• 제목/요약/키워드: PolyEtherKetoneKetone

검색결과 58건 처리시간 0.024초

Shear bond strength of composite resin to high performance polymer PEKK according to surface treatments and bonding materials

  • Lee, Ki-Sun;Shin, Myoung-Sik;Lee, Jeong-Yol;Ryu, Jae-Jun;Shin, Sang-Wan
    • The Journal of Advanced Prosthodontics
    • /
    • 제9권5호
    • /
    • pp.350-357
    • /
    • 2017
  • PURPOSE. The object of the present study was to evaluate the shear bonding strength of composite to PEKK by applying several methods of surface treatment associated with various bonding materials. MATERIALS AND METHODS. One hundred and fifty PEKK specimens were assigned randomly to fifteen groups (n = 10) with the combination of three different surface treatments (95% sulfuric acid etching, airborne abrasion with $50{\mu}m$ alumina, and airborne abrasion with $110{\mu}m$ silica-coating alumina) and five different bonding materials (Luxatemp Glaze & Bond, Visio.link, All-Bond Universal, Single Bond Universal, and Monobond Plus with Heliobond). After surface treatment, surface roughness and contact angles were examined. Topography modifications after surface treatment were assessed with scanning electron microscopy. Resin composite was mounted on each specimen and then subjected to shear bond strength (SBS) test. SBS data were analyzed statistically using two-way ANOVA, and post-hoc Tukey's test (P<.05). RESULTS. Regardless of bonding materials, mechanical surface treatment groups yielded significantly higher shear bonding strength values than chemical surface treatment groups. Unlike other adhesives, MDP and silane containing self-etching universal adhesive (Single Bond Universal) showed an effective shear bonding strength regardless of surface treatment method. CONCLUSION. Mechanical surface treatment behaves better in terms of PEKK bonding. In addition, self-etching universal adhesive (Single Bond Universal) can be an alternative bonding material to PEKK irrespective of surface treatment method.

Poly-ether-ketone-ketone (PEKK) 포스트로 수복한 근관 치료 치아의 정적 파절 저항성 및 파절 형태에 관한 평가 (Evaluation of static fracture resistances and patterns of pulpless tooth restored with poly-ether-ketone-ketone (PEKK) post)

  • 박하은;이철원;이원섭;양성은;이수영
    • 대한치과보철학회지
    • /
    • 제57권2호
    • /
    • pp.127-133
    • /
    • 2019
  • 목적: 본 연구의 목적은 주조 금속 포스트, 기성 섬유강화형 포스트 그리고 치과영역에서 새롭게 주목 받고 있는 재료인 polyetherketoneketone(PEKK)으로 제작한 포스트로 수복된 근관 치료 치아의 파절 강도 및 파절 양상에 대해 조사하는 것이다. 재료 및 방법: 총 21개의 하악 소구치를 포스트 재료에 따라 각각 7개씩 3개의 군으로 무작위로 분류하였다. 그룹 A는 주조 금속 포스트 코어; 그룹 B는 기성 섬유강화형 포스트 및 레진 코어; 그룹 C는 밀링된 PEKK 포스트 코어로 수복하였다. 모든 시편은 금속관으로 수복하였다. 각각의 시편들을 제작 후 만능 시험기를 사용하여 2 mm/min 속도로 치아 장축에 대해 135도의 정적 하중을 가하여 파절 강도를 측정하고, 파절 양상에 대해 조사하였다. 결과 분석은 유의수준 ${\alpha}=.05$에서 Kruskal-Wallis test 후 사후검정으로 Mann-Whitney U test를 시행하였다. 결과: PEKK 포스트 파절 강도는 주조 금속 포스트와 기성 섬유강화형 포스트에 비해 낮은 값을 보였다. 파절양상에 있어서는 육안과 현미경, 방사선 사진을 통해 살펴본 결과 금속 포스트 코어에서는 치근파절의 양상이 대부분 나타난 반면 기성 섬유 강화형포스트는 포스트의 탈락이 주로 발생하였다. PEKK 포스트 코어의 경우 치아와 포스트가 함께 파절되는 양상이 주로 나타났다. 결론: 치관부 치질이 심하게 손상된 치아 수복 시 적절한 재료의 선택이 필요하며, PEKK 포스트의 임상적 적용을 위해서는 강도 향상에 대한 연구가 더 필요할 것으로 보인다.

