• Title/Summary/Keyword: PEG treatment

Search Result 289, Processing Time 0.025 seconds

Penetration of PEG by Treatment Condition of Waterlogged Wood (수침고목재의 처리조건에 따른 PEG 침투상태)

  • Lee, Gyeong-Cheol;Lee, Jong-Shin
    • Journal of Conservation Science
    • /
    • v.29 no.3
    • /
    • pp.243-247
    • /
    • 2013
  • This study was conducted to investigate the penetration of PEG for conservation treatment conditions of archaeological waterlogged wood. The weight percent gain was examined, depending on the solvent of PEG, concentration and treatment period and temperature of treatment solutions. The penetration of PEG in the cell lumina of treatment woods was observed by scanning electron microscope. The results showed that the type of solvents had no influence on PEG penetration. In the concentration of the PEG treatment solutions, the weight percent gains (WPGs) were increased with increase in concentration of PEG. In terms of the period of the soaking treatment, a maximum WPGs were obtained for only 20 days. There was no distinctive difference in the WPGs by difference the temperature of the treatment. In conclusion, in the conservation of small size of archaeological waterlogged wood, it is confirmed that optimal solvent type and treatment period of PEG are water and 20 days, respectively.

Plywood Properties by PEG Treatment Conditions on Veneer (단판(單板)의 PEG 처리조건(處理條件)에 따른 합판(合板)의 성질(性質))

  • Suh, Jin-Suk;Doh, Geum-Hyun
    • Journal of the Korean Wood Science and Technology
    • /
    • v.17 no.2
    • /
    • pp.20-25
    • /
    • 1989
  • This study was carried out in order to investigate the treatment effect of PEG soln which is a common dimensional stabilizer to green log. sawing panel etc, on bonding product including plywood widely-used in secondary processing unit. The 30% concentration of aqueous PEG soln. with molecular weight of 400, 1.000 and 4,000 were prepared respectively, and also dipping the veneer in the PEG soln. spreading the PEG soln. on veneer and mixing the PEG soln. in the adhesive were allowed. Then the ratio of PEG impregnation on veneer, the adhesive strength of plywood were epitomized as follows: The ratio of impregnation by PEG 4,000 at dipping condition was highest. while that by PEG 400 at same condition was lowest. However, the effect of PEG molecular weight on the ratio of impregnation at spreading condition did not occur. 2. The adhesive strength was great in the order of 4,000>400>1,000 in molecular weight of PEG at dipping and spreading conditions. In case of mixing the PEG soln. in the adhesive, the adhesive strength was great in the order of 400>1,000>4,000 in molecular weight of PEG. Throughout three treatment conditions, PEG 400 was relatively favourable with about 10kg/$cm^2$ dry strength. 3. The adhesive strength was great 10 the order of spreading >dipping >mixing condition. 4. Although adhesive strength with the 30% concentration of aqueous PEG soln. was decreased by 35% and over, compared to control (non-treatment) adhesive strength, all types of PEG treatment except mixing the PEG soln. in the adhesive exceeded the standard dry strength for common use panel. 7.5kg/$cm^2$. 5. In warm water-proof test, the adhesive strengths by all PEG treatment conditions were less than the standard wet strength, 7.5kg cot, and also delamination of glue line occured mostly in mixing in the PEG soln. in the adhesive condition.

  • PDF

The Vacuum Freeze-Drying Experiment for Water-logged Wood Excavated from Wolpyongdong in Taejon (수침목재(水浸木材)의 동결건조(東結乾燥) 실험보고 -대전(大田) 월평동출토(月平洞出土) 유물을 중심(中心)으로-)

  • Kim, Kyoung-su;Yi, Yong-hee
    • Conservation Science in Museum
    • /
    • v.1
    • /
    • pp.27-35
    • /
    • 1999
  • To get the best result from vacuum freeze drying of water-logged wood, it is necessary for objects to find out the best conditions such as chemicals, appropriate concentration of solution, impregnation method and etc. Such best conditions could be set up by pre-treatment experiments. Two kinds of wood(Pinus densiflora S. et Z. and Quercus acutissima Carruth) were pre-treated by four methods: 2-step PEG treatment(PEG#200-PEG#4000), sorbitol treatment, PEG#200+PEG#4000 treatment, and sorbitol+PEG#4000 treatment. After those pre-treatment, vacuum freeze-drying was undertaken. Then the effect of dimensional stability were compared. When using 2-step PEG treatment, a solution of 60% PEG #4000 got the best dimensional stability for pine and in case of the oak, a solution of 40% PEG#4000 got the best. Sorbitol treatment got rather good result for the pine only when applied with 40% solution of sorbitol. Sorbitol, PEG#200+PEG#4000 and sorbitol+PEG#4000 treatments to the oak didn't affect on dimensional stability sufficiently.

