Chimie Douce Reaction to Layered High-$T_c$ Superconducting / Super-ionic Conducting Heterostructures

  • Kim, Young-Il;Hwang, Seong-Ju;Yoo, Han-Ill;Choy, Jin-Ho
    • The Korean Journal of Ceramics
    • /
    • 제4권2호
    • /
    • pp.95-98
    • /
    • 1998
  • We have developed new type of superconducting-superionic conducting nanohybrids, $Ag_xI_wBi_2Sr_2Ca_{n-1}Cu_nO_y$ (n=1 and 2) by applying the chimie douce reaction to the superconducting Bi-based cuprates. These nanohybrids can be achieved by the stepwise intercalation whereby the $Ag^+$ ion is thermally diffused into the pre-intercalated iodine sublattice of $IBi_2Sr_2Ca_{n-1}Cu_nO_y$. According to the X-ray diffraction analysis, the Ag-I intercalates are found to have an unique heterostructure in which the superionic conducting Ag-I layer and the superconducting $IBi_2Sr_2Ca_{n-1}Cu_nO_y$ layer are regularly interstratified with a remarkable basal increment of ~7.3$\AA$. The systematic XAS studies demonstrate that the intercalation of Ag-I accompanies the charge transfer between host and guest, giving rise to a change in hole concentration of $CuO_2$ layer and to a slight $T_c$ change. The Ag K-edge EXAFS result reveals that the intercalated Ag-I has a $\beta$-AgI-like local structure with distorted tetrahedral symmetry, suggesting a mobile environment for the intercalated $Ag^+$ ion. In fact, from ac impedance analyses, we have found that the Ag-I intercalates possess a fast ionic conductivity ($\sigma_i=10^{-1.4}\sim 10^{-2.6}\Omega^{-1}\textrm{cm}^{-1}\;at\;270^{\circ}C$ with an uniform activation energy ($\DeltaE_a=0.22\pm 0.02$ eV). More interesting finding is that these intercalates exhibit high electronic conducting as well as ionic ones ($t_i$=0.02~0.60) due to their interstratified structure consisting of superionic conducting and superconducting layers. In this respect, these new intercalates are expected to be useful as an electrode material in various electrochemical devices.

  • PDF

현수교 케이블 송기시스템 효율화를 위한 지역별 상대습도 환경 분석 (Analysis of Regional Relative Humidity Environment for Dehumidification System Efficiency of Suspension Bridge Cable)

  • 서동우;김가영
    • 한국산학기술학회논문지
    • /
    • 제19권7호
    • /
    • pp.88-94
    • /
    • 2018
  • 국내외 현수교량 주케이블의 경우, 부식을 방지하기 위해 송기시스템을 통하여 주케이블 내부 상대습도를 보통 $40%{\pm}5%$ 이하로 유지하고 있다. 국내 주케이블 송기시스템이 설치된 현수교량의 위치는 모두 지리적으로 온난다습한 기후에 노출되는 빈도가 높은 해안지역이며, 특히나 우리나라의 해안지역은 각 계절의 온도차 및 일교차가 크기 때문에 강재 부식에 더욱 열악한 조건이다. 본 연구에서는 지역별 환경분석을 수행함으로써 보편적으로 사용하고 있는 송기시스템의 가동기준 40%가 아닌 좀 더 효율적인 지역별 송기시스템 가동 기준을 수립하는데 기초자료로 활용하고자 하였다. 최근 국내에 가장 큰 영향을 끼친 태풍 BOLAVEN(2012)과 CHABA(2016) 기간의 상대습도 분포, 분석 기간(2012~2016) 중 내습한 모든 태풍의 기간을 제외한 여름철과 겨울철의 상대습도 분포, 기온과 연계한 겨울철 상대습도 분포 분석을 통해 지역별로 송기시스템 가동기준을 차별화하는 것에 대한 근거를 마련할 수 있었다. 미래 기후변화로 인한 해수면 온도 상승 및 강수량 증가의 영향을 고려할 때 더욱더 객관적인 지역별 송기시스템 가동기준이 필요할 것으로 판단되며, 이는 추후 현수교 주케이블의 송기시스템 가동에 대한 경제적 효율성을 높일 수 있을 것으로 사료된다.