새로운 Hyperbranchedpolyimidesandpolyamides: 합성, 말단기 변형, 경화 연구, 그리고 물리적 성질 (New Hyperbranched Polyimides and Polyamides: Synthesis, Chain-End Functionalizations, Curing Studies, and Some Physical Properties)

  • Baek, Jong-Beom;Chris B. Lyon;Tan, Loon-Seng
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2003년도 추계학술발표대회 논문집
    • /
    • pp.1-2
    • /
    • 2003
  • While aromatic polyimides and polyamides have found widespread use as high performance polymers, the present work addressed the need for organosoluble materials through the use of a hyperbranching scheme. The $AB_2$ monomers were prepared. The $AB_2$ monomers were then polymerized via aromatic fluoride-displacement and Yamazaki reactions to afford the corresponding hydroxyl-terminated hyperbranched polyimides (HT-PAEKI) and amine-terminated hyperbranched polyamides, respectively. HT-FAEKI was then functionalized with allyl and propargyl bromides as well as epichlorohydrin to afford allyl-terminated AT-PAEKI, propargyl-terminated PT-PAEKI, and epoxy (glycidyl)-terminated ET-PAEKI, in that order. All hyperbranched poly(ether-ketone-imide)s were soluble in common organic solvents. AT-PAEKI was blended with a bisphenol-A-based bismaleimide (BFA-BMI) in various weight ratios. Thermal, rheological, and mechanical properties of these blend systems were evaluated. Two characteristic hyperbranched polyamides, which the one has para-electron donating groups to the surface amine groups and the other has para-electron withdrawing groups to the surface amine groups, were selected to compare BMI curing behaviors. The electron rich polymer displayed ordinary Michael addition type exothermic reaction, while electron deficient polymer did display unusual curing behaviors. Based on analytical data, the later system provided the strong evidences to support room temperature curing of BMI by reactive intermediates instead of reactive primary amine groups on the macromolecule surface.

  • PDF

고분자 전해질 연료전지용 SPEEK 막의 어닐링에 의한 화학적 내구성 향상 (Increased Chemical Durability by Annealing of SPEEK Membrane for Polymer Electrolyte Fuel Cells)

  • 이미화;유동근;이혜리;나일채;박권필
    • 한국수소및신에너지학회논문집
    • /
    • 제34권6호
    • /
    • pp.673-681
    • /
    • 2023
  • Hydrocarbon-based polymer membranes to replace perfluorinated polymer membranes are being continuously researched. However, hydrocarbon-based membranes have a problem in that they are less durable than fluorine-based membranes. In this study, we sought to compare the annealing effect to improve the durability of sulfonated poly(ether ether ketone) (SPEEK). After membranes formation, thermogravimetric analysis and tensile strength were measured to compare changes in membranes properties due to annealing. After manufacturing the membrane and electrode assembly (MEA), the initial performance and chemical durability was compared with unit cell operation. During the 24-hour annealing process, the strength increased due to the increase in-S-O-S-crosslinking, and the sulfonic acid group decreased, leading to a decrease in I-V performance. By annealing, the hydrogen permeability was reduced to less than 1/10 of that of the nafion membrane, and as a result, open circuit voltage (OCV) and durability was improved. The SPEEK membranes annealed for 24 hours showed higher durability than the nafion 211 membranes of the same thickness.

DAAQ와 SPEEK를 이용한 전고상 슈퍼커패시터의 전기화학적 특성 (Electrochemical Characteristics of all solid supercapacitor based on DAAQ(1,5-diaminoanthraquinone) and SPEEK(sulfonated polyether ether ketone))

  • 김진용;김홍일;김한주;박수길
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.371-372
    • /
    • 2005
  • Supercapacitors are promising devices for delivering high power density. Digital communications, electric vehicles and other devices that require electrical energy at high power levels in relatively short pulses have prompted considerable research on supercapacitors. In recent years, solid electrolytes have been investigated for supercapacitors. Solid electrolytes are advantageous over liquid electrolytes in respect of easy handling and reliability without electrolyte leakage. In this preliminary study, an electrochemical supercapacitor in all solid configuration has been fabricated using CNF-DAAQ and poly-vinylidenefluoride(PVdF). A new type of Supercapacitor was constructed by using carbon nanofibers(CNFs) and DAAQ(l,5-diaminoanthraquinone) monomer. DAAQ was deposited on the carbon nanofibers by chemical polymerization with $(NH_4)_2S_2O_8$ as oxidant in the 0.1M $H_2SO_4$. Dried SPEEK powder was mixed with N-methyl pyrrolidone to make 10 wt.% solution in an ultrasonic bath, the slurry was cast over a glass substrate heated to $70^{\circ}C$ for solvent evaporation. And then we used solid electrolyte of SPEEK. The unit cell consist of DAAQ-CNF/electrolyte/Pt. From the analysis, it is clear that surface of carbon nanofibers was quite uniformly coated with DAAQ. The performance characteristics of the supercapacitors have been evaluated using Cyclic Voltammetry.

  • PDF

열가소성 방향족 폴리머의 결정화 특성에 대한 연구 (A Study on Crystallization of Thermoplastic Aromatic Polymer)

