• Title/Summary/Keyword: PSZ

Search Result 48, Processing Time 0.026 seconds

Fundamental Study on the Formation of Nanostructured Coating Layer (나노구조 용사코팅층의 형성에 관한 기초적 연구)

  • Kim, Y.S.
    • Journal of Power System Engineering
    • /
    • v.9 no.4
    • /
    • pp.90-95
    • /
    • 2005
  • The wire-arc process is a low-cost thermal spray method simply utilizes electrical energy to melt the feedstock wire. It is more userful for field applications, especially to coat large surface area. In this paper, a special Fe-based alloy coatings by using the wire-arc process were developed. Nanoscale composite coatings were achieved either during spraying or through a post heat treatment. As-sprayed Fe-based alloy coatings had been an amorphous matrix structure, after heating to $700^{\circ}C$ for 10 minutes a solid state transformation occurred in the some fraction of amorphous matrix which resulted in the formation of nanostructured recrystallized phase. Scanning electron microscopy (SEM) and field emotional scanning electron microscope(FE-SEM) were applied to analyze the microstructure of the coatings. Additionally hardness and bend resistance of the Fe-based alloy coatings were examined, and these results were compared with those of partially stabilized zirconia(PSZ) coatings by using the plasma spray process.

  • PDF

Zirconia galvani sensor for the measurement of oxygen activity (용존산소활량 측정용 지르코니아 갈바니 센서)

  • Oh, Young-Jei
    • Journal of Sensor Science and Technology
    • /
    • v.18 no.6
    • /
    • pp.441-448
    • /
    • 2009
  • Magnesia partially stabilized zirconia(Mg-PSZ) solid electrolytes for an improvement of thermal shock resistance, which is suitable for the measurement of oxygen activity in a molten steel, were prepared by post-thermal aging treatment. The steelmaking oxygen sensor elements were formed by an injection molding method, sintered at $1650^{\circ}C$, and then thermal aged ranged from 1250 to $1400^{\circ}C$. Sintered density and porosity were decreased as increasing the magnesia content in a zirconia-magnesia solid solution. Fractions of cubic phase to the synthesized Mg-PSZ solid electrolytes were ranged from 13.13 to 79.54.% after post-thermal aging treatment. Very dense microstructure without voids in the grains was obtained by the post-thermal aging process. Fine tetragonal phase crystallites precipitated on the cubic surface during post-thermal aging up to $1300^{\circ}C$ improve a thermal shock resistance and reappearance of electro motive force(EMF) curve.

Determination of Optimum Condition in Plasma Spraying Process (플라즈마용사공정에서의 최적 조건 결정에 관한 연구)

  • 최경수;박동화
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.2
    • /
    • pp.155-162
    • /
    • 1996
  • A Taguchi methodology study of the plasma spraying thermal barrier coating (TBC) layer is presented. The experiment parameters were designed by a L8-style orthogonal arrays approach. A Taguchi analysis was conduc-ted through the results of the coating properties which were affected by plasma spraying parameters. Zirconia (partially stbilized with ytrria: PSZ) was sprayed on TiAl intermetallic compound substrates, The coating layer was characterized by thickness microstructure and porosity using SEM and Image analyzer. The coating quali-ties are discussed with respect to thermal barrier effect thermal cycling test6 and adhesion strength test. An optimum condition of plasma spraying process which are derived from the Taguchi analysis could be found for high quality TBC.

  • PDF

Effect of Heat Treatment of powder on the Tribological Behavior of the Plasma Sprayed Zirconia Coating (분말 열처리가 지르코니아 용사코팅층의 마모특성에 미치는 영향)

  • 신종한;임대순;안효석
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2000.11a
    • /
    • pp.298-303
    • /
    • 2000
  • The 3 mol% yttria stabilized zirconia (3-Y PSZ) powder was heat treated at 50 0$^{\circ}C$ to evaporate the polymer binder and stabilize the tetragonal phase. The wear experiments were carried out on a ring-on-plate type reciprocating wear tester at selected temperatures with in the range room temperature to 600$^{\circ}C$ The results show that the heat treatment of powder decreases the wear rate due to the reduction of microcracks and pores in coatings and the stabilization of the tetragonal phase. Powder heat treatment enhanced the quality of the coating layer by removing remnant gases during coating process and the powder heat treatment at which tetragonal phase is stable diminished phase ratio of monoclinic. These two effects improved wear resistance characters.

