• 제목/요약/키워드: PZT(60/40)

검색결과 27건 처리시간 0.027초

Sol-Gel법으로 제작한 PZT(40/60)/(60/40) 이종층 박막의 강유전특성 (Ferroelectric Properties of the PZT(40/60)/(60/40) Heterolayered Thin Film Prepared by Sol-Gel Method)

  • 김경균;정장호;박인길;이성갑;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1998년도 춘계학술대회 논문집
    • /
    • pp.83-86
    • /
    • 1998
  • Ferroelectric PZT(40/67)/PZT(60/40)heterolayered thin films were Prepared by the alkoxide-based Sol-Gel method. PZT(40/60) and PZT(60/40) stock solutions were made and spin-coated on the P7Ti/Si02/Si substrate alternately. These PZT(40/60) and PZT(60/40) films were dried at 300$^{\circ}C$ for 30min to remove organic materials and were sintered at 650$^{\circ}C$ for 1 hour to crystalize into a perovskite structure. The coating and heating procedure were repeated 6 times to form heterolayered films. Increasing the number of coating, coercive field was decreased. The relative dielectric constant, loss, remanent polarization and coercive field of the 4-coated PZT heterolayered were 1200, 4.1[%], 30.794[${\mu}$C/㎡] and 147.22[kV/cm], respectively.

  • PDF

RF 스퍼터링법을 이용한 PZT(52/48)/BST(60/40) 이종층 박막의 유전 특성 (The Dielectric Properties of PZT(52/48)/BST(60/40) Heterolayered Thin Film Prepared bv RF Sputtering Method)

  • 권현율;김지헌;최의선;이성갑;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2004년도 하계학술대회 논문집 C
    • /
    • pp.1621-1623
    • /
    • 2004
  • The $Pb(Zr_{0.52}Ti_{0.48})O_3/(Ba_{0.6}Sr_{0.4})TiO_3$ [PZT(52/48)/BST(60/40)] heterolayered thin films were deposited on Pt/Ti/$SiO_2$/Si substrates by using the RF sputtering method with RF powers of 60,70,80,90[W]. All thin films showed the peaks of the tetragonal phase. Increasing the RF power, dielectric constant and loss of the PZT(52/48)/BST(60/40)] heterolayered thin films were decreased. The thickness ratio of PZT and BST thin films was 1/1. The relative dielectric constant and the dielectric loss of the PZT(52/48)/ BST(60/40) heterolayered thin films were 562 and 13%, respectively.

  • PDF

$Ar/O_2$ 비에 따른 PZT/BST 이종층 박막의 구조적 특성 (The Structural Properties of the PZT/BST Heterolayered Thin Films with $Ar/O_2$ Ratio)

  • 이의복;남성필;이상철;김지헌;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 하계학술대회 논문집 Vol.5 No.2
    • /
    • pp.607-610
    • /
    • 2004
  • The Pb $(Zr_{0.52}Ti_{0.48})O_3/(Ba_{0.6}Sr_{0.4}TiO_3$ [PZT(52/48)/BST(60/40)] heterolayered thin films were fabricated on the Pt/Ti/$SiO_2$/Si by RF sputtering method. The structural properties of the PZT(52/48)/BST(60/40) heterolayered thin films were investigated with Ar/$O_2$ ratio condition. All the PZT(52/48)/BST(60/40) heterolayered thin films had shown the PZT(111), (200) and BST(200) Peaks of the tetragonal structure. Increasing the Ar/$O_2$ ratio, the average roughness was increased. The thickness ratio of the to the PZT and BST thin film was 1:2. In the case of the PZT(52/48)/BST(60/40) heterolayered thin films with Ar/$O_2$ ratio of 80/20, the average roughness was 3.4 [nm].

  • PDF

PZT 이종층 후막의 구조적, 전기적 특성 (Structural and Electrical Properties of PZT Heterolayered Thick Films)

  • 이성갑;임성수;이영희;이종덕;박상만
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2005년도 제36회 하계학술대회 논문집 C
    • /
    • pp.1915-1917
    • /
    • 2005
  • PZT(40/60) and PZT(60/40) powders, prepared by the sol-gel method, were mixed with an organic vehicle and the PZT(40/60)/PZT(60/40) heterolayered thick films were fabricated by the screen-printing method on $Pt/Al_2O_3$ substrates. The structural properties such as DTA, X-ray diffraction and microstructure, were examined as a function of the applied pressure. In the DTA analysis, the formation of the polycrystalline perovskite phase was observed at around $880^{\circ}C$. The average thickness of the PZT heterolayered thick films which were coated five times was approximately $95-100{\mu}m$.

  • PDF

PZT 후막의 미세 구조적 특성에 조성과 전구체 용액의 코팅이 미치는 영향 (Effect of Composition and Coating of Precursor Solution on a Micro Structural Properties of PZT Thick Films)

  • 박상만;노현지;이성갑
    • 한국전기전자재료학회논문지
    • /
    • 제19권11호
    • /
    • pp.1014-1019
    • /
    • 2006
  • The influence of the number of solution coatings on the densification of the PZT thick films was studied. PZT powder and PZT precursor solution was prepared by a sol-gel method and PZT thick films were fabricated by the screen-printing method on the alumina substrates. The powder and solution of composition were (A) PZT(80/20)/PZT(20/80), (B) PZT(70/30)/PZT(30/70) and (C) PZT(60/40)/PZT(40/60), (D) PZT(52/48)/PT. The coating and drying procedure was repeated 4 times. And then the PZT precursor solution was spin-coated on the PZT thick films. A concentration of a coating solution was 0.5 moth and the number of coating was repeated from 0 to 6. The porosity of the thick films was decreased with increasing the number of coatings and the PZT thick films with 6-times coated showed the dense microstructure and thickness of about $60{\mu}m$. A grain size was increased with increasing the coating number. All PZT thick films showed the typical XRD patterns of a typical perovskite polycrystalline structure. The relative dielectric constant of PZT thick films was improved 30-100% as the number of coatings.

