  • We reported on characteristics of the piezoelectric ceramic-polymer composite for the application of the thick-film speaker. The PVDF-PZT composites were fabricated to incorporate the advantages of both ceramic and polymer with various mixing ratios by 3-roll mill mixer. The composite solutions were coated by the conventional screen-printing method on ITO electrode coated PET (Polyethylene terephthalate) polymer film. After depositing the top-electrode of silver-paste, 4 kV/mm of DC field was applied at $120^{\circ}C$ for 30 min to poling the composite films. The value of $d_{33}$ (piezoelectric charge constant) was increased when the PZT weight percent was increased. The maximum value of the $d_{33}$ was 24 pC/N at 70 wt% PZT. But the $g{33}$ (piezoelectric voltage constant) showed the maximum value of $32mV{\cdot}m/N$ at 65 wt% of PZT powder. The SPL (sound pressure level) of the speaker fabricated with the 65:35 composite film was about 68 dB at 1 kHz.

PZT-PSN 세라믹스의 WO3의 첨가량에 따른 압전 특성 (Piezoelectric Characteristics of PZT-PSN Ceramics Depending on WO3Addition)

  • 배숙희;김성곤;김철수;이경화;이상렬
    • 한국전기전자재료학회논문지
    • /
    • 제15권9호
    • /
    • pp.794-797
    • /
    • 2002
  • Piezoelectric properties of PZT-PSN ceramics were investigated as a function of WO$_3$ addition from 0 wt% to 6.0 wt%. The dielectric and piezoelectric characteristics of PZT-PSN ceramics have been investigated at different calcination (80$0^{\circ}C$~90$0^{\circ}C$) and sintering (110$0^{\circ}C$~130$0^{\circ}C$) temperatures. The grain size was increased with the addition of WO$_3$and the sintering temperatures. Anisotropic properties of electromechanical coupling coefficient and piezoelectric coefficient are proven to be dependent on processing temperatures and amount of addition. At the specimen with 0.6 wt% WO$_3$ addition, using calcination temperature of 80$0^{\circ}C$ and sintering temperature of 110$0^{\circ}C$ , mechanical quality factor(Q$_{m}$) and electromechanical coupling coefficient(k$_{p}$) showed the excellent results of 1560 and 0.48, respectively Experimental results indicated that the PZT-PSN system ceramics with WO$_3$impurity could be effectively used for the microtransformer and actuator applications, etc.etc.

PMW-PNN-PZT 세라믹스의 Bismuth 치환에 따른 미세구조 및 압전 특성 (Microstructure and Piezoelectric Properties of PMW-PNN-PZT Ceramics with Bismuth Substitution)

  • 김용진;류주현;신동찬
    • 한국전기전자재료학회논문지
    • /
    • 제29권6호
    • /
    • pp.332-336
    • /
    • 2016
  • In this study, in order to develop the composition ceramics for ultrasonic sensor with high $d_{33}*g_{33}$, $Pb_{1-3x/2}Bix(Mg_{1/2}W_{1/2})_{0.03}(Ni_{1/3}Nb_{2/3})_{0.09}(Zr_{0.5}Ti_{0.5})_{0.88}O_3$(PMW-PNN-PZT) system ceramics were prepared using CuO as sintering aids. And then, their microstructure, piezoelectric and dielectric characteristics were systemetically investigated with bismuth substitution. The PMW-PNN-PZT ceramic specimens could be sintered at sintering temperature of $940^{\circ}C$ by adding sintering aids. At x=0.015 specimen, the density, electromechanical coupling factor($k_p$), dielectric constant, piezoelectric constant($d_{33}$) and piezoelectric figure of merit($d_{33}*g_{33}$) indicated the optimal properties of $7.90g/cm^3$, 0.67, 2,511, 628 pC/N, and $17.7pm^2/N$, respectively, for duplex ultrasonic sensor application.

$MnO_2$가 첨가된 PZT-PSN압전세라믹의 압전 및 전기적특성 분석 (Ihe Electrical and Piezoelectric Characteristics of PZT-PSN ceramics added $MnO_2$)

  • 김성곤;김철수;박정호;이상렬
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.161-164
    • /
    • 2001
  • In this paper, we investigated the dielectric and piezoelectric properties of Pb(Sb, Nb)O$_3$-Pb(Zr, Ti)O$_3$ ceramic(PSN) for piezoelectric transformer and actuator etc. Effect of MnO$_2$ addition on the PSN ceramic was investigated. Anisotropic properties of electromechanical coupling factor and piezoelectric properties proved to be varied with amount of MnO$_2$ impurity and sintering temperature. The electromechanical coupling factor k$_{p}$ of 0.38 and the mechanical quality factor Q$_{m}$ of 1944 were obtained from the specimen with 0.4 wt% MnO$_2$ sintered at 115$0^{\circ}C$ addition. Experimental results indicated that the PSN ceramic with MnO$_2$ impurity can be effectively used for piezoelectric transformer and actuator.tor.

  • PDF

소결온도에 따른 PMN-PNN-PZT 미세구조 및 압전특성 (Microstructure and Piezoelectric Properties of PMN-PNN-PZT with the Sintering Temperature)

  • 이현석;류주현;윤현상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 Vol.19
    • /
    • pp.217-218
    • /
    • 2006
  • In this study, In order to develop the low temperature sintering multilayer piezoelectric actuator, PMN-PNN-PZT system ceramics were manufactured with the sintering temperature, and their microstructure and piezoelectric properties were investigated. At the composition ceramics sintered at $900^{\circ}C$, dielectric constant(${\varepsilone}_r$), electromechanical coupling factor($k_p$), piezoelectric constant($d_{33}$) and mechanical quality factor(Qm) showed the optimal value of 1095, 0.60, 363 and 1055, respectively, for multilayer piezoelectric actuator application.