  • PDF

The Characteristic of Agglomerate and Sintering of Y-PSZ Powders Prepared by Different Processes (제조방법에 따른 Y-PSZ 분말의 응집 및 소결특성)

  • Lee, Jong-Kook;Kim, Hwan;Hwang, Kyu-Hong
    • Journal of the Korean Ceramic Society
    • /
    • v.22 no.5
    • /
    • pp.9-16
    • /
    • 1985
  • Agglomeration of Y-PSZ and its related properties were studied. The ultrafine $ZrO_2$ powder containg 3 mol% $Y_2O_3$ was prepared by 1) coprecipitation method b) hot petroleum drying method c) sol-gel method and the characteristics of calcined powders and the microstructures of sintered body were observed. Powder prepared by the coprecipitation method was about 125$\AA$ in crystallite size and 0.1~1.0${\mu}{\textrm}{m}$ of intra-agglomerate pore size when calcined at $600^{\circ}C$ for 1 hour. because of small crystallite size and weak agglo merate strength resultant densification of sintered body was high. But above the temperature of 130$0^{\circ}C$ efflorescent phenomena due to anions attached to powder surface was observed. Powder prepared by hot petroleum drying method was 65$\AA$ in crystallite size and 1~10${\mu}{\textrm}{m}$ of intraagglome-rate pore size and it was observed that the agglemerates were formed during the calcining process. In this case despite of small crystallite size the rate of sintering was slow and the existing lenticular interagglomerate pore was not eliminated to the final stage of sintering. Powder prepared by sol-gel method showed solid agglomertes due to rapi dhydrolysis reaction. In this powder which involves strong solid agglomerates overall sintering rate was determined by the sintering between the agglomerates and therefore sinterability of powders made by sol-gel method was very poor.

  • PDF

Effects of Aging on Properties of MgO-Partially Stabilized Zirconia (마그네시아 부분안정화 지르코니아 소결체의 특성에 미치는 열처리 효과)

  • 정형진;오영제;이홍림
    • Journal of the Korean Ceramic Society
    • /
    • v.24 no.3
    • /
    • pp.243-250
    • /
    • 1987
  • The effects aging on some properties and thermal-shock behavior of zirconia partially stabilized with 9 mol% MgO (9MZ) were studied. 9MZ specimens were aged over $1200^{\circ}$-$1400^{\circ}C$ for 12hours subsequently, after sintering at $1650^{\circ}C$ for 4 hours. Fracture strength(both before and after thermal-shock test), linear thermal expansion, monoclinic fraction and phase transition by XRD, density, galvanic potential and microstructure were measured. Quantitative chemical analysis around the grain-boundary of the specimen aged at $1350^{\circ}C$ was also conducted by EDX. The aging of 9MZ specimen causes a thermal decomposition of cubic-$ZrO^{2}$ into the formation metastable tetragonal-$ZrO^{2}$ and MgO. The former increases the residual strength after thermal-shock test and the latter improves the thermal-shock resistance due to thermal conduction through the continuous magnesia phase and the formation of monoclinic phase content in matrix were increased with decreasing the aging temperature from $1400^{\circ}C$ to $1200^{\circ}C$. Galvanic potential of the aged specimen exhibited a proper emf characteristic.

