  • The batches having excess SiO2 to tetrasilicic mica KMg2.5 (Si4O10)F2 were melted at 1450℃. The fabricated samples were heat-treated for the nucleation and the crystallization. The crystallized samples were investigated on several properties. The tetrasilicic mica composition with excess 10 wt% SiO2 was successful both in glassifying and in crystallizing. The optimum temperatures for the nucleation and the crystallization were 680℃ and 1000-1100℃, respectively. The mica and the cristobalite crystallines were identified after heat-treatment. The properties of the samples processed appropriately were as follows, bulk density 2.64g/㎤, thermal expansion coefficient ∼80×10-7/℃, Vicker's hardness ∼105 Kgf/㎟, bending strength ∼666Kgf/㎟, dielectric constant ∼11.1, tan δ 2.5%, volume resistivity 2.35×107∼1.3×1011{{{{ OMEGA }}cm, surface roughness 6.984㎛.

  • PDF

Epoxy/EPDM계면의 최적처리 조건과 수명 예측 (The Optiomun Treatment Conditions an the Estimation of Life in the Interface between Epoxy/EPDM)

  • 오재한;배덕권;최운식;이경섭
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2000년도 하계학술대회 논문집 C
    • /
    • pp.1978-1980
    • /
    • 2000
  • Because the interfaces between two different materials are the weak-link in the underground power transmission systems, they affects the stability of insulation systems. In this paper, Epoxy/EPDM interface is selected and investigated the optimum condition by variation of interfacial conditions such as roughness of surface, spreading of oils, interfacial pressure and temperature. The breakdown times under the constant voltage below the breakdown voltage were also gamed. The breakdown voltage at the after laying time equivalent to is calculated by the V-t characteristic and the inverse power law. When this is done. the characteristic life exponent n is used and the long time breakdown voltage can be evaluated.

  • PDF

전해 크롬도금 대체용으로서의 CrC 스퍼터링에 관한 연구 (A study of CrC Sputtering as an Alternative Method for Cr Electroplating)

  • 임종민;최균석;이종무
    • 한국재료학회지
    • /
    • 제12권1호
    • /
    • pp.82-88
    • /
    • 2002
  • Chromium carbide films were deposited on high speed steels using a Cr_3C_2$ target by magnetron sputtering. Effects of the deposition parameters (power, Ar pressure and substrate temperature) on deposition rates and surface roughnesses of the films were investigated. The morphologies of those films were characterized by scanning electron microscopy and atomic force microscopy. The grain size of the samples deposited using dc-power is larger than that using equivalent rf-power. The hardness of the sample increases with increasing rf-power, whereas the elastic modulus nearly does not change with rf-power. The optimum sputter deposition conditions for chromium carbide on high speed steels in the corrosion resistance aspect were found to be the rf-power with small roughness.

연마판의 거칠기에 따르는 SiC 세라믹스의 굽힘강도 특성 (Bending Strength Properties of SiC Ceramics at Different Roughness Values of Polishing Plates)

  • 남기우;김은선
    • 대한기계학회논문집A
    • /
    • 제35권7호
    • /
    • pp.779-784
    • /
    • 2011
  • 본 논문은 첨가제 $SiO_2$를 가지는 3종류의 SiC 세라믹스의 연마판 거칠기에 따르는 균열 치유 연구를 실시하였다. 혼합물은 질소가스 분위기에서 2053 K, 35 MPa, 1시간 동안 소결하였다. SiC 세라믹스 시험편의 최적 균열 치유 조건은 1373 K에서 1시간이다. 균열부의 치유 물질은 SiC와 $O_2$의 산화반응에 의한 유리상 $SiO_2$이다. 최적 치유 조건에서 미연마 SiC 세라믹스의 굽힘 강도는 완전하게 회복되지 않았다. 그러나 SAY, SAYS-1 및 SAYS-2 시험편에서 경제적인 면을 고려하면 1시간 열처리에서 상온 굽힘 강도가 가장 높게 나타난 SAY 시험편이 우수하다. $125\;{\mu}m$ 연마판의 연마 시험편은 결함의 수나 크기가 줄어들었으나, 열처리 후에도 표면 미세 결함이 완전하게 치유되지 못하였다. $40\;{\mu}m$ 연마판의 연마 시험편은 1시간 열처리 후 표면 결함이나 기공은 거의 없었으며, 굽힘 강도는 $6\;{\mu}m$ 연마판 경면 시험편의 강도만큼 회복하였다.

