• Title/Summary/Keyword: Particle reinforced composites

Search Result 155, Processing Time 0.023 seconds

Microstructure and Thermal Behaviors of Droplets During the Formation of Particle Reinforced Metal Matrix Composites by Spray Casting Process (분사주조에 의한 입자강화 금속기지 복합재료의 제조시 액적의 열적거동과 미세조직에 대한 고찰)

  • Kim, Myung-Ho;Bae, Cha-Hurn;Jeong, Hae-Young;Park, Heung-Il
    • Journal of Korea Foundry Society
    • /
    • v.12 no.4
    • /
    • pp.326-334
    • /
    • 1992
  • Particle-reinforced metal matrix composites via the Osprey spray casting process were fabricated by injecting second phase particles of $Al_2O_3$(<$40{\mu}m$) and W($6{\mu}m$) into the spray of Cu droplets, and the thermal behaviors of the composite droplets during flight were considered theoretically on the basis of mixing modes between the Cu droplets and the reinforced particulates injected. It was found that the W-injected spray is comprised of particle-embedded droplets, and the $Al_2O_3-injected$ spray comprises particle-attached droplets. From the predicted results of the thermal behaviors of the composite droplets and preforms produced, it is concluded that the thermal behaviors of the composite droplets during flight, and during the subsequent deposition are strongly influenced by its mixing modes between the reinforced particulates and Cu droplets during flight.

  • PDF

Tensile Behavior of Fiber/Particle Hybrid Metal Matrix Composites (섬유/입자 혼합금속복합재료의 인장거동)

  • 정성욱;정창규;한경섭
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2002.10a
    • /
    • pp.139-142
    • /
    • 2002
  • This study presents a mathematical model predicting the stress-strain behavior of fiber reinforced (FMMCs) and fiber/particle reinforced metal matrix composites (F/P MMCs). MMCs were fabricated by squeeze casting method using Al2O3 short fiber and particle as reinforcement, and A356 aluminum alloy as matrix. The fiber/particle ratios of F/P MMCs were 2:1, 1:1, 1:2 with the total reinforcement volume fraction of 20 vol.%, and the FMMCs were reinforced with 10 vol,%, 15 vol. %, 20 vol. % of fibers. Tensile tests were conducted and compared with predictions which were derived using laminate analogy theory and multi-failure model of reinforcements. Results show that the tensile strength of FMMCs with 10 vol.% of fiber was well matched with prediction, and as the fiber volume increases, predictions become larger than experimental results. The difference between the prediction and experiment is considered to be a result of matrix allowance of fiber damage in tensile loading. As the fiber volume fraction in FMMCs increases, the fiber damage increases and so that the tensile strength is reduced. The strength of F/P MMCs approaches more closely to the prediction than FMMCs reinforced with 20 vol.% of fibers because F/P MMCs contains small quantity of fibers and thus has a positive effect in fiber strengthening.

  • PDF

Effect of SiC Particle Size on Hot Workability of AA2024/$SiC_P$ Composites (AA2024/$SiC_P$ 복합재료의 열간 가공성에 미치는 강화상 크기의 영향)

  • 고병철;홍흥기;유연철
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1997.03a
    • /
    • pp.81-84
    • /
    • 1997
  • The hot deformation behavior of SiCp/AA2024 composites reinforced with different sizes of SiCp reinforcements (1, 8, 15, 36, and 44${\mu}{\textrm}{m}$) was investigated by hot torsion tests. The hot restoration of the composites depending on the SiCp reinforcements particle size was studied from the effective stress - strain curves. Dynamic recrystallization (DRX) was occurred in the SiCp/AA2024 composites during the hot deformation at 320 - 43$0^{\circ}C$ under a strain rate of 1.0/sec. Also, the critical strain for DRX decreased with decreasing the reinforcement size of SiCp from 44 to 8${\mu}{\textrm}{m}$. The composite reinforced with SiCp of 8${\mu}{\textrm}{m}$ showed the highest flow stress (265 MPa) and the work hardening rate at 32$0^{\circ}C$ under a strain rate of 1.0/sec.

  • PDF

Investigation of Microstructure Inhomogeneity in SiCp-reinforced Aluminum Matrix Composites

  • Gacsi, Zoltan;Gur, C.Hakan;Makszimus, Andrea;Pieczonka, Tadeusz
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1303-1304
    • /
    • 2006
  • The type, volume fraction, size, shape and arrangement of embedded particles influence the mechanical properties of the particle reinforced metal matrix composites. This presents the investigation of the SiC particle and porosity distributions in various aluminum matrix composites produced by cold- and hot-pressing. The microstructures were characterized by optical microscopy and stereological parameters. SiC and porosity volume fractions, and the anisotropy distribution function were measured to establish the influence of the consolidation method.

