Evaluation of the genotoxicity and cytotoxicity in the buccal epithelial cells of patients undergoing orthodontic treatment with three light-cured bonding composites by using micronucleus testing

  • Toy, Ebubekir;Yuksel, Sengul;Ozturk, Firat;Karatas, Orhan Hakki;Yalcin, Muhammet
    • 대한치과교정학회지
    • /
    • 제44권3호
    • /
    • pp.128-135
    • /
    • 2014
  • Objective: This study evaluated the cytotoxicity and genotoxicity of fixed orthodontic treatment with three different light-cured orthodontic bonding composites by analyzing micronucleus (MN) formation in the buccal mucosa during a 6-month period. Methods: Thirty healthy volunteers were selected from consecutive patients referred for orthodontic treatment. Equilibrium 2 brackets and molar tubes (Dentaurum) were bonded with three different lightcured orthodontic bonding composites-Transbond XT (3M Unitek), Kurasper F (Kuraray Europe), or GrenGloo (Ormco Corporation)- to all teeth in both arches. Exfoliated buccal epithelial cells were scraped from the middle part of the inner cheeks with sterile cement spatulas before treatment and at 1, 3, and 6 months after treatment. MNs and nuclear alterations, such as karyorrhexis (KR), karyolysis (KL), and binucleated cells (BNs), were scored under a light microscope. Repeated measure ANOVA was used to calculate statistical differences in degenerative nuclear abnormalities. Results: MN rates did not significantly differ among different time points within the same cell type (p > 0.05). In contrast, the number of BNs in buccal epithelial cells significantly increased in all composite groups (p < 0.01, Transbond XT; p < 0.001, Kurasper F and GrenGloo). KL frequency significantly increased between the beginning and end of the study in the Kurasfer F ($0.80{\pm}0.79$ to $1.90{\pm}1.10$; p < 0.05) and GrenGloo ($1.30{\pm}1.06$ to $2.40{\pm}1.08$; p < 0.05) groups. Conclusions: After 6 months of fixed orthodontic treatment with different light-cured composites, morphological signs of cytotoxicity were observed but genotoxic effects were absent.

Low-shrinking composites. Are they reliable for bonding orthodontic retainers?

  • Uysal, Tancan;Sakin, Caglar;AI-Qunaian, Talal
    • 대한치과교정학회지
    • /
    • 제41권1호
    • /
    • pp.51-58
    • /
    • 2011
  • Objective: To evaluate the shear bond strength (SBS), fracture mode, wire pull out (WPO) resistance and microleakage between low-shrinking and conventional composites used as a lingual retainer adhesive. Methods: A total of 120 human mandibular incisor teeth, extracted for periodontal reasons, were collected. Sixty of them were separated into two groups. To determine the SBS, either Transbond-LR (3M-Unitek) or Silorane (3M-Espe) was applied to the lingual surface of the teeth by packing the material into standard cylindrical plastic matrices (Ultradent) to simulate the lingual retainer bonding area. To test WPO resistance, 20 samples were prepared for each composite where the wire was embedded in the composite materialand cured. Then tensile stress was applied until failure of the composite occurred. The remaining 60 teeth were divided into two groups and multi-stranded 0.0215-inch diameter wire was bonded with the same composites. Microleakage was evaluated by the dye penetration method. Statistical analyses were performed by Wilcoxon, Pearson chi-square, and Mann-Whitney-U tests at p < 0.05 level. Results: The SBS and WPO results were not statistically significant between the two groups. Significant differences were found between the groups in terms of fracture mode (p < 0.001). Greater percentages of the fractures showed mix type failure (85%) for Silorane and adhesive (60%) for Transbond-LR. Microleakage values were lower in low-shrinking composite than the control and this difference was found to be statistically significant (p < 0.001). Conclusions: Low-shrinking composite produced sufficient SBS, WPO and microleakage values on the etched enamel surfaces, when used as a lingual retainer composite.

다양한 교정용 접착제의 표면거칠기와 표면에너지 요소 분석 (Surface roughness and surface free energy components of various orthodontic adhesives)

  • 안효범;안석준;남동석
    • 대한치과교정학회지
    • /
    • 제36권5호
    • /
    • pp.360-368
    • /
    • 2006
  • 치과용 재료의 표면특성은 세균 부착에 중요한 역할을 한다. 본 연구의 목적은 다섯 종류의 광중합 교정용 접착제(불소를 방출하지 않는 세 종류의 콤포지트 레진, 불소를 방출하는 콤포지트 레진 한 종류, 레진 변형 글래스아이오노머 시멘트 한 종류)의 표면특성을 평가하는 것이다. 표면거칠기는 공초점 레이저주사전자현미경을 이용하여 측정하였고, 접촉각과 표면에너지 요소는 sessile drop method를 이용하여 분석하였다. 본 연구의 결과 교정용 접착제간 표면거칠기는 각 재료간 표면거칠기 차이가 $0.05\;{\mu}m$ 이하로 상대적으로 적지만 각 재료 사이에 유의성 있는 차이를 보였다. Transbond XT와 Enlight는 Monolok2와 Lightbond 보다 유의하게 덜 거칠었다. 접촉각과 표면에너지 구성성분은 접착제 사이에 유의성 있는 큰 차이를 보였는데 특히 레진 변형 글래스아이오노머와 콤포지트 레진 접착제간에 접촉각과 표면에너지에서 커다란 차이를 보였다. 레진 변형 글래스아이오노머의 경우 콤포지트 레진 접착제에 비해 유의하게 작은 접촉각과 높은 표면에너지를 보였으며 콤포지트 레진 접착제보다 강한 극성, 특히 강한 염기성 경향을 보였다 본 연구는 레진 변형 글래스아이오노머가 콤포지트 레진 접착제에 비해 세균 부착에 유리한 환경을 제공한다는 것을 보여주었다.