Properties of IZTO Thin Films on Glass with Different Thickness of SiO2 Buffer Layer

  • Park, Jong-Chan;Kang, Seong-Jun;Yoon, Yung-Sup
    • 한국세라믹학회지
    • /
    • 제52권4호
    • /
    • pp.290-293
    • /
    • 2015
  • The properties of the IZTO thin films on the glass were studied with a variation of the $SiO_2$ buffer layer thickness. $SiO_2$ buffer layers were deposited by plasma-enhanced chemical vapor deposition (PECVD) on the glass, and the In-Zn-Tin-Oxide (IZTO) thin films were deposited on the buffer layer by RF magnetron sputtering. All the IZTO thin films with the $SiO_2$ buffer layer are shown to be amorphous. Optimum $SiO_2$ buffer layer thickness was obtained through analyzing the structural, morphological, electrical, and optical properties of the IZTO thin films. As a result, the IZTO surface roughness is 0.273 nm with a sheet resistance of $25.32{\Omega}/sq$ and the average transmittance is 82.51% in the visible region, at a $SiO_2$ buffer layer thickness of 40 nm. The result indicates that the uniformity of surface and the properties of the IZTO thin film on the glass were improved by employing the $SiO_2$ buffer layer and the IZTO thin film can be applied well to the transparent conductive oxide for display devices.

기계적인 가공방법에 의한 마이크로 렌즈 금형가공 (The Micro Lens Mold Processing in Mechanical Fabrication Method)

  • 정재엽;이동주;제태진;최두선;이응숙;홍성민
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2003년도 춘계학술대회 논문집
    • /
    • pp.1885-1888
    • /
    • 2003
  • As high technology industries such as IT and display have developed, demand for application parts of micro lens and lens array has been extremely increasing. According to these trends, many researchers are studying on the fabrication technology for parts of the micro lens by a variety of methods such as MEMS, Lithography, LIGA and so on. In this paper, we have performed researches related to ultra precision micro lens, lens array mold and fabrication of Lenticular lens mold for three-dimensional display by using mechanical micro end-milling and fly-cutting fabrication method. Tools used in this research were a diamond tool of R 150$\mu\textrm{m}$. Cutting conditions set up feed rate, spindle revolution. depth of cut and dwell time as variables. And we analyzed surface quality variation of the processed products according to the cutting conditions, and then carried out experiments to search the optimum conditions. Through this research, we have confirmed that we can fabricate the ultra precision micro lens mold with surface roughness Ra=20nm and the holographic lens mold by using micro end-milling and fly-cutting fabrication method. Furthermore, we demonstrated problems happened in the fabrication of the micro lens and established the foundation of experimental study for formulating its improvement plan.

  • PDF

일차파괴된 암반사면의 전단강도 및 보강설계법 고찰 (A study on the determination of shear strength and the support design of pre-failed rock slope)

  • 조태진;김영호
    • 터널과지하공간
    • /
    • 제5권2호
    • /
    • pp.104-113
    • /
    • 1995
  • Shear strength of the discontinuity on which the pre-failure of rock slope was occurred during surface excavation was measured through the direct shear test using core samples obtained in-situ. Internal friction angle was increased as the roughness of discontinuity surface(JRC) was increased. Results of the tilt test using core samples of higher JRC also showed very similar trend as those of the direct shear test. When the samples replicated from natural cores were used int he tilt test, results of friction angles showed almost perfect continuation of the residual friction angles from the direct shear test. However, when the gouge material existed in the discontinuity the internal friction angle strongly depended upon the rate of filling thickness to the height of asperity irrespective of the JRC. Based on the results of both direct shear test and tilt test internal friction angle and cohesion of discontinuity, which reflect the in-situ conditions fo pre-sliding failure and also can be used for the optimum design of support system, were assessed. Two kinds of support measures which were expected to increase the stability of rock slope were considered; lowering of slope face angle and installation of rock cable. But, it was found that the first method might lead to more unstable conditions of rock slope when the cohesion of discontinuity plane was negligibly low and in that case the support systems of any kind which could exert actual resisting force were needed to ensure the permanent stability of rock slope.

