Ba치환된 $Pb(Mg_{1/3}Nb_{2/3})O_3$-$PbTiO_3$-$PbZrO_3$계 세라믹스의 압전 및 변위특성에 관한 연구 (Piezoelectric and strain characteristics of PMN-PT-PZ ceramics with Ba addition)

  • 지승한;이덕출;이능헌
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제10권1호
    • /
    • pp.20-25
    • /
    • 1997
  • In this study, piezoelectric actuator samples were fabricated using 0.375PMN-0.37OPT-0.255PZ system ceramics with Barium substitution and the strain properties of them were investigated. Dielectric constant of the specimens increased with the increase of Ba content up to 5mol% and decreased with futher addition of Ba. The largest piezoelectric coefficient and electromechanical coupling coefficient were observed at the sintering temperature of 1250'C and Barium content of 5mol%. The characteristics of strain hysteresis was found largely with varing the sintering temperature on the single round type, and the strain is proportional to piezoelectric coefficient.

  • PDF

Li2O-Bi2O3 첨가가 Pb(Mg1/3Nb2/3)0.65Ti0.35O3 세라믹의 압전 특성에 미치는 영향 (Effect of Li2O-Bi2O3 Addition on the Piezoelectric Properties of Pb(Mg1/3Nb2/3)0.65Ti0.35O3 Ceramics)

  • 김재혁;김시연;최정식;여동훈;신효순;남산
    • 한국분말재료학회지
    • /
    • 제26권5호
    • /
    • pp.405-409
    • /
    • 2019
  • Piezoelectric ceramic specimens with the $Pb(Mg_{1/3}Nb_{2/3})_{0.65}Ti_{0.35}O_3$ (PMN-PT) composition are prepared by the solid state reaction method known as the "columbite precursor" method. Moreover, the effects of the $Li_2O-Bi_2O_3$ additive on the microstructure, crystal structure, and piezoelectric properties of sintered PMN-PT ceramic samples are investigated. The addition of $Li_2O-Bi_2O_3$ lowers the sintering temperature from $1,200^{\circ}C$ to $950^{\circ}C$. Moreover, with the addition of >5 wt.% additive, the crystal structure changes from tetragonal to rhombohedral. Notably, the sample with 3 wt.% additive exhibits excellent piezoelectric properties ($d_{33}=596pC/N$ and Kp = 57%) and a sintered density of $7.92g/cm^3$ after sintering at $950^{\circ}C$. In addition, the sample exhibits a curie temperature of $138.6^{\circ}C$ at 1 kHz. Finally, the compatibility of the sample with a Cu electrode is examined, because the energy-dispersive X-ray spectroscopy data indicate the absence of interdiffusion between Cu and the ceramic material.

CuO 첨가에 따른 0.4Pb$(Mg_{1/3}Nb_{2/3})O_3-0.25PbZrO_3-0.35PbTiO_3$ 세라믹스의 압전특성과 미세조직의 변화 (Effect of CuO Additions on Microstructures and Piezoelectric Properties of the 0.4Pb$(Mg_{1/3}Nb_{2/3})O_3-0.25PbZrO_3-0.35PbTiO_3$ Ceramics)

  • 전소현;김민수;정순종;김인성;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.194-194
    • /
    • 2008
  • Lead oxide based ceramics, represented by PZT, are the most widely used materials for piezoelectric actuators, sensors, and transducers due to their excellent piezoelectric properties. In particular, high-performance multilayered piezoelectric ceramics for advanced electronic components have drawn great attention. In order to develop piezoelectric ceramics capable of being sintered at low temperature for multilayer piezoelectric device applications, the effect of CuO additions on the microstructures and electromechanical properties of the 0.4Pb$(Mg_{1/3}Nb_{2/3})O_3-0.25PbZrO_3-0.35PbTiO_3$ ceramics was investigated. The samples with CuO addition were synthesized by ordinary sintering technique. X-ray diffractions indicated that all samples formed a single phase perovskite structure. The addition of CuO improved the sinterability of the samples and caused an increase in the density and grain size at low temperature. The optimum sintering temperature was lowered by CuO additions. Excellent piezoelectric and electromechanical responses, $d_{33}$ ~ 663 pC/N, $k_p$ ~ 0.72, were obtained for the samples of high density with 0.1 wt% CuO addition sintered at $1050^{\circ}C$ for 4 h in air. These results show that the piezoelectric properties of PMNZT ceramics can be improved by controlling the microstructure and this system is potentially a good candidate as multilayer piezoelectric device for a wide range of electro-mechanical transducer applications.