신호 제거 궤환부의 전류 제어 적응형 알고리즘을 이용한 IMT-2000용 선형화 증폭기 제작 (Fabrication of IMT-2000 Linear Power Amplifier using Current Control Adaptation Method in Signal Cancelling Loop)

  • 오인열;이창희;정기혁;조진용;라극한
    • 대한전자공학회논문지TC
    • /
    • 제40권1호
    • /
    • pp.24-36
    • /
    • 2003
  • IMT-2000 서비스의 전송제한은 3GPP에 규정하고 있다. IS-95A 서비스보다 IMT-2000 서비스는 3배의 대역폭을 가짐으로 해서 Peak to Average가 높아졌고, 이 때문에 인접채널에 대한 영향을 줄이는 쪽으로 더 주위 깊게 설계하여야 하는 어려움이 발생하였다. 이러한 요소에 가장 민감하게 동작하는 모듈이 이동통신 시스템에 최종단에 위치하여 멀리까지 서비스를 가능케 하는 HPA(High Power Amplifier)이다. HPA는 Pl㏈ 근처에 동작시킴으로 인해 3차 5차 신호로 인해 인접채널에 영향을 미치며, 신호가 포화됨으로 인해 왜곡이 발생한다. 이에 HPA를 어떻게 선형화 시킬 수 있을 것이냐가 중요한 요소로써 작용하는데, 본 논문에서는 가장 복잡한 구조로 이루어져 있지만 선형화 방법에 있어 탁월한 개선 능력을 갖는 Feed-forward 방식을 설계 제작하였다. 본 논문은 Feed-forward의 1차 궤환부인 신호 제거 궤환부에서 얻어진 전류를 검출하여 알고리즘을 수행케 함으로써 환경변화에서도 무리 없이 동작하는 적응형 40Watt Feed-forward 선형화 증폭기가 되도록 하였다. 일반적인 RF 출력 신호를 검출하는 방식은 회로가 복잡하며, 합성기 출력에서 검출을 하기 때문에 신호검출의 정확성에서도 떨어지는 단점이 있다. 또한 선형화 증폭기의 최종 출력에서의 에러 신호를 감지하여 최적화시키는 알고리즘 역시 기존 방식인 Pilot 신호를 이용하지 않고 에러량 검출 방식을 적용하셔 W-CDMA용 선형화 증폭기가 되도록 하였다. 결과적으로 54㏈의 이득특성을 얻으면서 IW에서 40W 출력시까지 어느 동작에서도 30㎑ 대역폭 내에서 -26㏈m Max@3.515㎒ ACPR(Adjacent Channel Power Ratio) 특성, 48㏈c Max@±5㎒ ACLR (Adjacent Channel Leakage Power Ratio) 특성을 모두 만족하여 3GPP의 국제규격을 만족하는 선형화 증폭기가 되도록 하였다.

보건용 마스크 초미세먼지 제거 성능 평가 및 재사용 연구 (Performance and reusability of certified and uncertified face masks)

  • 이해범;김서정;주흥수;조희주;박기홍
    • 한국입자에어로졸학회지
    • /
    • 제15권4호
    • /
    • pp.191-202
    • /
    • 2019
  • In this study, performance (particle removal efficiency and breathing resistance) of several commercially available face masks (electrostatic filter masks (KF80 certified), a nanofiber filter mask (KF80 certified), and an uncertified mask) with their filter structure and composition were evaluated. Also, effects of relative humidity (RH) of incoming air, water and alcohol exposure, and reusability on performance of face masks were examined. Monodisperse and polydisperse sodium chloride particles were used as test aerosols. Except the uncertified mask filter, PM2.5 removal efficiency was found to be higher than 90%, and the nanofiber filter mask had the highest quality factor due to the low pressure drop and high removal efficiency (nanofibers were arranged in a densely packed pore structure and contained a significant amount of fluorine in addition to carbon and oxygen). In the case of the KF80 certified mask, the removal efficiency was little affected when the RH of incoming air increased. When the mask filters were soaked in water, the removal efficiency of mask filters was degraded. In particular, the uncertified mask filter showed the highest removal efficiency degradation (26%). When the mask was soaked in alcohol, the removal efficiency also decreased with the greater degree than the water soaking case. The nanofiber mask filter showed the strongest resistance to alcohol exposure among tested mask filters. During evaluation of reusability of masks in real life, the removal efficiency of certified mask filter was less than 4% for 5 consecutive days (2 hours per day), while the removal efficiency of uncertified mask filter significantly decreased by 30% after 5 days.

