• 제목/요약/키워드: Plastic Strain Ratio

검색결과 244건 처리시간 0.033초

이속압연에 의해 제조된 AA1100 판재의 소성변형비 예측 (Prediction of the Macroscopic Plastic Strain Ratio in AA1100 Sheets Manufactured by Differential Speed Rolling)

  • 최재권;조재형;김형욱;강석봉;최시훈
    • 대한금속재료학회지
    • /
    • 제48권7호
    • /
    • pp.605-614
    • /
    • 2010
  • Conventional rolling (symmetric) and differential speed rolling (DSR) were both applied to AA1050 sheets at various velocity ratios, from 1 to 2 between the top and bottom rolls. An electron backscatter diffraction (EBSD) technique was used to measure texture inhomogeneity through the thickness direction. After the annealing process, the annealing texture of the DSR processed sheets was different from that of conventionally rolled sheets. The velocity ratio between the top and bottom rolls affected the texture inhomogeneity and macroscopic plastic strain ratio of the AA1050 sheets. A prediction for the macroscopic plastic strain ratio of AA1050 sheets was carried out using a visco-plastic self-consistent (VPSC) polycrystal model. The strain ratio directionality that was predicted using the VPSC polycrystal model was in good agreement with experimental results.

알루미늄 5182-폴리프로필렌 샌드위치 판재의 소성변형비 및 집합조직의 발달 (Pastic Strain Ratio and Texture Evolution of Aluminum/Polypropylene/Aluminum Sandwich Sheets)

  • 김기주;정효태
    • 한국자동차공학회논문집
    • /
    • 제14권2호
    • /
    • pp.57-66
    • /
    • 2006
  • AA5182-polypropylene sandwich sheet was manufactured, and the mechanical properties evaluation was executed in order to identify $L{\ddot{u}}ders$ band that causes fabrication process problem and especially surface roughness. To identify formability, deformation behavior, plastic strain ratio (R-value) and pole figure were measured, and texture analysis was performed. In the case of sandwich sheet, the unstable deformation behavior has decreased. As well, for sandwich sheet, A1 skin could manage the most of load, and the elongation has improved about 45% more than that of A1 skin. The plastic strain ratio of A1 skin and sandwich panel, which indicates serration behavior, was obtained from instantaneous plastic strain ratio evaluation. Also, the planar anisotropy of sandwich sheet has decreased more than that of A1 skin. According to these results, the sandwich sheet produced lightening effect and could control unstable deformation characteristic, that is, surface roughness caused by $L{\ddot{u}}ders$ band. Furthermore, it was proved that the texture control of the rolling attachment of A1 skin is necessary to improve the formability of the sandwich panel.

강재 기둥-보 구조물의 피로곡선 연구 (Study for Woehler Fatigue Line of Steel Beam-to-Column Structure)

  • 공병승
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2005년도 춘계학술대회 논문집
    • /
    • pp.700-705
    • /
    • 2005
  • This study presents a fatigue line with a plastic rotational angle to a great extent of plastic strain of Low-Cycle-fatigue period, such as earthquake, etc. This fatigue line with a plastic rotational angle is measured and analysed more simply in practice rather than Woehler's fatigue line which is developed in stress variation of the structure. It shows that the slope of fatigue line with a plastic rotational angle is equal to that with plastic strain through the experiments by proving the correlation that the plastic strain ratio is directly proportional to the plastic rotational angle in plastic hinge.

