• 제목/요약/키워드: Normal Elasticity

검색결과 197건 처리시간 0.021초

Strain elastography of tongue carcinoma using intraoral ultrasonography: A preliminary study to characterize normal tissues and lesions

  • Ogura, Ichiro;Sasaki, Yoshihiko;Sue, Mikiko;Oda, Takaaki
    • Imaging Science in Dentistry
    • /
    • 제48권1호
    • /
    • pp.45-49
    • /
    • 2018
  • Purpose: The aim of this study was to evaluate the quantitative strain elastography of tongue carcinoma using intraoral ultrasonography. Materials and Methods: Two patients with squamous cell carcinoma (SCC) who underwent quantitative strain elastography for the diagnosis of tongue lesions using intraoral ultrasonography were included in this prospective study. Strain elastography was performed using a linear 14 MHz transducer (Aplio 300; Canon Medical Systems, Otawara, Japan). Manual light compression and decompression of the tongue by the transducer was performed to achieve optimal and consistent color coding. The variation in tissue strain over time caused by the compression exerted using the probe was displayed as a strain graph. The integrated strain elastography software allowed the operator to place circular regions of interest (ROIs) of various diameters within the elastography window, and automatically displayed quantitative strain (%) for each ROI. Quantitative indices of the strain (%) were measured for normal tissues and lesions in the tongue. Results: The average strain of normal tissue and tongue SCC in a 50-year-old man was 1.468% and 0.000%, respectively. The average strain of normal tissue and tongue SCC in a 59-year-old man was 1.007% and 0.000%, respectively. Conclusion: We investigated the quantitative strain elastography of tongue carcinoma using intraoral ultrasonography. Strain elastography using intraoral ultrasonography is a promising technique for characterizing and differentiating normal tissues and SCC in the tongue.

SUKI 중재에 의한 중년 여성의 윗입술근피에 미치는 연구 (The Study on the Effect of the Middle-aged Women's Upper lips musculo-cutaneous by SUKI® program)

  • 이수범;홍성균
    • 융합정보논문지
    • /
    • 제11권2호
    • /
    • pp.194-200
    • /
    • 2021
  • 본 연구의 목적은 6주간 중년여성을 대상으로 SUKI 중재 프로그램이 윗입술근피에 미치는 영향에 대해 알아보고자 진행되었다. 실험대상자는 총 20명이었으며, 6주간 주 3회 씩 안면부의 윗입술 근피에 대한 Pattern T1, Pattern T2, Pattern T3, Pattern T4의 SUKI 중재프로그램을 실시하였고, 결과는 다음과 같았다. 윗입술근피의 군내 비교에서는 일부이지만 실험군에서 유의한 차이가 있었다. 따라서, SUKI 중재 프로그램이 윗입술근피의 탄력 향상에 일부 도움을 줄 수 있는 것으로 나타났다(p<.05). 본 연구에서는 제한적이지만, 중년여성의 안면부에 위치하고 있는 윗입술근피의 탄력 감소 문제가 입 주위에 각종 주름을 발생시켜 여성의 외모에 대한 자신감을 잃게 하고 있다는 것을 근간으로 SUKI 중재 프로그램을 활용하였다. 또한 이것은 정상적인 안면근피가 영향을 끼치는 용모에 대한 의미로서, 중년여성의 생애주기에 맞는 적정한 안면근피의 관리에 의한 용모관리를 할 수 있는 일부방법을 제시하고자 하였다. 결론적으로 추후 다양한 실험자들에게 여성의 얼굴 피부미용과 주름을 예방하고 입 주위 안면근피의 탄력향상에 도움을 줄 수 있는 방법에 대한 새로운 연구자료로 활용될 수 있기를 기대하고자 한다.