카드뮴 이온으로 완전히 치환한 제올라이트 A를 진공 탈수한 구조와 이것에 요오드를 흡착한 결정구조 (Crystal Structures of Vacuum Dehydrated Fully $Cd^{2+}$-Exchanged Zeolite A and of Its iodine Sorption Complex)

  • 장세복;한영욱;김양
    • 한국결정학회지
    • /
    • 제4권2호
    • /
    • pp.54-62
    • /
    • 1993
  • Cd2+ 이온으로 이온교환된 제올라이트 A를 650℃에서 2 ×10-6 T orr의 진공하에서 탈수한 구조 (a:l2.189(2)A)와 이 결정에 요오드가 흡착된 구조 (a:l2.168(2) A)를 21℃에서 입방공간군 Pm3m를 사용하여 단결정 X-선회절법으로 해석하고 정밀화하였다. 탈수한 가In-A의 구조 는 Full-rmoix 최소자승법 정밀화 계산에서 I > 3σ(I)인 186개의 독립반사를 사용하여 최종오차인자를 Rl:0.057, Ra:0.003 까지 정밀화 계산하였고, 이 결정을 요오드로 흡착시킨 구조는 181 개의 독립 반사를 사용하려 Rl = 0.082, R2 : 0.085가지 정밀화시켰다. 두 결정에서 단위세포당 6개의 Cd2+ 이온은 서로 다른 2개의 3회 회전축상에 위치 하고 있었다. 요오드가 흡착된 구조에서 4개의 Cd2+ 이온 은 0(3)의 (111) 평면에서 큰 동공쪽으로 약 0.68(1) A 들어간 I3- 이온이 결합하고 있고 나머지 2개의 Cd2+ 이온은 0(3)의 (111) 평면에서 소다라이트 동공 깊숙히 약 0.68(1) A 들어간 자리에 위치 하고 있다. 단위세포당 약 4개의 I이온이 큰 동공내에 흡착되었다. 각각의 I-는 6-링 Cd2+와 골조의 8-링 산소에 다리를 놓고 있으며 0(1)-I(1)-I(2) 각도는 172(1)˚로써 거의 선형이고 약한 전 하이동 착물을 골조의 8-링 산소와 이루고 있다. 큰 동공 내에 존재하는 I이온은 부분적으로 탈수된 효In-A에서 요오드 증기와 물분자가 반응하여 H+이온과 I-이온이 생성된 후 다시 I이온과 l2 분자와 반응하여 생성되었을 것이다.

  • PDF

TiN/Ti 다층막 코팅된 생체용 Ti-30Ta-xZr 합금의 부식특성 (Corrosion Characteristics of TiN/Ti Multilayer Coated Ti-30Ta-xZr Alloy for Biomaterials)

  • 김영운;조주영;최한철
    • Corrosion Science and Technology
    • /
    • 제8권4호
    • /
    • pp.162-169
    • /
    • 2009
  • Pure titanium and its alloys are drastically used in implant materials due to their excellent mechanical properties, high corrosion resistance and good biocompatibility. However, the widely used Ti-6Al-4V is found to release toxic ions (Al and V) into the body, leading to undesirable long-term effects. Ti-6Al-4V has much higher elastic modulus than cortical bone. Therefore, titanium alloys with low elastic modulus have been developed as biomaterials to minimize stress shielding. For this reason, Ti-30Ta-xZr alloy systems have been studied in this study. The Ti-30Ta containing Zr(5, 10 and 15 wt%) were 10 times melted to improve chemical homogeneity by using a vacuum furnace and then homogenized for 24 hrs at $1000^{\circ}C$. The specimens were cut and polished for corrosion test and Ti coating and then coated with TiN, respectively, by using DC magnetron sputtering method. The analyses of coated surface were carried out by field emission scanning electron microscope(FE-SEM). The electrochemical characteristics were examined using potentiodynamic (- 1500 mV~+ 2000 mV) and AC impedance spectroscopy(100 kHz~10 mHz) in 0.9% NaCl solution at $36.5{\pm}1^{\circ}C$. The equiaxed structure was changed to needle-like structure with increasing Zr content. The surface defects and structures were covered with TiN/Ti coated layer. From the polarization behavior in 0.9% NaCl solution, The corrosion current density of Ti-30Ta-xZr alloys decreased as Zr content increased, whereas, the corrosion potential of Ti-30Ta-xZr alloys increased as Zr content increased. The corrosion resistance of TiN/Ti-coated Ti-30Ta-xZr alloys were higher than that of the TiN-coated Ti-30Ta-xZr alloys. From the AC impedance in 0.9% NaCl solution, polarization resistance($R_p$) value of TiN/Ti coated Ti-30Ta-xZr alloys showed higher than that of TiN-coated Ti-30Ta-xZr alloys.

