• Title/Summary/Keyword: Oxidation temperature

Search Result 2,414, Processing Time 0.039 seconds

A Study on Removal of Color in Dyeing Wastewater by Ozone Oxidation (오존산화에 의한 염색체수의 색도 제거에 관한 연구)

  • 정순형;최준호
    • Journal of environmental and Sanitary engineering
    • /
    • v.18 no.4
    • /
    • pp.45-51
    • /
    • 2003
  • This study was conducted to remove the color in dyeing wastewater by ozone oxidation process, and the results were summarized as follows ; The 18.3% of BOD and 56.3% TOC were removed as decreasing with pH 1 in dyeing wastewater, containing the polyester reducing process. It showed that terephthalic acid was precipitated at low pH. The color of dyeing wastewater was removed by the first order reaction, and the reaction rate constants at pH 3, 7, 12 were investigated $0.234{\;}min^{-1},{\;}0.215{\;}min^{-1}{\;}and{\;}0.201{\;}min^{-1}$ respectively. It showed that color was more effectively removed with direct reaction of ozone than radical reaction(non-direct reaction). As increasing of the water temperature, the reaction rate constants were increased slightly. It indicated that activity of ozone was improved at high water temperature.

Fabrication of $Al_2O_3/SiC$ Composite Through Oxidation of SiC (SiC의 산화에 의한 $Al_2O_3/SiC$ 복합체의 제조)

  • 김경환;이홍림;이형민;홍기곤
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.5
    • /
    • pp.535-543
    • /
    • 1997
  • The surface of SiC particles were partially oxidized to produce SiO2 layers on the SiC particles to prepare Al2O3/SiC composite by formation of mullite bonds between the grains of Al2O3 and SiC during sintering at 1$600^{\circ}C$. This process is considered to enable the sintering of Al2O3/SiC composite at lower temperature and also to relieve the stress, produced by thermal expansion mismatch between Al2O3 and SiC. In fact, Al2O3/SiC composite prepared by oxidation of SiC was observed to be more effectively sintered and densified at lower temperature. Maximum density, flexural strength and microhardness were obtained with 5.65 vol% of mullite content in Al2O3/SiC composite.

  • PDF

PRESERVATION OF QUALITY AFTER BROWN RICE DRYING

  • Goto, Kiyokazu;Miwa, Yoshihiro
    • Proceedings of the Korean Society for Agricultural Machinery Conference
    • /
    • 1996.06c
    • /
    • pp.878-885
    • /
    • 1996
  • The brown rice drying is effective for energy saving and cost reduction. However, deterioration after drying is one problem, because the skin damage occurs during the drying. So, the measures to preserve the quality has been investigated. One of major quality deteriorations is the oxidation of fat which is contained in the bran layer. So, milling should be carried out to remove the fat as soon as possible after brown rice drying. And the low temperature storage is also worth to be examined for prevention of oxidation. The effect of skin damage on the increase of fat oxidation was clarified. For the grain of skin damage, the increased of fatty acid vaule was remarkable after 70 days elapsed from occurrence of skin damage even in $15\;^{\circ}C$ condition. Therefore it is impossible to keep grain as brown rice form after brown rice drying. For the clean rice and excessively milled rice, the quality can be preserved even in high temperature of $30\;^{\circ}C$. Therefore the brown rice drying can b applied practically using the clean rice technique.

  • PDF

Advanced Lubricants for Heat Engines

  • Hsu, S.M.;Li, H.;Perez, J.M.;Ku, C.S.;Wang, J.
    • Tribology and Lubricants
    • /
    • v.11 no.5
    • /
    • pp.47-54
    • /
    • 1995
  • An advanced liquid lubricants for heat engines has been developed and tested successfully in a prototype engine. The lubricant possesses superior oxidation stability and high temperature stability and is capable of surviving for a minimum of three minutes at 425$^{\circ}$C (800$^{\circ}$C) at the ring zone and maintains stability at an oil sump temperature of 171$^{\circ}$C. The lubricant has been evaluated by the Cummins Engine Co. Out of a field of several dozens of lubricant, six lubricant was selected for a prototype 200 hours endurance testing. The NIST lubricant was one of the two lubricants that successfully finished the endurance testing. This paper describes the key lubricant considerations including oxidation and thermal stability, volatility, deposit control. The engine test conditions and the results will be presented.

Conversion and Aging Characteristics of Oxidation Catalyst for Natural Gas Vehicle with Lean-burn System (린번 천연가스자동차용 산화촉매의 정화 및 열화특성)

  • 최병철;윤성식;정종우
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.11 no.2
    • /
    • pp.134-139
    • /
    • 2003
  • This study was carried out to investigate the aging and conversion characteristics of oxidation catalysts for a natural gas vehicle with lean-bum system. The conversion of $CH_4$ was observed over the various composition ratio of PMs(Precious metals) and washcoating methods. On the fresh catalysts, Pd affected on the activity of $CH_4$ at low temperature more than other PMs in Pd-only and Rh/Pd/Pt catalysts. The activity at low temperature increased as a mount of Pd increases. On the aged catalysts, the $CH_4$ conversion efficiency of Pd-only catalyst with mono-layer washcoat decreased more than that of the other catalysts of $CH_4$ conversion. It was observed that the thermal durability of Rh/Pd/Pt catalysts with double-layer washcoat was better than the single washcoat catalyst.