이노시톨과 피틴산이 피부에 미치는 영향 (The Effect of Inositol and Phytic Acid on Skin)

  • 조춘구;한창규;송환
    • 대한화장품학회지
    • /
    • 제30권4호
    • /
    • pp.515-524
    • /
    • 2004
  • 쌀눈에서 추출한 inositol과 phytic acid를 화장품에 적용하기 위해 피부에 미치는 영향에 대해 연구하였다 $20{\~}40$대의 아시안 여성 45명을 대상으로 7주간 inositol $0{\~}3.0\;wt\%$와 phytic acid $0{\~}1.50\;wt%$가 함유된 스킨로션을 제조, 사용 후 피부의 수분, 유분, 탄력, 주름에 미치는 영향에 대해서 알아보았다 Inositol $1.0\;wt\%가$ 함유된 스킨로션을 사용한 경우 피부의 수분 함유량은 $19\%$ 증가하였으며, 주름은 $12.4\%$ 개선되었고, 피부탄력은 $12.4\%$ 증가되었다. 또한 phytic acid $0.50\;wt\%$를 함유한 스킨 로션을 사용한 경우 피부의 수분은 $71.6\%$ 증가하였으며, 주름은 $16.9\%$ 감소하였고, 탄력은 $21.9\%$가 증가하였다. Inositol과 phytic acid를 지성과 건성피부에 적용한 결과 $2{\~}4$주 후면 정상피부의 유분량으로 조절됨을 알 수 있었다 Inositol과 phytic acid는 모두 피부개선에 효과적이나, phytic acid는 민감한 피부에는 적용하기 어려운 점이 있다. 따라서 $1.0\;wt\%의$ inositol에 $0{\~}0.5\;wt\%$의 phytic acid를 첨가한 스킨로션을 제조하여 그 효과에 대해서 알아보았다. 이 경우 $1.0\;wt\%$의 phytic acid에 $1.0\;wt\%$의 inositol을 사용한 경우 수분은 $63.8\%$, 탄력은$17.2\%$ 증가하였으며, 주름은 $17.4\%$ 개선되었고, 피부 유분량은 약 2주 후에 정상적인 상태로 개선됨을 알 수 있었다. 따라서 inositol $1.0\;wt\%$$0.10\;wt\%$의 phytic acid를 첨가하여도 피부 개선효과가 나타남을 알 수 있다. 본 연구의 결과 내에서 $1.0\;wt\%$의 phytic acid와 $1.0\;wt\%$의 inositol을 사용한 경우 적은 양으로도 피부 개선 효과가 우수한 상승효과가 나타남을 알 수 있었다.

초경량(超輕量) 폴리머 콘크리트의 응력(應力)-변형특성(變形特性) (Stress-Strain Properties of Surlightweight Polymer Concrete)

  • 성찬용;김경태;민정기;김영익;윤준노;정현정
    • 농업과학연구
    • /
    • 제25권2호
    • /
    • pp.271-277
    • /
    • 1998
  • 본 연구는 폴리머와 인공경량 세골재 및 인공경량 조골재를 사용한 초경량 폴리머 콘크리트의 응력-변형특성을 구명한 것으로서, 이 연구를 통해 얻어진 결과를 요약하면 다음과 같다. 1. 동탄성 계수는 $1.514{\times}10^5{\sim}1.916{\times}10^5kgf/cm^2$로써 보통 시멘트 콘크리트의 48~96%정도이며, 인공경량 세골재의 양이 적을수록 크게 나타났다. 2. 정탄성계수는 $2.552{\times}10^4{\sim}4.386{\times}10^4kgf/cm^2$으로 보통 시멘트 콘크리트의 8~22%정도로 작게 나타났고, 포아손수도 보통 시멘트 콘크리트보다 작게 나타났다. 3. 응력-변형율곡선은 모든 배합에서 응력의 증가와 함께 증가하다가 최대하중에서 파괴된후 급격한 감소를 보였으며, 보통 시멘트 콘크리트보다 취성이 크게나타났다. 4. 최대응력하에서의 변형율은 P1에서 $6.975{\times}10^{-3}$으로 가장 크게 나타났고, P9에서 $1.600{\times}10^{-3}$으로 가장 작게 나타났으며, 인공경량 조골재의 양이 많을수록 작게 나타났다.

  • PDF

Strain elastography of palatal tumors in conjunction with intraoral ultrasonography, computed tomography, and magnetic resonance imaging: 2 case reports

  • Ogura, Ichiro;Toshima, Hiroo;Akashiba, Tohru;Ono, Junya;Okada, Yasuo
    • Imaging Science in Dentistry
    • /
    • 제50권1호
    • /
    • pp.73-79
    • /
    • 2020
  • Computed tomography (CT) and magnetic resonance imaging (MRI) can be useful for the evaluation of palatal lesions, and strain elastography (performed together with intraoral ultrasonography) is a relatively new sonographic imaging modality. This report describes 2 clinical cases in which strain elastography was used to assess palatal tumors in conjunction with intraoral ultrasonography, CT, and MRI. In the first case, diagnosed as a myoepithelioma, the strain was determined to be 0.000% (strain of normal tissue, 0.556%). In the second case, diagnosed as an adenoid cystic carcinoma, the determined strain was 0.000% (strain of normal tissue, 1.077%). Therefore, we conclude that intraoral strain elastography can be useful for evaluating palatal lesions.

