  • The rear side contact recombination in the crystalline silicon solar cell could be reduced by back surface field. We formed polycrystalline silicon as a back surface field through crystallization of amorphous silicon. A thin silicon oxide applied to the passivation layer. We used quasi-steady-state photoconductance measurement to analyze electrical properties with various annealing condition. And, blister formed on surface of wafer during the annealing process. We observed the blister after varied annealing process with wafer of various surface. Shape and density of blister is influenced by various annealing temperature and process time. As the annealing temperature became higher, the average diameter of blister is decreased and total number of blister is increased. The sample with the $600^{\circ}C$ annealing temperature and 1 min annealing time exhibited the highest implied open circuit voltage and lifetime. We predicted that the various shape and density of blister affects the lifetime and implied open circuit voltage.

  • PDF

Thin Film Amorphous/Bulk Crystalline Silicon Tandem Solar Cells with Doped nc-Si:H Tunneling Junction Layers

  • 이선화;이준신;정채환
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2015년도 제49회 하계 정기학술대회 초록집
    • /
    • pp.257.2-257.2
    • /
    • 2015
  • In this paper, we report on the 10.33% efficient thin film/bulk tandem solar cells with the top cell made of amorphous silicon thin film and p-type bulk crystalline silicon bottom cell. The tunneling junction layers were used the doped nanocrystalline Si layers. It has to allow an ohmic and low resistive connection. For player and n-layer, crystalline volume fraction is ~86%, ~88% and dark conductivity is $3.28{\times}10-2S/cm$, $3.03{\times}10-1S/cm$, respectively. Optimization of the tunneling junction results in fill factor of 66.16 % and open circuit voltage of 1.39 V. The open circuit voltage was closed to the sum of those of the sub-cells. This tandem structure could enable the effective development of a new concept of high-efficiency and low cost cells.

  • PDF

금속연료전지에서 이온교환막이 전기전도에 미치는 영향 (The Effect of Ion Exchange Membrane on the Electrical Conduction in Metal Fuel Cell)

  • 김용혁
    • 전기학회논문지
    • /
    • 제59권12호
    • /
    • pp.2235-2239
    • /
    • 2010
  • In this study, The cation exchange membrane and the anion exchange membrane affect in electrical conduction of metal fuel cell was investigated. Magnesium material as anode electrode and the NaCl solution dissolved with 5~15wt% as electrolyte were used for the metal fuel cell. It was found that magnesium slag where flows toward the air electrode was suppressed by using ion exchange membrane. The open circuit voltage variation during discharge has very flat pattern by using ion exchange membrane, but the case which is not the exchange membrane, the open circuit voltage increased according to time. When using the anion exchange membrane, the electric current was higher case of the cation exchange membrane, as a result of higher equivalent conductivity in anion Cl-. The cation exchange membrane was observed with the fact that the output power is excellent in compared with anion exchange membrane.

정전류 기능이 부가된 고전력 밀도의 통신기용 개방형 전원장치 (Open frame type Power Module for Telecommunication of High Power Density)

  • 연제선;안태영
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2004년도 추계학술대회 논문집 전기기기 및 에너지변환시스템부문
    • /
    • pp.143-146
    • /
    • 2004
  • This is a thesis that 100W class open frame type power module of a quarter-brick size appropriate for telecommunication is reported. The input voltage is established between 36 and 75 in range in order for power module to be utilized for the telecommunication, and output were set at 3.3V and 30A. A number of parts used for transformer, inductor, and hit sink are composed of PCB in order for DC-DC converter to be lowered below 8 mm. A constant current control circuit was annexed to the system as well as basic protection prototypes such as over-voltage, over-current, and over-temperature were well considered to enhance more credibility, and were tested. As a result, high circuit performance and credibility turned out to be significant.

  • PDF

휴대전원용 직접알코올 연료전지의 OCV특성 연구 (Operating Characteristics on Coupling of Fuel-Cell System with Natural Gas Reformer)

  • 박세준;최용성;이경섭
    • 전기학회논문지P
    • /
    • 제58권4호
    • /
    • pp.592-596
    • /
    • 2009
  • DAFC(direct alcohol fuel cell) takes the same structure and operational principle with PEMFC(Proton exchange membrane fuel cell). However, DAFC, which uses liquid alcohol instead of hydrogen as fuel, is able to be used as a portable power for small-scaled electronic devices such as MP3, PMP, and mobile phone because alcohol is quite convenient steady-state compound to carry and store it. This paper presents the OCV(open circuit voltage) characteristics of the cases which are alcohol species and different weight rate of ethanol, respectively. The OCV of methanol fuel cell is slightly higher 0.2V than ethanol one, and 8% wt. rate ethanol is rated as the most appropriate fuel for DAFC.