  • PDF

$\textrm{SrTiO}^3$ 와 과잉 MgO가 첨가된 $\textrm{Pb(Mg_{1/3}Nb_{2/3})O}_3$ - $\textrm{PbTiO}^3$ 계 세라믹스의 유전 및 변위 특성 (Dielectric and Strain Properties of PMN-PT Ceramics Doped with $\textrm{SrTiO}^3$ and excess MgO)

  • 이상훈
    • 전자공학회논문지T
    • /
    • 제36T권3호
    • /
    • pp.7-12
    • /
    • 1999
  • 본 논문은 (1-x-y)PMN-yPT-xST세라믹스의 유전 및 변위특성을 ST의 양에 따라 조사하였다. ST의 성분은 1∼ 6㏖%이내로 변화시켰고 과잉 MgO에 따른 조성변화에 따라 결과를 조사하였다. ST의 성분의 증가에 따라 유전상수는 5㏖%인 조성에서 최대값을 나타내었다. 큐리온도는 ST의 성분이 증가함에 따라 선형적으로 감소하였다. 항전계와 잔류분극은 l㏖%인 조성에서 최대값을 나타내었다. 과잉 MgO의 효과에 따라 유전상수는 0.8PMN-0.12PT-0.04ST조성에서 MgO를 3㏖%까지 과잉 첨가함에 따라 증가하였으나 변위특성은 감소함을 나타내었다.

  • PDF

초음파 전동기용 0.125PMN-0.435PT-0.44PZ 세라믹스의 유전 및 압전특성 (Dielectric and Piezoelectric Properties of 0.125PMN-0.435PT-0.44PZ Ceramics for Ultrasonic footer Applications)

  • 김진수
    • 센서학회지
    • /
    • 제6권5호
    • /
    • pp.392-399
    • /
    • 1997
  • 본 연구에서는 $0.125Pb(Mg_{1/2}Nb_{2/3})O_{3}-0.435PbTiO_{3}-0.44PbZrO_{3}$의 조성을 갖는 hard계 압전 재료에 0.5 wt%의 $MnO_{2}$를 첨가하였으며, 이 시편으로 초음파 전동기를 제작하고자, 소결 온도에 따른 시편의 유전 및 압전특성에 대하여 연구하였다. 실험 결과, $1270^{\circ}C$의 소결 온도에서 다음과 같이 가장 우수한 압전특성을 나타냈다. 즉 시편의 밀도는 $7.72\;g/cm^{3}$ 유전상수는 570, 유전손실은 0.82 %f, 잔류분극 Pr은 $19.18{\mu}C/cm^{2}$ 항전계 Ec는 9.63 kW/cm, 전기기계 결합계수 kp는 55.1%, 기계적 품질계수 Qm은 886이 되었다. 또한 $1270^{\circ}C$ 에서 소결된 시편의 유전상수 및 유전손실을 주파수 변화와 온도 변화에 따라 조사하였다.

  • PDF

High Magnetoelectric Properties in 0.68Pb(Mg1/3Nb2/3)O3-0.32PbTiO3 Single Crystal and Terfenol-D Laminate Composites

  • Ryu, Jung-Ho;Priya, Shashank;Uchino, Kenji;Kim, Hyoun-Ee;Viehland, Dwight
    • 한국세라믹학회지
    • /
    • 제39권9호
    • /
    • pp.813-817
    • /
    • 2002
  • Magnetoelectric(ME) laminate composites of $Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3 (PMN-PT)$ and Terfenol-D were prepared by sandwiching single crystals of PMN-PT between Terfenol-D disks. The magnetoelectric voltage coefficient (dE/dH) of the composite was determined to be 10.30 V/cm${\cdot}$Oe, at 1 kHz and under a dc magnetic bias of 0.4 T. The value of dE/dH is ∼80 times higher than either that of naturally occurring magnetoelectrics or artificially-grown magnetoelectric composites. This superior magnetoelectric voltage coefficient is attributed to the high piezoelectric voltage constant as well as the high elastic compliance of PMN-PT single crystal and the large magnetostrictive response of Terfenol-D.

Effect of Internal Bias Field on Poling Behavior in Mn-Doped Pb(Mg1/3Nb2/3)O3-29 mol%PbTiO3 Single Crystal

  • Lee, Geon-Ju;Kim, Hwang-Pill;Lee, Ho-Yong;Jo, Wook
    • 한국전기전자재료학회논문지
    • /
    • 제34권5호
    • /
    • pp.382-385
    • /
    • 2021
  • Electrical poling is a crucial step to convert ferroelectrics to piezoelectrics. Nevertheless, no systematic investigation on the effect of poling has been reported. Given that the poling involves an alignment of spontaneous polarization, the condition for poling should be different when a material has an internal bias field that influences the domain stability. Here, we present the effect of poling profile on the dielectric and piezoelectric properties in Mn-doped Pb(Mg1/3Nb2/3)O3-29 mol%PbTiO3 single crystal with an internal bias field. We showed that both the dielectric permittivity and the piezoelectric coefficient were further enhanced when the poling procedure ends with a field application along the opposite direction to the internal bias field. We expect that the current finding would give a clue to understanding the true mechanism for the electrical poling.

