  • Medical polymers require sterilization and must be able to maintain material properties for a specified shelf life. Sterilization can be achieved by using gamma or e-beam exposure. In this study, accelerated aging tests of poly(ether-block-amide) (PEBA) copolymer samples is presented. PEBA copolymer samples with different polyether content that result in Shore hardness of 35D to 72D, were sterilized using e-beam radiation followed by accelerated aging at $55^{\circ}C$. E-beam sterilization effect on molecular weight and mechanical property has performed and analyzed. The average molecular weight significantly reduced as a result of ageing. The enlarged proportion of low molecular weight chains in the aged samples is consistent with the generation of degradation products produced by oxidative chain scission. Also E-beam materials have shown decreased tensile strength and elongation. Overall, this study demonstrated that the medical grade PEBA was significantly affected by radiation exposure over aging time, particularly at high irradiation doses. For medical use in case of radiation sterilization required, it is recommended to avoid Pebax material. If Pebax material must be in use for medical device, recommend to use alternate sterilization method such as Ethylene Oxide sterilization.

Poly(ether block amide) (PEBA) Based Membranes for Carbon Dioxide Separation (이산화탄소 분리를 위한 PEBA공중합체 기반 분리막)

  • Lee, Jae Hun;Patel, Rajkumar
    • Membrane Journal
    • /
    • v.29 no.1
    • /
    • pp.1-10
    • /
    • 2019
  • Poly(ether block amide) (PEBA) is one of the commercially important class of block copolymer very much suitable specifically for $CO_2$ separation. Gas separation membrane need to have good mechanical strength as well as high gas permeability. The crystalline polyamide (PA) block provides the mechanical strength while the rubbery polyether (PE) group being $CO_2$-philic facilitate $CO_2$ permeation though the membrane. Composition of thermoplastic and rubbery phase in the polymer are changed to fit into suitable gas separation application. Although PEBA has good permeability, the selectivity of the membrane can be enhanced by incorporating molecular sieve without affection much the gas permeability. Mixed matrix membrane (MMM), a class of composite membrane combine the advantage of polymer matrix with the inorganic fillers. However, there are some disadvantages based on the compatibility of the inorganic fillers and polymeric phase. This review covers both the advantage and limitations of PEBA block copolymer based composite membrane.

Preparation of PEBA/PDMS Blend Membranes for Separation of Carbon Dioxide (PEBA/PDMS 블렌드막의 제조 및 이산화탄소 분리 특성 연구)

  • Park, You-In;Kang, Ha-Sung;Nam, Mi-Yeon;Lee, Eun-Woo;Kim, Beom-Sik;Lee, Sang-Hak;Suh, Jeong-Kwon;Suh, Dong-Hak;Feng, Xianshe
    • Membrane Journal
    • /
    • v.19 no.1
    • /
    • pp.83-88
    • /
    • 2009
  • Poly(ether block amide) (PEBA)/poly(dimethyl-siloxane) (PDMS) blend membranes (PEBA : PDMS = 5 : 2, 6 : 1 wt%) were prepared through the solution-casting and phase inversion process in order to demonstrate their superior performance in carbon dioxide separation. PDMS and PEBA (4033) were also prepared by the same method using n-butanol as a solvent. To study the gas permeation properties, the membranes were characterized with SEM and tested with carbon dioxide and nitrogen at $35^{\circ}C$ and pressure ranging from 3 to 5 atm. In conclusion, PEBA/PDMS blend membranes were shown to have selectivity for $CO_2/N_2$ separation that is 4 to 5 magnitudes greater than that of PDMS membrane at 3 atm.

Synthesis and Characterization of Thermoplastic Elastomer Poly(ether-b-amide) Containing Aromatic Moiety (방향족 구조가 포함된 열가소성 탄성체 Poly(ether-b-amide)의 합성 및 특성)

  • Lee, Ji Hun;Kim, Hyung Joong
    • Polymer(Korea)
    • /
    • v.38 no.5
    • /
    • pp.596-601
    • /
    • 2014
  • Polyamide (PA) oligomers, which are the hard segment of poly(ether-block-amide) (PEBA), presenting thermoplastic and high performance elastomeric properties were prepared by polycondensation between 4-aminobenzoic acid and 12-aminododecanoic acid. Subsequently PEBAs were obtained by addition polymerization of the PA oligomers and various molecular weights of poly(tetramethylene glycol) (PTMG). The structure of the final PEBA was identified by using FTIR and $^1H$ NMR and the thermal properties depending on changes in the structure of hard segment were collected by using DSC and UTM analysis. As the results, the melt temperature ($T_m$), the initial modulus, and the maximum strength of PEBAs increased with an increase in aromatic moiety up to 30% without reducing crystallinity.

