) of natural sand primarily increases the yield stress of the SDC. The mineral admixtures at various replacement ratios strongly contribute to the yield stress and plastic viscosity of SDC due to inter particle friction and cohesion.