  • PDF

흙-토목섬유 Interface 특성에 관한 연구 (A Study on the Characteristics of the Soil-Geotextile Interface)

  • 고홍석;고남영;홍순영
    • 한국농공학회지
    • /
    • 제33권2호
    • /
    • pp.82-93
    • /
    • 1991
  • The objective of this paper is to show that the soil-geotextile interaction needs to he addressed in addition to the usual tensile and modulus properties when the geotextile is being designed for a specific application. The soil-geotextile interaction can be directly assessed by standard direct shear test. The data presented here show that the shear strength paramaters describing the soil-geotextile interface can he greatly influenced by the type of the geotextile. In this investigation, we examined nine different geotextiles of varying construction and surface textures with two standard soil, under five loading conditions, and compared the shear strength and the frictional resistance with the corresponding values of soil itself The following conclusions were drawned from this study. 1. The shear stress-strain curve shows that there are the residual shear stresses at the soil-geotextile interface. Because of the hydraulic gradient between the soil and the geotextile, the excessive pore water can migrate into the geotextile and among the filaments and dissipate through the soil-geotextile interface. 2. The shear strength of the soil-geotextile interface is affected by the moisture content of the soil. At moisture content lower than the optimum water content of the Proctor compaction test, the shear strength of the soil-geotextile interface is greater. 3. The type and surface roughness of the geotextile have the greatest influence on the interface friction angle between the soil and the geotextile.

  • PDF

정공전달고분자와 유기형광염료의 혼합물 박막이 이용된 발광소자의 에너지 전달특성 연구 (Studies on the Energy Transfer in LED Containing the Layer made of the Blends of Hole Transporting Polymer and Organic Phosphorescent Dye)

  • 김유진;정숙
    • 한국전기전자재료학회논문지
    • /
    • 제17권11호
    • /
    • pp.1192-1198
    • /
    • 2004
  • Hole transporting polymer(poly[N-(p-diphenylamine)phenylmethacrylamide], PDPMA) was doped with nile red dye at various concentrations to study the influence of doping on the energy transfer during light emitting processes. Organic LEDs composed of ITO/blend(PDPMA -nile red)/ Alq$_3$/Al as well as thin films of blend(PDPMA -nile red)/ Alq$_3$ were manufactured for investigating photoluminescence, electroluminescence, and current-voltage characteristics. Atomic Force Microscopy was also used to observe surface morphology of the blend films. It was found that such doping. significantly influences the efficiency of the energy transfer from the Alq$_3$ layer to blended layer and the optical/electrical properties could be optimized by choosing the right concentration of the dye molecule. The results also showed a interesting correlation with the morphological aspect, i.e. the optimum luminescence at the concentration with the least surface roughness. When the concentration of nile red was 0.8 wt%, the maximum energy transfer could be achieved.

Cosputtering법으로 증착한 ZnO박막의 Al도핑농도가 미세구조 및 물리적 특성에 끼치는 효과 (Effects of Al Doping Concentration on the Microstructure and Physical Properties of ZnO Thin Films Deposited by Cosputtering)

  • 임근빈;이종무
    • 한국재료학회지
    • /
    • 제15권9호
    • /
    • pp.604-607
    • /
    • 2005
  • Dependence of the crystallinity, surface roughness, carrier concentration, carrier mobility, electrical resistivity and transmittance of Al-doped ZnO films deposited on glass substrates by RF-magnetron sputtering on effects of the ratio of the RF power for AlZnO to that for ZnO (R) have been investigated. X-ray diffraction spectra show strong preferred orientation along the c-axis. The full width at half maximum (FWHM) of the ZnO (002) peak decreases slightly as R increases in the range of R<1.0, whereas it increases substantially in the range of R>1.0. Scanning electron micrographs (SEM) show that the ZnO film surface becomes coarse as R increases. The carrier concentration and the carrier mobility in the ZnO thin film are maximal for R=1.5 and 1.0, respectively. The electrical resistivity is minimal for R=1.0 The transmittance of the ZnO:Al film tends to increase, but to decrease slightly in the range of R>0.5. It may be concluded that the optimum R value is 1.0, considering all these analysis results. The cause of the changes in the structure and physical properties of ZnO thin films with R are also discussed.