High Temperature Oxidation of TiAl-based XD 45 and XD47 Intermetallics (TiAl계 XD45, XD47 금속간 화합물의 고온산화거동)

  • 심웅식;이동복
    • Journal of the Korean institute of surface engineering
    • /
    • v.35 no.4
    • /
    • pp.193-198
    • /
    • 2002
  • Alloys of XD45 (Ti45A12Nb2Mn-0.8vol%TiB$_2$) and XD47 (Ti47A12Nb2Mn-0.8vol%TiB$_2$) were oxidized between 800 and $1000^{\circ}C$ in air, and their oxidation characteristics were studied. The oxide scales consisted primarily of an outer $TiO_2$ layer, an intermediate $Al_2$$O_3$-rich layer, and an inner mixed layer of ($TiO_2$+$Al_2$$O_3$). Nb tended to present at the lower part of the oxide scale, whereas Mn at the upper part of the oxide scale. The Pt marker tests indicated that the outer oxide layer grew primarily by the outward diffusion of Ti and Mn, and the inner mixed layer by the inward transport of oxygen.

Effect of SiC on the Mullite-Cordierite Composite Properties

  • Motaman, A.;Amin, S.A.;Jahangir, A.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1067-1070
    • /
    • 2006
  • Experimental samples were produced with mullite and cordierite powders with SiC. Effects of temperature, atmosphere and additive on the composite properties were investigated by XRD, STA and PSA methods. Results show that samples containing calcinate cordierite and calcinate mullite with SiC baked in air atmosphere have not suitable properties at the temperature range of $1380-1450^{\circ}C$ due to SiC intensive oxidation, while argon atmosphere decrease SiC oxidation. Using $Bi_2O_3$ as the additive, cordierite phase formation and prevention from SiC oxidation at low temperatures were achieved, leading to the improvement of physical and mechanical properties

  • PDF

Formation of $Al_2O_3$-Composites by the Melt Oxidation of an AlZnMg-alloy (AlZnMg-합금의 용융산화에 의한 $Al_2O_3$-복합재료의 형성)

  • 김일수;김상호;강정윤
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.9
    • /
    • pp.985-994
    • /
    • 1996
  • The initiation and growth of $\alpha$-Al2O3/metal composites by the directed oxidation of molten commercial AlZnMg-alloy at 1223-1423K were investigated. Spontaneous bulk growth did not occur on the alloy alone. but the uniform initiation and growth of the composite were obtained by putting a thin layer of SiO2 particles on the surface of the alloy. Without SiO2 the external surface of the oxide layer was convered by MgO and MgAl2O4. But with the SiO2 reaction initiate the porous ZnO layers were found on the growth surface. The higher process temperature yielded a lower metal content. The oxidation product of $\alpha$-Al2O3 was found to be oriented with c-axis parallel to th growth direction. The growth rates increased with temperature and the apparent activation energy was 111.8 kJ/mol.

  • PDF

Physical and Chemical Investigation of Substrate Temperature Dependence of Zirconium Oxide Films on Si(100)

  • Chun, Mi-Sun;Moon, Myung-Jun;Park, Ju-Yun;Kang, Yong-Cheol
    • Bulletin of the Korean Chemical Society
    • /
    • v.30 no.11
    • /
    • pp.2729-2734
    • /
    • 2009
  • We report here the surface behavior of zirconium oxide deposited on Si(100) substrate depending on the different substrate temperatures. The zirconium oxide thin films were successfully deposited on the Si(100) surfaces applying radio-frequency (RF) magnetron sputtering process. The obtained zirconium oxide films were characterized by X-ray photoelectron spectroscopy (XPS) for study about the chemical environment of the elements, X-ray diffraction (XRD) for check the crystallinity of the films, spectroscopic ellipsometry (SE) technique for measuring the thickness of the films, and the morphology of the films were investigated by atomic force microscope (AFM). We found that the oxidation states of zirconium were changed from zirconium suboxides ($ZrO_{x,y}$, x,y < 2) (x; higher and y; lower oxidation state of zirconium) to zirconia ($ZrO_2$), and the surface was smoothed as the substrate temperature increased.

EFFECT OF BASE OILS CHARACTERISTICS ON ATF PERFORMANCE

  • Moon, Woo-Sik;Yang, Si-Won
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2001.06a
    • /
    • pp.191-197
    • /
    • 2001
  • Performance requirements for automatic transmission fluids have been changing to reflect the design changes of automatic transmission. The major purpose for these design changes is to improve fuel economy and drivability. The use of special base oils like API Group III and IV base oils has increased in order to formulate high performance ATF. In this study. the effect of base oils characteristics on ATF performance is investigated, mainly regarding differences in frictional characteristics with deterioration. Moreover, low-temperature fluidity. oxidation stability. and seal compatibility are also compared for four different ATFs. From the investigation, it was found that the use of Group III and IV base oils in ATF has several benefits in low temperature viscosity. oxidation stability and SAE No.2 friction characteristics.

  • PDF