• Title/Summary/Keyword: Pt Thin Films

Search Result 829, Processing Time 0.031 seconds

Control of Grain Size of PZT Thin Film through Seed Layers (Seed Layer를 통한 PZT 박막의 결정립 크기 조절)

  • Kim, Tae-Ho;Kim, Ji-Young;Lee, In-Sup
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.05b
    • /
    • pp.273-278
    • /
    • 2000
  • In order to study effects of interface layers between PZT films and electrodes for MFM(Metal-Ferroelectric-Metal) structure capacitors, we have fabricated the capacitors with the Pt/PZT/interface-layer/Pt/$TiO_2/SiO_2/Si$ structure. $PT(PbTiO_3)$ interface layers were formed by sol-gel deposition and PbO, $ZrO_2$ and $TiO_2$ thin layers were deposited by reactive sputtering. $TiO_2$ interface layers result in the finest grains of PZT films compared to $PbO_2$ and $ZrO_2$ layers. On the other hand, PT interface layers result in improved morphology of PZT films and do not significantly change ferroelectric properties. It is also observed that seed layers at the middle and top of PZT films do not give significant effects on grain size but the PT seed layer at the interface between the bottom electrode and the PZT films results in the small grain size.

  • PDF

Electrical Properties of SCT Ceramic Thin Film with Top Electrode (상부전극에 따른 SCT 세라믹 박막의 전기적 특성)

  • Cho, C.N.;Kim, J.S.;Shin, C.G.;Choi, W.S.;Kim, C.H.;Park, Y.P.;Yoo, Y.G.;Lee, J.U.
    • Proceedings of the KIEE Conference
    • /
    • 1999.07d
    • /
    • pp.1501-1503
    • /
    • 1999
  • The $(Sr_{0.85}Ca_{0.15})TiO_3$(SCT) thin films are deposited on Pt-coated electrode$(Pt/TiO_2/SiO_2/Si)$ using RF sputtering method. Ag, Cu, Al, Pt films for the formation of top eletrode were doposited on SCT thin films by thermal evaporator and sputtering. The effects of top electodes have be studied on SCT samples with a variety of top electrode materials.

  • PDF

$SnO_2$-based thin film gas sensors in array for recognizing inflammable gases (가연성 가스 인식을 위한 $SnO_2$계열의 박막 가스센서)

  • 이대식;심창현;이덕동
    • Journal of the Korean Vacuum Society
    • /
    • v.10 no.3
    • /
    • pp.289-297
    • /
    • 2001
  • Highly-porous $SnO_2$thin films were prepared for recognizing and detecting of the inflammable gases, like butane, propane, LPG, carbon monoxide. To obtain sensing films, Sn, Pt/Sn, Au/Sn, and Pt,Au/Sn films were deposited employing a thermal evaporator for Sn film and a sputter for novel metals of Pt or/and Au. These films were annealed for 2 h at $700^{\circ}C$ to form $SnO_2$-based thin films. The films showed the tetragonal structure and also exhibited many defects and porosity, which could give high sensitivity to thin films. The thin films showed high sensitivity and reproductivity to the tested gases(butane, propane, LPG, and carbon monoxide) to even to low gas concentrations in range of workplace environmental standards. Especially, Pt/$SnO_2$film showed the highest sensitivity to butane, LPG, and carbon monoxide. And pure $SnO_2$ film manifested the highest sensitivity to propane. By using the sensing patterns from the films, we could reliably recognize the kinds and the quantities of the tested inflammable gases within the range of the threshold limit values(TLV) and the lower explosion limit(LEL) through the principal component analysis(PCA).