Experiment on Conservation Treatment Method(PEG, Sucrose and Lactitol) and Degree of State-change with RH of Waterlogged Archaeological Wood (수침고목재(水浸古木材)의 보존(保存)을 위한 PEG, Sucrose, Lactitol 처리(處理) 및 습도조건(濕度條件)에 따른 상태변화(狀態變化) 실험(實驗))

  • Yi, Yong-hee;Kim, Soo-choul;Park, Young-man;Kim, Kyoung-su
    • Conservation Science in Museum
    • /
    • v.2
    • /
    • pp.19-25
    • /
    • 2000
  • In order to studies proper conservation treatment condition of waterlogged archaeological wood excavated from wetland in Shinchang-dong, Kwangju, 2 kinds of wooden objects were treated with PEG(Poly-Ethylene Glycol), sucrose and lactitol and their size stability and relative humidity were analyzed and compared each other. The result showed that Quercus spp. had the highest size stability in 2 Step-PEG treatment using PEG#200(MW:200) and PEG#4000 (MW:3,350) and Acer spp. was the highest in treatment using only PEG#4000. In relative humidity test after treatment 2 Step-PEG treatment showed the lowest size stability. In the meantime, sucrose and lactitol-treated sample was fast for penetration, sucrose-treated sample showed a sharp increase for penetration in as high as 84% humidity condition and medicine flew out a lot and lactitol-treated sample got enlarged with fine cracking(splitting) in relative humidity test. In relative humidity test, the samples showed cracking(splitting) in all treatment materials except for 2 Step-PEG treatment. This study showed that waterlogged archaeological wood excavated from Shinchang-dong had the highest size stability and highest adaptation to humidity change in case of treatment with 2 Step-PEG.

Measuring PEG Retentions and EMCs of PEG Impregnated Softwood Specimens after Heat-treatment (PEG 주입 침엽수 시편의 열처리 후 PEG 잔류량과 평형함수율 측정)

  • Hong, Seung-Hyun;Kim, Chung-Ho;Lim, Ho-Mook;Kang, Ho-Yang
    • Journal of the Korean Wood Science and Technology
    • /
    • v.41 no.3
    • /
    • pp.173-180
    • /
    • 2013
  • This study was carried to provide basic data for the research of the effect of PEG impregnation on preventing wood from cracking during heat treatment. Three popular softwood species were selected for investigating the PEG penetration rate and retention depending on PEG molecular weight, PEG retention after heat treatment and their EMCs. The average retentions of PEG400 were reversely proportional to the basic densities of three species and those of the other PEGs showed similar behaviour as well. It is obvious that PEG retention decreased as PEG molecular weight increased with a species. PEG impregnation increased or decreased the moisture contents of the specimens within 2%, and increased their basic densities by 16.8% as a maximum. The Weight Percentage Losses of PEG400 during heat treatment were the largest among three PEG levels, which implied that lower molecular weight PEG leached more than the highers. There was less difference in EMC between PEG impregnated and control specimens at low RH, but their difference increased at high RH.

Effects of Polyethylene Glycol Treatment for Improvement of Preservative Penetration and Prevention of Drying Check of Preservative Treated Round Post (방부처리 원주가공재의 방부제 침윤도 향상 및 건조 할렬 방지를 위한 폴리에틸렌 글리콜 처리 효과)

  • Lee, Jong-Shin;Yoon, Sun-Mi
    • Journal of the Korean Wood Science and Technology
    • /
    • v.30 no.4
    • /
    • pp.27-32
    • /
    • 2002
  • We investigated the effect of polyethylene glycol(PEG) treatment of preservative treated green japanese cedar(Cryptomeria japonica) round posts on their preservative penetration and check formation during the air drying. The round rods were dip-treated in 10% preservative solution of Basilit CFK for 1 day, followed by application(3, 5, and 10 times) with 50% PEG-400 solution, and then dried for 30 days under natural conditions. The rate of preservative penetration into sapwood was a low by 23.2% without PEG treatment, whereas that was a high by about 51.2~64.5% with PEG treatment. From these results, it was assumed that PEG played an affirmative role in the penetration of preservative components loaded onto the surface of round rods by dipping. During the air drying, the formation of drying checks decreased significantly with increasing application times of PEG. Even though some drying checks in PEG treated rods were developed, the number and size of checks was reduced remarkably by PEG treatment. After 2 months of outdoor exposure, PEG treatment failed to reduce checking in preservative-treated rods whereas finishing of polyurethane resin lacquer after PEG treatment was significantly effective in preventing check development.

Effects of PEG Treatment on Seed Viability and Seedling Emergence in Rice, Barley and Wheat (벼, 보리, 밀 종자의 PEG 처리가 종자활력과 포장출아에 미치는 영향)

