Fabrication of Metal-Semiconductor Interface in Porous Silicon and Its Photoelectrochemical Hydrogen Production

  • Oh, Il-Whan;Kye, Joo-Hong;Hwang, Seong-Pil
    • Bulletin of the Korean Chemical Society
    • /
    • 제32권12호
    • /
    • pp.4392-4396
    • /
    • 2011
  • Porous silicon with a complex network of nanopores is utilized for photoelectrochemical energy conversion. A novel electroless Pt deposition onto porous silicon is investigated in the context of photoelectrochemical hydrogen generation. The electroless Pt deposition is shown to improve the characteristics of the PS photoelectrode toward photoelectrochemical $H^+$ reduction, though excessive Pt deposition leads to decrease of photocurrent. Furthermore, it is found that a thin layer (< 10 ${\mu}m$) of porous silicon can serve as anti-reflection layer for the underlying Si substrate, improving photocurrent by reducing photon reflection at the Si/liquid interface. However, as the thickness of the porous silicon increases, the surface recombination on the dramatically increased interface area of the porous silicon begins to dominate, diminishing the photocurrent.

수전해·연료전지 가역셀에서 이중 가스 확산층의 효과 (Effect of Double Porous Layer on a Polymer Electrolyte Unitized Regenerative Fuel Cell)

  • 황철민;박대흠;정영관;김경훈;김종수
    • 한국수소및신에너지학회논문집
    • /
    • 제24권4호
    • /
    • pp.320-325
    • /
    • 2013
  • TUnitized reversible fuel cells (URFC) combine the functionality of a fuel cell and electrolyzer in one unitized device. For a URFC with proton exchange membrane, a titanium (Ti)-felt is applied to the gas diffusion layer (GDL) substrate at the oxygen electrode, and additionally titanium (Ti)-powders and TiN-powders are loaded in the GDL substrate as a micro porous layer (MPL). Double porous layer with TiN MPL was not acceptable for the URFC because both of fuel cell performance and electrolysis performance are degraded. The double porous layer with Ti-powder loading in the Ti-felt substrate influence rearly for the electrolysis performance. In contrast, the change of pore-size distribution brings a significant improvement of fuel cell performance under fully humidification conditions. This fact indicates that the hydrophobic meso-pores in the GDL play an important role for mass transport.

Boussinesq 방정식을 사용하여 투수방파제의 월파 수치해석 (Numerical Simulation of Wave Overtopping on a Porous Breakwater Using Boussinesq Equations)

  • 휜탄트;이창훈;안석진
    • 한국해안·해양공학회논문집
    • /
    • 제29권6호
    • /
    • pp.326-334
    • /
    • 2017
  • 1개층 Boussinesq 방정식과 2개층 Boussinesq 방정식을 사용하여 투수방파제를 지나는 파랑의 월파고를 구하였다. 1개층 Boussinesq 방정식으로 Lee 등(2014)이 유도한 식을 사용하였고, 2개층 Boussinesq 방정식은 Cruz 등(1997)의 방법을 따라서 유도하였다. 수치실험을 통해 천단고가 낮은 투수방파제를 지나는 고립파의 월파고(Navier-Stokes 방정식으로 구함)가 천단고가 높은 투수방파제를 지나는 통과파고(1개층 Boussinesq 방정식으로 구함)보다 더 작고, 천단고가 해저에 있는 투수방파제를 지나는 통과파고(2개층 Boussinesq 방정식으로 구함)보다 더 크다는 것을 확인하였다. 고립파의 파고가 낮을수록 또는 투수방파제의 폭이 좁을수록 1개층 및 2개층 Boussinesq 방정식으로 구한 통과파고가 Navier-Stokes 방정식으로 구한 월파고에 근접한 것을 확인하였다.