  • PDF

Mechanical Properties of SiC Particulate Reinforced Mg Matrix Composites Fabricated by Melt Stirring Method (용탕교반법에 의한 SiC 입자강화 Mg기 복합재료의 기계적 특성)

  • Lim, Suk-Won;Choh, Takao;Park, Young-Jin
    • Journal of Korea Foundry Society
    • /
    • v.13 no.5
    • /
    • pp.441-449
    • /
    • 1993
  • SiC particulate reinforced magnesium matrix composites were fabricated by melt stirring method. The effet of several factors on mechanical properties and the efficiency of melt stirring method from the viewpoint of these properties were investigated. The tensile strength increased and the elongation decreased with decrease of the particle size or the increase of the paticulate volume fraction for pure magnesium matrix and Mg-5%Zn alloy matrix composites. A longer stirring time improved the tensile strength of these composites. The tensile strength of Mg-5%Ca alloy matrix composites which shows no uniform paticulate distribution was a little lower than that of matrix alloy. Rapid solidification rate is preferred for the improved tensile strength of these composites. The pure magnesium matrix and Mg-5%Zn alloy matrix composites have tensile strength of about 400MPa. This value agrees with the tensile strength of some magnesium matrix composites fabricated by liquid infiltration method or powder metallurgy method at the same volume fraction of reinforcements of whisker or particle. Therefore, the melt stirring method which has the advantages of simple process is considered to be efficient in fabricating magnesium matrix composites.

  • PDF

Investigation of Reinforced Distribution in Fabrication Process of Metal Matrix Composites by Combined Stirring Process (복합교반법에 의한 금속복합재료의 제조공정에 따른 강화재의 분산성 검토)

  • 이동건;강충길
    • Composites Research
    • /
    • v.14 no.5
    • /
    • pp.1-11
    • /
    • 2001
  • The particulates reinforced metal matrix composites(PMMC) have a number of interesting mechanical properties. including high strength and good resistance to wear at high temperature and low thermal expansion. The equipment structure to obtain the homogeneous distribution in composites are proposed for the continuous pouring of reinforcement at the desired temperature. The particulates reinforced metal matrix composites(A357/SiCp) were fabricated by the process of the combined stirring method with the various fabrication process. The combined stirring method to niform distribution of particle is consisted of two stirring force both electro-magnetic stirring generated from induction heating and mechanical stirring with graphite stirrer. PMMC billets were fabricated with the volume fractions ranged from 0% to 20% and particle sizes ranged from 14${\mu}{\textrm}{m}$ to 25${\mu}{\textrm}{m}$. It is important to cont the size of primary $\alpha$-Al solid particles because it could become the cause of the particle pushing or capture phenomena from the fact that secondary dendrite arm spacing size depends on the cooling rate during the solidification in hypoeutectic Al-Si alloy. Therefore, the effect of primary $\alpha$-Al on the reinforcement distribution in matrix alloys has been investigated. The microstructure of PMMC fabracated with various volume fractions(0%, 10%, and 20%) and particle size were observed.

  • PDF

Characterization of Wear Resistance of Particle Reinforced Al Matrix Composite Manufactured by Centrifugal Spray Casting (분사주조한 Al기지 입자강화 복합재료의 마모특성)

  • Bae, Cha-Hurn;Choi, Hak-Kyu;Bang, Kuk-Soo
    • Journal of Korea Foundry Society
    • /
    • v.24 no.2
    • /
    • pp.108-114
    • /
    • 2004
  • $Al_2O_3$, SiC reinforced Al matrix composites were fabricated by centrifugal spray casting method and their wear resistance characteristics have been studied. Particles are generally uniformly distributed in the microstructure of as-cast specimens. In order to investigate the effect of secondary deformation, hot rolling was performed for each specimen of pure Al matrix composites with a reduction of 10, 20, 30, 40 and 50% at $400{\sim}500^{\circ}C$, respectively. Microstructure of specimen showed that particle distribution density and hardness increased because of increasing of reduction ratio. Wear test with a various sliding velocity of 1.98, 2.38, 2.88 and 3.53m/sec showed that the wear resistance characterization of composite improved remarkably compared to the normal alloy and performs without reinforced particles. Microstructural observation for the worn surface of pure Al specimens without particles showed that a change in wear mechanism seemed to separate layer by surface fatigue. In other case of Al composite reinforced with $Al_2O_3$ and SiC, the grinder type of wear mechanism was shown.