  • 박동철;박창욱;신도훈;김윤해
    • Composites Research
    • /
    • 제31권2호
    • /
    • pp.63-68
    • /
    • 2018
  • 열가소성 복합재료는 다양한 장점에도 불구하고 기계적 특성이 낮아 고성능 항공산업 분야에서는 제한적으로 사용되어 왔으나 최근 열가소성 방향족 폴리머 복합재들이 많이 연구/활용되고 있다. 본 연구에서는 대표적인 열가소성 방향족 폴리머인 PEEK와 PPS Neat 수지 필름을 DSC 기기를 이용하여 가열, 냉각 및 재 가열 사이클을 연속적으로 수행하여 유리전이온도 및 용융온도 등의 특성변화를 확인하고 냉각속도에 따른 결정화도(Crystallinity)의 차이를 평가하였다. 1차 가열단계에서 각 폴리머의 용융온도보다 높은 온도에 5분간 유지시켜 이전 열이력을 제거하였고 2차 냉각단계에서 냉각속도를 분당 2, 5, 10, 20 및 $40^{\circ}C$로 조절/적용함으로서 결정화반응을 제어하였으며, 3차 가열단계에서 재가열하여 용융엔탈피를 측정함으로서 결정화도 차이를 확인하였다. 높은 비정질 영역을 가진 시편의 첫 번째 가열시 냉각결정화 현상이 일어나고 뚜렷한 유리상 전이구역을 확인할 수 있었던 반면에 결정질 영역이 증가된 재가열시에는 냉각결정화 현상이 일어나지 않고 상대적으로 유리상 전이구역이 약해지는 것을 확인하였다. 2차 냉각단계에서 냉각속도가 느려짐에 따라 결정화도가 높아졌는데 PEEK의 경우 냉각속도의 차이에 따라 21.9~39.3% 결정화도를 보였으며, PPS는 29.1~31.2% 결정화도 차이를 얻을 수 있었다.

전극 촉매 Pt-Ni 및 Pt-Co를 이용한 수전해용 공유가교 CL-SPEEK/HPA 막전극의 특성 (Characteristics of CL-SPEEK/HPA Membrane Electrodes with Pt-Ni and Pt-Co Electrocatalysts for Water Electrolysis)

  • 우제영;이광문;지봉철;정장훈;문상봉;강안수
    • 한국수소및신에너지학회논문집
    • /
    • 제21권1호
    • /
    • pp.26-34
    • /
    • 2010
  • The electrocatalystic prperties of Pt-Co and Pt-Ni with heteropolyacids (HPAs) entrapped in covalently cross-linked sulfonated poly(ether ether ketone) (CL-SPEEK)/HPA membranes were investigated for water electrolysis. The HP As, including molybdophosphoric acid (MoPA), and tungstophosphoric acid (TPA) were both used as membrane additives and electrocatalysts. The membrane electrode assembly (MEA) was prepared by a nonequilibrium impregnation-reduction (I-R) method. $Pt(NH_3)_4Cl_2$, $NiCl_2$ and $CoCl_2$ as electrocatalytic materials and $NaBH_4$ as reducing agent were used. I order to enhance electrocatalytic activity, the catalyst layer prepared above was electrodeposited (Dep) with HP A. Surface morphologies and physico-chemical properties of MEA were investigated by means of SEM, EDX and XRD. The electrocatalytic properties of composite membranes such as the cell voltage and coulombic charge in CV were in the order of magnitude: CL-SPEEK/MoPA40 (wt%) > CL-SPEEK/TPA30 > Nafion117. In the optimum cell applications for water electrolysis, the cell voltage of Pt/CL-SPEEK-MoPA40/Pt-Co (Dep-MoPA) and Pt/CL-SPEEK-TPA30/Pt-Co (Dep-TPA) was 1.75 Vat $80^{\circ}C$ and $1\;A/cm^2$ and voltage efficiency was 87.1%. Also, the observed activity of Pt-Co (84:16 atomic ratio by EDX) is a little higher than that of Pt-Ni (86: 14). The current density peak of electrodeposited electrodes were better a little than those of unactivated electrodes based on the same membranes.

심한 치조골 소실이 있는 상악 무치악 환자에서 Pekkton telescopic attachment를 이용한 임플란트 피개의치 증례 (A case of maxilla implant overdenture using Pekkton telescopic attachment with severe alveolar bone resorption)

  • 박하은;이원섭;이철원;이수영
    • 대한치과보철학회지
    • /
    • 제57권2호
    • /
    • pp.189-194
    • /
    • 2019
  • 심한 치조골 흡수를 동반한 편악 무치악 환자의 보철 수복시 대합치열의 상태를 고려하여 올바른 교합평면을 설정하고, 교합력이 균일하게 분산될 수 있는 치료가 제공되어야 한다. 임플란트 유지 피개의치는 소수의 임플란트로 치조골 흡수가 심한 완전 무치악 환자에게 총의치보다 우수한 유지와 안정성을 주는 치료이다. 최근 치과 영역에서 소개된 신소재 polyaryletherketone (PAEK) 기반의 폴리머(Pekkton ivory, Cendres + $M{\acute{e}}taux$ SA, Biel / Bienne, Switzerland)를 사용한 telescopic 어태치먼트는 전형적인 telescopic 코핑의 이점을 가지며, 내마모성이 뛰어나며, 기존의 임플란트 피개의치에 비해 가볍고 경제적인 장점이 있다. 본 증례에서는 상악 완전 무치악 환자에 임플란트를 5개 식립하여, Pekkton으로 내 외관이 제작된 텔레스코픽 어태치먼트를 활용한 임플란트 유지 피개의치를 제작하고, 하악은 임플란트 고정성 보철로 수복하였다. 심미적 및 기능적으로 만족스러운 결과를 얻었기에 이를 보고하는 바이다.