  • PDF

저온소결 PMN-PNN-PZT세라믹스의 소결온도에 따른 미세구조 및 강유전특성 (Microstructure and Ferroelectric Properties of Low Temperature Sintering PMN-PNN-PZT Ceramics with Sintering Temperature)

  • 류주현;이현석;이상호
    • 한국전기전자재료학회논문지
    • /
    • 제19권12호
    • /
    • pp.1118-1122
    • /
    • 2006
  • In this study, in order to develop the low temperature sintering multilayer piezoelectric actuator, PMN-PNN-PZT system ceramics were manufactured and their microstructure, ferroelectric and piezoelectric properties were investigated. By increasing sintering temperature, remanent polarization$(P_r)$ was increased due to the increase of sinterability and grain size. However, coercive $field(E_c)$ showed an opposite tendency to remanent polarization owing to the feasibility of domain wall motion. At the sintering temperature of $900^{\circ}C$, dielectric $constant({\varepsilon}_r)$, electromechanical coupling $factor(k_p)$, piezoelectric $constant(d_{33})$ and mechanical quality $factor(Q_m)$ showed the optimal value of 1095, 0.60, 363 and 1055, respectively, for multilayer piezoelectric actuator application.

소결조제 Li2CO3 첨가에 따른 PZW-PMN-PZT 압전 세라믹의 압전 및 유전 특성 (Piezoelectric and Dielectric Properties of PZW-PMN-PZT Piezoelectric Ceramic according to Sintering Aid Li2CO3 Addition)

  • 이갑수;이일하;류주현;류성림
    • 한국전기전자재료학회논문지
    • /
    • 제20권12호
    • /
    • pp.1034-1038
    • /
    • 2007
  • In order to develop the composition ceramics capable of being sintered at low temperature with high piezoelectric properties for multilayer piezoelectric actuator application, PZW-PMN-PZT system ceramics were manufactured according to sintering aid $Li_2CO_3$ addition and their microstructural, dielectric and piezoelectric properties were investigated. The crystal structure of the specimens showed a perovskite phase and no pyrochlore or other second phase was detected. At the sintering temperature of $900\;^{\circ}C,\;0.2\;wt%Li_2CO_3$ added specimen showed a optimum values of kp = 0.562, $d_{33}\;=\;360\;pC/N$ and Qm = 1184, respectively.

소결온도에 따른 PMN-PNN-PZT 세라믹스의 압전 및 유전 특성 (Piezoelectric and Dielectric Properties of PMN-PNN-PZT with the Sintering Temperature)

  • 이유형;류주현;이상호;윤현상;류성림
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.290-291
    • /
    • 2007
  • In this study, in order to develop low temperature sintering ceramics for multilayer piezoelectric actuator, sensers, transducers, PMN-PNN-PZT ceramics were manufacrtured with the sintering temperature, and their piezoelectric and dielectric properties were investigated. At the composition ceramics sintered at $900^{\circ}C$, desity, dielectric constant$({\varepsilon}_r)$, electromechanical coupling factor(kp), piezoelectric constant$(d_{33})$ and mechanical quality factor(Qm) showed the optimal value of $7.86g/cm^3$, 1417, 0.634, 410pC/N and 1138, respectively.

  • PDF

불순물 첨가에 따른 저온소결 PMN-PNN-PZT 세라믹스의 압전 및 유전특성 (Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PMN-PNN-PZT Ceramics according to the addition of dopant)

  • 이상호;이창배;정광현;류주현;홍재일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.33-34
    • /
    • 2005
  • In this study, in odor to develop low temperature sintering multilayer piezoelectric actuator and ultrasonic vibrator, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3$ and $Na_2CO_3$ as sintering aids and their piezoelectric and dielectric characteristics were investigated according to the addition of dopant CuO and $Fe_2O_3$, respectively. The CuO added PMN-PNN-PZT ceramics improved mechanical quality factor Qm due to the acceptor doping effect. And also, $Fe_2O_3$ reacted as softner in this composition system in addition to the increase of grain size and sinterability. Taking into consideration electromechanical coupling factor kp of 0.62, dielectric constant $\varepsilon_r$, of 1275, Piezoelectric $d_{33}$ constant of 377[pC/N] and mechanical quality factor Qm of 975, it was concluded that the ceramics with the $Fe_2O_3$, added composition sintered at 900[$^{\circ}C$] were best for the multilayer piezoelectric actuator and ultrasonic vibrator application.

  • PDF

PZT틀 이용한 Air gap 안테나의 주파수 특성에 관한 연구 (Frequency properties of Air gap Antenna using PZT)

  • 김영훈;우형관;임승혁;송준태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 춘계학술대회 논문집 전자세라믹스 센서 및 박막재료 반도체재료 일렉트렛트 및 응용기술
    • /
    • pp.164-167
    • /
    • 2000
  • This paper investigated that resonant frequencies of microstrip patch antenna were tunable when piezoelectric materals were used as the antenna substrates. The resonant frequencies of the air-gap antenna using the piezoelectric substrate were able to be controlled by applied AC voltage. The frequency variation of the antenn was great when PZT were applied voltage of the resonant frequency.

  • PDF