Rheology and morphology of concentrated immiscible polymer blends

  • Mewis, Jan;Jansseune, Thomas;Moldenaers, Paula
    • Korea-Australia Rheology Journal
    • /
    • 제13권4호
    • /
    • pp.189-196
    • /
    • 2001
  • The phase morphology is an important factor in the rheology of immiscible polymer blends. Through its size and shape, the interface between the two phases determines how the components and the interface itself will contribute to the global stresses. Rheological measurements have been used successfully in the past to probe the morphological changes in model blends, particularly for dilute systems. For more concentrated blends only a limited amount of systematic rheological data is available. Here, viscosities and first normal stress differences are presented for a system with nearly Newtonian components, the whole concentration range is covered. The constituent polymers are PDMS and PIB, their viscosity ratio can be changed by varying the temperature. The data reported here have been obtained at 287 K where the viscosities of the two components are identical. By means of relaxation experiments the measured stresses are decomposed into component and interfacial contributions. The concentration dependence is quite different for the two types of contribution. Except for the component contributions to the shear stresses there is no clear indication of the phase inversion. Plotting either the interfacial shear or normal stresses as a function of composition produces in some cases two maxima. The relaxation times of these stresses display a similar concentration dependence. Although the components have the same viscosity, the stress-component curves are not symmetrical with respect to the 50/50 blend. A slight elasticity of one of the components seems to be the cause of this effect. The data for the more concentrated blends at higher shear rates are associated with a fibrillar morphology.

  • PDF

시험방법에 따른 친환경 경량콘크리트의 상대동탄성 계수 비교 (Relative Dynamic Modulus of Elasticity Comparison of the Eco-friendly Lightweight Concreate According to the Experimental Method)

  • 이수형;이한백
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2016년도 춘계 학술논문 발표대회
    • /
    • pp.181-182
    • /
    • 2016
  • We developed eco-friendly lightweight concrete in order to apply eco-friendly lightweight concrete into structural wall or slab of shallow depth urban railway system. However, since lightweight aggregate has different structural feature of porous and it has been overvalued at current KS standard when applied, we did compare the characteristics of freezing and thawing of normal weight aggregate concrete by comparative test method(KS, ASTM). According to test method, there was a big difference of dynamic elastic modulus in lightweight concrete rather than in normal weight aggregate concrete. The big absorption factor in lightweight aggregate is main reason for that. For more detail, in KS law in which only 14 days water curing is carried out, the big amount of moisture in lightweight aggregate is frozen and high heaving pressure occurs and finally that lead to destruction of lightweight concrete. Therefore, it is considered that in case of lightweight concrete, resistibility against freezing and thawing has been undervalued in domestic KS law compared to ASTM law, which is overseas standard. So, a variety of examination about testing criteria and rule would be necessary for exact assessment of lightweight concrete.

  • PDF

The effects of different cement dosages, slumps and pumice aggregate ratios on the freezing and thawing of concrete

  • Turkmen, Ibrahim;Demirboga, Ramazan;Gul, Rustem
    • Computers and Concrete
    • /
    • 제3권2_3호
    • /
    • pp.163-175
    • /
    • 2006
  • This research was conducted to determine effect of pumice aggregate ratio, cement dosage and slumps on freeze-thaw resistance, density, water absorption and elasticity of concrete. In the first batch, $300kg/m^3$ cement dosage were kept constant and pumice ratios were changed as 25%, 50%, 75% and 100% of replacement for normal aggregate by volume for $3{\pm}1cm$, $5{\pm}1cm$ and $7{\pm}1cm$ slumps. Other batches were prepared with $200kg/m^3$, $250kg/m^3$, $350kg/m^3$, $400kg/m^3$ and $500kg/m^3$ cement dosages and 25% pumice aggregate +75% normal aggregate at a constant slump. Test results showed that when pumice-aggregate ratio decreased the density and freeze-thaw resistance of concretes increased. With increasing of cement dosage in the mixtures, density of the concretes increased, however, freeze-thaw resistance of concretes decreased. Water absorption of the concrete decreased with increasing cement dosage but increased with the pumice ratio. Water absorption of the concrete also decreased after freeze-thaw cycles. Freeze-thaw resistance of concretes was decreased with increasing the slumps.