NH3-Air-C3H8 분위기에서 Nitrocarburisng시 형성된 Compound Layer의 조직제어 (Structural Control of the Compound Layers formed during Nitrocarburising in NH3-Air-C3H8 Atmospheres)

  • 김영희;최광웅
    • 열처리공학회지
    • /
    • 제8권4호
    • /
    • pp.289-301
    • /
    • 1995
  • The effect of Air/$C_3H_8$ gas addition on the compound layer growth of steels nitrocarburised in $NH_3+Air+C_3H_8$ mixed gas atmospheres was investigated. It is considered that amount of residual $NH_3$ was varied according to alternation of Air/$C_3H_8$ mixing ratio and volume content. The compound layer formed from nitrocarburising was composed of ${\varepsilon}-Fe_{2-3}$(C, N) and ${\gamma}^{\prime}-Fe_4$(C, N). According as Air/$C_3H_8$ mixing ratio increased, the superficial content of ${\gamma}^{\prime}-Fe_4$(C, N) within the compound layer was increased, at the same time the growth rate of compound layer and porous layer was increased. In the case of alloy steel at the fixed gas composition, the growth rate of compound layer and porous layer was worse than carbon steel and compound layer phase composition structure primarily consisted of E phase. As the carbon content of materials was increasing in the given gas atmospheres, the growth rate of compound layer and porous layer was increased and the superficial content of ${\varepsilon}-Fe_{2-3}$(C, N) within the compound layer was increased.

  • PDF

방풍펜스가 후방에 놓인 야적모래입자의 비산에 미치는 영향에 관한 연구 (Shelter Effect of Porous Fences on the Saltation of Sand Particles in an Atmospheric Boundary Layer)

  • 박기철;이상준
    • 대한기계학회논문집B
    • /
    • 제24권9호
    • /
    • pp.1175-1184
    • /
    • 2000
  • Effects of porous wind fences on the wind erosion of particles from a triangular sand pile were investigated experimentally. The porous fence and sand pile were installed in a simulated atmospheric boundary layer. The mean velocity and turbulent intensity profiles measured at the sand pile location were well fitted to the atmospheric boundary layer over the open terrain. Flow visualization was carried out to investigate the motion of windblown sand particles qualitatively. In addition, the threshold velocity were measured using a light sensitive video camera with varying the particle size, fence porosity $\varepsilon$ and the height of sand pile. As a result, various types of particle motion were observed according to the fence porosity. The porous wind fence having porosity $\varepsilon$=30% was revealed to have the maximum threshold velocity, indicating good shelter effect for abating windblown dust particles. With increasing the sand particle diamter, the threshold velocity was also increased. When the height of sand pile is lower than the fence height, threshold velocity is enhanced.

유리연마슬러지를 사용한 다공성 소재의 미세구조 및 물리적 특성에 관한 연구 (Microstructure and Physical Properties of Porous Material Fabricated from a Glass Abrasive Sludge)

  • 추용식;권춘우;이종규;심광보
    • 한국세라믹학회지
    • /
    • 제43권5호
    • /
    • pp.277-283
    • /
    • 2006
  • A porous material with a surface layer was fabricated from glass abrasive sludge and expanding agents. The glass abrasive sludges were mixed with expanding agents and compacted into precursors. These precursors were sintered in the range of $700-900^{\circ}C$ for 20 min. The sintered porous materials had a surface layer with smaller pores and inner parts with larger pores. The surface layer and closed pores controlled water absorption. As the expanding agent fraction and the sintering temperature increased, the porosity and pore size increased. The porous materials with $Fe_2O_3$ and graphite as the expanding agents had a low absorption ratio of about 3% or lower while the porous material with $CaCO_3$ as the expanding agent had a higher absorption ratio and more open pores.

Synthesis of TCO-free Dye-sensitized Solar Cells with Nanoporous Ti Electrodes Using RF Magnetron Sputtering Technology

  • Kim, Doo-Hwan;Heo, Jong-Hyun;Kwak, Dong-Joo;Sung, Youl-Moon
    • Journal of Electrical Engineering and Technology
    • /
    • 제5권1호
    • /
    • pp.146-150
    • /
    • 2010
  • A new type of dye-sensitized solar cell (DSC) based on a porous type Ti electrode without using a transparent conductive oxide (TCO) layer is fabricated for low-cost high-efficient solar cell application. The TCO-free DSC is composed of a glass substrate/dye-sensitized $TiO_2$ nanoparticle/porous Ti layer/electrolyte/Pt sputtered counter electrode. The porous Ti electrode (~350 nm thickness) with high conductivity can collect electrons from the $TiO_2$ layer and allows the ionic diffusion of $I^-/I_3{^-}$ through the hole. The vacuum annealing treatment is important with respect to the interfacial necking between the metal Ti and porous $TiO_2$ layer. The efficiency of the prepared TCO-free DSC sample is about 3.5% (ff: 0.48, $V_{oc}$: 0.64V, $J_{sc}$: 11.14 mA/$cm^2$).