  • PDF

ZnO thin film Gas sensors for detection of TMA gas with Pt/Ti thin film heater (Pt/Ti 발열체가 내장된 TMA 가스 측정용 ZnO 박막 가스 센서)

  • 류지열;박성현;최혁환;권태하
    • Journal of the Korean Institute of Telematics and Electronics A
    • /
    • v.33A no.6
    • /
    • pp.127-135
    • /
    • 1996
  • To increase the sensitivity and the selectivity of the sensors to TMA gas, the composition ratio and the growth conditions of the ZnO films are studied. Annealing of the ZnO films in the various time ranges and temperatures in the oxygen is carried out to enhance the stbility of the electrical resistance. Pt/Ti heater deposited on backside of the substrates in used to control the operating temperature of th esensor. The ZnO thin film sensors doped to 4.0 wt% $Al_{2}$O$_{3}$ 1.0wt.% TiO$_{2}$ and 0.2wt.% V$_{2}$O$_{5}$ exhibited a high sensitivity and an excellent selectivity for TMA gas. The sensors made with the thin films annealed at 700$^{\circ}$C for 60 minutes in the oxygen atmosphere had a good stability and linearity. The heater deposited in the ratio of 1 to 1 (Pt:Ti) had a good heating properties. The sensors fabricated using above conditions showed a good response to the actual gases of a mackerel at a step of deterioration after death.

  • PDF

The Influence of $O_2$ Gas on the Etch Characteristics of FePt Thin Films in $CH_4/O_2/Ar$ gas

  • Lee, Il-Hoon;Lee, Tea-Young;Chung, Chee-Won
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.02a
    • /
    • pp.408-408
    • /
    • 2012
  • It is well known that magnetic random access memory (MRAM) is nonvolatile memory devices using ferromagnetic materials. MRAM has the merits such as fast access time, unlimited read/write endurance and nonvolatility. Although DRAM has many advantages containing high storage density, fast access time and low power consumption, it becomes volatile when the power is turned off. Owing to the attractive advantages of MRAM, MRAM is being spotlighted as an alternative device in the future. MRAM consists of magnetic tunnel junction (MTJ) stack and complementary metal- oxide semiconductor (CMOS). MTJ stacks are composed of various magnetic materials. FePt thin films are used as a pinned layer of MTJ stack. Up to date, an inductively coupled plasma reactive ion etching (ICPRIE) method of MTJ stacks showed better results in terms of etch rate and etch profile than any other methods such as ion milling, chemical assisted ion etching (CAIE), reactive ion etching (RIE). In order to improve etch profiles without redepositon, a better etching process of MTJ stack needs to be developed by using different etch gases and etch parameters. In this research, influences of $O_2$ gas on the etching characteristics of FePt thin films were investigated. FePt thin films were etched using ICPRIE in $CH_4/O_2/Ar$ gas mix. The etch rate and the etch selectivity were investigated in various $O_2$ concentrations. The etch profiles were studied in varying etch parameters such as coil rf power, dc-bias voltage, and gas pressure. TiN was employed as a hard mask. For observation etch profiles, field emission scanning electron microscopy (FESEM) was used.

  • PDF

Growth and characterization of Eu-doped bismuth titanate (BET) thin films deposited by sol-gel method

  • Kang Dong-Kyun;Kim Byong-Ho
    • Proceedings of the Korean Society Of Semiconductor Equipment Technology
    • /
    • 2006.05a
    • /
    • pp.194-197
    • /
    • 2006
  • Lead-free bismuth-layered perovskite ferroelectric europium-substituted $Bi_{4}Ti_{3}O_{12}(BTO)$ thin films have been successfully deposited on Pt/Ti/$SiO_2$/Si substrate by a sol-gel spin-coating process. $Bi(TMHD)_3,\;Eu(THMD)_3,\;Ti(OiPr)_4$ were used as the precursors, which were dissolved in 2-methoxyethanol. The thin films were annealed at various temperatures from $600^{\circ}\;to\;720^{\circ}C$ in oxygen ambient for 1 hr, which was followed by post-annealed for 1 hr after depositing a Pt electrode to enhance the electrical properties. X-ray diffraction (XRD) and scanning electron microscopy (SEM) were used to analyze the crystallinity and surface morphology of layered perovskite phase, respectively. The remanent polarization value of the BET thin films annealed at $720^{\circ}C\;was\;25.95{\mu}C/cm^2$ at an applied voltage of 5 V.

