• Title/Summary/Keyword: PbTiO3

Search Result 1,277, Processing Time 0.03 seconds

A Study on Microstructures and Dielectric Properties in $Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3-BaTiO_3$ Solid Solution ($Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3-BaTiO_3$ 고용체의 미세구조와 유전특성에 관한 연구)

  • Park, Hyun;Lee, Eung-Sang
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.10
    • /
    • pp.1240-1246
    • /
    • 1994
  • While sintering the Pb(Mg1/3Nb2/3)O3-PbTiO3-BaTiO3 system through solid-reaction route, pyrochlore(Pb3Nb4O13) phase while reduces the dielectric constant is inevitably formed. Substitution of Pb(Mg1/3Nb2/3)O3 with PbTiO3 and BaTiO3 can retard the occurrence of pyrochlore phase. The perovskite solid-solution without containing pyrochlore phase can be obtained when we consolidated the materials consisting of PbTiO3 and BaTiO3 at 1200℃ for 2 hours. The sintered body composed of 0.8Pb(Mg1/3Nb2/3)O3-0.1PbTiO3-0.1BaTiO3 composition showed the diffused phase transition(DPT) phenomena and the maximum value of dielectric constant at 0℃ (Tc') with the value of 1.3×104.

  • PDF

Formation of $PbTiO_3$ Thin Films by Thermal Diffusion from Multilayrs (다층 구조로부터 열 확산에 의한 $PbTiO_3$ 박막의 제조)

  • 서도원;최덕균
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.6
    • /
    • pp.510-516
    • /
    • 1993
  • $PbTiO_3$ thin films have been formed by rapid thermal annealing(RTA) of $TiO_2$/Pb/$TiO_2$ multilayer films deposited on Si wafers by RF sputtering. Based on the optimal depositon conditions of TiO2 and Pb, $TiO_2$/Pb/$TiO_2$ three layers were deposited for 900$\AA$ each. These films were subjected to RTA process at the temperatures ranging from $400^{\circ}C$ to $900^{\circ}C$ for 30 seconds in air, and were analyzed by X-ray diffraction and transmission electron microscopy to investigate the phases and the microstructures. As a result, perovskite $PbTiO_3$ phases was obtained above $500^{\circ}C$ with the trace of unreacted $TiO_2$. RBS analysis revealed the anisotropic behavior of diffusion that the diffusivity of Pb to the bottom $TiO_2$ layer was faster than that of Pb to the top $TiO_2$ layer. The amorphous Pb-silicate was formed between film and Si substrate due to the diffusion of Pb, but Pb-silicate existed locally at the interface and the amount of that phase was very small. Therefore the effect of bottom $TiO_2$ layer as a diffusion barrier was confirmed. $PbTiO_3$ films formed by current technique showed a relative dielectric constant of 60, and the maximum breakdown field reached 170kV/cm.

  • PDF

The Effect of PbO on Sintering of Undoped PbTiO3 Ceramics Prepared by Sol-Gel Processing (PbO가 Sol-Gel Process로 제조된 순수 PbTiO3 세라믹스의 소결에 미치는 영향)

  • 김선욱;윤만순;김남흥
    • Journal of the Korean Ceramic Society
    • /
    • v.29 no.5
    • /
    • pp.335-340
    • /
    • 1992
  • Undoped PbTiO3 ceramics was successfully prepared by using sol-gel process, which had not been fabricated due to its microcracks created by anisotropic stress during phase transition from cubic to tetragonal phase. Fabrication of undoped PbTiO3 ceramics via sol-gel processing was very much affected by the PbO content of the samples as well as PbO vapor from sintering atmosphere. Excess PbO was found to promote rapid grain growth in PbTiO3 ceramics. After sintering at 1100$^{\circ}C$ average grain size of PbTiO3 ceramics with excess PbO was about 8 times greater than that of stoichiometric composition, which may be due to PbO liquid phase from excess PbO.

  • PDF

Ferroelectric Phase Transition Behavior in $(Na_{1/2}Bi_{1/2})TiO_3-PbTiO_3$ System ($(Na_{1/2}Bi_{1/2})TiO_3-PbTiO_3$ 고용체의 강유전 상전이 거동)

  • 홍국선;조서용;박승익
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.8
    • /
    • pp.915-921
    • /
    • 1995
  • The morphotropic phase boundary and phase transitions of the solid solutiion system, (1-x)(Na1/2Bi1/2)TiO3-PbTiO3+xPbTiO3 were studied by investigating changes in crystal structure, variations in permittivity with temperature, and calorimetric behavior. It was observed that the morphotropic phase boundary (MPB) of this solid solutiion system was at near 14 mol% of PbTiO3. Compositions containing less than 10mol% PbTiO3 (x<0.1) exhibited a phase transition, i.e. ferroelectric rhombohedrallongrightarrowparaelectric paraelectric cubic, with increasing temperature. Composition containing more than 14 mol% PbTiO3 (x 0.14) showed a phase transition from ferroelectric tetragonal to paraelectric cubic. In the composition range of 0.1$\varepsilon$ (T) curve, which coincided with a phase transition from ferroelectric rhombohedral to an intermediate phase, was also found.