Number of Graphene Layers As a Modulator of the Open-circuit Voltage of Graphene-Based Solar Cell

  • 임규욱;이경재;임종태;강태희;정석민;홍병희;염근영
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제41회 하계 정기 학술대회 초록집
    • /
    • pp.113-113
    • /
    • 2011
  • Impressive optical properties of graphene have been attracting the interest of researchers, and, recently, the photovoltaic effects of a heterojunction structure embedded with few layer graphene (FLG) have been demonstrated. Here, we show the direct dependence of open-circuit voltage (Voc) on numbers of graphene layers. After unavoidably adsorbed contaminants were removed from the FLGs, by means of in situ annealing, prepared by layer-by-layer transfer of the chemically grown graphene layer, the work functions of FLGs showed a sequential increase as the graphene layers increase, despite of random interlayer-stacking, resulting in the modulation of photovoltaic behaviors of FLGs/Si interfaces.

  • PDF

LB 초박막의 전압발생 (Generation of Open Circuit Voltage in LB Ultra Thin Films)

  • 권영수;강도열
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1988년도 전기.전자공학 학술대회 논문집
    • /
    • pp.796-798
    • /
    • 1988
  • Langmuir-Blodgett(LB) films of arachic acid and TCNQ(tetracyanoquinodimethane) were prepared in the sample of Al/LB film/Al type where Al are electrodes, and polarization in LB film and dipolar moment of molecules in the films were measured by themally stimulated current(TSC). It is ascertaind in our experiments that dipolar mament of $C_{12}$TCNQ molecule was about 13-15 debye and the moment was directed from the alkyle chain toward TCNQ. Generation of the open circuit voltage was investigated on the z-type and Hetero structure of LB films.

  • PDF

높은 전력밀도를 갖는 개방형 DC-DC 컨버터 모듈에 관한 연구 (A Study on Open-Frame Type DC-DC Converter Module with High Power Density)

  • 연제선;안태영
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2004년도 하계학술대회 논문집 B
    • /
    • pp.1266-1268
    • /
    • 2004
  • This is a thesis that a quarter-brick size of 100W class open-frame type on board power module comprising telecommunication application is reported. The input voltage is established between 36 and 75 in range in order for power module to be utilized for the telecommunication application, and output were set at 3.3V and 30A. A number of parts used for transformer, inductor, and hit sink are composed of PCB in order for DC-DC converter to be lowered below 8 mm. A constant current control circuit was annexed to the system as well as basic protection prototypes such as over-voltage, over-current, and over-temperature were well considered to enhance more credibility, and were tested. As a result, high circuit performance and credibility turned out to be significant.

  • PDF

수소연료를 이용하는 원자층증착 박막전해질 세라믹연료전지의 초기성능 저하에 관한 연구 (A Study on the Initial Performance Degradation of Hydrogen-Fueled Ceramic Fuel Cell with Atomic Layer-Deposited Thin-Film Electrolyte)

  • 지상훈
    • 한국수소및신에너지학회논문집
    • /
    • 제32권5호
    • /
    • pp.410-416
    • /
    • 2021
  • The initial electrochemical performance of ceramic fuel cell with thin-film electrolyte was evaluated in terms of peak power density ratio, open circuit voltage ratio, and activation/ohmic resistance ratios at 500℃. Hydrogen and air were used as anode fuel and cathode fuel, respectively. The peak power density ratio reduced as ~17% for 40 minutes, which rapidly decreased in the early stage of the performance evaluation but gradually decreased. The open circuit voltage ratio decreased with respect time; however, its time behavior was remarkably different with the reduction behavior of the peak power density ratio. The activation resistance ratio increased as ~15% for 40 minutes, which was almost similar with the time behavior of the peak power density ratio.

플라즈마 원자층증착 초박막전해질 수소 세라믹연료전지의 초기성능 저하 (Initial Performance Degradation of Hydrogen-Fueled Ceramic Fuel Cell with Plasma-Enhanced Atomic Layer-Deposited Ultra-Thin Electrolyte)

  • 지상훈
    • 한국수소및신에너지학회논문집
    • /
    • 제32권5호
    • /
    • pp.340-346
    • /
    • 2021
  • The initial electrochemical performance of ceramic fuel cell with thin-film electrolyte fabricated by plasma-enhanced atomic layer deposition method was evaluated in terms of peak power density ratio, open circuit voltage ratio, and activation/ohmic resistance ratios at 500℃. Hydrogen and air were used as anode fuel and cathode fuel, respectively. The peak power density ratio reduced as ~52% for 30 min, which continually decreased as time increased but degradation rate gradually decreased. The open circuit voltage ratio decreased with respect time; however, its behavior was evidently different from the reduction behavior of the peak power density. The activation resistance ratio increased as ~127% for 30 min, which was almost similar with the reduction behavior of the peak power density ratio.