초기 산화 피막의 형성이 다공성 알루미나 막 제작에 미치는 영향 (Effect of the Formation of an Initial Oxide Layer on the Fabrication of the Porous Aluminium Oxide)

  • 박영옥;김철성;고태준
    • 한국자기학회지
    • /
    • 제18권2호
    • /
    • pp.79-83
    • /
    • 2008
  • 본 논문에서는 초기 산화 피막의 형성이 전기화학적 방법을 이용한 다공성 알루미나 막 제작에 미치는 영향을 살펴보았다. 다공성 알루미나 막의 제작은 전해 연마된 알루미늄 포일을 사용하여 두 치체의 양극산화 과정을 통해 이루어졌으며 양극산화 시초기 산화 피막이 알루미나 막 표면의 기공구조형성에 미치는 영향을 알아보고자 일차 양극산화 전 1 V의 낮은 전압으로 약 10nm두께의 산화 피막을 형성하였다. 이후 옥살산 용액 안에서 40V의 전압으로 양극산화 과정을 수행한 결과 양극산화 반응은 매우 안정적이었으며 측정된 양극산화 전류 역시 일정하게 유지됨을 알 수 있었다. 이와 달리 초기 산화 피막이 형성되지 않았을 경우 양극산화 과정은 매우 불안정하였으며 양극산화 과정동안 전류가 계속적으로 증가함을 보였다. 이러한 결과를 통해 알루미늄 포일 표면에 초기 산화 피막을 형성함으로써 전기장의 불균일한 분포에 의해 발생하는 표면 손상을 방지하며 안정적인 양극산화 과정을 통해 다공성 알루미나 산화 막을 제작할 수 있음을 확인하였다.

양극산화와 나노 다이아몬드 분말 봉공처리에 의한 마그네슘의 경도와 부식에 관한 연구 (Study on Hardness and Corrosion Resistance of Magnesium by Anodizing and Sealing Treatment With Nano-diamond Powder)

  • 강수영;이대원
    • 한국분말재료학회지
    • /
    • 제21권4호
    • /
    • pp.260-265
    • /
    • 2014
  • In this study, in order to increase surface ability of hardness and corrosion of magnesium alloy, anodizing and sealing with nano-diamond powder was conducted. A porous oxide layer on the magnesium alloy was successfully made at $85^{\circ}C$ through anodizing. It was found to be significantly more difficult to make a porous oxide layer in the magnesium alloy compared to an aluminum alloy. The oxide layer made below $73^{\circ}C$ by anodizing had no porous layer. The electrolyte used in this study is DOW 17 solution. The surface morphology of the magnesium oxide layer was investigated by a scanning electron microscope. The pores made by anodizing were sealed by water and aqueous nano-diamond powder respectively. The hardness and corrosion resistance of the magnesium alloy was increased by the anodizing and sealing treatment with nano-diamond powder.

양극산화에 의한 다공성 알루미나 막의 기체투과 특성 (Gas Permeation Characteristics of Porous Alumina Membrane Prepared by Anodic Oxidation)

  • 함영민
    • 환경위생공학
    • /
    • 제13권3호
    • /
    • pp.72-78
    • /
    • 1998
  • For investigation into gas permeation characteristics, the porous alumina membrane with asymmetrical structure, having upper layer with 10 nanometer under of pore diameter and lower layer with 36 nanometer of pore diameter, was prepared by anodic oxidation using DC power supply of constant current mode in an aqueous solution of sulfuric acid. The aluminium plate was pre-treated with thermal oxidation, chemical polishing and electrochemical polishing before anodic oxidation. Because the pore size depended upon the electrolyte, electrolyte concentration, temperature, current density, and so on, the the membranes were prepared by controling the current density, as a very low current density for upper layer of membrane and a high current density for lower layer of membrane. By control of current quantity, the thicknesses of upper layer of membranes were about $6{\;}{\mu}m$ and the total thicknesses of membranes were about $80-90{\;}{\mu}m$. We found that the mechanism of gas permeation depended on model of the Knudsen flow for the membrane prepared at each condition.