  • 이성춘;김진희;정춘화
    • KOREAN JOURNAL OF CROP SCIENCE
    • /
    • v.41 no.2
    • /
    • pp.145-156
    • /
    • 1996
  • The effects of priming with different polyethylene glycol (PEG 6, 000) solutions on the germination, emergence characteristics and early plant growth in rice, barley and wheat were investigated. Rice, barley and wheat seeds were subjected to various priming conditions of osmotic potentials (-0. 75, -1.00 and -1.50 MPa) of PEG, and incubation period were 5 days at 25, 20, 2$0^{\circ}C$, respectively. The percentage of water absorption was highest in barely, and lowest in rice, and all the treatments enhanced water absorption in barley, but showed no significant effects in rice and wheat. Respiration quotient was lower than none PEG treatment seeds, and those of barley and wheat were higher than rice regardless of PEG concentration, and that of rice increased with high PEG concentration. Total germination percentage of osmoconditioning seeds with PEG was higher than that of none treatment seed, and those of barley and wheat were significant. The artificially deteriorated seeds with PEG treatment seeds after ageing treatment could recover to nearly the same germination level as that of the control seeds. The effects of coating polymer were higher than osmoconditioning with PEG, and germination characteristics in rice showed varietal difference at PVP and waterlock at recoated seeds after PEG treatment. Osmoconditioning with PEG reduced mean germination and emergence time, but there was no difference among PEG concentrations. The plant height of PEG treaed seed in rice was taller and those of barely and wheat showed varietal difference, and those of polymer-coated seed after PEG treatment were different among the polymers. The dry weight of PEG treatment were different among the crops, and those were increased with the high PEG concentration. The emergence percentage of PEG-treated seed were higher than none-treated seed, and those were decreased with the increased PEG concentration, and the highest emergence percentage of rice, barley and wheat were 90, 50 and 50% soil moisture content, respectively. The time to emergence in rice was longer than barley and wheat, and those in rice was shortened in high soil moisture content, and barley and wheat were shortened in low soil moisture content.

  • PDF

Humidity-Controlled Drying of PEG-Treated Waterlogged Woods (PEG처리 수침고목재의 조습건조)

  • Lee, Kwang-Hee;Kim, Soo-Chul;Park, Won-Kyu
    • Journal of Conservation Science
    • /
    • v.27 no.1
    • /
    • pp.91-100
    • /
    • 2011
  • This study is to examine the PEG concentration, and drying humidity and drying periods of humidity-controlled drying(HCD) for conservation of waterlogged woods(Pinus densiflora S. et Z.), and dimension stability of HCD were compared with those of air-drying and vacuum freeze-drying(VFD). Dimension stability of vacuum freeze-drying was the most excellent, i.e., PEG crystal was uniformly distributed in woods. Increasing concentrations of PEG, dimension stability of HCD was increased and drying periods decreased. Dimension stability of HCD after the treatment with the high concentration(70%) of PEG soaking was similar to those of VFD after the treatment with the low concentration(40%) of PEG soaking. In conclusion, high concentration(about 70% in water) PEG solution was the most suitable as a pre-treatment for HCD of waterlogged woods. However, drying should be maintained with enough high humidity and longer period.

Dimensional Stabilization of Japanese Larch by Poly(ethylene glycol) Treatment (폴리에틸렌글리콜(PEG) 처리에 의한 일본잎갈나무의 치수안정화)

  • 정재열;한규성
    • Journal of Korea Foresty Energy
    • /
    • v.20 no.2
    • /
    • pp.41-45
    • /
    • 2001
  • Japanese Larch(Larix kaempferi) was treated with aqueous solutions(30%, 40%, 50%) of polyethylene glycols(PEG, #1000, #1500, #4000, #6000) for the dimensional stabilization. The antiswelling efficiency(ASE) was measured for the evaluation of the dimensional stabilization. The weight percent gains(WPGs) of the woods treated with 40% solutions were higher than those of the others, and the highest WPG was achieved by treatment with 40% solution of PEG #1500. The ASE decreased with increasing molecular weight of PEG. ASE of woods treated with PEG #1000 and PEG #1500 were higher than those of the others.

  • PDF

Determination of PEG Concentration and Solvent Selection for Freeze-Drying of Highly-Degraded Waterlogged Woods (고함수율 수침고목재의 동결 건조를 위한 PEG 전처리 농도 및 용매 설정)

  • Kim, Soo-Choul;Park, Won-Kyu;Yi, Yong-Hee
    • Journal of Conservation Science
    • /
    • v.9 no.1
    • /
    • pp.40-47
    • /
    • 2000
  • Dimension stability was examined after PEG pretreatment and post freeze-drying treatment in order to determine the PEG(#3350) concentration and solvent for pre-treatment of freeze-drying of highly-degraded waterlogged ash woods(Fraxinus spp.; ca. 5,700 BP) excavated from peat lands at Pyungtack, Kyounggi-do. At the low concentration (<30-40%) of PEG soaking in both water and t-butanol, the weight increases abruptly, but at high concentration (>50%) gradually, consequently, taking longer treatment time. PEG loading was higher in t-butanol solution than in water. However, the best dimesional stability was obtained from freeze-drying after lower PEG solution (40% in water) soaking. Low dimensional stability, found in the samples treated with higher PEG solutions (60%-70% in t-butanol), might come from incomplete freezing and excess PEG absorbing moisture. The samples air-dried after 70% PEG treatment had collapse defects. In conclusion, the use of low concentration (about 40% in water) PEG solution was the most suitable pretreatment for freeze drying of highly-degraded waterlogged ash woods.