The Effect of the Reinforced Particles on the Mechanical and Fracture Behaviors of the SiC/Al2O3/Vinyl-Ester Composites (SiC/Al2O3/Vinyl-Ester 복합재료의 강화재 입자가 기계적 특성 및 파괴거동에 미치는 영향)

  • Kim, Da Jin Sol;Yun, Yu Seong;Kwon, Oh Heon
    • Journal of the Korean Society of Safety
    • /
    • v.32 no.3
    • /
    • pp.1-7
    • /
    • 2017
  • Particle reinforced composites are materials that have enhanced physical properties by adding particle reinforcements to polymer materials and have been applied to a wide range of fields such as the aerospace, bio-technology and automative industry. In this study, particle reinforced composites were prepared by mixing $SiC/Al_2O_3$ to the vinyl ester as the thermoset resin. The purpose of this study is to evaluate mechanical properties and fracture behavior by the tensile test and single edge notch specimen according to the addition ratio of reinforcement. Addition of 1 and 2 wt% of the particle reinforcement to the vinyl-ester resin was effective for the strength improvement. However, when it was more than 3 wt%, its strength was decreased. Also the highest elastic modulus obtained as 3.19 GPa was found at the 2 wt% addition of reinforcement. Futhermore the fracture toughness was evaluated by the energy release rate and the maximum critical energy release rate was obtained when 1 wt% reinforcement. The results show that the limit of adding of $SiC/Al_2O_3$ for improvement of the mechanical and fracture performance is 2 wt% reinforcement particles.

Application of the full factorial design to modelling of Al2O3/SiC particle reinforced al-matrix composites

  • Altinkok, Necat
    • Steel and Composite Structures
    • /
    • v.21 no.6
    • /
    • pp.1327-1345
    • /
    • 2016
  • $Al_2O_3$/SiC particulate reinforced (Metal Matrix Composites) MMCs which were produced by using stir casting process, bending strength and hardening behaviour were obtained using an analysis of variance (ANOVA) technique that uses full factorial design. Factor variables and their ranges were: particle size $2-60{\mu}m$; the stirring speed 450 rpm, 500 rpm and the stirring temperature $620^{\circ}C$, $650^{\circ}C$. An empirical equation was derived from test results to describe the relationship between the test parameters. This model for the tensile strength of the hybrid composite materials with $R^2$ adj = 80% for the bending strength $R^2$ adj = 89% were generated from the data. The regression coefficients of this model quantify the tensile strength and bending strengths of the effects of each of the factors. The interactions of all three factors do not present significant percentage contributions on the tensile strength and bending strengths of hybrid composite materials. Analysis of the residuals versus was predicted the tensile strength and bending strengths show a normalized distribution and thereby confirms the suitability of this model. Particle size was found to have the strongest influence on the tensile strength and bending strength.

Effects of Processing Parameters on the Mechanical Properties of Aluminium Matrix Composites (알루미늄 기지 금속복합재료의 기계적 성질에 미치는 제조변수의 영향)

  • Kim, J.D.;Koh, S.W.;Kim, H.J.
    • Journal of Power System Engineering
    • /
    • v.9 no.4
    • /
    • pp.130-136
    • /
    • 2005
  • The effects of additional Mg content, the size and volume fraction of reinforcement phase on the mechanical properties of ceramic particle reinforced aluminium matrix composites fabricated by pressureless metal infiltration process were investigated. The hardness of $SiC_p/AC8A$ composites increased gradually with an increase in the additive Mg content, while the bending strength of $SiC_p/AC8A$ composites increased with an increase in additive Mg content up to 5%. However, this decreased when the level of additive Mg content was greater than 5% due to the formation of coarse precipitates by excessive Mg reaction and an increase in the porosity level. The hardness and strength of the composites increased with decreasing the size of SiC particle. It was found that the composites with smaller particles enhanced the interfacial bonding than those with bigger particles from fractography of the composites. The hardness of $Al_2O_{3p}/AC8A$ composites increased gradually with an increase in the volume fraction, however, the bending strength of $Al_2O_{3p}/AC8A$ composites decreased when the volume fraction of alumina particle was greater than 40% owing to the high porosity level.

  • PDF