강섬유 특성에 따른 고강도 콘크리트의 압축 및 휨 거동 (Compressive and Flexural Behavior of High-Strength Concrete Incorporating Different Types of Hooked-End Steel Fibers)

  • 정우진;김애화;윤현도
    • 한국공간구조학회논문집
    • /
    • 제23권2호
    • /
    • pp.69-78
    • /
    • 2023
  • This paper investigates the effects of aspect ratio and volume fraction of hooked-end normal-strength steel fibers on the compressive and flexural properties of high-strength concrete with specified compressive strength of 60 MPa. Three types of hooked-end steel fibers with aspect ratios of 64, 67 and 80 were considered and three volume fractions of 0.25%, 0.50% and 0.75% for each steel fiber were respectively added into each high-strength concrete mixture. The test results indicated that the addition of normal-strength steel fibers is effective to improve compressive and flexural properties of high-strength concrete but fiber aspect ratio had little effect on the modulus of elasticity and compressive strength. As steel fiber content and aspect ratio increased, flexural beahvior of notched high-strength concrete beams was effectively improved.

왕겨재를 혼입(混入)한 콘크리트의 공학적(工學的) 특성(特性)에 관(關)한 실험적(實驗的) 연구(硏究) (An Experimental study on the Engineering Properties of Concrete with Rice-Husk Ash)

  • 성찬용;유병인;김경태;정현정;김영익
    • 농업과학연구
    • /
    • 제24권2호
    • /
    • pp.207-217
    • /
    • 1997
  • 본 연구는 보통 포틀랜드 시멘트와 천연골재 및 왕겨재를 혼입한 왕겨재 콘크리트의 공학적 특성을 실험적으로 구명한 것으로서, 연구를 통하여 얻어진 결과를 요약하면 다음과 같다. 1. 단위중량은 $2,216{\sim}2,325kgf/m^3$정도의 범위로서 보통 시멘트 콘크리트에 비해 1~6%정도 감소되었다. 2. 각 강도는 왕겨재를 결합재량의 10%를 혼입한 콘크리트에서 가장 크게 나타났으며, 보통 시멘트 콘크리트에 비해 압축강도는 8%, 인장 강도는 17%, 휨인장강도는 18% 증가되었다. 3. 초음파진통속도는 3,252~4,016 m/s 정도로서 보통 시멘트 콘크리트와 유사하게 나타났으며, 왕겨재를 10% 혼입한 콘크리트에서 가장 높은 값을 보였다. 4. 동탄성계수는 $242{\times}10^3{\sim}306{\times}10^3kgf/cm^2$정도로 보통 시멘트 콘크리트의 90~113%로써 보통 시멘트 콘크리트와 유사하게 나타났으며, 왕겨재를 10% 혼입한 콘크리트에서 가장 높게 나타났다. 5. 정탄성계수는 $185{\times}10^3{\sim}306{\times}10^3kgf/cm^2$정도로 보통 시멘트 콘크리트와 유사하게 나타났으며, 왕겨재를 10% 혼입한 콘크리트에서 가장 크고, 포아손수는 보통 시멘트 콘크리트보다 작게 나타났으며, 동탄성계수는 정탄성계수 보다 11~30%정도 크게 나타났다. 6. 내구성은 왕겨재의 혼입량이 많을수록 증가되었으며, 왕겨재를 10% 혼입한 콘크리트와 20% 혼입한 콘크리트의 내구성은 보통 시멘트 콘크리트보다 각각 1.3배와 1.6배 정도 크게 나타났다. 7. 적정량의 왕겨재를 혼입하여 콘크리트를 제조할 경우, 왕겨재 콘크리트의 물리 역학적 성질이 보통 시멘트 콘크리트보다 우수할 뿐만 아니라, 농업 부산물의 재활용으로 인한 경제적 측면에서도 많은 기여를 할 수 있을 것이다.

  • PDF