Characterization of Poly(ether-block-amide)s Prepared from Oligomeric Polyamide 12 via Dispersion Polymerization (분산중합에 의한 폴리아미드 12 올리고머의 제조와 그를 이용한 Poly(ether-block-amide)의 특성)

  • Kim, Doo-Hyeon;Lee, Ji-Hun;Kim, Hyung-Joong
    • Polymer(Korea)
    • /
    • v.36 no.4
    • /
    • pp.513-518
    • /
    • 2012
  • Polyamide 12 (PA12) oligomers (oPA1) were prepared by dispersion polymerization of ${\omega}$-amino carboxylic acid and dibasic acid in a dispersion medium, thermally stable hydrocarbon liquid paraffin, YK-D130 (a step polymerization). The molecular weight and various properties of other oligomeric PAs (oPA2) obtained by bulk polymerization without the medium were compared with those of oPA1s. The oPA1s showed lighter white color and narrower molecular weight distribution than oPA2s at the same molecular weight. Moreover elastomeric poly(ether-block-amide) (PEBA)s were synthesized with oPA1 and oPA2 as hard segments and poly(tetramethylene glycol) (PTMG) as a soft segment. The molecular weight distribution, and mechanical property of the PEBA originated from the both oligomeric PAs were characterized.

Gas Permeation Properties of Carbon Dioxide and Methane for $PEBAX^{TM}$/TEOS Hybrid Membranes ($PEBAX^{TM}$/TEOS 하이브리드 분리막을 통한 이산화탄소와 메탄의 기체투과특성)

  • Kim, Hyunjoon
    • Korean Chemical Engineering Research
    • /
    • v.49 no.4
    • /
    • pp.460-464
    • /
    • 2011
  • Poly(ether-block-amide)(PEBA, $PEBAX^{TM}$) resin is a thermoplastic elastomer combining linear chains of hard-rigid polyamide block interspaced soft-flexible polyether block. It was believed that the hard polyamide block provides the mechanical strength and permeation selectivity, whereas gas transport occurs primarily through the soft polyether block. The objective of this work was to investigate the gas permeation properties of carbon dioxide and methane for $PEBAX^{TM}$-1657 membrane and compare with those obtained for other grade of $PEBAX^{TM}$, $PEBAX^{TM}$-2533. And the organic/inorganic hybrid membranes were prepared using $PEBAX^{TM}$ and TEOS(tetraethoxysilane) by sol-gel process, and gas permeation properties were studied. $PEBAX^{TM}$-2533 membrane exhibited higher gas permeability coefficients than $PEBAX^{TM}$-1657 membrane. This was explained by the increase of chain mobility. The permeability coefficients for $PEBAX^{TM}$/TEOS hybrid membranes were higher than pure $PEBAX^{TM}$ membranes. This results were explained by the reduction of crystallinity of polyamide block by the introduction of TEOS. Ideal separation factor of hybrid membranes does not change much. This might be due to the increase of solubility selectivity.

Antimicrobial Effects of Photodynamic Therapy Using Blue Light Emitting Diode with Photofrin and Radachlorine against Propionibacterium acnes

  • Kwon, Pil-Seung
    • Korean Journal of Clinical Laboratory Science
    • /
    • v.47 no.1
    • /
    • pp.6-10
    • /
    • 2015
  • Photodynamic therapy (PDT) apply photosensitizers and light. The purpose of this study was to evaluate the in vitro efficacy of PDT using blue LED (light emitting diode) with photofrin and radachlorin for Propionibacterium acnes. The colony forming units method was used to assess the antibacterial activity. Suspension (1 mL) containing P. acnes at $1{\times}10^5CFU/mL$ were prepared and then 2 fold serial diluted to $12.5{\mu}g/mL$ from $50{\mu}g/mL$ concentration of photofrin and radachlorin. After 60 minutes incubation, light was irradiated for 10 to 30 minutes using the following light source of wavelength 460 nm, each energy density 36, 72 and $108J/cm^2$. Bacterial growth was evaluated after 72 hours incubation in a Phenylethanol Blood Agar (PEBA) culture. In addition, flow cytometric analysis were performed to measure the live cell after PDT. Also transmission electron microscopy (TEM) was employed to evaluate the effect of pathogens by PDT. The PDT Group was perfectly killed to all kind of photosensitizers dose of $12.5{\mu}g/mL$ with irradiation of 10 minutes. Also other Groups were killed to all kind of photosensitizers dose of $6.25{\mu}g/mL$ with irradiation time of 20 and 30 minutes. The flow cytometry showed a lower number of viable bacteria in the PDT group compared to the control group. The images of the TEM results were showed in cytoplasmic membrane damage and partially deformed to cell morphologies. These results suggest that radachlorin and photofrin combine blue LED PDT can be effectively treated when was proved treatment for acnes therapy.