  • PDF

Thermal Stress Analysis of Functuonally Graded Ceramic/Metal Composites(I)-Plasma Spraying Material- (경사기능성 세라믹/금속 복합재료의 열응력 해석(1)-플라즈마 용사재-)

  • Song, Jun-Hee;Lim, Jae-Kyoo;Chung, Se-Hi
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.21 no.3
    • /
    • pp.439-446
    • /
    • 1997
  • A traditional notion of composites has been composed as a uniform dispersoid, but now it is proposed without regard to such rule with process development. Functionally Graded Material(FGM) consists of a new material design that is to make intentionally irregular dispersion state. In this study, thermal stress analysis of plasma spraying PSZ/NiCrAlY gradient material was conducted theoretically using a finite-element program. A formations of the model are direct bonding material(NFGM) and FGM with PSZ and NiCrAlY component element. The temperature conditions were $700^{\circ}C$ to 1100.deg. C assuming a cooling-down precess up to room temperature. Fracture damage mechanism was analyzed by the parameters of residual stress.

Effect of Degrees of Powder Mixing on the Synthesis of $Ti_3Si$ and $TiSi_2$ by Mechanical Alloying (기계적 합금화시 $Ti_3Si$$TiSi_2$ 합성에 미치는 분말 혼합도의 영향)

  • 변창섭
    • Journal of Powder Materials
    • /
    • v.6 no.1
    • /
    • pp.103-110
    • /
    • 1999
  • Different sizes of Si powder and milling medium materials (steel and partially stabilized zirconia (PSZ)) were used to synthesize $Ti_3Si$ and $TiSi_2$ by mechanical aollying (MA) of Ti-25.0.at.%Si and Ti-66.7at.% Si powder mixtures. the formation of each titanium silicide did not occur even after 360 min of MA of as-re-ceived Si and Ti powder mixtures due to the lack of homogeneity. $Ti_3Si$, however, was synthesized after 240 min of MA of Ti and 60 min-premilled Si powder mixture. ${\alpha}-TiSi_2$ and $TiSi_2$ were produced by jar milling of Ti and 60 min-premilled Si powder mixture for 48 hr and high -energy PSZ ball-milling in a steel vial for 360 min. The formation of each titanium silicide was characterized by a slow reaction rate as the reactants and product(s) coexisted for a certain period of time. The formation of $Ti_3Si$ and $TiSi_2$ and the reaction rates appeared to be influenced by the Si particle size, the homogeneity of the powder mixtures and the milling medium materials.

  • PDF

Effect of Milling Medium Materials on Mechanical Alloying of Mo-25.0at%Si Powder Mixture (Mo-25.0at%Si 혼합분말의 기계적 합금화에 미치는 밀링매체 재료의 영향)

  • 박상보
    • Journal of Powder Materials
    • /
    • v.5 no.1
    • /
    • pp.64-70
    • /
    • 1998
  • Milling media of steel and partially stabilized zirconia(PSZ) were used to produce $Mo_3$Si by mechanical alloying(MA) of Mo-25.0at%Si elemental powder mixture. The effect of milling medium materials on MA of the powder mixture have been investigated by XRD and DTA. The reaction rate and the end-product noticeably depended upon the milling medium material. The formation of $Mo_3$Si and $Mo_5Si_3$phases by PSZ ball-milling took place after 15 hr of MA and was characterized by a slow reaction rate as Mo, Si, $Mo_5Si_3$ and $Mo_3$Si coexisted for a long period of milling time. The formation of a new phase by steel ball-milling, however, did not take Place even after 96 hr of MA. DTA and annealing results showed that $Mo_5Si_3$ and $Mo_3$Si were formed after heating the ball-milled powder specimens to different temperatures. At low temperatures, Mo and Si were transformed into $Mo_5Si_3$. At high temperatures, the formation of $Mo_3$Si can be partially attributed to the reaction, 7Mo+Si+$Mo_5Si_3$-.4$Mo_3$Si . The formation of $Mo_3$Si and Mo5Si3 phases by mechanical alloying of the powder mixture and the relevant reaction rate appeared to depend upon the milling medium material as well as the thermodynamic properties of the end-products.

  • PDF