Microhybrid versus nanofill composite in combination with a three step etch and rinse adhesive in occlusal cavities: five year results

  • Tuncer, Safa;Demirci, Mustafa;Oztas, Evren;Tekce, Neslihan;Uysal, Omer
    • Restorative Dentistry and Endodontics
    • /
    • 제42권4호
    • /
    • pp.253-263
    • /
    • 2017
  • Objectives: The aim of the study was to evaluate the 5-year clinical performance of occlusal carious restorations using nanofill and microhybrid composites, in combination with 3-step etch-and-rinse adhesives, in patients who were going to commence orthodontic treatment. Materials and Methods: A total of 118 restorations for occlusal caries were conducted prior to orthodontic treatment. Occlusal restorations were performed both with Filtek Supreme XT (3M ESPE) and Filtek Z250 (3M ESPE) before beginning orthodontic treatment with fixed orthodontic bands. Restorations were clinically evaluated at baseline and at 1, 2, 3, 4, and 5-year recalls. Results: None of the microhybrid (Filtek Z250) and nanofill (Filtek Supreme XT) composite restorations was clinically unacceptable with respect to color match, marginal discoloration, wear or loss of anatomical form, recurrent caries, marginal adaptation, or surface texture. A 100% success rate was recorded for both composite materials. There were no statistically significant differences in any of the clinical evaluation criteria between Filtek Z250 and Filtek Supreme XT restorations for each evaluation period. Conclusions: The composite restorations showed promising clinical results relating to color matching, marginal discoloration, wear or loss of anatomical form, recurrent caries, marginal adaptation, and surface texture at the end of the 5-year evaluation period.

교정용 브라켓의 간접 접착법

  • 차봉근
    • 대한치과의사협회지
    • /
    • 제37권7호통권362호
    • /
    • pp.530-535
    • /
    • 1999
  • Detailed finishing of the occlusion is a clinical skill that has become difficult with the development of fixed appliances. Accuracy of bracket placement definitely improves with indirect technique, Several methods for the placement of orthodontic brackets on dental casts are currently used in the indirect bonding technique. These include attachment by means of bonding resins, adhesive tapes or sticky wax. This article presents the indirect procedures of our clinic, which use paste-paste chemically cured composites. Detailed laboratory and clinical procedure for dual tray method and other application of indirect bonding will be presented.

  • PDF

광중합기의 광원에 따른 브라켓 전단결합강도 비교 (Comparison of the shear bond strength of brackets in regards to the light curing source)

  • 차정열;이기준;박선형;김태원;유형석
    • 대한치과교정학회지
    • /
    • 제36권3호
    • /
    • pp.198-206
    • /
    • 2006
  • 제논 플라즈마 아크 광중합기나 LED 광중합기가 치과영역에 소개된 이후로 기존의 텅스텐 할로겐 광중합기를 사용할 때에 비해 교정장치의 부착시간이 현저하게 줄어들 수 있게 되었다. 제논 플라즈마 아크 광중합기에 대한 중합시간과 전단강도에 대해서는 여러 연구가 있어왔던 반면, LED 광중합기를 이용하여 교정용장치의 부착을 위한 중합시간에 대한 연구는 미진하다. 본 연구의 목적은 LED 광중합기의 중합시간에 따른 결합강도를 플라즈마 아크 광중합기와 비교하여 적절한 브라켓의 부착강도를 얻기 위해 요구되는 중합시간을 알아보는데 있다. 120개의 발치된 사람의 소구치에 컴포짓 레진으로 브라켓을 부착시킨 후 4초, 6초, 8초 동안 플라즈마 아크 광원과 LED 광원으로 각각 중합시켰다. 그 후 결합강도를 만능시험기(Universal Testing Machine)로 계측한 결과, 플라즈마 아크 광중합기에서는 4초 이상에서, LED 광중합기에서는 8초 이상의 중합시간에서 기존의 할로겐 광원을 40초간 노출시켰을 때와 비슷한 전단결합강도를 나타내었다. 플라즈마 아크 광중합기와 LED 광중합기의 중합시간이 접착제 잔류지수 (adhesive remnant index) 수치에 대해 영향을 미치지 않았다.