PZT[$Pb(ZrTi)O_3$]의 XRF 분석용 SRM 개발에 관한 연구 (A study on the development of SRM for XRF analysis of PZT[$Pb(ZrTi)O_3$])

  • 김영만;정찬이;임창호;최범석
    • 분석과학
    • /
    • 제10권6호
    • /
    • pp.439-444
    • /
    • 1997
  • 압전 세라믹스 [$Pb(ZrTi)O_3$] 소재에 대하여 신속하고 정확하게 분석할 수 있는 X-선 형광분석용 표준물질 12종을 제작하였다. 특히 매질효과의 제거, 보관성, 균질성 등을 고려하여 융제($Li_2B_4O_7/LiBO_2=4/1$)로 시료를 16배 희석하여 제작하였다. 네 곳의 분석기관에서 X-선 형광분광기로 12개의 표준물질에 포함된 11 원소에 대하여 검정곡선을 작성해 본 결과 PbO, $ZrO_2$, $TiO_2$, SrO, $WO_3$, $La_2O_3$, $Cr_2O_3$, MgO, $Nb_2O_5$, $MnO_2$들은 correlation factor가 0.998을 넘는 대단히 좋은 직선을 얻었다. 그러나 ZnO의 correlation factor는 0.977로 비교적 낮았으며, 이는 표준시료 중 ZnO의 함량이 10ppm 정도로 낮았기 때문이다. 본 연구에서 제작한 XRF 분석용 표준물질을 이용하면 PZT 중의 주 부성분 원소의 함량을 간편하고 신속 정확하게 분석결과를 얻을 수 있다.

  • PDF

PMN-PT-BT계 세라믹스의 유전 및 전기적 특성(II) (A study on Dielectric and Electrical Properties Using PMN-PT-BT Ceramics(II))

  • 지승한;이능헌;이회규;이덕출
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1994년도 추계학술대회 논문집 학회본부
    • /
    • pp.196-198
    • /
    • 1994
  • The dielectric and electrical properties of $Pb(Mg_{1/3}Nb_{2\3})O_3-PbTiO_3-BaTiO_3$ have been investigated. Perovskite crystalline phase of the specimens are confirmed by XRD at $1270^{\circ}C$. The curie temperature is around $40^{\circ}C$ with the amount of $BaTiO_3$ and $PbTiO_3$. Every specimens shows the slim loop hysteresis curves which is electrostrictive characteristic. The strain vs. applied voltage characteristics exhibits nonlinear relationship, and the specimen of 0.85PMN-0.125PT-0.025BT shows the largest strain.

  • PDF

ITO박막/세라믹유전체 구조의 이동통신 주파수대역용 박형 전파흡수체의 설계 및 제조 (Design and Fabrication of Thin Microwave Absorbers of ITO/Dielectric Structures Used for Mobile Telecommunication Frequency Bands)

  • 윤여춘;김성수
    • 한국재료학회지
    • /
    • 제13권4호
    • /
    • pp.259-265
    • /
    • 2003
  • For the aim of thin microwave absorbers used in mobile telecommunication frequency band, this study proposed a high permittivity dielectrics(λ/4 spacer) coated with ITO thin films of 377 $\Omega$/sq(impedance transformer). High frequency dielectric properties of ferroelectric ceramics, electrical properties of ITO thin films and microwave absorbing properties of ITO/dielectrics were investigated. Ferroelectric materials including $BaTiO_3$(BT), 0.9Pb($Mg_{1}$3/Nb$_{2}$3/)$O_3$-0.1 $PbTiO_3$(PMN-PT), 0.8 Pb (Mg$_{1}$3/$Nb_{2}$3/)$O_3$-0.2 Pb($Zn_{1}$3$_Nb{2}$3/)$O_3$(PMN-PZN) were prepared by ceramic processing for high permittivity dielectrics,. The ferroelectric materials show high dielectric constant and dielectric loss in the microwave frequency range. The microwave absorbance (at 2 ㎓) of BT, 0.9PMN-0.1PT, and 0.8PMN-0.2PZN were found to be 60%(at a thickness of 3.5 mm), 20% (2.5 mm), and 30% (2.5 mm), respectively. By coating the ITO thin films on the ferroelectric substrates with λ/4 thickness, the microwave absorbance is greatly improved. Particularly, when the surface resistance of ITO films is closed of 377 $\Omega$/sq, the reflection loss is reduced to -20 ㏈(99% absorbance). This is attributed to the wave impedance matching controlled by ITO thin films at a given thickness of high permittivity dielectrics of λ/4 (3.5 mm for BT, 2.5 mm for PMN-PT and PMN-PZN at 2 ㎓). It is, therefore, successfully proposed that the ITO/ferroelectric materials with controlled surface resistance and high dielectric constant can be useful as a thin microwave absorbers in mobile telecommunication frequency band.