DGS 방식 DC Block을 이용한 증폭기의 설계 (Design of An Amplifier using DGS Block)

  • 이경희;정용채
    • 한국전자파학회논문지
    • /
    • 제12권3호
    • /
    • pp.432-438
    • /
    • 2001
  • 본 논문은 Defected Ground Structure(DGS)를 DC block에 적용한 후 DC block의 부분인 λ/4-결합 선로의 간격과 길이의 변화를 EM 시뮬레이션과 실제 제작을 통하여 알라보았다. 그 결과 일반적인 DC block을 사용할때와 동일 출력 조건하에서 DGS 구조의 DC block의 λ/4-결합선로사이의 간격이 0.1 mm에서 0.46 mm로 0.36 mm만큼 늘어나고λ/4-결합 선로의 길이는 71.7 mm에서 13.32 mm로 4.5 mm만큼 줄어드는 것을 알 수 있었다. 또한 Blocking 캐패시터, 일반적인 DC block, DGS 구조의 DC block을 사용하는 세 종류의 전력증폭기를 제작한 후 특성을 확인해 보았다. 먼저 각 증폭기의 산란 파라미커 특성을 살펴본 결과 3.2$\pm$0.05 GHz의 주파수 대역에서 세 증폭기 모두 유사한 이득 특성과 산란 파라미터 특성을 갖음을 알수 있었다. 그리고 3.2 GHz의 CW 신호를 인가하여 주신호의 출력 전력이 25dBm 일 때 하모닉 특성을 스펙트럼 분석기로 분석한 결과 캐패시티를 사용시에는 주신호와 2차 하모닉 성분과의 차이가 -44.83dBc 일반적인 DC block과 DGS DC block 사용시에는 -66.84와 -64.33 dBc로서 일반적인 DC block 사용시와 DGS block 사용시에 하모닉 특성이 거의 일치함을 확인하였다.

  • PDF

Synthesis of Tellurium Sorption Complexes in Fully Dehydrated and Fully Ca2+-exchanged Zeolites A and X and their Single-crystal Structures

  • Lim, Woo-Taik;Park, Jong-Sam;Lee, Sang-Hoon;Jung, Ki-Jin;Heo, Nam-Ho
    • Bulletin of the Korean Chemical Society
    • /
    • 제30권6호
    • /
    • pp.1274-1284
    • /
    • 2009
  • Single crystals of fully dehydrated and fully $Ca^{2+}$-exchanged zeolites A (|$Ca_6$|[$Si_{12}Al_{12}O_{48}$]-LTA) and X (|$Ca_{46}$| [$Si_{100}Al_{92}O_{384}$]-FAU) were brought into contact with Te in fine pyrex capillaries at 623 K and 673 K, respectively, for 5 days. Crystal structures of Te-sorbed $Ca^{2+}$-exchanged zeolites A and X have been determined by single-crystal X-ray diffraction techniques at 294 K in the cubic space group Pm$\overline{3}$ m (a = 12.288(2) $\AA$) and Fd $\overline{3}$ (a = 25.012(1) $\AA$), respectively. The crystal structures of pale red-brown |$Ca_6Te_3$|[$Si_{12}Al_{12}O_{48}$]-LTA and black coloured |$Ca_{46}Te_8$| [$Si_{100}Al_{92}O_{384}$]-FAU have been refined to the final error indices of $R_1/wR_2\;=\;0.1096/0.2768\;and\;R_1/wR_2$ = 0.1054/ 0.2979 with 204 and 282 reflections for which $F_o\;>\;4{\sigma}(F_o)$, respectively. In the structure of |Ca6Te3|[$Si_{12}Al_{12}O_{48}$]- LTA, 6 $Ca^{2+}$ ions per unit cell were found at one crystallographic positions, on 3-fold axes equipoints of opposite 6-rings. In |$Ca_{46}Te_8$|[$Si_{100}Al_{92}O_{384}$]-FAU, 46 $Ca^{2+}$ ions per unit cell were found at four crystallographically distinct positions: 3 $Ca^{2+}$ ions at Ca(1) fill the 16 equivalent positions of site I, 21 $Ca^{2+}$ ions at Ca(2) fill the 32 equivalent positions of site I’, 10 and 12 $Ca^{2+}$ ions at Ca(3) and Ca(4), respectively, fill the 32 equivalent positions of site II. The Te clusters are stabilized by interaction with cations and framework oxygen. In sodalite units, Te-Te distances of 2.86(10) and 2.69(4) $\AA$ in zeolites A and X, respectively exhibited strong covalent properties due to their interaction with $Ca^{2+}$ ions. On the other hand, in large cavity and supercage, those of 2.99(3) and 2.76(11) $\AA$ in zeolites A and X, respectively, showed ionic properties because alternative ionic interaction was formed through framework oxygen at one end and $Ca^{2+}$ cations at the other end.