Fiber-Reinforcements of Composite Restorations

  • Cho, Kyung-Mo
    • 대한치과보존학회:학술대회논문집
    • /
    • 대한치과보존학회 2001년도 춘계학술대회
    • /
    • pp.258-258
    • /
    • 2001
  • Fiber-reinforced materials have highly favorable mechanical properties. and their strength-to-weight ratios are superior to those of most alloys. When compared to metals they offer many other advantages as well. including non-corrosiveness. translucency. good bonding properties. and ease ofrepair. Fiber-reinforced materials can be categorized to pre-impregnated. impregnation required. dental laboratory products. chairside products and prefabricated posts. so it is not suprising that fiber-reinforced composites have potential for use in many applications in dentistry. Fiber-reinforced materials can be utilized in frameworks for crowns. anterior or posterior fixed prostheses. chairs ide tooth replacements. periodontal splints. customized posts. prefabricated posts. orthodontic retention. denture reinforcements and in implants dentistry. To realize the full potential of using fiber-reinforced composite restorations. it is essential that the clinician and laboratory technician understand concepts of tooth preparation and framework design. Also practitioner may appreciate the background information and other details about the materials themselves so that identify the rationale for their use in various clinical situations. select well-suited materials. and carry out related procedures. Understanding the material properties and take many attentions. fiber-reinforced materials will give more esthetic. more easy. more strong and more reliable restorations.ations.

  • PDF

고정원 강화를 위해 치면에 부착한 fiber-reinforced composite과 스테인리스강 와이어의 피로한도 비교 (Comparison of the fatigue limit of fiber-reinforced composites and stainless steel wires when attached to the tooth surface for anchorage reinforcement)

  • 김문정;박수병
    • 대한치과교정학회지
    • /
    • 제35권4호
    • /
    • pp.302-311
    • /
    • 2005
  • 본 연구는 고정원을 강화하는데 사용되는 fiber-reinforced composite (FRC)과 스테인리스강 와이어의 피로 한도를 치아의 생리적 동요도가 허용되는 조건에서 비교하여 FRC의 임상적 유용성을 알아보기 위해 시행되었다. 스테인리스강 와이어군은 각형과 원형 와이어군으로 나누고 FRC군은 uni-directional군과 woven군, 그리고 각각의 군에 있어서 치간 부위에 레진을 코팅한 군과 코팅하지 않은 군으로 나누었다 각 군간의 피로한도를 일반적인 교정치료기간을 재현한 $5{\times}10^5cycle$의 피로한도 내에서 측정하여 비교하였다. 그 결과 스테인리스강 와이어에서는 각형 와이어가 원형 와이어보다 피로한도가 더 높았지만 통계적으로 유의하지는 않았다 (p>0.05) 치간부위를 레진으로 코팅한 FRC와 코팅하지 않은 FRC 모두 uni-directional군이 woven군보다 피로한도가 더 높게 나타났으며 (p<0.05) 그 값은 치간 부위를 레진으로 코팅한 FRC가 코팅하지 않은 FRC보다 더 높게 나타났다(p<0.05). 스테인리스강 와이어와 FRC 모두 임상적으로 유용한 $5{\times}10^5cycle$의 피로한도 내에서는 파절되지 않았기 때문에 둘 다 고정원 강화를 위해 사용하여도 충분하며 또한 심미성이 요구되거나 부가적인 장치의 부착이 필요한 곳에서는 FRC를 사용하여도 충분하리라 생각된다.

Plasma arc curing system을 이용한 브라켓의 접착에 관한 연구 (A STUDY ON THE SHEAR BOND STRENGTH BY PLASMA ARC CURING SYSTEM FOR BRACKET BONDING)

  • 김정윤;김종수;권순원
    • 대한소아치과학회지
    • /
    • 제28권4호
    • /
    • pp.638-642
    • /
    • 2001
  • 최근에 소개된 Plasma arc lamp를 이용한 고광도 광조사기는 조사되는 광도를 크게 증가시켜 필요한 조사시간을 단축시키고자하는 연구의 결과중 하나이다. 교정 임상에서 브라켓의 접착시 고광도 광조사기를 사용하여 시술시간을 줄인다면 환자뿐만 아니라, 술자에게도 시간적이나 경제적으로 많은 도움을 줄 것이다. 이 연구의 목적은 Plasma arc light를 사용하여 접착시킨 브라켓의 치면에 대한 전단강도를 측정하고 이를 기존의 할로겐 램프를 이용한 광중합 방법과 비교해보기 위함이다. I군은 할로겐 램프를 사용하는 $XL3000^{(R)}$을 이용하여 총 50초간 광중합하였고 II군은 plasma arc lamp를 사용하는 $Flipo^{(R)}$를 이용하여 2초간 광중합하였으며 III군도 $Flipo^{(R)}$를 이용하여 총 5초간 광중합하여 전단강도 측정을 시행한 결과는 다음과 같다. 1. 세 군의 전단강도의 평균은 비슷한 수치를 나타내었다. 2. 세 군간의 통계학적 유의 차가 없었다(p>0.05).