  • PDF

Fabrication and Properties of SGT thin film by RF Magnetron Sputtering Method (RF 마그네트론 스펴터링법에 의한 SCT 박막의 제초 및 특성)

  • 김진사;백봉현;김충혁;최운식;박용필;박건호;이준웅
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1998.06a
    • /
    • pp.325-329
    • /
    • 1998
  • In this paper, the (Sr$_{1-x}$ Ca$_{x}$)TiO$_3$(SCT) thin films were deposited at various substrate temperature using RF magnetron sputtering method on optimized Pt-coated electrodes (Pt/TiN/SiO$_2$/Si). An influence of substrate temperature and annealing temperature on the structural and dielectric properties are investigated. The substrate temperature changed from 100[$^{\circ}C$] to 500[$^{\circ}C$] and crystalline SCT thin films were deposited abode 400[$^{\circ}C$]. All thin films had (111) preferred orientation, the (100) oriented films were obtained at the substrate temperature above 400[$^{\circ}C$]. The dielectric constant changes almost linearly in the temperature region of -80~+90[$^{\circ}C$], the temperature characteristics of the dielectric loss exhibited a stable value within 0.1, then not affected by substitutional contents. The capacitance characteristics appears a stable value within $\pm$5[%].

  • PDF

Crystallization of FePt/MgO(100) magnetic thin films (FePt/MgO(100) 자성박막의 결정화 연구)

  • Jeung, Ji-Wook;Cho, Tae-Sik;Yi, Min-Soo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.278-279
    • /
    • 2005
  • The crystallization of FePt/MgO(100) magnetic thin films of various thicknesses has been studied using synchrotron x-ray scattering, atomic force microscope, and vibrating sample magnetometer. In film with a 500-${\AA}$-thick, ordered (fct) FePt phase was dominantly crystallized into perpendicular (001) grains keeping the magnetically easy c-axis normal to the film plane during annealing. In film with a 812-${\AA}$-thick, however, longitudinal (110) grains keeping the c-axis parallel to the film plane were grown on top of the perpendicular (001) grains. The behavior of the magnetic properties was consistent with the thickness dependence of the crystallization. We attribute the thickness dependence of the crystallization to the substrate effect, which prefers the growth of the c-axis oriented perpendicular grains near the film/substrate interfacial area.

  • PDF

Effect of $LaNiO_3$ electrodes on Structural and Ferroelectric Proerties of $Bi_{3.25}Eu_{0.75}Ti_3O_{12}$ Thin films ($Bi_{3.25}Eu_{0.75}Ti_3O_{12}$ 박막의 구조 및 강유전 특성에 미치는 $LaNiO_3$전극의 영향)

  • Kim, K.T.;Kim, C.I.;Lee, C.I.;Kim, T.A.
    • Proceedings of the KIEE Conference
    • /
    • 2004.11a
    • /
    • pp.75-78
    • /
    • 2004
  • $Bi_{3.25}Eu_{0.75}Ti_3O_{12}$ (BET) thin films were deposited on the $LaNiO_3$ (LNO (100))/Si and Pt/Ti/$SiO_2$/Si substrates by the metal-organic decomposition method. Structural and dielectric properties of BLT thin films for the applications in nonvolatile ferroelectric random access memories were investigated. Both the structure and morphology of the films were analyzed by x-ray diffraction (XRD) and atomic force microscope (AFM). Even at low temperatures $650^{\circ}C$, the BET thinfilms were successfully deposited on LNO bottom electrode and exhibited (001) and (117) orientation. Compared with the Pt electrode films, the BET thin films on the LNO electrode annealed at $650^{\circ}C$ showed better dielectric constantsand remanent polarization. The BET thin films on the LNO electrode for the annealing temperature of $650^{\circ}C$, the remanent polarization Pr and coercive field were $45.6\;C/cm^2$ and 171 kV/cm, respectively.

  • PDF