아황산금나트륨염을 이용한 Au 범프용 금도금층의 표면형상 및 우선적 결정 성장방향 (Surface Morphology and Preferred Orientation of Gold Bump Layer formed by using $Na_3[Au(SO_3)_2]$)

  • 김인수;양성훈;박종완
    • 한국재료학회지
    • /
    • 제5권6호
    • /
    • pp.673-681
    • /
    • 1995
  • 아황산금나트륨염을 이용하여 형성된 약 20$\mu\textrm{m}$ 금도금층의 표면형상 및 우선적 결정 성장 방향에 대하여 전류밀도, 온도, 농도, pH, 교만속도, 금이온농도가 미치는 영향에 대하여 연구하였다. 표면형상은 cathode 근처의 금이온농도가 증가하는 조건[전류밀도(13.0mA/$\textrm{cm}^2$2$\longrightarrow$4.6mA/$\textrm{cm}^2$)], 온도 (3$0^{\circ}C$$\longrightarrow$6$0^{\circ}C$), pH(12.0$\longrightarrow$9.0), 교반효과(Orpm$\longrightarrow$3200rpm), 금이온농도(10g /1$\longrightarrow$l4g/1)으로 갈수록 porous한 조직에서 미세한 조직으로의 변화가 관찰되었다. X선분석에 의하면 금도금층의 결정성장의 주방향은 표면형상과 밀접한 관계를 나타내었으며 표면형상이 미세화되는 조건인 전류밀도(13.0$\longrightarrow$14.6mA/$\textrm{cm}^2$), pH(12.0$\longrightarrow$9.0)는 감소 할수록, 온도(3$0^{\circ}C$$\longrightarrow$6$0^{\circ}C$), 교반속도(0rPm$\longrightarrow$3200rpm), 금이온농도(10g/1$\longrightarrow$g/1)]는 증가 할수록 결정성장의 주회절피크는 (111)에서 (220)으로 그 성장면이 변하고 있음이 조사되었다.

  • PDF

송산리 고분군의 지구물리학적 조사를 통한 고분축조방법 고찰 (A Study on the Construction Method of the Songsanri Tombs Using Geophysical Exploration Method)

  • 서만철;이창환;정계옥;김동현
    • 보존과학회지
    • /
    • 제6권1호
    • /
    • pp.61-70
    • /
    • 1997
  • 자력, 자연전위, 비저항 측정을 포함하는 지구물리탐사를 송산리고분군 지역에 적용한 결과 지하구조물의 위치, 고분축조 지반 및 원지반의 차이점 등에 대한 정보를 비교적 정확하게 얻을 수 있었다. 비저항의 분포로 확인된 기존 지반의 지역에서는 자연전위 값도 매우 낮다. 기존 지반의 경우 03 mv/m의 매우 낮은 전위차와 1000 1500 ohm-m의 상대적으로 높은 비저항치를 보이는 반면, 고분축조지역의 지반은 $-20\~30mV/m$의 큰 자연전위값과 200 ohm-m이내의 낮은 비저항을 보여 매우 대조적이다. 전기비저항 및 자연전위분포로 볼 때 백제시대 당시 고분축조를 위하여 절개했던 부분이 남북방향으로 약 35 m정도이었음을 알 수 있다. 원래의 지반과 고분축조를 위해 굴착한 부분의 지반의 매질이 확연히 다르다는 것은 고분축조가 동굴을 파서 그 내부에 축조했다기 보다는 전체 축조부지를 절개하여 평탄화한 후 모형을 만들어 축조한 후 그 후에 다시 파낸 암석부스러기 및 흙을 채워 원래 지형을 복원하였을 것으로 해석된다. 그 후 모형을 내부로부터 제거하여 고분을 축조하였을 것으로 사료된다.

  • PDF