Polarized Raman Scattering Study of Highly(111)-oriented PZT Films in the Rhombohedral-Phase Field

  • 이현정;박정환;장현명
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2003년도 춘계학술발표강연 및 논문개요집
    • /
    • pp.174-174
    • /
    • 2003
  • Highly (111)-oriented PZT [Pb(Zrl-xTix)O3] thin films in the Zr-rich rhombohedral phase-field were successfully fabricated on Pt(111)/Ti/SiO2/Si substrates by combining PLD method with sol-gel process. These highly (111)-oriented films can be used as model systems for polarized Raman scattering study of PZT in the rhombohedral-Phase field because the (111)-direction is the principal off-center axis of the rhombohedral ferroelectricity. For this purpose, we have fabricated PZT films employing two distinctive compositions : one with Zr/Ti = 90/10 (abbreviated as PZT90/10) and the other with Zr/Ti= 60/40 (PZT60/40). The PZT90/10 film belongs to the octahedrally distorted FR(LT) phase with a cell-doubled structure, whereas the PZT60/40 is in the high-temperature FR(HT) phase-field at room temperature. To clearly separate E(TO) phonon modes from Al(TO) modes of the (111)-oriented rhombohedral film, we have suitably devised Z(X,Y)Z and Z(X,X)Z backscattering geometries for E(TO) and Al (TO), respectively. The polarized scattering experiment demonstrated that both types of (111)-oriented rhombohedral films closely followed the Raman selection rule.

  • PDF

기판온도에 따른 PZT(4060)/(6040) 다층 박막의 유전 특성 (Dielectric Properties of PZT(4060/6040) Multilayered Thin Films with Substrate Temperature)

  • 한상욱;이상헌;이성갑;배선기;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 하계학술대회 논문집 Vol.5 No.2
    • /
    • pp.667-670
    • /
    • 2004
  • The dielectric properties of PZT(4060)/(6040) multilayered thin films with substrate temperature were investigated. PZT(4060)/(6040) thin films were deposited by RF sputtering method on Pt/Ti/$SiO_2$/Si substrates with different substrate temperature of $200{\sim}700^{\circ}C$. Increasing the substrate temperature, perovskite structure was increased, and PZT (001), (110), (002), (200) peaks were increased. The relative dielectric constant and dielectric loss of PZT(4060)/(6040) multilayered thin films at the substrate temperature of $700^{\circ}C$ were 843 and 2.45, respectively at 1000(Hz).

  • PDF

Ferroelectric Properties of PZT Heterolayered Thick Films

  • Lee, Sung-Gap;Shim, Young-Jae;Lee, Young-Hie;Bae, Seon-Gi
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.200-201
    • /
    • 2005
  • PFerroelectric PZT heterolayered thick films were fabricated by the alkoxide-based sol-gel method. PZT(40/60) and PZT(60/40) paste were made and alternately screen-printed on the $Al_2O_3$ substrates. We have introduced a press-treatment to obtain a good densification of screen printed films. The porosity of the thick films were decreased with increasing the applied pressure and the thick films pressed at 0.6 ton/$cm^2$ showed the dense microstructure and thickness of about 76${\mu}m$. The remanent polarization and coercive field increased with increasing applied pressure and the values for the PZT thick films pressed at 0.6 ton/$cm^2$ were 17.04${\mu}Ccm^2$, 78.09 kV/cm, respectively.

  • PDF

Sol-gel법으로 제조된 Tb-doped PZT(60/40) 박막의 강유전 특성 (Ferroelectric properties of sol-gel derived Tb-doped PZT thin films)

  • 손영훈;김경태;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 추계학술대회 논문집 Vol.16
    • /
    • pp.51-54
    • /
    • 2003
  • Tb-doped lead zirconate titanate($Pb_{1.1}(Zr_{0.6}Ti_{0.4})O_3$; PZT) thin films on $Pt(111)/Ti/SiO_2/Si(100)$ substrates prepared by a sol-gel method. Films have a Zr/Ti ratio of 60:40 and perovskite phase structure. The effect on the structural and electrical properties of films measured according to Tb content. Dielectric and ferroelectric properties of PZT thin films were altered significantly by Tb-doping. The PZT thin film with higher dielectric constant and improved leakage current characteristic was obtained by adding 0.3 mol% Tb. At 100 kHz, the dielectric constant and the dielectric loss of the 0.3 mol% Tb-doped PZT thin film were 1611 and 0.24, respectively The remanent polarization(2Pr) of the 0.3 mol% Tb-doped PZT thin film was $61.4\;{\mu}C/cm^2$ and the coercive field was 61.9 kV/cm. Tb-doped PZT thin films showed improved fatigue characteristics comparing to the undoped PZT thin film.

  • PDF