  • PDF

기둥-보 연결 강구조물의 소성회전각에 의한 피로곡선 연구 (A Study on the Fatigue Line with Plastic Rotaional Angle for Steel Structure of the Beam-to-Column Joints)

  • 공병승
    • 한국강구조학회 논문집
    • /
    • 제10권2호통권35호
    • /
    • pp.221-232
    • /
    • 1998
  • 본 연구에서는 지진 등과 같이 소성변형의 범위가 큰 Low-Cycle-Fatigue 범주에서 구조물의 응력변동을 중심으로 사용되는 기존의 피로곡선인 S-N선도 보다 실질적으로 간단하게 측정하여 분석할 수 있는 소성회전각에 의한 피로곡선을 제시하였다. 이는 소성힌지가 생성되는 곳의 소성변형율과 구조물의 소성회전각이 서로 정비례를 이루는 상관관계임을 입증하여, 실험을 통하여 밝혀진 소성변형율의 피로곡선의 기울기와 소성회전각의 기울기가 서로 같은 값을 가짐을 보여 주었다. 이론은 Manson과 Coffin의 변형을 피로곡선을 도입하였고, 실험은 ECCS 주관하에 실시하였으며, 수치해석을 통하여 소성힌지 부위의 위치와 정확한 소성변형율을 산정할 수 있었다.

  • PDF

비대칭 압연 패스 회수에 따른 AA1050 Al 판재의 집합조직과 소성변형비 변화 (Texture and Plastic Strain Ratio Changes with the Number of Passes of Asymmetric Rolling in AA1050 Al Alloy Sheet)

  • 남수권;정해봉;김인수
    • 소성∙가공
    • /
    • 제19권8호
    • /
    • pp.502-507
    • /
    • 2010
  • The physical and mechanical properties and formability of sheet metals depend on preferred crystallographic orientations (texture). In this research work, the texture development and formability (plastic strain ratios) of AA1050 Al alloy sheets after 3 and 10 passes of asymmetric rolling and subsequent heat treatment were investigated. The plastic strain ratios of 10 passes asymmetrically rolled and subsequent heat treated samples are 1.3 times higher than those of the initial AA1050 Al alloy sheets. The ${\Delta}r$ of 10 passes of asymmetrically rolled and subsequent heat treated samples is 1/30 times lower than those of the initial AA1050 Al alloy sheets. The plastic strain ratios of 10 passes of asymmetrically rolled and subsequent heat treated Al sheets are higher than those of 3 passes ones. These results could be attributed to the formation of $\gamma$-fiber, ND//<111>, and the other texture components by means of asymmetric rolling in Al sheets.

강 용접 열영향부 놋치 선단 의 소성 스트레인 평가에 관한 연구 (A Study on Evaluation of Plastic Strain at Notch Tip of Weld HAZ in Steel)

  • 김태영;임재규;정세희
    • Journal of Welding and Joining
    • /
    • 제2권1호
    • /
    • pp.41-48
    • /
    • 1984
  • Recrystallization technique was applied to analyze plastic strain at the notch tip of coarse grain HAZ in mild steel (SB 41) and high strength steel (SA 588). The notch tip of specimen was deformed by three point bending. Accumulated displacement (Crack Opening Displacement ${delta}t$) by the monotonic and cyclic loading under room temperature and hot strain embrittlement temperature ($250^{\circ}C$) was 0~1.0mm. Recrystallization heat treatment conditions were $650^{circ}C{ imes}3hr$ for SB 41 and $700^{circ}C{ imes}3hr$ for SA 588. The experimental results obtained were as follows ; 1) Distribution of the effective plastic strain at plastic zone was appeared by the function of crack opening displacement, and plastic zone or the effective plastic strain increased with crack opening displacement. 2) Plastic strain at notch tip of HAZ due to accumulated hot strain calculated as follows. .epsilon. over bar $_{p}$ = .epsilon. over bar $_{cr}$ (x/ $R_{x}$ ) $^{m}$ (m=0.25) 3) Work hardending ratio of notch tip for hot strain was linearly increased with .epsilon. over bar $_{max}$ and dependent upon the material types.s.