  • PDF

Pyroelectric property of $Pb(Mg_{1/3}Nb_{2/3}O_3-PbTiO_3$ ceramics for pyroelectric sensor application (초전센서 응용을 위한 $Pb(Mg_{1/3}Nb_{2/3}O_3-PbTiO_3$ 세라믹계 초전특성)

  • 황학인;정종만;박준식
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.8 no.4
    • /
    • pp.667-672
    • /
    • 1998
  • Pyroelectric properties of $Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3$ ceramics prepared by the columbite precursor method have been investigated as a function of the sintering temperature in the range of $1000^{\circ}C$ to $1250^{\circ}C$. The $Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3$ ceramics show typical relaxor ferroelectric behavior. The optimum condition for obtaining samples with high densities and improved pyroelectric properties occur at a sintering temperature of $1250^{\circ}C$ and sintering times of 2 hours. The $Pb(Mg_{1/3}Nb_{2/3}O_3-PbTiO_3$ ceramics show the possibility for pyroelectric sensors with pyrostat.

  • PDF

Shaping and Sintering of $Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3$ System powders by Slurry Process (Slurr법에 의한 $Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3$계 미분말의 성형과 소결성)

  • 김복희;최석홍
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.11
    • /
    • pp.1267-1275
    • /
    • 1996
  • Green sheet was prepared by tape casting in the composition of (1-x)Pb(Mg1/3Nb2/3)O3-PbTiO3 system using Pb(Mg1/3Nb2/3)O3 and PbTiO3 synthesized with PbO, Nb2O5 MgO and TiO2 The densest green sheet was obtained in the weight ratio 70:30 of powder to binder. Green sheet wasmultilayered in metal mould and formed into lamination at 7$0^{\circ}C$, 300kg/cm2 The lamination was sintered at 110$0^{\circ}C$ 2hr, Dielectric constant and Curie temperature of disc type sintered body was highered with increasing the amount of PbTiO3 and was in the range of 19000-21000, -7~45$^{\circ}C$ respectively. Green and sintered relative density of lamination was 61% and 95% respectively.

  • PDF

Fabrication of $PbTiO_3$ Thin Film by Chemical Vapor Deposition Technique (화학증착법에 의한 $PbTiO_3$ 박막의 재료)

  • 윤순길;김호기
    • Journal of the Korean Ceramic Society
    • /
    • v.23 no.6
    • /
    • pp.33-36
    • /
    • 1986
  • The $PbTiO_3$is well known materials having remarkable ferroelectric piezoelectric and pyro-electric properties. Thin films of the lead titanite has been successfully fabricated by Chemical Vapor Deposition on the borosilicate glass and titanium substrate. The $PbTiO_3$ thin film deposited on the borosilicate glass using the $PbCl_2$, $TiCl_4$ dry oxygen and wet oxygen at different temperatures (50$0^{\circ}C$-$700^{\circ}C$) grows along the (001) preferred orientation. On the other hand the $PbTiO_3$ thin film deposited on the titanium substrate using the PbO grows along the (101) preferred orientation. Growth orientation of deposited $PbTiO_3$ depends on the reaction species irrespective of substrate materials. Maximum dielectic constant and loss tangent of the $PbTiO_3$ thin film deposited on the titanium substrate are about 90 and 0.02 respectively, . Deposition rates of $PbTiO_3$ deposited on the borosilicate glass and titanium substrate are 10-15 ${\mu}{\textrm}{m}$/hr. Titanium dioxide interlayer formed be-tween $PbTiO_3$ film and titanium substrate material, It improved the adhesion of the film.

  • PDF

Fabrication of Undoped PbTiO3 Ceramics via Sol-Gel Processing (Sol-Gel Processing에 의한 순수 $PbTiO_3$ Ceramics 제조)

  • 김선욱;윤만순;임종인;김성숭;김남흥
    • Journal of the Korean Ceramic Society
    • /
    • v.29 no.3
    • /
    • pp.211-215
    • /
    • 1992
  • Crack free PbTiO3 ceramics were produced by sol-gel processing using alkoxide, which has not been reported to be successful. The PbTiO3 gels were prepared from Ti alkoxide and lead acetate without any dopants. They were calcined at $600^{\circ}C$ and miled to produce fine PbTiO3 powder. It was pressed into discs and they were sintered at 110$0^{\circ}C$ for a few hours. The sintered ceramics were relativley hard and dense as having about 96% of theoretical density of PbTiO3. Fabrication of pure PbTiO3 ceramics by sol-gel processing is possibly due to their small grain size and uniform distribution of residual stress created during cubic-tetragonal transition over large number of small grains in fine grain PbTiO3 ceramics.

  • PDF

Properties of Multilyer Condensor with Composition Change in the System of Pb(Mg1/3Nb2/3)O3-PbTiO3 (Pb(Mg1/3Nb2/3)O3-PbTiO3계의 조성변화에 의한 다층 콘덴서 물성)

  • 김복희
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.2
    • /
    • pp.123-128
    • /
    • 1998
  • Multilayer ceramic capacitors(MLCC) were prepared by laminating the layer of composition with dif-ferent Curie temperature to improve temperature coefficient in the Pb(Mg1/3Nb2/3)O3-PbTiO3 binary system. Green sheet was formed by tape casting using Pb(Mg1/3Nb2/3)O3-PbTiO3 and PbTiO3 synthesized with solid state reaction of PBO. Nb2O5 MgO and TiO2. Green sheet with electrode of 70Ag-30Pd was laminated under 300 kg/cm2 at 70$^{\circ}C$ and sintered at 1100$^{\circ}C$ for 2hr. Curie temperatues for MLCC with 10 layers of pure PMN and 0.9PMN-0.1PT were lowered to -22$^{\circ}C$ and 36$^{\circ}C$ respectively. MLCC with 7 layers of PMN and 3 layers of 0.9PMN-0.1PT showed nearly zero temperature coefficient of capacitance in the range of -20∼30$^{\circ}C$ and sum of dissipation factor of each layer.

  • PDF