  • PDF

금속판재의 성형성 (Formability of Sheet Metals)

  • 이동녕
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1994년도 박판성형기술의 진보
    • /
    • pp.11-23
    • /
    • 1994
  • Formability of sheet metals can be evaluated using tensile testing. Easily measured tensile properties such as yield strength, tensile strength, elongation, strain hardening exponent, strain rate sensitivity and plastic strain ratio are important parameters to evaluated the sheet formability. This paper briefly explains how these properties are related to deep drawability and stretchability. The plastic anisotropy of sheet metals is usually attributed to the crystallographic texture. However dislocation distribution may influence the anisotropy.

ECAP 한 후 열처리한 알루미늄 AA 1050 합금 판재의 집합조직과 소성변형비 변화 (Plastic Strain Ratio and Texture of the ECAPed and Heat-treated Aluminum AA 1050 Sheet)

  • ;이민구;박병현;김인수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 추계학술대회 논문집
    • /
    • pp.369-372
    • /
    • 2005
  • A study on the microstructure, the texture and the formability of the samples after ECAPed and subsequent heat-treated AA 1050 aluminum alloy sheet have been carried out. The specimens after the ECAP showed a very fine grain size, a decrease of <100> // ND. The <110>// ND textures appears in the specimens after the ECAP and subsequent heat-treatment at $400^{\circ}C$ for 1 hour. One of the most important properties in sheet metals is formability. The r-value or plastic strain ratio has was as a parameter that expressed the formability of sheet metals. The change of the plastic Strain ratios after the ECAP and subsequent heat-treatment conditions were investigated and it was found that they were two times higher than those of the initial Al sheets. This could be attributed to the formation above texture components through the ECAP and subsequent heat-treatment of AA 1050 Aluminum alloy sheet.

  • PDF

ECAP로 심한 전단 소성변형한 후 열처리한 AA 1050 알루미늄 합금 판재의 집합조직과 소성변형비 (Texture and Plastic Strain Ratio of the Severe Shear Deformed with ECAP and Heat-treated AA 1050 Aluminum Alloy Sheet)

  • ;이민구;박병현;김인수
    • 소성∙가공
    • /
    • 제14권6호
    • /
    • pp.553-558
    • /
    • 2005
  • A study on the microstructure, the texture and the formability of the samples after ECAPed and subsequent heat-treated AA 1050 aluminum alloy sheet have been carried out. The specimens after the ECAP showed a very fine grain size, a decrease of <100> // ND, and an increase of <111> // ND textures. The $\{111\}<112>,\;\{123\}<634>,\;\{110\}<001>,\;\{112\}<111>,\;\{110\}<111>,\;and\;\{013\}<231>$ texture components were increased in the specimens after the ECAP and subsequent heat-treatment at $400^{\circ}C$ for 1 hour. One of the most important properties in sheet metals is formability. The r-value or plastic strain ratio has was as a parameter that expressed the formability of sheet metals. The change of the plastic strain ratios after the ECAP and subsequent heat-treatment conditions were investigated and it was found that they were two times higher than those of the initial Al sheets. This could be attributed to the formation above texture components through the ECAP and subsequent heat-treatment of AA 1050 Aluminum alloy sheet.

알루미늄 5182/폴리프로필렌/알루미늄 5182 샌드위치 판재의 소성변형비 및 평면이방성 (Plastic Strain Ratio and Planar Anisotropy of AA5182/Polypropylene/AA5182 Sandwich Sheets)

  • 김기주;정효태
    • 소성∙가공
    • /
    • 제13권4호
    • /
    • pp.365-373
    • /
    • 2004
  • The sheet formability of single AA5182 sheets and sandwich sheets comprising of AA5182/polypropylene/AA5182 (AA/PP/AA) was studied. Rolling without lubrication and subsequent recrystallization annealing led to the formation of favorable {111}//ND fiber textures in AA5182 sheets, which provided a higher plastic strain ratio of $R_m=1.5$. $R_m$ value of 1.58 was obtained in the AA/PP/Ah sandwich sheet sample. Furthermore, a proper combination of the sample direction of the upper and lower skin sheet gave rise to an optimization of the sheet formability of the sandwich sheets.